Improved heat and corrosion resistance of high electrical conductivity Al-Mg-Si alloys by multi-alloying of Ce, Sc and Y
Source abstract
Abstract
In order to improve the corrosion and heat resistance of Al-Mg-Si alloy conductor materials, Ce, Sc, Y and Zr were added in Al-Mg-Si alloy to regulate the microstructure. The Al-Mg-Si-Ce-Sc-Y alloy was designed with excellent pitting and intergranular corrosion resistance by obtaining the micron-sized Fe-containing second phase with a lower potential difference to Al matrix, more dispersed grain boundary precipitates with a higher proportion of Si particles, narrower width of PFZ and ideal distribution of intergranular precipitates. The Al-Mg-Si-Ce-Sc-Y alloy also maintained higher hardness, strength and electrical conductivity after overaging and annealing and the corrosion/heat resistance mechanisms were proposed.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (54)
Show source-provided references
1. Integrated modeling of friction stir welding of 6xxx series Al alloys: process, microstructure and properties10.1016/j.pmatsci.2011.05.003 ↗
2. Simultaneously enhanced strength and ductility of 6xxx Al alloys via manipulating meso-scale and nano-scale structures guided with phase equilibrium10.1016/j.jmst.2019.09.029 ↗
3. Optimization of electrical conductivity and strength combination by structure design at the nanoscale in Al-Mg-Si alloys10.1016/j.actamat.2015.07.039 ↗
4. Characterization of mechanical and corrosion properties of cryorolled Al 1100 alloy: Effect of annealing and solution treatment10.1016/S1003-6326(21)65705-9 ↗
5. Effect of laser shock peening on corrosion behaviors of ultra-high strength Al-Zn-Mg-Cu alloys prepared by spray forming and ingot metallurgy10.1016/j.corsci.2022.110458 ↗
6. Optimization of the pre-aging treatment for an AA6022 alloy at various temperatures and holding times10.1016/j.jallcom.2015.05.188 ↗
7. Pre-aging to improve bake hardening in a twin-roll cast Al-Mg-Si alloy10.1016/j.msea.2004.08.069 ↗
8. Grain boundary structures and their correlation with intergranular corrosion in an extruded Al-Mg-Si-Cu alloy10.1016/j.matchar.2020.110695 ↗
9. Intergranular corrosion of AA6082 Al-Mg-Si alloy extrusion: The influence of trace Cu and grain boundary misorientation10.1016/j.jallcom.2020.157228 ↗
10. Size effect in the Al3Sc dispersoid-mediated precipitation and mechanical/electrical properties of Al-Mg-Si-Sc alloys10.1016/j.jmst.2020.03.056 ↗
11. A modified processing route for high strength Al-Mg-Si aluminum conductors based on twin-roll cast strip10.1016/j.jmatprotec.2019.116463 ↗
12. On the microstructural origins of improvements in conductivity by heavy deformation and ageing of Al-Mg-Si alloy 610110.1016/j.matchar.2021.111073 ↗
13. Insights into the electrochemical response of a partially recrystallized Al-Mg-Si alloy and its relationship to corrosion events10.1016/j.electacta.2019.03.220 ↗
14. Mechanical properties and corrosion behavior of artificially aged Al-Mg-Si alloy10.1016/j.jmrt.2019.11.040 ↗
15. Effect of the thickness reduction on intergranular corrosion in an under-aged Al-Mg-Si-Cu alloy during cold-rolling10.1016/j.corsci.2018.07.018 ↗
16. Effects of La addition on the mechanical properties and thermal-resistant properties of Al-Mg-Si-Zr alloys based on AA 620110.1016/j.matdes.2011.07.003 ↗
17. Effect of Ce addition on castability, mechanical properties and electric conductivity of Al-0.3Si-0.2Mg alloy10.1179/1743133615Y.0000000002 ↗
18. Precipitation sequence in Al-Mg-Si-Sc-Zr alloys during isochronal aging10.1016/j.mtla.2019.100437 ↗
19. Tailored precipitation route for the effective utilisation of Sc and Zr in an Al-Mg-Si alloy10.1016/j.mtla.2020.100656 ↗
20. Effect of cold plastic deformation and subsequent aging on the strength properties of Al-Mg2Si alloys with combined (Sc+Zr) and (Sc+Hf) additions10.1016/j.jallcom.2019.153426 ↗
21. Microstructure evolution and performances of Al-0.7Mg-0.6Si-0.2Ce-X (X=Sc, Y and Zr) alloys with high strength and high electrical conductivity10.1016/j.jallcom.2021.162654 ↗
22. The influence of Si and Mg content on the microstructure, tensile ductility, and stretch formability of 6xxx alloys10.1007/s11661-013-1740-9 ↗
23. Study of the precipitate evolution mechanism in an Al-Mg-Si-Cu alloy with Si-rich and low Cu composition10.1016/j.matchar.2022.112167 ↗
24. Initial precipitation and hardening mechanism during non-isothermal aging in an Al-Mg-Si-Cu 6005A alloy10.1016/j.matchar.2014.05.007 ↗
25. Microstructure and properties of novel Al-Ce-Sc, Al-Ce-Y, Al-Ce-Zr and Al-Ce-Sc-Y alloy conductors processed by die casting, hot extrusion and cold drawing10.1016/j.jmst.2020.03.073 ↗
26. ASTM G110, Standard Practice for Evaluating Intergranular Corrosion Resistance of Heat Treatable Aluminum Alloys by Immersion in Sodium Chloride + Hydrogen Peroxide Solution, (2015).
27. Non-isothermal aging: A heat treatment method that simultaneously improves the mechanical properties and corrosion resistance of ultra-high strength Al-Zn-Mg-Cu alloy10.1016/j.jallcom.2020.156286 ↗
28. Mechanical properties and microstructure evolution of ultra-high strength Al-Zn-Mg-Cu alloy processed by room temperature ECAP with post aging10.1016/j.msea.2018.06.047 ↗
29. Strength-ductility synergy of selective laser melted Al-Mg-Sc-Zr alloy with a heterogeneous grain structure
30. Transient Thermal Field Analysis in ACCC Power Lines by the Green’s Function Method10.3390/en13010280 ↗
31. New method for calculating the heating of the conductor10.3390/en12142769 ↗
32. Accurate simulations of thermal field of operational conductors10.1088/1757-899X/231/1/012100 ↗
33. Evaluation of corrosion resistance of AA6082-T651 aluminium alloy after laser shock peening by means of cyclic polarisation and ElS methods10.1016/j.corsci.2012.03.019 ↗
34. Improvement of corrosion resistance of AA2024-T3 using femtosecond laser peening without protective and confining medium10.1016/j.corsci.2018.08.030 ↗
35. Localized corrosion of ultrafine-grained Al-Mg model alloys10.1016/j.electacta.2009.11.016 ↗
36. Effect of Zn/Mg ratios on SCC, electrochemical corrosion properties and microstructure of Al-Zn-Mg alloy10.1016/j.jallcom.2018.05.063 ↗
37. Effects of pH and chloride concentration on pitting corrosion of AA6061 aluminum alloy10.1016/j.corsci.2008.03.006 ↗
38. Study of Al alloy corrosion in neutral NaCl by the pitting scan technique10.1016/j.matchemphys.2010.02.022 ↗
39. Laser alloyed Al-W coatings on aluminum for enhanced corrosion resistance10.1016/j.apsusc.2014.12.037 ↗
40. The crystal structure of the β' phase in Al-Mg-Si alloys10.1016/j.actamat.2007.02.032 ↗
41. Anodisation of aluminium alloy AA7075 – Influence of intermetallic particles on anodic oxide growth10.1016/j.corsci.2019.108319 ↗
42. Insight into the localized strain effect on micro-galvanic corrosion behavior in AA7075-T6 aluminum alloy10.1016/j.corsci.2020.109174 ↗
43. Scanning Kelvin probe force microscopy as a means of predicting the electrochemical characteristics of the surface of a modified AA4xxx/AA3xxx (Al alloys) brazing sheet10.1016/j.electacta.2012.10.051 ↗
44. Sc-containing hierarchical phase structures to improve the mechanical and corrosion resistant properties of Al-Mg-Si alloy10.1016/j.matdes.2022.110699 ↗
45. Nano-phase transformation of composite precipitates in multicomponent Al-Mg-Si(-Sc) alloys10.1016/j.jmst.2021.09.037 ↗
46. A summary of corrosion properties of Al-rich solid solution and secondary phase particles in Al alloys10.3390/met7030084 ↗
47. The inhibition effect of some amino acids towards the corrosion of aluminum in 1M HCl+1M H2SO4 solution10.1016/j.apsusc.2004.12.016 ↗
48. A study of the crystallographic pitting behavior of Al-0.54Mg-0.66Si aluminum alloy in acidic chloride solutions10.1016/j.matchar.2018.12.024 ↗
49. Initial formation of corrosion products on pure zinc and MgZn2 examinated by XPS10.1016/j.corsci.2013.10.029 ↗
50. Surface and cut-edge corrosion behavior of Zn-Mg-Al alloy-coated steel sheets as a function of the alloy coating microstructure10.1007/s12540-015-5411-9 ↗
51. Corrosion behaviour of AA6082 Al-Mg-Si alloy extrusion: Recrystallized and non-recrystallized structures10.1016/j.corsci.2018.08.047 ↗
52. Corrosion behaviour of AA6082 Al-Mg-Si alloy extrusion: The influence of quench cooling rate10.1016/j.corsci.2019.01.030 ↗
53. Effect of Sn on microstructure and corrosion behaviors of Al-Mg-Si alloys10.1016/j.matchar.2019.109836 ↗
54. Effect of Ag addition on the precipitation evolution and interfacial segregation for Al-Mg-Si alloy10.1016/j.actamat.2019.09.015 ↗