journal article·2020-08

Investigation of CMAS resistance of sacrificial plasma-sprayed mullite-YSZ protective layer on 8YSZ thermal barrier coating

Huanjie Fang, Weize Wang, Jibo Huang, Dongdong Ye

Corrosion Science· Volume 173
Publisher page

Abstract

Abstract A double-ceramic-layer (DCL) plasma-sprayed YSZ coating comprised of a mullite-YSZ protective layer towards suppressing CMAS attack was prepared in this study. The resistance of DCL coating to molten CMAS at 1300 °C was systematically investigated through phase structure as well as microstructural analysis. It was clearly revealed that the DCL coating exhibited an enhanced CMAS resistance owing to the formation of CaAl2Si2O8 layer. After 4 hours of exposure, YSZ coatings have been significantly penetrated (at least 250 μm), whereas correspondingly no CMAS was found in DCL coatings; the penetration depth in DCL coatings increased to approximately 100 μm as the duration last up to 12 h. In addition, the DCL coating performed a larger contact angle than that of YSZ coatings within the same time, promoting the resistance to CMAS.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Advanced ceramic materials synthesis · Nuclear Materials and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (46)

Show source-provided references
1. Some recent trends in research and technology of advanced thermal barrier coatings10.1016/S1270-9638(02)00003-2 ↗
2. Overview on advanced thermal barrier coatings10.1016/j.surfcoat.2010.08.151 ↗
3. Thermal-barrier coatings for more efficient gas-turbine engines10.1557/mrs.2012.232 ↗
4. Lifetime and failure modes of plasma sprayed thermal barrier coatings in thermal gradient rig tests with simultaneous CMAS injection10.1016/j.surfcoat.2017.04.071 ↗
5. Investigation of the resistance of open-column-structured PS-PVD TBCs to erosive and high-temperature corrosive attack10.1016/j.surfcoat.2017.05.003 ↗
6. Environmental degradation of thermal barrier coatings by molten deposits10.1557/mrs.2012.230 ↗
7. Microstructure and thermo-physical properties of yttria stabilized zirconia coatings with CMAS deposits10.1016/j.jeurceramsoc.2011.04.006 ↗
8. Step-by-step investigation of degradation mechanisms induced by CMAS attack on YSZ materials for TBC applications10.1016/j.surfcoat.2013.08.055 ↗
9. Tailoring the EB-PVD columnar microstructure to mitigate the infiltration of CMAS in 7YSZ thermal barrier coatings10.1016/j.jeurceramsoc.2016.07.027 ↗
10. A comparison between the erosion behaviour of thermal spray and electron beam physical vapour deposition thermal barrier coatings10.1016/S0043-1648(99)00214-8 ↗
11. Evaluation of plasma sprayed YSZ thermal barrier coatings with the CMAS deposits infiltration using impedance spectroscopy10.1016/j.pnsc.2011.12.007 ↗
12. Novel thermal barrier coatings that are resistant to high-temperature attack by glassy deposits10.1016/j.actamat.2007.08.028 ↗
13. Plasma sprayed nanostructured GdPO4 themral barrier coatings: preparation, microstructure and CMAS corrosion resistance10.1111/jace.14924 ↗
14. Impermeable CeO2 overlay for the protection of plasma sprayed YSZ thermal barrier coating from molten sulfate-vanadate salts10.1016/j.surfcoat.2018.11.048 ↗
15. Molten silicate interactions with plasma sprayed thermal barrier coatings: role of materials and microstructure10.1016/j.jeurceramsoc.2019.01.023 ↗
16. Adsorbability and spreadability of calcium-magnesium-alumino-silicate (CMAS) on Al-modified 7YSZ thermal barrier coating10.1016/j.ceramint.2016.09.106 ↗
17. Investigation of CMAS resistance of sacrificial suspension sprayed alumina topcoats on EB-PVD 7YSZ layers
18. EB-PVD alumina (Al2O3) as a top coat on 7YSZ TBCs against CMAS/VA infiltration: deposition and reaction mechanisms10.1016/j.jeurceramsoc.2018.03.027 ↗
19. Corrosion resistant plasma sprayed (Y0.8Gd0.2)3Al5O12/YSZ thermal barrier coatings towards molten calcium-magnesium-alumina-silicate10.1016/j.ceramint.2019.01.114 ↗
20. Hot corrosion behaviour of La2(Zr0.7Ce0.3)2O7 thermal barrier coating ceramics exposed to molten calcium magnesium aluminosilicate at different temperatures10.1016/j.corsci.2015.08.031 ↗
21. Hot corrosion behavior of LaMgAl11O19 ceramic coated with molten CMAS deposits at temperature of 1250 °C in air10.1016/j.jallcom.2016.05.272 ↗
22. 2ZrO2·Y2O3 thermal barrier coatings resistant to degradation by molten CMAS: part I, optical basicity considerations and processing10.1111/jace.13210 ↗
23. Hot corrosion behavior of BaLa2Ti3O10 exposed to calcium-magnesium-alumina-silicate at elevated temperatures10.1016/j.ceramint.2018.03.021 ↗
24. Corrosion resistance and thermal-mechanical properties of ceramic pellets to molten calcium-magnesium-alumina-silicate (CMAS)10.1016/j.ceramint.2019.06.223 ↗
25. Structure and properties of mullite—a review10.1016/j.jeurceramsoc.2007.03.017 ↗
26. Defects/CMAS corrosion resistance relationship in plasma sprayed YPSZ coating10.1016/j.jallcom.2016.10.074 ↗
27. Thermal cycling performance of La2Ce2O7/50 vol.%YSZ composite thermal barrier coating with CMAS corrosion10.1016/j.jeurceramsoc.2018.02.025 ↗
28. Plasma-sprayed thermal barrier coatings with enhanced splat bonding for CMAS and corrosion protection10.1007/s11666-015-0345-9 ↗
29. Thermochemical interaction of thermal barrier coatings with molten CaO-MgO-Al2O3-SiO2 (CMAS) deposits10.1111/j.1551-2916.2006.01209.x ↗
30. Thermal-gradient testing of thermal barrier coatings under simultaneous attack by molten glassy deposits and its mitigation10.1016/j.surfcoat.2010.02.026 ↗
31. Comparison of CMAS corrosion and sintering induced microstructural characteristics of APS thermal barrier coatings10.1016/j.jmst.2018.09.046 ↗
32. The effect of sintering additives on the hydrothermal and corrosive degradation of Y-TZP10.4028/www.scientific.net/KEM.113.199 ↗
33. Influence of sintering aids on sintering and mechanical properties of 3Y-TZP/Al2O3 (40 vol%) composite10.1023/A:1019975002162 ↗
34. Densification and mechanical properties of B4C with Al2O3 as a sintering aid10.1111/j.1151-2916.2000.tb01647.x ↗
35. Thermochemical interaction of thermal barrier coatings with molten CaO-MgO-Al2O3-SiO2 (CMAS) deposits10.1111/j.1551-2916.2006.01209.x ↗
36. Calcium-rich CMAS corrosion induced microstructure development of thermal barrier coatings10.1016/j.surfcoat.2017.05.076 ↗
37. Effect of thermal exposure on hardness and Young’s modulus of EB-PVD yttria-partially-stabilized zirconia thermal barrier coatings10.1016/j.ceramint.2005.01.018 ↗
38. The effect of heat treatment on the stiffness of zirconia top coats in plasma-sprayed TBCs10.1016/S1359-6454(01)00065-9 ↗
39. Novel thermal barrier coatings repel and resist molten silicate deposits10.1016/j.scriptamat.2018.12.028 ↗
40. High temperature wettability between CMAS and YSZ coating with tailored surface microstructures10.1016/j.matlet.2018.06.066 ↗
41. Effects of roughness on the wettability of high temperature wetting system10.1016/j.surfcoat.2015.12.092 ↗
42. Hot corrosion behavior and wettability of calcium–magnesium–alumina–silicate (CMAS) on LaTi2Al9O19 ceramic10.1016/j.corsci.2019.108199 ↗
43. A method for correcting the contact angle from the θ/2 method10.1016/S0927-7757(03)00064-5 ↗
44. Viscosity of magmatic liquids: a model10.1016/j.epsl.2008.03.038 ↗
45. An estimation of the surface tension for silicate glass melts at 1400 °C using statistical analysis
46. CMAS resistance characteristics of LaPO4/YSZ thermal barrier coatings at 1250 °C-1350 °C10.1016/j.corsci.2019.04.014 ↗