Abstract

Pitting behavior of 321 stainless steel (SS) in sodium chloride solution was studied by potentiostatic pulse technique triggering pits. Pure TiN inclusion and complex inclusion with core-shell structure are found in 321 SS. The former has no effect on pitting performance, while CaS in the latter is the exact inducer of pitting. Mechanism of pitting initiation and propagation induced by complex inclusions was proposed. When CaS content differs little, inhibition effect of TiN shell on pitting propagation is the main reason why a complex inclusion with higher TiN content is more resistant to pitting.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Microstructure and Mechanical Properties of Steels · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (50)

Show source-provided references
1. Coupling effect of microstructure and hydrogen absorbed during service on pitting corrosion of 321 austenitic stainless steel weld joints10.1016/j.corsci.2019.108339 ↗
2. Temperature change induce crack mode transition of 316L stainless steel in H2S environment revealed by dislocation configurations10.1016/j.corsci.2021.109896 ↗
3. The effect of martensite on stress corrosion crack initiation of austenitic stainless steels in high-temperature hydrogenated water10.1016/j.corsci.2021.109600 ↗
4. Direct drive friction welding effect on mechanical and electrochemical characteristics of titanium stabilized austenitic stainless steel (AISI 321) research reactor thick tube10.1016/j.jmapro.2019.03.016 ↗
5. Investigation on the multi-pass gas tungsten arc welded Bi-metallic combination between nickel-based superalloy and Ti-stabilized austenitic stainless steel10.1557/jmr.2017.235 ↗
6. The effect of TiN inclusions and deformation-induced martensite on the corrosion properties of AISI 321 stainless steel10.1016/j.engfailanal.2013.06.021 ↗
7. Theoretical and experimental investigation into laser surface melting of 321 austenitic stainless steel
8. Application limits of stainless steels in the petroleum industry10.1002/maco.200303781 ↗
9. In vitrocorrosion studies of stainless-steel dental substrates duringPorphyromonas gingivalisbiofilm growth in artificial saliva solutions: providing insights into the role of resident oral bacterium10.1039/D0RA05500J ↗
10. Influence of Ti, C and N concentration on the intergranular corrosion behaviour of AISI 316Ti and 321 stainless steels10.1016/j.actamat.2006.11.021 ↗
11. Effect of prior plastic deformation and deformation rate on the corrosion resistance of AISI 321 austenitic stainless steel10.1016/j.msea.2018.12.093 ↗
12. Influence of the heterogeneity of AISI-321 steel on its pitting in chloride-containing media10.1007/s11003-007-0029-9 ↗
13. Effect of calcium content on inclusions during the ladle furnace refining process of AISI 321 stainless steel10.1007/s12613-020-1981-8 ↗
14. Corrosion behavior of metastable AISI 321 austenitic stainless steel: investigating the effect of grain size and prior plastic deformation on its degradation pattern in saline media10.1038/s41598-019-48594-3 ↗
15. Revisiting the effect of molybdenum on pitting resistance of stainless steels10.1007/s42864-021-00099-1 ↗
16. Understanding the pitting mechanism of super ferritic stainless steel in bromide solutions: the role of Ti/Nb–Mo precipitates with a core–shell structure10.1016/j.corsci.2022.110176 ↗
17. Improved corrosion performance of selective laser melted stainless steel 316L in the deep-sea environment10.1016/j.corcom.2021.09.002 ↗
18. The role of hydrogen in the corrosion and cracking of steels – a review10.1016/j.corcom.2021.10.005 ↗
19. 2001 W.R. Whitney award lecture: understanding the corrosion of stainless steel10.5006/1.3281676 ↗
20. Insight into TiN inclusion induced pit corrosion of interstitial free steel exposed to aerated NaCl solution10.1016/j.jmrt.2021.04.046 ↗
21. Initial microzonal corrosion mechanism of inclusions associated with the precipitated (Ti, Nb)N phase of Sb-containing weathering steel
22. Initiation mechanism of pitting corrosion in weld heat affected zone of duplex stainless steel10.1016/j.corsci.2022.110278 ↗
23. Effects of non-metallic inclusions on the initiation of pitting corrosion in 11 % Cr ferritic stainless steel examined by micro-droplet cell10.1016/j.corsci.2006.08.017 ↗
24. New insights into the mechanism of localised corrosion induced by TiN-containing inclusions in high strength low alloy steel10.1016/j.jmst.2021.12.075 ↗
25. Failure analysis on abnormal leakage of TP321 stainless steel pipe in hydrogen-eliminated system of nuclear power plant10.1016/j.engfailanal.2018.02.021 ↗
26. Determination of conditions leading to localized corrosion initiation on UNS-S32100 (AISI-321) stainless-steels in nuclear-power-plant environments10.1016/0029-5493(95)00989-P ↗
27. Influence of the microstructure on the corrosion behaviour of low-carbon martensitic stainless steel after tempering treatment10.1016/j.corsci.2014.03.036 ↗
28. Determination of pitting initiation of duplex stainless steel using potentiostatic pulse technique10.1016/j.electacta.2010.02.035 ↗
29. Use of the potentiostatic pulse technique to study and influence pitting behavior of 317L stainless steel10.1149/1945-7111/ab7983 ↗
30. The combined effect of chemical and structural factors on pitting corrosion induced by MnS-(Cr, Mn, Al)O duplex inclusions10.5006/2581 ↗
31. Statistical analysis of the pitting corrosion induced by potentiostatic pulse tests of wrought and SLM 316L stainless steels10.1016/j.corsci.2021.110036 ↗
32. Application of potentiostatic pulse technique and statistical analysis in evaluating pitting resistance of aged 317L stainless steel10.1002/maco.201810622 ↗
33. Influence of potentionstatic pulse technique on pitting behavior and pitting resistance of 317L stainless steel
34. On the Volta potential measured by SKPFM – fundamental and practical aspects with relevance to corrosion science10.1080/1478422X.2019.1583436 ↗
35. Towards a better understanding of localised corrosion induced by typical non-metallic inclusions in low-alloy steels10.1016/j.corsci.2020.109150 ↗
36. Influence of inclusions on initiation of pitting corrosion and stress corrosion cracking of X70 steel in near-neutral pH environment10.1016/j.corsci.2018.11.007 ↗
37. Dissolution kinetics of the sulfide-oxide complex inclusion and resulting localized corrosion mechanism of X70 steel in deaerated acidic environment10.1016/j.corsci.2020.108815 ↗
38. Role of inclusions in the pitting initiation of pipeline steel and the effect of electron irradiation in SEM10.1016/j.corsci.2017.10.029 ↗
39. Passivity of (Mn,Cr)S inclusions in type 304 stainless steel: the role of Cr and the critical concentration for preventing inclusion dissolution in NaCl solution10.1016/j.corsci.2020.109060 ↗
40. Role of Al2O3 inclusions on the localized corrosion of Q460NH weathering steel in marine environment10.1016/j.corsci.2018.04.007 ↗
41. Mechanism of (Mg,Al,Ca)-oxide inclusion-induced pitting corrosion in 316L stainless steel exposed to sulphur environments containing chloride ion10.1016/j.corsci.2012.09.044 ↗
42. Investigation into the influence of laser melting on the sulphide inclusions in AISI 416 stainless steel10.1016/j.corsci.2011.07.042 ↗
43. Operando electrochemical TEM, ex-situ SEM and atomistic modeling studies of MnS dissolution and its role in triggering pitting corrosion in 304L stainless steel10.1016/j.corsci.2022.110184 ↗
44. Influence of the structure defining factors on the corrosion-electrochemical behavior of iron and stainless steel10.1134/S1070363209090266 ↗
45. Cerium addition to CaS inclusions in stainless steel: insolubilizing water-soluble inclusions and improving pitting corrosion resistance10.1016/j.corsci.2020.109222 ↗
46. The role of titanium in pitting corrosion of commercial stainless-steels
47. Effect of complex inclusions on pit initiation in 18-percent chromium-8-percent nickel stainless-steel type-303, type-304, and type-32110.5006/1.3293599 ↗
48. Microelectrochemical measurements of the dissolution of single MnS inclusions, and the prediction of the critical conditions for pit initiation on stainless steel10.1149/1.1360205 ↗
49. Initiation of corrosion pits at inclusions on 304 stainless steel10.1149/1.2048462 ↗
50. Localized corrosion: passive film breakdown vs. pit growth stability: Part III. A unifying set of principal parameters and criteria for pit stabilization and salt film formation10.1149/2.0251811jes ↗