Effect of surface finishing on the oxidation characteristics of a Fe-21Cr-32Ni alloy in supercritical carbon dioxide
Source abstract
Abstract
The effect of surface finishing on the oxidation behavior of a Fe-21Cr-32Ni alloy in supercritical carbon dioxide (650 ºC for 1000 h) was studied. After exposure, the cross-section of the specimen showed a typical inner-outer oxide layers structure with subsurface carburization. Reduced oxidation and carburization rates were identified for the ground surface, where a much thinner Cr-rich oxide scale and a shallower carburization depth were observed. Grinding introduced an ultra-fine grained layer and a highly deformed layer on the metal surface, where Cr diffusion rate was significantly enhanced. The high Cr diffusion led to the transition from internal to external oxidation by favoring the formation of a thin/protective Cr-rich oxide layer. This continuous Cr-rich oxide layer not only protected the substrate matrix from further oxidation, but also reduced the permeability of carbon into the oxides, thus improving the oxidation and carburization resistance of the ground specimen.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Advanced materials and composites · Nuclear Materials and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (43)
Show source-provided references
1. Initial oxidation and chromium diffusion. I. Effects of surface working on 9–20% Cr steels10.1016/j.corsci.2003.09.004 ↗
2. G.R. Holcomb, C.S. Carney, R.P. Oleksak, J.H. Tylczak, Ö. Doğan, Oxidation behavior of Fe-and Ni-base alloys in supercritical CO2 and related environments, in: The 6th International Supercritcal CO2 Power Cycles Symposium, Pittsburgh, Pennsylvania, 2018.
3. Effect of surface finish on high-temperature oxidation of steels in CO2, supercritical CO2, and air10.1007/s11085-019-09938-6 ↗
4. The effect of surface finish on the scaling behavior of stainless steel in steam and supercritical water10.1007/s11085-013-9380-4 ↗
5. Corrosion mechanism of a Ni-based alloy in supercritical water: impact of surface plastic deformation10.1016/j.corsci.2015.06.032 ↗
6. Effect of ultrasonic impact peening on the corrosion of ferritic–martensitic steels in supercritical water10.1016/j.jnucmat.2014.11.028 ↗
7. Effect of surface modification on the corrosion resistance of austenitic stainless steel 316L in supercritical water conditions10.1016/j.supflu.2013.05.002 ↗
8. Corrosion mechanisms of 316L stainless steel in supercritical water: the significant effect of work hardening induced by surface finishes10.1016/j.corsci.2019.05.014 ↗
9. Corrosion of austenitic and ferritic-martensitic steels exposed to supercritical carbon dioxide10.1016/j.corsci.2011.06.002 ↗
10. Corrosion of austenitic alloys in high temperature supercritical carbon dioxide10.1016/j.corsci.2012.03.029 ↗
11. Structural evolution of a Ni alloy surface during high-temperature oxidation10.1007/s11085-017-9821-6 ↗
12. Effect of silicon on corrosion of Fe-20Cr and Fe-20Cr-20Ni alloys in wet CO2 with and without HCl at 650 °C10.1016/j.corsci.2020.109096 ↗
13. Effects of silicon and water vapour on corrosion of Fe-20Cr and Fe-20Cr-20Ni alloys in CO2 at 650 A degrees C10.1007/s11085-016-9681-5 ↗
14. Effects of surface treatments on environmentally-assisted cracking susceptibility of Alloy 182 in BWR environment10.1016/j.corsci.2021.109555 ↗
15. Effect of Fe on corrosion of Ni-20Cr and Ni-30Cr alloys in wet CO2 gas at 650 and 700 °C10.1016/j.corsci.2019.04.007 ↗
16. Corrosion behaviour of Ni-Cr alloys in wet CO2 atmosphere at 700 and 800 degrees C10.1016/j.corsci.2018.10.029 ↗
17. Corrosion behavior of FBR structural materials in high temperature supercritical carbon dioxide10.1299/jpes.4.252 ↗
18. Characterization of chromia scales formed in supercritical carbon dioxide10.1080/09603409.2017.1389371 ↗
19. Oxidation and carburizing of FBR structural materials in carbon dioxide10.1016/j.pnucene.2014.07.038 ↗
20. The carburization behavior of alloy 800HT in high temperature supercritical-CO210.1016/j.matlet.2021.130067 ↗
21. Corrosion and carburization behavior of chromia-forming heat resistant alloys in a high-temperature supercritical-carbon dioxide environment10.1016/j.corsci.2015.07.007 ↗
22. The effect of residual stress on the preferential intergranular oxidation of Alloy 60010.1016/j.corsci.2016.05.022 ↗
23. Self-diffusion in Cr2o3.1. chromium diffusion in single-crystals10.1080/01418619208201560 ↗
24. Self-diffusion in Cr2o3.2. oxygen diffusion in single-crystals10.1080/01418619208201561 ↗
25. Self-diffusion in Cr2o3.3. chromium and oxygen grain-boundary diffusion in polycrystals10.1080/01418619208201562 ↗
26. Diffusion of iron in Cr2O3: polycrystals and thin films10.1016/j.msea.2004.09.033 ↗
27. Diffusion of cations in chromia layers grown on iron-base alloys10.1007/BF00665632 ↗
28. Oxidation kinetics and mechanisms of Ni-base alloys in pressurised water reactor primary conditions: influence of subsurface defects10.1016/j.corsci.2011.07.024 ↗
29. High-resolution characterization of the internal and external oxidation of austenitic alloys in supercritical water10.1016/j.scriptamat.2021.113814 ↗
30. Understanding the surface oxide evolution of T91 ferritic-martensitic steel in supercritical water through advanced characterization10.1016/j.actamat.2020.05.016 ↗
31. Theoretical analysis of the diffusion processes determining the oxidation rate of alloys10.1149/1.2779605 ↗
32. The role of noncrystalline films in the oxidation and corrosion of metals10.1007/BF01058831 ↗
33. Effect of silicon on the oxidation resistance of 9% Cr steels10.1016/S0169-4332(02)01505-2 ↗
34. Analytical electron-microscopy of a selective oxide scale formed on 20-percent-Cr-25-percent-Ni-Nb stainless-steel10.1007/BF00656580 ↗
35. Effect of alloy composition on the selective oxidation of ternary Fe-Si-Cr, Fe-Mn-Cr model alloys10.1002/sia.2732 ↗
36. The oxidation of iron chromium manganese alloys at 900-degrees-C10.1007/BF00938460 ↗
37. Effect of Mn on oxide formation by Fe-Cr and Fe-Cr-Ni alloys in dry and wet CO2 gases at 650 degrees C10.1016/j.corsci.2016.07.014 ↗
38. Effects of cerium and manganese on corrosion of Fe-Cr and Fe-Cr-Ni alloys in Ar-20CO(2) and Ar-20CO(2)-20H(2)O gases at 650 degrees C10.1016/j.corsci.2015.08.012 ↗
39. On the breakaway oxidation of Fe9Cr1Mo steel in high pressure CO210.1016/j.actamat.2017.02.034 ↗
40. Corrosion of 9Cr steel in CO2 at intermediate temperature II: mechanism of carburization10.1007/s11085-011-9272-4 ↗
41. A study on the solubility and distribution of carbon in oxides10.1016/0038-1098(85)91021-X ↗
42. Carbon transport through oxide scales on Fe-Cr alloys10.1007/BF00751801 ↗
43. Effect of Fe on corrosion of Ni-20Cr and Ni-30Cr alloys in wet CO2 gas at 650 and 700 degrees C10.1016/j.corsci.2019.04.007 ↗