Corrosion of SS310 and Alloy 740 in high temperature supercritical CO2 with impurities H2O and O2
Source abstract
Abstract
Abstract This study investigated corrosion performance of SS310 and Alloy 740 in supercritical CO2 with the impurity of 100 ppm H2O or O2 at 600 °C and 30 MPa for up to 1000 h. The addition of 100 ppm H2O remarkably enhanced general and localized oxidations while the presence of O2 led to the opposite tendency. Alloy 740 exhibited better resistance to carburization compared to SS310, possibly due to the higher solubility of carbides in Ni-based alloys than those in Fe-based alloys. Both alloys exhibit near parabolic oxidation behavior and acceptable corrosion resistance in the supercritical CO2 environments.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (68)
Show source-provided references
1. Compatibility of candidate structural materials in high-temperature S-CO2 environment
2. Corrosion of alloy haynes 230 in high temperature supercritical carbon dioxide with oxygen impurity additions10.1007/s11085-016-9654-8 ↗
3. Angelino · 1968
4. The supercritical thermodynamic power cycle10.1016/0013-7480(68)90105-8 ↗
5. Thermal desalination via supercritical CO2 Brayton cycle: optimal system design and techno-economic analysis without reduction in cycle efficiency10.1016/j.applthermaleng.2019.02.039 ↗
6. Development of a 1 MWe supercritical CO2brayton cycle test loop
7. Testing of a 10 MWe supercritical CO2 turbine
8. Sridharan · 2017
9. Overview on corrosion in supercritical fluids10.1016/j.supflu.2016.07.022 ↗
10. Effect of pressure and impurities on oxidation in supercritical CO210.1002/maco.201810652 ↗
11. Corrosion Behavior Of Different Metallic Materials In Supercritical CO2 at 550°C and 250 bars
12. Corrosion of 9Cr steel in CO2 at intermediate temperature I: mechanism of void-induced duplex oxide formation10.1007/s11085-011-9271-5 ↗
13. Corrosion of austenitic and ferritic-martensitic steels exposed to supercritical carbon dioxide10.1016/j.corsci.2011.06.002 ↗
14. Chapter 4 - High-temperature materials
15. Corrosion of materials in supercritical carbon dioxide environments
16. Corrosion of austenitic alloys in high temperature supercritical carbon dioxide10.1016/j.corsci.2012.03.029 ↗
17. Characterization of chromia scales formed in supercritical carbon dioxide10.1080/09603409.2017.1389371 ↗
18. Materials considerations for supercritical CO2 turbine cycles
19. Corrosion and carburization behavior of chromia-forming heat resistant alloys in a high-temperature supercritical-carbon dioxide environment10.1016/j.corsci.2015.07.007 ↗
20. Resistance of high-nickel, heat-resisting alloys to air and to supercritical CO2 at high temperatures10.1007/s11085-017-9820-7 ↗
21. The effect of CO2 pressure on chromia scale microstructure at 750 °C10.1007/s11837-018-2963-4 ↗
22. Effect of CO2 gas pressure on composition, growth rate, and structure of duplex oxide formed on 9Cr steel at 550 °C10.1016/j.corsci.2019.108252 ↗
23. Corrosion performance of heat-resisting steels and alloys in supercritical carbon dioxide at 650 °C and 15 MPa10.1016/j.energy.2019.03.014 ↗
24. Oxidation and carburization of alloys exposed to impure supercritical CO2
25. Materials corrosion in high temperature supercritical carbon dioxide
26. Effects of CO and O2 impurities on supercritical CO2 corrosion of alloy 62510.1007/s11661-018-4727-8 ↗
27. Corrosion of heat exchanger alloys in open-fired sCO2 power cycles
28. Pint · 2019
29. Effect of pressure on supercritical CO2 compatibility of structural alloys at 750 °C10.1002/maco.201508783 ↗
30. Modelling of the degradation of martensitic stainless steels by the Boudouard reaction10.1016/j.corsci.2020.108699 ↗
31. Quadakkers · 2011 · 194
32. Effect of cobalt content on the oxidation and corrosion behavior of Ni–Fe-Based superalloy for ultra-supercritical boiler applications10.1007/s11085-017-9783-8 ↗
33. ASTM, G1-03 · 2003
34. Understanding the pitting corrosion mechanism of pipeline steel in an impure supercritical CO2 environment10.1016/j.supflu.2018.04.009 ↗
35. Effect of pressure on the corrosion and carburization behavior of chromia-forming heat-resistant alloys in high-temperature carbon dioxide environments10.1016/j.corsci.2016.06.004 ↗
36. Roine · 2006 · 448
37. The effect of water vapor on passive-layer stability and corrosion behavior of Fe–Al–Cr base alloys10.1023/B:OXID.0000016277.86061.25 ↗
38. Oxidation behavior of Fe-20Cr-25Ni-Nb austenitic stainless steel in high-temperature environment with small amount of water vapor10.1016/j.corsci.2018.09.016 ↗
39. Young · 2008
40. The oxidation behavior of the new nickel-based superalloy Inconel 740 with and without Na2SO4 deposit10.1016/j.surfcoat.2003.12.003 ↗
41. The mechanism of breakthrough of protective chromium oxide scales on Fe-Cr alloys10.1016/S0010-938X(67)80003-9 ↗
42. 1.17 - oxidation in steam and steam/Hydrogen environments
43. Birks · 2006
44. Oxidation of ferritic and ferritic–martensitic steels in flowing and static supercritical water10.1016/j.corsci.2015.10.017 ↗
45. Corrosion behaviors of four stainless steels with similar chromium content in supercritical carbon dioxide environment at 650 °C10.1016/j.corsci.2019.04.043 ↗
46. Internal oxidation and carburisation of heat-resistant alloys10.1016/S0010-938X(02)00182-8 ↗
47. Water vapor effects on corrosion of Fe–Cr and Fe–Cr–Ni alloys containing silicon in CO2 gas at 818 °C10.1007/s11085-015-9536-5 ↗
48. Corrosion and carburization behaviour of Ni-xCr binary alloys in a high-temperature supercritical-carbon dioxide environment10.1007/s11085-017-9811-8 ↗
49. Penetration of protective chromia scales by carbon10.1016/j.scriptamat.2014.01.009 ↗
50. Effect of pressures on the corrosion behaviours of materials at 625°C10.1007/s11837-016-2201-x ↗
51. Corrosion and stress corrosion cracking of UNS S31008 and UNS N08810 alloys in supercritical water
52. TEM examination of precipitation behaviour of M23C6 and sigma phases and dislocations in SS 310S under creep deformation at 800 °C10.1017/S1431927615003724 ↗
53. Precipitation in creep resistant austenitic stainless steels10.1179/026708301101508972 ↗
54. Atomic origins of water-vapour-promoted alloy oxidation10.1038/s41563-018-0078-5 ↗
55. High-temperature corrosion of Cr2O3-forming alloys in CO-CO2-N2 atmospheres10.1007/BF01052021 ↗
56. The oxidation behaviour of metals and alloys at high temperatures in atmospheres containing water vapour: a review10.1016/j.pmatsci.2007.11.001 ↗
57. Corrosion of 9-12Cr ferritic–martensitic steels in high-temperature CO210.1016/j.corsci.2016.01.009 ↗
58. Corrosion behavior of steels and nickel alloys in superheated steam10.5006/0010-9312-22.5.147 ↗
59. Mechanistic insights into the oxidation behavior of Ni alloys in high-temperature CO210.1016/j.corsci.2017.06.005 ↗
60. Microstructures of chromia scales grown in CO210.1179/0960340914Z.00000000056 ↗
61. Sub-scale depletion and enrichment processes during high temperature oxidation of the nickel base alloy 625 in the temperature range 900–1000 °C10.1007/s11085-010-9225-3 ↗
62. Modelling compositional changes in nickel base alloy 602 CA during high temperature oxidation10.1179/0960340914Z.00000000082 ↗
63. Effects of alloyed aluminum and titanium on the oxidation behavior of INCONEL 740 superalloy10.1016/j.jallcom.2015.10.198 ↗
64. Structural evolution of a Ni alloy surface during high-temperature oxidation10.1007/s11085-017-9821-6 ↗
65. Lai · 2007
66. Davis · 2000
67. Alloys SS316 and Hastelloy-C276 in supercritical CO2 at high temperature10.1007/s11085-015-9589-5 ↗
68. Effect of dissolved oxygen content on the oxide structure of Alloy 625 in supercritical water environments at 700 °C10.1016/j.corsci.2013.11.034 ↗