journal article·2021-02

Crystallization-dependent transition of corrosion resistance of an Fe-based bulk metallic glass under hydrostatic pressures

Zhen Gan, Cheng Zhang, Zhan-Rong Zhang, Zheng-Jie Chen, Lin Liu

Corrosion Science· Volume 179
Publisher page

Abstract

Abstract We reported a crystallization-dependent transition of corrosion resistance of an Fe-based bulk metallic glass (BMG) under hydrostatic pressures. When the crystallized volume fracture (Vf) is below a critical value of 30 %, the corrosion resistance remains almost unaffected as that in the as-cast BMG; when the Vf is higher than this critical value, the corrosion resistance decreases, and the passivation dynamics changes significantly. The underlying mechanism is understood by the competitions among the passivation, pitting kinetics, and micro galvanic effects. When Vf was above 30 %, a tri-phase structure formed such that micro galvanic effect induced stable pitting starts to dominate the corrosion.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metallic Glasses and Amorphous Alloys · Glass properties and applications · Surface Roughness and Optical Measurements

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (66)

Show source-provided references
1. Microstructural studies of crystallization of a Zr-based bulk metallic glass10.1016/S1359-6454(03)00225-8 ↗
2. Processing of bulk metallic glass10.1002/adma.200902776 ↗
3. Nanoscale size effects in crystallization of metallic glass nanorods10.1038/ncomms9157 ↗
4. Effect of a controlled volume fraction of dendritic phases on tensile and compressive ductility in La-based metallic glass matrix composites10.1016/j.actamat.2004.05.025 ↗
5. Flash Joule heating for ductilization of metallic glasses10.1038/ncomms8932 ↗
6. Origin of pressure-induced crystallization of Ce75Al25 metallic glass10.1038/ncomms7493 ↗
7. Stress-driven crystallization via shear-diffusion transformations in a metallic glass at very low temperatures10.1103/PhysRevB.91.214103 ↗
8. Effect of crystallinity on the impact toughness of a La-based bulk metallic glass10.1016/S1359-6454(00)00052-5 ↗
9. On-demand release of corrosion-inhibiting ions from amorphous Al-Co-Ce alloys10.1038/nmat1451 ↗
10. On the microstructure-tensile property correlation in bulk metallic glass matrix composites with crystalline dendrites10.1016/j.actamat.2012.06.032 ↗
11. Compelling rejuvenated catalytic performance in metallic glasses
12. Element-resolved corrosion analysis of stainless-type glass-forming steels10.1126/science.1230081 ↗
13. Comparison of the corrosion of bulk amorphous steel with conventional steel10.1016/j.corsci.2009.09.016 ↗
14. Nanocrystalline composites with high strength obtained in Zr-Ti-Ni-Cu-Al bulk amorphous alloys10.1063/1.124254 ↗
15. Critical crystallization for embrittlement in metallic glasses10.1103/PhysRevLett.115.265502 ↗
16. Experimental evidence for the critical size of heterogeneity areas for pitting corrosion of Cr-Zr alloys in 6 M HCl10.1016/S0010-938X(97)00107-8 ↗
17. Localized corrosion of Al90Fe5Gd5 and Al87Ni8.7Y4.3 alloys in the amorphous, nanocrystalline and crystalline states: resistance to micrometer-scale pit formation10.1016/S0013-4686(02)00830-7 ↗
18. Corrosion behaviors of bulk metallic glasses Fe66.7C7.0Si3.3B5.5P8.7Cr2.3Al2.0Mo4.5 having different crystal volume fractions10.1016/j.matchemphys.2008.05.061 ↗
19. Devitrification of Fe-based amorphous metal SAM 1651 and the effect of heat-treatment on corrosion behavior10.1149/1.3148325 ↗
20. Structure inhibited pit initiation in a Ni-Nb metallic glass10.1016/j.corsci.2009.12.014 ↗
21. Effects of crystallization on the corrosion resistance of Fe-based amorphous coatings10.1016/j.corsci.2012.02.003 ↗
22. Simulated body fluid electrochemical response of Zr-based metallic glasses with different degrees of crystallization10.1016/j.msec.2013.06.007 ↗
23. Crystallization, phase evolution and corrosion of Fe-based metallic glasses: an atomic-scale structural and chemical characterization study10.1016/j.actamat.2014.02.027 ↗
24. Corrosion resistance of Fe-Cr-based amorphous alloys: an overview10.1016/j.jnoncrysol.2016.04.009 ↗
25. Thermally induced structure evolution on the corrosion behavior of Al-Ni-Y amorphous alloys10.1016/j.corsci.2018.08.046 ↗
26. A review of studies on corrosion of metals and alloys in deep-sea environment10.1016/j.oceaneng.2014.05.003 ↗
27. A stochastic analysis of the effects of hydrostatic pressure on the pit corrosion of Fe-20Cr alloy10.1016/j.electacta.2009.02.010 ↗
28. Effect of hydrostatic pressure on the corrosion behavior of Ni-Cr-Mo-V high strength steel10.1016/j.corsci.2010.04.025 ↗
29. Effect of hydrostatic pressure on the corrosion behavior of a low alloy steel10.1149/2.040303jes ↗
30. Degradation in pitting resistance of 316L stainless steel under hydrostatic pressure10.1016/j.electacta.2016.05.169 ↗
31. Electrochemical corrosion behavior of TC11 alloy in sulfate solution at high temperature and high pressure10.20964/2017.06.90 ↗
32. Hydrostatic pressure effects on corrosion behavior of X70 pipeline steel in a simulated deep-sea environment10.1016/j.jelechem.2018.05.010 ↗
33. Influence of hydrostatic pressure on the corrosion behavior of 90/10 copper-nickel alloy tube under alternating dry and wet condition10.1016/j.corsci.2018.10.036 ↗
34. New understanding of the effect of hydrostatic pressure on the corrosion of Ni-Cr-Mo-V high strength steel10.1016/j.corsci.2013.04.013 ↗
35. Effect of hydrostatic pressure on the corrosion behavior of HVOF-sprayed Fe-based amorphous coating10.1016/j.jallcom.2018.05.100 ↗
36. Design of Fe-based bulk metallic glasses with improved wear resistance10.1021/acsami.8b11561 ↗
37. Enhanced mechanical properties due to structural changes induced by devitrification in Fe-Co-B-Si-Nb bulk metallic glass10.1016/j.actamat.2010.07.047 ↗
38. The corrosion behavior of amorphous and nanocrystalline Fe73.5Cu1Nb3Si15.5B7 alloy10.1016/j.corsci.2011.03.023 ↗
39. A highly efficient and self-stabilizing metallic glass catalyst for electrochemical hydrogen generation10.1002/adma.201603880 ↗
40. Kinetics and crystallization path of a Fe-based metallic glass alloy10.1016/j.actamat.2017.01.031 ↗
41. Crystal growth limitation as a critical factor for formation of Fe-based bulk metallic glasses10.1016/j.actamat.2014.09.025 ↗
42. Classification of bulk metallic glasses by atomic size difference, heat of mixing and period of constituent elements and its application to characterization of the main alloying element10.2320/matertrans.46.2817 ↗
43. Evaluation of corrosion rate from polarization curves not exhibiting a Tafel region10.1016/j.corsci.2005.06.014 ↗
44. In situ EC-AFM study of the effect of nanocrystals on the passivation and pit initiation in an Al-based metallic glass10.1016/j.corsci.2014.02.005 ↗
45. The effect of electrode size and surface heterogeneity on electrochemical properties of ultrananocrystalline diamond microelectrode10.1016/j.jelechem.2015.08.016 ↗
46. The analysis of electrode impedances complicated by the presence of a constant phase element10.1016/S0022-0728(84)80324-1 ↗
47. Technical note: concerning the conversion of the constant phase element parameter Y0 into a capacitance10.5006/1.3280607 ↗
48. Enabling long term monitoring of dopamine using dimensionally stable ultrananocrystalline diamond microelectrodes10.1088/2053-1591/3/9/094001 ↗
49. Surface fouling of ultrananocrystalline diamond microelectrodes during depamine detection: improving lifetime via electrochemical cycling10.1021/acschemneuro.8b00257 ↗
50. Effect of high temperature on the corrosion behavior and passive film composition of 316L stainless steel in high H2S-containing environment10.1016/j.corsci.2020.108844 ↗
51. Electrochemical behaviour of the MA8 Mg alloy in minimum essential medium10.1016/j.corsci.2020.108552 ↗
52. Metastable pitting of aluminum and criteria for the transition to stable pit growth10.1149/1.2059275 ↗
53. Influence of incorporated Mo and Nb on the Mott-Schottly behavior of anodic films formed on AISI 304L10.1016/j.corsci.2010.04.021 ↗
54. Wear behavior and corrosion properties of Fe-based thin film metallic glasses10.1016/j.jallcom.2015.07.256 ↗
55. Differences in pitting growth kinetics between Zr60Ni25Al15 and Zr60Cu25Al15 metallic glasses exposed to a 0.6 M NaCl aqueous solution10.1016/j.corsci.2017.09.007 ↗
56. Understanding multi-element alloy passivation in acidic solution using operando methods10.1016/j.elecom.2017.05.015 ↗
57. Localized corrosion behavior of a single-phase non-equimolar high entropy alloy10.1016/j.electacta.2019.03.104 ↗
58. Passivation of a corrosion resistant high entropy alloy in non-oxidizing sulfate solution10.1016/j.actamat.2018.10.026 ↗
59. Constant-phase-element behavior caused by resistivity distributions in films10.1149/1.3499565 ↗
60. Understanding the relation between pitting corrosion resistance and phase fraction of S32101 duplex stainless steel10.1016/j.corsci.2019.01.001 ↗
61. Passive films at the nanoscale10.1016/j.electacta.2012.03.158 ↗
62. Designing for high corrosion-resistant high nitrogen martensitic stainless steel based on DFT calculation and pressurized metallurgy method10.1016/j.corsci.2019.07.007 ↗
63. Ab initio development of a high-strength corrosion-resistant austenitic steel10.1016/j.actamat.2008.06.021 ↗
64. Acid corrosion process of Fe-based bulk metallic glass10.1016/j.corsci.2012.05.004 ↗
65. Effect of SiC particulates on the corrosion behavior of extruded AZ91/SiCp composites during the early stage of exposure10.1149/2.0631514jes ↗
66. Influence of hydrostatic pressure on the thermodynamics and kinetics of metal corrosion