Effect of fluoride ion concentration and fluctuating conditions on titanium bipolar plate in PEM water electrolyser environment
Source abstract
Abstract
In this work, we investigated the corrosion behavior and passive film of commercial pure titanium (TA1) bipolar plates in a simulated proton exchange membrane (PEM) water electrolyser anode environment under different concentrations of fluoride ions and fluctuation conditions. Our findings indicate that the denseness and protective ability of the passive film are weakened by fluoride ions, leading to severe corrosion damage of TA1. The dynamic potential loading altered the anodic reaction process of potentiodynamic polarization, resulting in a reduced corrosion current density. However, the stability of the passive film was still affected, and the Ti-oxides in the passive films decreased.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Battery Materials · Fuel Cells and Related Materials · Hydrogen Storage and Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (88)
Show source-provided references
1. Porous transport layers for proton exchange membrane electrolysis under extreme conditions of current density, temperature, and pressure
2. Designing the next generation of proton-exchange membrane fuel cells10.1038/s41586-021-03482-7 ↗
3. Energy and fuels from electrochemical interfaces10.1038/nmat4738 ↗
4. Critical review—identifying critical gaps for polymer electrolyte water electrolysis development10.1149/2.1441704jes ↗
5. Analysis and assessment of a hydrogen production plant consisting of coal gasification, thermochemical water decomposition and hydrogen compression systems10.1016/j.enconman.2017.11.047 ↗
6. Photovoltaic solar energy conversion for hydrogen production by alkaline water electrolysis: conceptual design and analysis10.1016/j.enconman.2016.11.057 ↗
7. Material degradation of components in polymer electrolyte membrane (PEM) electrolytic cell and mitigation mechanisms: a review10.1016/j.rser.2019.05.007 ↗
8. An electrochemical study of a PEM stack for water electrolysis10.1016/j.ijhydene.2011.06.019 ↗
9. A review of proton exchange membrane water electrolysis on degradation mechanisms and mitigation strategies10.1016/j.jpowsour.2017.09.006 ↗
10. Investigation of a novel concept for hydrogen production by PEM water electrolysis integrated with multi-junction solar cells10.1016/j.enconman.2017.05.059 ↗
11. Thermodynamic analysis and optimization of photovoltaic/thermal hybrid hydrogen generation system based on complementary combination of photovoltaic cells and proton exchange membrane electrolyzer10.1016/j.enconman.2018.12.106 ↗
12. Current status, research trends, and challenges in water electrolysis science and technology10.1016/j.ijhydene.2020.03.109 ↗
13. Protective coatings on stainless steel bipolar plates for proton exchange membrane (PEM) electrolysers10.1016/j.jpowsour.2015.12.071 ↗
14. Materials for proton exchange membrane water electrolyzer bipolar plates10.1016/j.ijhydene.2016.11.106 ↗
15. A comprehensive review on PEM water electrolysis10.1016/j.ijhydene.2013.01.151 ↗
16. Acidic or alkaline? Towards a new perspective on the efficiency of water electrolysis10.1149/2.0271611jes ↗
17. The investment costs of electrolysis – a comparison of cost studies from the past 30 years10.1016/j.ijhydene.2017.11.115 ↗
18. Corrosion behavior of three bipolar plate materials in simulated SPE water electrolysis environment10.1016/j.ijhydene.2012.04.146 ↗
19. Performance of Ti–Ag-deposited titanium bipolar plates in simulated unitized regenerative fuel cell (URFC) environment10.1016/j.ijhydene.2011.01.154 ↗
20. Honeycomb-like nanocomposite Ti-Ag-N films prepared by pulsed bias arc ion plating on titanium as bipolar plates for unitized regenerative fuel cells10.1016/j.jpowsour.2011.10.022 ↗
21. High-durability titanium bipolar plate modified by electrochemical deposition of platinum for unitized regenerative fuel cell (URFC)10.1016/j.jpowsour.2009.10.002 ↗
22. Bipolar plate development with additive manufacturing and protective coating for durable and high-efficiency hydrogen production10.1016/j.jpowsour.2018.06.078 ↗
23. Factors affecting corrosion behavior of SS316L as bipolar plate material in PEMFC cathode environments10.1016/j.ijhydene.2012.04.026 ↗
24. Corrosion characteristics of SS316L as bipolar plate material in PEMFC cathode environments with different acidities10.1016/j.ijhydene.2010.10.067 ↗
25. Influence of temperature on corrosion behavior, wettability, and surface conductivity of 304 stainless steel in simulated cathode environment of proton exchange membrane fuel cells10.1016/j.ijhydene.2021.04.119 ↗
26. Analysis of the corrosion behavior of Al alloy bipolar plate for proton exchange membrane fuel cell (PEMFC) under operating thermal conditions10.1080/15435075.2011.621474 ↗
27. An overview of polymer electrolyte membrane electrolyzer for hydrogen production: modeling and mass transport10.1016/j.jpowsour.2016.01.012 ↗
28. PEM electrolysis for production of hydrogen from renewable energy sources10.1016/j.solener.2004.09.003 ↗
29. Impact of power converter current ripple on the degradation of PEM electrolyzer performances10.3390/membranes12020109 ↗
30. Electrolyzer durability at low catalyst loading and with dynamic operation10.1149/2.0231915jes ↗
31. Activity and durability of iridium nanoparticles in the oxygen evolution reaction10.1149/2.0151611jes ↗
32. Impact of the voltage fluctuation of the power supply on the efficiency of alkaline water electrolysis10.1016/j.ijhydene.2016.05.141 ↗
33. Influence of the power supply on the energy efficiency of an alkaline water electrolyser10.1016/j.ijhydene.2009.02.017 ↗
34. Corrosion of metallic bipolar plates accelerated by operating conditions in a simulated PEM fuel cell cathode environment10.1016/j.renene.2022.05.153 ↗
35. Online measurements of fluoride ions in proton exchange membrane water electrolysis through ion chromatography10.1016/j.jpowsour.2020.229179 ↗
36. Hydrogen⎕oxygen proton-exchange membrane fuel cells and electrolyzers10.1016/0378-7753(90)85013-3 ↗
37. Membrane degradation in PEM water electrolyzer: numerical modeling and experimental evidence of the influence of temperature and current density10.1016/j.ijhydene.2014.11.111 ↗
38. Corrosion of structural components of proton exchange membrane water electrolyzer anodes: a review10.1016/j.jpowsour.2022.232469 ↗
39. Validation and characterization of suitable materials for bipolar plates in PEM water electrolysis10.1016/j.ijhydene.2015.04.155 ↗
40. High-pressure PEM water electrolyser: a review on challenges and mitigation strategies towards green and low-cost hydrogen production10.1016/j.enconman.2022.115985 ↗
41. Dynamic hydrogen production from PV & wind direct electricity supply – modeling and techno-economic assessment10.1016/j.ijhydene.2020.08.044 ↗
42. TiZrNbTa)90Mo10 high-entropy alloy: electrochemical behavior and passive film characterization under exposure to Ringer’s solution10.1016/j.corsci.2020.108513 ↗
43. Corrosion of titanium and titanium alloys
44. Influence of uv light on passive behavior of the 304 stainless steel in acid solution10.1016/j.jpcs.2013.01.005 ↗
45. The passive behaviour of ferritic stainless steel containing alloyed tin in acidic media10.1039/C5RA23698C ↗
46. Metastable pitting corrosion behavior and characteristics of passive film of laser powder bed fusion produced Ti–6Al–4V in NaCl solutions with different concentrations10.1016/j.corsci.2023.111017 ↗
47. Corrosion behavior and characteristics of passive films of laser powder bed fusion produced Ti–6Al–4V in dynamic Hank’s solution10.1016/j.matdes.2021.109907 ↗
48. How do titanium and Ti6Al4V corrode in fluoridated medium as found in the oral cavity? An in vitro study10.1016/j.msec.2014.11.055 ↗
49. The effect of fluoride ions on the corrosion behavior of pure titanium in 0.05M sulfuric acid10.1016/j.electacta.2014.05.055 ↗
50. Corrosion behaviour of a wrought Ti-6Al-3Nb-2Zr-1Mo alloy in artificial seawater with various fluoride concentrations and pH values10.1016/j.matdes.2022.110416 ↗
51. Tuning microstructure and improving the corrosion resistance of a Ti-6Al-3Nb-2Zr-1Mo alloy via solution and aging treatments10.1016/j.corsci.2022.110694 ↗
52. Tuning microstructure and enhancing corrosion property of Ti-6Al-3Nb-2Zr-1Mo alloy through electron beam surface melting10.1016/j.corsci.2022.110520 ↗
53. Effect of Cu on the passivity of Ti–xCu (x = 0, 3 and 5 wt%) alloy in phosphate-buffered saline solution within the framework of PDM-II10.1016/j.electacta.2021.138466 ↗
54. The analysis of electrode impedances complicated by the presence of a constant phase element10.1016/S0022-0728(84)80324-1 ↗
55. On the use of the power-law model for interpreting constant-phase-element parameters
56. Characterization of the porosity of silicon nitride thin layers by electrochemical impedance spectroscopy10.1016/j.electacta.2017.01.008 ↗
57. Dependence of semiconductive properties of titanium oxide film on the growth rate and formation potential10.1023/A:1023330610633 ↗
58. Electrochemical behavior of 2205 duplex stainless steel in NaCl solution with different chromate contents10.1007/s11665-011-0030-1 ↗
59. Effect of solution concentration on semiconducting properties of passive films formed on austenitic stainless steels10.1016/j.corsci.2009.09.003 ↗
60. Effect of annealing temperatures on microstructural evolution and corrosion behavior of Ti-Mo titanium alloy in hydrochloric acid10.1016/j.corsci.2021.110079 ↗
61. Capacitance-voltage measurements and flat-band potential determination on Zr-doped α-Fe2O3 single-crystal electrodes10.1016/S0022-0728(83)80638-X ↗
62. Passivity breakdown of titanium in LiBr solutions10.1149/2.035401jes ↗
63. Inhibition effect of chromate on the passivation and pitting corrosion of a duplex stainless steel in LiBr solutions using electrochemical techniques10.1016/j.corsci.2007.03.002 ↗
64. Electrochemical corrosion and passive behavior of a new high-nitrogen austenitic stainless steel in chloride environment10.1016/j.matchemphys.2022.126837 ↗
65. Tuning the microstructure to improve corrosion resistance of additive manufacturing high-entropy alloy in proton exchange membrane fuel cells environment10.1016/j.corsci.2023.110969 ↗
66. XPS analysis of adsorption of oxygen molecules on the surface of Ti and TiNx films in vacuum10.1016/0368-2048(92)80016-2 ↗
67. Comparison of the corrosion behavior of pure titanium and its alloys in fluoride-containing sulfuric acid10.1016/j.corsci.2015.11.003 ↗
68. Structure and composition of passive titanium oxide films10.1016/S0921-5107(97)00043-3 ↗
69. Electrochemical properties, chemical composition and thickness of passive film formed on novel Ti–20Nb–10Zr–5Ta alloy10.1016/j.electacta.2013.03.086 ↗
70. X-ray photoelectron spectroscopic studies of anodically synthesized self aligned TiO2 nanotube arrays and the effect of electrochemical parameters on tube morphology10.1016/j.matchemphys.2011.12.041 ↗
71. Is niobium more corrosion-resistant than commercially pure titanium in fluoride-containing artificial saliva?10.1016/j.electacta.2017.03.015 ↗
72. Influence of fluoride content on the barrier layer formation and titanium dissolution in ethylene glycol–water electrolytes10.1016/j.electacta.2012.05.093 ↗
73. Passive film of 18-8 stainless steel structure and its function10.1016/0010-938X(73)90031-0 ↗
74. Coupling between dissolution and passivation revisited – Kinetic parameters of anodic oxidation of titanium alloys in a fluoride-containing electrolyte10.1016/j.jelechem.2014.09.016 ↗
75. TiO2 nanotubes: synthesis and applications10.1002/anie.201001374 ↗
76. Electrochemical and XPS studies of titanium for biomaterial applications with respect to the effect of hydrogen peroxide10.1002/jbm.820280115 ↗
77. Electrochemical impedance spectroscopy study of the passive oxide film on titanium for implant application10.1016/0013-4686(95)00465-3 ↗
78. A state-of-the-art review on passivation and biofouling of Ti and its alloys in marine environments10.1016/j.jmst.2017.11.021 ↗
79. Corrosion of additively manufactured alloys: a review10.5006/2926 ↗
80. Effect of fluoride and albumin concentration on the corrosion behavior of Ti–6Al–4V alloy10.1016/S0142-9612(02)00315-0 ↗
81. The influence of fluoride ions on the passive dissolution of titanium10.1016/0013-4686(79)87084-X ↗
82. Electrochemical anodic dissolution kinetics of titanium in fluoride-containing perchloric acid solutions at open-circuit potentials10.1149/1.3153148 ↗
83. The effect of fluoride ion on the anodic behavior of titanium in sulfuric acid10.1149/1.2404124 ↗
84. Passivity of AlCrFeMnTi and AlCrFeCoNi high–entropy alloys in Hanks’ solution10.1016/j.corsci.2022.110828 ↗
85. Effects of competitive anion adsorption (Br− or Cl−) and semiconducting properties of the passive films on the corrosion behavior of the additively manufactured Ti–6Al–4V alloys10.1016/j.corsci.2020.108789 ↗
86. The history of the point defect model for the passive state: a brief review of film growth aspects10.1016/j.electacta.2010.11.005 ↗
87. Electrochemical investigation of the effects of hydrogen on the stability of the passive film on iron10.1016/S0013-4686(01)00882-9 ↗
88. Quantitative analysis of repassivation kinetics of ferritic stainless steels based on the high field ion conduction model10.1016/S0013-4686(99)00415-6 ↗