Abstract

Abstract The effect of long-time thermal aging on corrosion behavior of type 316H stainless steel in molten chloride salt was studied. The results showed the long-time aging at 700 °C promoted the precipitation of both M23C6 carbide (dominant) and η phase at the grain boundaries and within the grains. Post-corrosion characterization showed the thermally-aged 316H experienced ~23% less weight loss than the as-received 316H and the Cr depleted region in the thermally-aged 316H was also much thinner than the as-received one. The mechanisms responsible for the different corrosion behaviors of the specimens were discussed based on the experimental observation.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · High Temperature Alloys and Creep · Microstructure and Mechanical Properties of Steels

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (40)

Show source-provided references
1. Progress in research and development of molten chloride salt technology for next generation concentrated solar power plants10.1016/j.eng.2020.06.027 ↗
2. A comprehensive review on Dish/Stirling concentrated solar power systems: design, optical and geometrical analyses, thermal performance assessment and applications
3. M. Jonemann, Advanced thermal storage system with novel molten salt, National Renewable Energy Laboratory. NREL/SR-5200-58595.
4. Basic properties of eutectic chloride salts NaCl-KCl-ZnCl2 and NaCl-KCl-MgCl2 as HTFs and thermal storage media measured using simultaneous DSG-TGA10.1016/j.solener.2018.01.067 ↗
5. Materials compatibility for the next generation of concentrated solar power plants10.1016/j.ensm.2018.02.023 ↗
6. Thermal energy storage using chloride salts and their eutectics10.1016/j.applthermaleng.2016.07.046 ↗
7. Corrosion of alloys in a chloride molten salt (NaCl-LiCl) for solar thermal technologies10.1016/j.solmat.2016.05.052 ↗
8. Mehos · 2017 · 5500
9. M. Mehos, C. Turchi, J..Vidal, M..Wagner, Z..Ma, C..Ho, W..Kolb, C..Andraka, A..Kruizenga, Concentrating solar power Gen3 demonstration roadmap, National Renewable Energy Laboratory. NREL/TP-5500-67464.
10. Materials compatibility for the next generation of concentrated solar power plants10.1016/j.ensm.2018.02.023 ↗
11. Corrosion behavior of 316H and Ni-based alloys in a ternary NaCl-KClMgCl2 molten salt10.1016/j.solener.2018.06.094 ↗
12. Excellent corrosion resistance of 316 stainless steel in purified NaCl-MgCl2 eutectic salt at high temperature10.1016/j.corsci.2020.108473 ↗
13. Effects of alloying elements on the corrosion behavior of Ni-based alloys in molten NaCl-KCl-MgCl2 salt at different temperatures10.1016/j.corsci.2018.08.021 ↗
14. Corrosion behaviour of 316H stainless steel in molten FLiNaK eutectic salt containing graphite particles10.1016/j.corsci.2019.108174 ↗
15. Corrosion behaviors of 316 stainless steel and Inconel 625 alloy in chloride molten salts for solar energy storage10.1515/htmp-2020-0077 ↗
16. Numerical simulation of grain boundary carbides evolution in 316H stainless steel10.1016/j.jnucmat.2018.05.074 ↗
17. Kinetics of transformation of delta ferrite during creep in a type 316(N) stainless steel weld metal10.1016/S0921-5093(03)00371-X ↗
18. Nanoscale co-precipitation and mechanical properties of a high-strength low-carbon steel10.1016/j.actamat.2010.11.054 ↗
19. Pre-cipitation in AISI 316L(N) during creep tests at 550 and 600C up to 10 years10.1016/j.jnucmat.2006.12.027 ↗
20. Microstructure evolution and mechanical properties of 316H weld metal during aging10.1080/02670836.2020.1743597 ↗
21. Metallographic observations on the formation and occurrence of ferrite, sigma phase, and carbides in austenitic stainless steels10.1016/0026-0800(70)90004-2 ↗
22. Correlation between microstructure and intergranular corrosion behavior of low delta-ferrite content AISI 316L aged in the range 550–700°C10.1016/j.jallcom.2017.02.273 ↗
23. Effects of ageing conditions on the precipitates evolution, chromium depletion and intergranular corrosion susceptibility of AISI 316L: experimental and modeling results10.1016/j.msea.2003.12.017 ↗
24. Variation of mechanical characteristics evolution in AISI 316 austenitic stainless steel subjected to long-term thermal aging at elevated temperature10.1007/s11223-017-9835-y ↗
25. Intergranular stress corrosion cracking in simulated BWR water of 316L stainless steels manufactured with different procedures10.1016/j.corsci.2021.109344 ↗
26. Effects of dissolved hydrogen and surface condition on the intergranular stress corrosion cracking initiation and short crack growth behavior of non-sensitized 316 stainless steel in simulated PWR primary water10.1016/j.corsci.2017.02.003 ↗
27. Accelerated test for evaluation of intergranular stress corrosion cracking initiation characteristics of non-sensitized 316 austenitic stainless steel in simulated pressure water reactor environment10.1016/j.corsci.2016.11.019 ↗
28. The strain for stress-corrosion crack initiation in type-316 stainless-steel in high-temperature water10.1016/0010-938X(92)90107-E ↗
29. The microstructure evolution and its effect on corrosion properties of 18Cr-12Ni-2,5Mo steel annealed at 500–900°C
30. Transformation of austenite during isothermal annealing at 600–900°C for heat-resistant stainless steel10.1016/j.jallcom.2013.03.102 ↗
31. Phase instabilities during high temperature exposure of 316 Austenitic stainless steel10.1007/BF02647659 ↗
32. Bowen · Metall. Trans. · 1970 · 1 · 169510.1007/BF02642019 ↗
33. First-principles molecular dynamics modeling of the molten fluoride salt with Cr solute10.1016/j.jnucmat.2014.03.014 ↗
34. Synergistic effects of impurities and sensitisation on inter granular corrosion and stress corrosion cracking in type 316H austenitic stainless steel10.1179/bcj.1996.31.2.133 ↗
35. Oxidation of stainless steel 316L-Oxide grains with pronounced inhomogeneous composition10.1016/j.corsci.2018.12.035 ↗
36. Effect of machining on oxide development in type 316L stainless steel in high-temperature hydrogenated water10.1016/j.corsci.2021.109444 ↗
37. The effect of martensite on stress corrosion crack initiation of austenitic stainless steels in high-temperature hydrogenated water10.1016/j.corsci.2021.109600 ↗
38. Effect of partial replacement of carbon by nitrogen on intergranular corrosion behavior of high nitrogen martensitic stainless steels10.1016/j.jmst.2019.06.004 ↗
39. The oxidation behaviour 304 stainless steel in oxygenated high temperature water10.1016/j.corsci.2010.09.001 ↗
40. Chromium depletion and void formation in Fe-Ni-Cr alloys during molten salt corrosion and related processes