Hydrogen-assisted fatigue crack-propagation in a Ni-based superalloy 718, revealed via crack-path crystallography and deformation microstructures
Source abstract
Abstract
Abstract Fatigue crack-growth (FCG) of Ni-based superalloy 718 was investigated under gaseous hydrogen environment (external hydrogen) and uniformly pre-charged state (internal hydrogen). Under external hydrogen, intergranular fracture predominated, whereas dislocation slip-band or twin boundary fracture were prevalent under internal hydrogen. This failure mode divergence encompassed unique characteristics of macroscale FCG response, leading to both cycle- and time-dependent cracking. The intergranular cracking was ascribed to short-circuit diffusion of hydrogen along grain boundaries. Meanwhile, the material’s inherently inhomogeneous deformation mode exerts harmfulness when hydrogen was uniformly distributed inside the specimen, causing slip-bands or twin boundaries to become the weakest links for fracture.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · High Temperature Alloys and Creep · Nuclear Materials and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (100+)
Show source-provided references
1. Alloy 718 at pratt & whitney: historical perspective and future challenges
2. Ni-based superalloys for turbine discs10.1007/s11837-999-0005-y ↗
3. Alloy 718 for oilfield applications10.1007/s11837-012-0238-z ↗
4. Hydrogen-enhanced cracking of superalloys10.1007/BF02660868 ↗
5. Hydrogen embrittlement in nickel-based superalloy 718: relationship between γ’ + γ’’ precipitation and the fracture mode
6. Study of the effect of hydrogen charging on the tensile properties and microstructure of four variant heat treatments of nickel alloy 71810.1016/j.ijhydene.2017.02.149 ↗
7. Effects of precipitation phases on the hydrogen embrittlement sensitivity of Inconel 71810.1016/S1468-6996(02)00039-6 ↗
8. Hydrogen-assisted failure in Ni-based superalloy 718 studied under in situ hydrogen charging: the role of localized deformation in crack propagation10.1016/j.actamat.2017.02.059 ↗
9. Hydrogen assisted crack initiation and propagation in a nickel-based superalloy10.1016/j.actamat.2016.05.003 ↗
10. Some aspects of the precipitation of metastable intermetallic phases in INCONEL 71810.1007/BF02647549 ↗
11. Strengthening mechanisms in Inconel 718 superalloy10.1179/030634583790421032 ↗
12. Effect of double aging treatment on structure in Inconel 718 alloy10.1023/B:JMSC.0000020036.96777.9c ↗
13. Delta phase precipitation in Inconel 71810.1016/j.matchar.2004.07.004 ↗
14. Aging of the Inconel 718 alloy between 500 and 750 °C10.1557/JMR.1997.0306 ↗
15. Study of the effect of δ phase on hydrogen embrittlement of Inconel 718 by notch tensile tests10.1016/j.corsci.2004.06.008 ↗
16. Multi-scale and spatially resolved hydrogen mapping in a Ni–Nb model alloy reveals the role of the δ phase in hydrogen embrittlement of alloy 71810.1016/j.actamat.2016.02.053 ↗
17. On the role of precipitates in hydrogen trapping and hydrogen embrittlement of a nickel-based superalloy10.1016/j.corsci.2018.10.019 ↗
18. The role of localized deformation in hydrogen-assisted crack propagation in 21Cr-6Ni-9Mn stainless steel10.1016/j.actamat.2009.04.027 ↗
19. Hydrogen environment embrittlement of stable austenitic steels10.1016/j.ijhydene.2012.08.071 ↗
20. Role of γ′ characteristic on the hydrogen embrittlement susceptibility of Fe–Ni–Cr alloys10.1016/j.corsci.2015.09.003 ↗
21. Deformation behaviour of γ″ strengthened inconel 71810.1016/0001-6160(88)90139-3 ↗
22. Shearing of γ″ precipitates and formation of planar slip bands in Inconel 718 during cyclic deformation10.1016/j.scriptamat.2004.11.023 ↗
23. On the origin of planar slip in f.c.c. Alloys10.1016/0001-6160(89)90143-0 ↗
24. Hydrogen embrittlement understood10.1007/s11663-015-0325-y ↗
25. Hydrogen embrittlement phenomena and mechanisms10.1515/corrrev-2012-0502 ↗
26. The predominant role of strain-induced vacancies in hydrogen embrittlement of steels: overview10.1016/j.actamat.2018.12.013 ↗
27. The role of hydrogen and other interstitials in the mechanical behavior of metals10.1007/s13632-016-0319-4 ↗
28. Equilibrium aspects of hydrogen-induced cracking of steels10.1016/0001-6160(74)90061-3 ↗
29. Enumeration of the hydrogen-enhanced localized plasticity mechanism for hydrogen embrittlement in structural materials10.1016/j.actamat.2018.12.014 ↗
30. Lattice defects dominating hydrogen-related failure of metals10.1016/j.actamat.2008.06.031 ↗
31. Hydrogen-enhanced localization of plasticity in an austenitic stainless steel10.1007/BF02669644 ↗
32. Hydrogen embrittlement of ferritic steels: observations on deformation microstructure, nanoscale dimples and failure by nanovoiding10.1016/j.actamat.2012.06.014 ↗
33. On the formation and nature of quasi-cleavage fracture surfaces in hydrogen embrittled steels10.1016/j.actamat.2010.11.024 ↗
34. Hydrogen-assisted failure in a twinning-induced plasticity steel studied under in situ hydrogen charging by electron channeling contrast imaging10.1016/j.actamat.2013.04.030 ↗
35. The dual role of coherent twin boundaries in hydrogen embrittlement10.1038/ncomms7164 ↗
36. Interpretation of hydrogen-assisted fatigue crack propagation in BCC iron based on dislocation structure evolution around the crack wake10.1016/j.actamat.2018.06.041 ↗
37. The roles of internal and external hydrogen in the deformation and fracture processes at the fatigue crack tip zone of metastable austenitic stainless steels10.1016/j.scriptamat.2018.08.003 ↗
38. Mechanistic dissimilarities between environmentally influenced fatigue-crack propagation at near-threshold and higher growth rates in lower strength steels10.1179/msc.1982.16.11.529 ↗
39. Fatigue crack growth of two pipeline steels in a pressurized hydrogen environment10.1016/j.corsci.2013.10.014 ↗
40. Unified evaluation of hydrogen-induced crack growth in fatigue tests and fracture toughness tests of a carbon steel10.1016/j.ijfatigue.2017.06.006 ↗
41. Fatigue limit of carbon and Cr Mo steels as a small fatigue crack threshold in high-pressure hydrogen gas10.1016/j.ijhydene.2018.09.026 ↗
42. Low cycle fatigue behavior of inconel 718 at 298 K and 823 K10.1007/BF02667395 ↗
43. Inhomogeneous deformation in INCONEL 718 during monotonic and cyclic loadings10.1007/BF02647316 ↗
44. The low cycle fatigue of three wrought nickel-base alloys10.1007/BF02643144 ↗
45. Frequency and wave-form effects on the fatigue crack growth behavior of alloy 718 at 298 K and 823 K10.1007/BF02646402 ↗
46. Fatigue behaviour of two nickel-base alloys I: experimental results on low cycle fatigue, fatigue crack propagation and substructures
47. Material performance of age-hardened beryllium–copper alloy, CDA-C17200, in a high-pressure, gaseous hydrogen environment10.1016/j.ijhydene.2017.04.270 ↗
48. Fatigue crack growth behavior of laser-annealed IN 718 alloy in hydrogen10.1016/j.corsci.2004.03.012 ↗
49. Walter · 1973
50. James · 1975
51. Fatigue crack growth properties of Ni-base alloys in high pressure hydrogen at room temperature10.2472/jsms.38.539 ↗
52. Permeability, solubility and diffusivity of hydrogen isotopes in stainless steels at high gas pressures10.1016/j.ijhydene.2006.05.008 ↗
53. Diffusion coefficients of hydrogen in Ni-Cu and Ni-Co alloys10.2320/matertrans1960.27.233 ↗
54. Hydrogen diffusion coefficients through Inconel 718 in different metallurgical conditions10.1016/j.corsci.2013.11.002 ↗
55. Development of new strain Gage for high-pressure hydrogen gas use10.1007/s11340-013-9816-4 ↗
56. ASTM, E647-08-1 · 2010
57. Hydrogen permeation behavior in IN718 and GH761 superalloys10.1007/BF02651595 ↗
58. Theory and application of electron channelling contrast imaging under controlled diffraction conditions10.1016/j.actamat.2014.04.018 ↗
59. A review of strain analysis using Electron backscatter diffraction10.1017/S1431927611000055 ↗
60. Pronounced transition of crack initiation and propagation modes in the hydrogen-related failure of a Ni-based superalloy 718 under internal and external hydrogen conditions10.1016/j.corsci.2019.108186 ↗
61. A new mechanism in hydrogen-enhanced fatigue crack growth behavior of a 1900-MPa-class high-strength steel10.1007/s10704-012-9760-9 ↗
62. Hydrogen-induced intergranular fracture of steels10.1016/S0013-7944(00)00124-7 ↗
63. Grain boundary transport of hydrogen in nickel10.1016/0036-9748(82)90273-3 ↗
64. Intercrystalline hydrogen transport in nanocrystalline nickel10.1016/0956-716X(91)90114-G ↗
65. Accelerated diffusion of hydrogen along grain boundaries in nickel10.1016/1359-6454(95)00446-7 ↗
66. Contribution of triple junctions to the diffusion anomaly in nanocrystalline materials10.1016/j.scriptamat.2007.03.057 ↗
67. Grain size and grain-boundary effects on diffusion and trapping of hydrogen in pure nickel10.1016/j.actamat.2012.09.004 ↗
68. First-principles investigation of hydrogen trapping and diffusion at grain boundaries in nickel10.1016/j.actamat.2015.07.031 ↗
69. Hydrogen diffusion in ultrafine-grained palladium: roles of dislocations and grain boundaries10.1016/j.actamat.2016.01.069 ↗
70. Atomistic study of hydrogen embrittlement of grain boundaries in nickel: I. fracture10.1016/j.jmps.2017.01.020 ↗
71. First-principles study on the grain boundary embrittlement of metals by solute segregation: part II. Metal (Fe, Al, Cu)-Hydrogen (H) systems10.1007/s11661-010-0380-6 ↗
72. Effect of hydrogen environment on the separation of Fe grain boundaries10.1016/j.actamat.2016.01.067 ↗
73. Hydrogen-induced intergranular failure in nickel revisited10.1016/j.actamat.2012.01.040 ↗
74. Hydrogen embrittlement controlled by reaction of dislocation with grain boundary in alpha-iron10.1016/j.ijplas.2018.08.013 ↗
75. A statistical, physical-based, micro-mechanical model of hydrogen-induced intergranular fracture in steel10.1016/j.jmps.2009.10.005 ↗
76. Influence of solute hydrogen on the interaction of screw dislocations with vicinal twin boundaries in nickel10.1016/j.scriptamat.2019.08.010 ↗
77. The role of intergranular fracture on hydrogen-assisted fatigue crack propagation in pure iron at a low stress intensity range10.1016/j.msea.2018.07.014 ↗
78. Hydrogen-induced ductility loss of precipitation-strengthened Fe-Ni-Cr-based superalloy10.1016/j.msea.2018.10.040 ↗
79. Dislocation structures adjacent to fatigue crack tips in stainless steel10.1007/BF02656408 ↗
80. Fine subgrain structure adjacent to fatigue cracks10.1016/0001-6160(72)90008-9 ↗
81. Cyclic deformation of ferritic steel—II10.1016/0956-7151(91)90142-N ↗
82. Transmission electron microscopy of the crack tip region of fatigued copper single crystals10.1007/BF02649636 ↗
83. In-situ SEM study of fatigue crack growth behaviour in IN71810.1016/S0142-1123(03)00172-5 ↗
84. The effect of hydrogen on dislocation dynamics10.1016/S0013-7944(01)00011-X ↗
85. Correlation between dislocation organization and slip bands: TEM and AFM investigations in hydrogen-containing nickel and nickel–chromium10.1016/j.actamat.2015.03.016 ↗
86. Dislocations in Lithium fluoride crystals10.1016/S0081-1947(08)60457-9 ↗
87. Simulation of dislocation patterns in multislip10.1016/S1359-6462(02)00185-9 ↗
88. Influence of hydrogen on dislocation self-organization in Ni10.1016/j.actamat.2017.05.073 ↗
89. Increase in dislocation density in cold-deformed Pd using H as a temporary alloying addition10.1016/j.scriptamat.2013.01.005 ↗
90. Roughness-induced crack closure: an explanation for microstructurally sensitive fatigue crack growth10.1007/BF02644220 ↗
91. Plastic zone sizes in fatigued specimens of INCO 71810.1007/BF02818660 ↗
92. Reduction of cohesion in ionic crystals by dislocations10.1063/1.1736081 ↗
93. Elastic energy release from slip bands during fracture10.1063/1.1931143 ↗
94. Numerical simulations of hydrogen–dislocation interactions in fcc stainless steels: part II: hydrogen effects on crack tip plasticity at a stress corrosion crack10.1016/S1359-6454(02)00009-5 ↗
95. Numerical simulations of hydrogen–dislocation interactions in fcc stainless steels.: part I: hydrogen–dislocation interactions in bulk crystals10.1016/S1359-6454(02)00008-3 ↗
96. Hydrogen-enhanced localized plasticity—a mechanism for hydrogen-related fracture10.1016/0921-5093(94)90975-X ↗
97. Hydrogen effects on the interaction between dislocations10.1016/S1359-6454(97)00349-2 ↗
98. Strengthening materials by engineering coherent internal boundaries at the nanoscale10.1126/science.1159610 ↗
99. The interaction mechanism of screw dislocations with coherent twin boundaries in different face-centred cubic metals10.1016/j.scriptamat.2005.11.072 ↗
100. Chemomechanical effects on the separation of interfaces occurring during fracture with emphasis on the hydrogen-iron and hydrogen-nickel system10.1016/j.actamat.2015.07.057 ↗