Abstract

We reveal differences in composition and structure of passive films and repassivation rate of titanium in 3.5 wt% NaCl and in 6 M HNO 3. Titanium in 6 M HNO 3 shows worse corrosion resistance than in 3.5 wt% NaCl due to higher defect concentration and lower TiO 2 content despite the thicker passive film, which is the result of accelerated cathodic process and promoted dissolution/formation dynamic equilibrium of passive film in 6 M HNO 3 . Repassivation rate in 3.5 wt% NaCl is higher although film growth rate is lower, as the film exhibits good barrier effect when it is thin. Our results provide insights needed to guide application of titanium in SNFR plants.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Titanium Alloys Microstructure and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (75)

Show source-provided references
1. Effect of pH on the corrosion and repassivation behavior of TA2 in simulated seawater10.3390/ma14226764 ↗
2. Corrosion of titanium alloys in high temperature near anaerobic seawater10.1016/j.corsci.2015.12.011 ↗
3. A review of corrosion of titanium grade 7 and other titanium alloys in nuclear waste repository environments10.5006/1.3280899 ↗
4. Influence of sulfides on the passivation behavior of titanium alloy TA2 in simulated seawater environments10.1016/j.apsusc.2018.07.068 ↗
5. Corrosion performance and surface analysis of Ti–Ni–Pd–Ru–Cr alloy in nitric acid solution10.1016/j.corsci.2014.11.010 ↗
6. Thermal oxidation of titanium to improve corrosion resistance in boiling nitric acid medium10.1016/j.surfcoat.2013.07.010 ↗
7. Effect of heat input on microstructural changes and corrosion behavior of commercially pure titanium welds in nitric acid medium10.1007/s11665-008-9335-0 ↗
8. Effect of metal ions in a heated nitric acid solution on the corrosion behavior of a titanium–5% tantalum alloy in the hot nitric acid condensate10.1016/j.jnucmat.2012.08.009 ↗
9. A review on UREX processes for nuclear spent fuel reprocessing10.1016/j.nucengdes.2019.110410 ↗
10. Corrosion studies on materials of construction for spent nuclear fuel reprocessing plant equipment10.1016/0022-3115(93)90432-X ↗
11. Correlation between intergranular corrosion and impurities of extra high purity austenitic stainless steels10.1299/jpes.4.105 ↗
12. Towards a reliable determination of the intergranular corrosion rate of austenitic stainless steel in oxidizing media10.1016/j.corsci.2016.02.020 ↗
13. The stress corrosion cracking performance of pure zirconium and zirconium alloys in highly oxidizing nitric acid10.1016/0010-938X(95)00166-H ↗
14. Corrosion resistance of zirconium and zirconium-titanium alloy in hot nitric acid10.1016/0921-5093(95)80067-5 ↗
15. Corrosion-resistant Ti-xNb-xZr alloys for nitric acid applications in spent nuclear fuel reprocessing plants10.1007/s11661-011-0701-4 ↗
16. Synergistic effect of F- ions and scratch on the dynamic corrosion behavior of ZTi6010.1016/j.corsci.2022.110355 ↗
17. Repassivation behavior of titanium in artificial saliva investigated with a photon rupture method10.1016/j.electacta.2010.08.090 ↗
18. The corrosion/wear mechanisms of Ti–6Al–4V alloy for different scratching rates10.1016/j.wear.2006.11.025 ↗
19. Cavitation corrosion and repassivation kinetics of titanium in a heavy brine LiBr solution evaluated by using electrochemical techniques and confocal laser scanning microscopy10.1016/j.electacta.2011.09.034 ↗
20. Effects of biological factors on the repassivation current of titanium10.2320/matertrans.45.1635 ↗
21. In-situ XAFS and SERS study of self-healing of passive film on Ti in Hank's physiological solution10.1016/j.apsusc.2019.143657 ↗
22. Analysis of the effect of formation potential on the electrochemical response of doped titanium oxides10.1016/j.electacta.2016.12.048 ↗
23. Effect of alloying elements on corrosion properties of high corrosion resistant titanium alloys in high concentrated sulfuric acid
24. Effect of oxidizing ions on the corrosion behavior of SiN stainless steel in high-temperature nitric acid solution10.1016/j.electacta.2023.141917 ↗
25. Orientation dependence of corrosion resistance of a near-alpha Ti35 alloy applied in nuclear industry10.1016/j.jnucmat.2022.153873 ↗
26. Corrosion behaviour of Ti–6Al–7Nb and Ti–6Al–4V ELI alloys in the simulated body fluid solution by electrochemical impedance spectroscopy10.1016/j.electacta.2006.06.018 ↗
27. Evaluation of corrosion behaviour of Ti–25Mo alloy in chloride medium10.1007/s10800-010-0210-y ↗
28. Corrosion and passivation behavior of laser powder bed fusion produced Ti-6Al-4V in static/dynamic NaCl solutions with different concentrations10.1016/j.corsci.2021.109728 ↗
29. Electrochemical and passive characterization of a beta type Ti45Zr38Al17 cast rod in nitric acid medium10.1016/j.electacta.2012.08.047 ↗
30. Effect of immersion time on the passive and electrochemical response of annealed and nano-grained commercial pure titanium in Ringer's physiological solution at 37 °C10.1016/j.msec.2016.10.057 ↗
31. Electrochemical behavior assessment of micro- and nano-grained commercial pure titanium in H2SO4 solutions10.1007/s11665-016-2489-2 ↗
32. Corrosion characterization of titanium alloys by electrochemical techniques10.1016/j.electacta.2005.02.121 ↗
33. The influence of chloride and sulphate ions on the corrosion behavior of Ti and Ti-6Al-4V alloy in oxalic acid10.1016/j.electacta.2008.12.060 ↗
34. Corrosion behaviour of AISI type 304L stainless steel in nitric acid media containing oxidizing species10.1016/j.corsci.2010.09.023 ↗
35. On the passive and semiconducting behavior of severely deformed pure titanium in Ringer's physiological solution at 37 °C: a trial of the point defect model10.1016/j.msec.2017.02.046 ↗
36. XPS and EIS study of the passive film formed on orthopaedic Ti–6Al–7Nb alloy in Hank's physiological solution10.1016/j.electacta.2007.12.041 ↗
37. Studies on corrosion of titanium and air-oxidized titanium in fluorinated nitric acid10.1007/s12666-019-01667-3 ↗
38. The effect of fluoride ions on the corrosion behavior of pure titanium in 0.05M sulfuric acid10.1016/j.electacta.2014.05.055 ↗
39. Oxides formed on titanium by polishing, etching, anodizing, or thermal oxidizing
40. Stability and open circuit breakdown of the passive oxide film on titanium10.1016/0013-4686(88)80206-8 ↗
41. Enhancing the surface integrity and corrosion resistance of Ti-6Al-4V titanium alloy through cryogenic burnishing10.1007/s00170-016-9000-y ↗
42. Insights into stress corrosion cracking in scratched area of alloy 690TT steam generator tubes
43. Repassivation behavior of 316L stainless steel in borate buffer solution: kinetics analysis of anodic dissolution and film formation10.1016/j.apsusc.2015.09.018 ↗
44. Quantitative analysis of repassivation kinetics of ferritic stainless steels based on the high field ion conduction model10.1016/S0013-4686(99)00415-6 ↗
45. The kinetics of anodic dissolution and repassivation on stainless steel 304L in solutions containing nitrate10.1149/1.3574367 ↗
46. Predicting SCC susceptibility of austenitic stainless steel by rapid scratching electrode technique10.4028/www.scientific.net/MSF.289-292.969 ↗
47. Effects of applied anodic potential and pH on the repassivation kinetics of pure aluminium in aqueous alkaline solution10.1007/s100080050135 ↗
48. Corrosion behaviour of the amorphous Mg65Y10Cu15Ag10 alloy10.1016/S0010-938X(02)00131-2 ↗
49. Relationship between amorphous structure and corrosion behaviour in a Zr–Ni metallic glass10.1016/j.corsci.2012.02.017 ↗
50. Anodic behaviour of scratched silver electrodes in alkaline solution10.1016/0013-4686(80)87006-X ↗
51. Reactions of scratched copper electrodes in aqueous solutions10.1149/1.2127233 ↗
52. Effects of tungsten and nickel on repassivation rate of stainless steels in chloride solution by electrochemical method10.1002/maco.200503965 ↗
53. Theory of the oxidation of metals10.1088/0034-4885/12/1/308 ↗
54. A Study on the localized corrosion and repassivation kinetics of Fe-20Cr- x Ni ( x = 0–20 wt%) stainless steels via electrochemical analysis10.1016/j.corsci.2015.07.022 ↗
55. The repassivation kinetics study of Alloy 800 in high-temperature pressurized water10.1016/j.elecom.2015.08.017 ↗
56. Development of a scratch electrode system in high temperature high pressure water10.1016/j.corsci.2015.03.006 ↗
57. Repassivation behavior of alloy 690TT in simulated primary water at different temperatures10.1016/j.jmst.2020.06.044 ↗
58. Re-passivation rate and conduction mechanism of surface film on copper in nitrite solutions10.1016/j.corsci.2022.110447 ↗
59. Effects of Si on the repassivation kinetics and SCC susceptibility of stainless steels10.1149/1.2953522 ↗
60. Enhanced corrosion resistance by engineering crystallography on metals
61. Alloy design employing high Cr concentrations for Mo-free stainless steels with enhanced corrosion resistance10.1016/j.corsci.2018.06.021 ↗
62. Effects of alloying elements, Cr, Mo and N on repassivation characteristics of stainless steels using the abrading electrode technique10.1016/j.matchemphys.2005.10.016 ↗
63. Comparison of the corrosion behavior of pure titanium and its alloys in fluoride-containing sulfuric acid10.1016/j.corsci.2015.11.003 ↗
64. NIST X-ray Photoelectron Spectroscopy Database, NIST Standard Reference Database 20, Version 4.1 (Data compiled and evaluated by A.V. Naumkin, A. KrautVass, S.W. Gaarenstroom, and C.J. Powell). 〈http://srdata.nist.gov/xps/〉.
65. Effect of molybdenum content on corrosion resistance and corrosion behavior of Ti-Mo titanium alloy in hydrochloric acid
66. Corrosion mechanisms of austenitic stainless steels in nitric media used in reprocessing plants10.1016/j.jnucmat.2007.10.017 ↗
67. Passivity–the key to our metals-based civilization10.1351/pac199971060951 ↗
68. Repassivation of titanium and surface oxide film regenerated in simulated bioliquid10.1002/(SICI)1097-4636(19980615)40:4<530::AID-JBM3>3.0.CO;2-G ↗
69. J.A. Dean, 1999. Lange's Handbook of Chemistry, fifteenth ed., Lange's Handbook of Chemistry.
70. Superior corrosion resistance of Ti-Al-Zr alloy in aggressive nitric acid environments10.1007/s11665-020-05300-z ↗
71. Corrosion resistance of Ti-based metallic glass coating in concentrated nitric acid10.1016/j.matchemphys.2013.11.061 ↗
72. Corrosion behaviour of single (Ti) and duplex (Ti–TiO2) coating on 304L stainless steel in nitric acid medium10.1016/j.matchemphys.2011.08.016 ↗
73. The dissolution and repassivation of new titanium surfaces in alkaline methanolic solution: part I. The phenomena10.1149/1.2096913 ↗
74. Electrochemical impedance spectroscopy study of the passive films of alloy 22 in low pH nitrate and chloride environments10.1016/j.electacta.2006.08.043 ↗
75. Synergistic effects of fluoride and chloride on general corrosion behavior of AISI 316 stainless steel and pure titanium in H2SO4 solutions10.1016/j.corsci.2017.10.028 ↗