Correlation between the microstructure and corrosion behaviour of copper/316 L stainless-steel dissimilar-metal welded joints
Source abstract
Abstract
Abstract In this study, the correlation between the microstructure and corrosion behaviour of copper/316 L stainless-steel dissimilar-metal welded joints on an electrolytic copper cathode plate was experimentally investigated. Clear phase separation was noted in the weld metal with the γ- and e-Cu phase dominating the Fe-rich and Cu-rich zones, respectively. The difference in the corrosion resistance of these zones means that multiple galvanic corrosion couples are formed in different joint areas. Strong galvanic corrosion between the γ and e-Cu phases caused the shedding of the γ phase particles from the surface, thereby producing corrosion pits and eventually leading to joint failure.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · Concrete Corrosion and Durability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (63)
Show source-provided references
1. Continuous electrolytic refining process of cathode copper with non-dissolving anode10.1016/j.mineng.2019.02.032 ↗
2. Electrolytic production of copper from chalcopyrite10.1016/j.coelec.2020.04.011 ↗
3. Production of copper cathode from oxidized copper ores by acidic leaching and two-step precipitation followed by electrowinning10.1016/j.hydromet.2012.12.004 ↗
4. The effect of additives on anode passivation in electrorefining of copper10.1016/j.cep.2006.10.005 ↗
5. Design of optimal electrolyte circulation based on the kinetic modelling of copper dissolution in silver electrorefining10.1016/j.hydromet.2020.105403 ↗
6. Effect of jet flow between electrodes on power consumption and the apparent density of electrolytic copper powders10.1016/j.powtec.2018.11.078 ↗
7. Effect of pulse parameter on pulsed electrodeposition of copper on stainless steel10.1179/026708408X344680 ↗
8. James · 1983
9. James · 1980
10. Microstructures and mechanical properties of laser-arc hybrid welded dissimilar pure copper to stainless steel10.1016/j.optlastec.2018.09.050 ↗
11. Study on welding such dissimilar materials as AISI 304 stainless steel and DHP copper in a sea-water environment. Influence of weld metals on corrosion10.1016/0924-0136(95)02073-X ↗
12. Experimental investigation of temperature field and fusion zone microstructure in dissimilar pulsed laser welding of austenitic stainless steel and copper10.1016/j.jmapro.2020.03.037 ↗
13. Macrosegregation in dissimilar-metal fusion welding10.1016/j.actamat.2016.03.004 ↗
14. Effects of tensile strength on friction welding condition and weld faying surface properties of friction welded joints between pure copper and austenitic stainless steel
15. Gas tungsten arc welding of copper to stainless steel for ultra-high vacuum applications10.1016/j.jmatprotec.2019.116490 ↗
16. Influence of processing parameters on the characteristics of stainless steel/copper laser welding10.1016/j.jmatprotec.2015.03.003 ↗
17. MIG-TIG double-sided arc welding of copper-stainless steel using different filler metals10.1016/j.jmapro.2020.04.013 ↗
18. Corrosion behavior of immersion silver printed circuit board copper under a thin electrolyte layer10.1016/j.engfailanal.2020.104807 ↗
19. Correlation of microstructure and stress corrosion cracking initiation behaviour of the fusion boundary region in a SA508 Cl. 3-Alloy 52M dissimilar weld joint in primary pressurized water reactor environment10.1016/j.corsci.2017.12.011 ↗
20. Stress corrosion cracking of fusion boundary for 316L/52M dissimilar metal weld joints in borated and lithiated high temperature water10.1016/j.corsci.2017.01.024 ↗
21. Local electrochemical properties of fusion boundary region in SA508-309L/308L overlay welded joint10.1016/j.corsci.2019.04.021 ↗
22. Liquid separation effects in Fe−Cu alloys solidified under different cooling rates10.1007/BF02654269 ↗
23. Effect of grain size on the electrical conductivity of copper–iron alloys10.1016/j.jallcom.2017.05.244 ↗
24. Composites of copper and cast iron fabricated via the liquid: in the vicinity of the limits of strength in a non-deformed condition10.1016/j.matchar.2017.06.025 ↗
25. Corrosion behavior of an equiatomic CoCrFeMnNi high-entropy alloy compared with 304 stainless steel in sulfuric acid solution10.1016/j.corsci.2018.02.031 ↗
26. Passivity in metals and alloys10.1016/S0010-938X(79)80104-3 ↗
27. The nucleation and growth of corrosion pits on stainless steel10.1016/0010-938X(93)90133-2 ↗
28. Atomistic details of oxide surfaces and surface oxidation: the example of copper and its oxides10.1016/j.surfrep.2015.07.001 ↗
29. In-situ optical view onto copper oxidation–role of reactive interfaces and self-heating10.1016/j.corsci.2019.108112 ↗
30. Copper alloying content effect on pitting resistance of modified 00Cr20Ni18Mo6CuN super austenitic stainless steels10.1016/j.corsci.2020.108791 ↗
31. Galvanic corrosion behavior of copper–drawn steel for grounding grids in the acidic red soil simulated solution10.1007/s40195-020-01071-7 ↗
32. Reduction of austenite-ferrite galvanic activity in the heat-affected zone of a Gleeble-simulated grade 2205 duplex stainless steel weld10.1016/j.corsci.2019.108198 ↗
33. Influence of the secondary phase on micro galvanic corrosion of low carbon bainitic steel in NaCl solution10.1016/j.matchar.2018.03.021 ↗
34. Macro-galvanic effect and its influence on corrosion behaviors of friction stir welding joint of 7050-T76 Al alloy10.1016/j.corsci.2019.108360 ↗
35. Relationship between the microstructure and local corrosion properties of weld metal in austenitic stainless steels10.1016/j.corsci.2020.108867 ↗
36. ASTM G1-03 · 2011
37. Localized corrosion behavior of non-Equiatomic NiFeCrMnCo multi-principal element Alloys10.1016/j.electacta.2020.136749 ↗
38. Comprehending the role of individual microstructural features on electrochemical response and passive film behaviour in type 304 austenitic stainless steel10.1016/j.corsci.2020.109187 ↗
39. Effect of overload on the oxidation behavior of CF8A austenitic stainless steel in a high-temperature water environment10.1016/j.corsci.2019.108219 ↗
40. Microstructural evolution and oxidation behaviour of CF8A austenitic stainless steel during corrosion fatigue in a simulated pressurised water reactor environment10.1016/j.corsci.2019.108286 ↗
41. Eelectrochemical properties and corrosion resistance of carbon-ion-implanted magnesium10.1016/j.corsci.2014.01.015 ↗
42. Improvement on corrosion resistance and biocompability of ZK60 magnesium alloy by carboxyl ion implantation10.1016/j.corsci.2020.108729 ↗
43. Long-term anticorrosion behaviour of polyaniline on mild Steel10.1016/j.corsci.2006.11.007 ↗
44. Anticorrosive behavior of hydroxyapatite as an environmentally friendly pigment10.1016/S0010-938X(01)00118-4 ↗
45. Electrochemical test methods for evaluating organic coatings on metals: an update. Part III: multiple test parameter measurements110.1016/S0300-9440(97)00099-4 ↗
46. The effect of fluoride ions on the corrosion behavior of pure titanium in 0.05M sulfuric acid10.1016/j.electacta.2014.05.055 ↗
47. Corrosion behavior of as-cast Mg–5Sn based alloys with in additions in 3.5 wt% NaCl solution10.1016/j.corsci.2019.108318 ↗
48. Synergistic effects of fluoride and chloride on general corrosion behavior of AISI 316 stainless steel and pure titanium in H2SO4 solutions10.1016/j.corsci.2017.10.028 ↗
49. Thermal stability of the passive film formed on 316L stainless steel surface studied by ToF-SIMS10.1016/j.corsci.2019.108395 ↗
50. Determination of effective capacitance and film thickness from constant-phase-element parameters10.1016/j.electacta.2009.10.065 ↗
51. Characterization of zirconium oxides part II: new insights on the growth of zirconia revealed through complementary high-resolution mapping techniques10.1016/j.corsci.2020.108491 ↗
52. Establishing a correlation between interfacial microstructures and corrosion initiation sites in Al/Cu joints by SEM–EDS and AFM–SKPFM10.1016/j.corsci.2013.10.039 ↗
53. SKPFM measured Volta potential correlated with strain localisation in microstructure to understand corrosion susceptibility of cold-rolled grade 2205 duplex stainless steel10.1016/j.corsci.2015.06.035 ↗
54. Understanding crystallographic orientation dependent dissolution rates of 90Cu-10Ni alloy: New insights based on AFM/SKPFM measurements and coordination number/electronic structure calculations10.1016/j.corsci.2019.108320 ↗
55. Correlation of surface Volta potential with galvanic corrosion initiation sites in solid-state welded Ti-Cu bimetal using AFM-SKPFM10.1016/j.corsci.2018.06.026 ↗
56. The role of constituent phases on corrosion initiation of NiAl bronze in acidic media studied by SEM–EDS, AFM and SKPFM10.1016/j.corsci.2013.11.017 ↗
57. Contribution of the flowing conditions to the galvanic corrosion of the copper/AISI 316L coupling in highly concentrated LiBr solutions10.1016/j.corsci.2012.10.039 ↗
58. Galvanic series of different stainless steels and copper- and aluminium-based materials in acid solutions10.1016/j.corsci.2012.10.032 ↗
59. Imposed potential measurements to evaluate the pitting corrosion resistance and the galvanic behaviour of a highly alloyed austenitic stainless steel and its weldment in a LiBr solution at temperatures up to 150 °C10.1016/j.corsci.2010.11.013 ↗
60. The effect of temperature on the galvanic corrosion of the copper/AISI 304 pair in LiBr solutions under hydrodynamic conditions10.1016/j.corsci.2009.10.032 ↗
61. The influence of Reynolds number on the galvanic corrosion of the copper/AISI 304 pair in aqueous LiBr solutions10.1016/j.corsci.2009.07.003 ↗
62. Variations of galvanic currents and corrosion forms of 2024/Q235/304 tri-metallic couple with multivariable cathode/anode area ratios: experiments and modeling10.1016/j.electacta.2020.136947 ↗
63. Microstructural evolution and corrosion behaviour of thermally aged dissimilar metal welds of low-alloy steel and nickel-based alloy10.1016/j.corsci.2019.03.032 ↗