A study on the multiple stages of oxidation kinetics in a single crystal nickel-based superalloy
Source abstract
Abstract
Abstract Two stages of mass gain kinetics were observed in a single crystal nickel-based superalloy that corresponds to the growth of various layers. However, only one stage appeared in the intermediate layer, while the inner Al2O3 and outer NiO layers exhibited two stages. This abnormal kinetics behavior was attributed to the undermining effect of simple tetragonal structure Ta2O5 phases on the continuous hexagonal structure Al2O3. Furthermore, the Cr concentration gradient in the γ’-free zone transformed from depletion to enrichment with increase of exposure time, while Ni displayed a converse trend. This phenomenon further promoted the different growth kinetics of various layers.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · High Temperature Alloys and Creep · Catalytic Processes in Materials Science
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Reed · 2008
2. 1987
3. Oxidation of a NiCrAlYSi overlayer with or without a diffusion barrier deposited by one-step arc ion plating10.1016/j.corsci.2010.02.022 ↗
4. Isothermal oxidation behavior of a gradient NiCoCrAlSiY coating deposited by arc ion plating on a Ni-based single crystal superalloy10.1016/j.corsci.2009.03.036 ↗
5. Oxidation behavior characteristics of an aluminized Ni-based single crystal superalloy CM186LC between 900 °C and 1100 °C in air
6. Long-term oxidation behavior and mechanism of DD6 Ni-based single crystal superalloy at 1050 °C and 1100 °C in air10.1016/j.jallcom.2017.02.031 ↗
7. Microstructural evolution of oxidation film on a single crystal nickel-based superalloy at 980 °C10.1007/s11085-017-9787-4 ↗
8. Oxidation behavior of the nickel-based superalloy at 980 °C10.1007/s40195-017-0598-z ↗
9. Oxidation behavior of a single-crystal Ni-base superalloy between 900 and 1000 ◦C in air10.1016/j.jallcom.2009.10.261 ↗
10. Oxidation of single crystal PWA 1483 at 950 ◦C in flowing air10.1016/j.corsci.2008.06.033 ↗
11. Oxidation behavior of a single-crystal Ni-base superalloy in Air-I: At 800 and 900 °C in air10.1023/A:1023604214245 ↗
12. Oxidation behavior and mechanism of a Ni-based single crystal superalloy with single α-Al2O3 film at 1000 °C10.1016/j.apsusc.2017.03.116 ↗
13. Oxidation behavior of single crystal nickel-based superalloys: intermediate temperature effects at 450-550 °C10.1080/02670836.2018.1471436 ↗
14. The influence of CrTaO4 layer on the oxidation behavior of a directionally-solidified nickel-based superalloy at 850-900 °C10.1016/j.jallcom.2017.07.066 ↗
15. Influence of surface roughness on the behavior of a Ni-4.0Cr-5.7Al single crystal superalloy10.1016/j.apsusc.2018.01.226 ↗
16. Oxidation of nickel-based single-crystal superalloys for industrial gas turbine applications10.1016/j.actamat.2010.09.027 ↗
17. Effect of alloying elements and microstructure on the cyclic oxidation performance of three nickel-based superalloys
18. Oxidation behavior of a single-crystal Ni-base superalloy in Air-II: At 1000, 1100 and 1150 °C in air10.1023/A:1024629716452 ↗
19. Influence of Ta content on hot corrosion behavior of a directionally solidified nickel-base superalloy10.1016/j.jallcom.2014.08.259 ↗
20. Effect of Ti and Ta on the oxidation of a complex superalloy10.1007/BF00603531 ↗
21. Oxidation behavior of a single-crystal Ni-base superalloy in air at 900, 1000 and 1100 °C10.1007/s11085-006-9016-z ↗
22. Experimental observations in support of the dynamic-segregation theory to explain the reactive-element effect10.1007/BF01046818 ↗
23. Influence of humidity on high-temperature oxidation of Inconel 600 alloy: oxide layers and residual stress study10.1016/j.apsusc.2013.07.117 ↗
24. High temperature oxidation resistance of Ni-(5∼13)Co-(10∼16)Cr-(5∼9)W-5Al-(1∼1.5)Ti-(3∼6)Ta alloys10.1007/s12540-016-6305-1 ↗
25. Role of volatilization of molybdenum oxides during the cyclic oxidation of high-Mo containing Ni-based single crystal superalloys10.1016/j.corsci.2017.08.025 ↗
26. The effect of surface machining on the high temperature oxidation of a single crystal Ni-based superalloy10.2320/matertrans.M2014077 ↗
27. Comparison of chromia growth kinetics in a Ni-based superalloy, with and without shot-peening10.1016/j.corsci.2015.07.033 ↗
28. Isothermal oxidation behavior of Ni-Al-Co-Cr-Mo-Ti alloy at 850 °C and 950 °C10.1016/j.proeng.2011.12.540 ↗
29. The effect of alloyed nickel on the short-term high temperature oxidation behavior of Co-Re-Cr-based alloys10.1016/j.corsci.2015.01.004 ↗
30. The oxidation characteristics of the nickel-based superalloy, RR1000, at temperatures of 700∼900 °C10.3184/096034012X13341417107382 ↗
31. Oxidation behavior and microstructure degeneration of cast Ni-based superalloy M951 at 900 °C10.1016/j.apsusc.2019.02.150 ↗
32. Birks · 2006
33. Wood · 1983
34. In situ oxidation analysis on Co-Al-W-Ti-Ta single-crystal alloy in an environmental TEM10.1016/j.corsci.2020.108725 ↗
35. Oxidation behavior of a single-crystal Ni-based superalloy over the temperature range of 850-950 °C in air10.1016/j.apsusc.2019.04.089 ↗
36. Al effect in transport properties of nickel oxide and its relevance to the oxidation of nickel10.1016/j.mseb.2011.05.035 ↗
37. Self-diffusion in α-Al2O3 I. Aluminium diffusion in single crystals10.1080/01418619408242929 ↗