Effect of oxygen on corrosion of an alumina-forming duplex steel in static liquid lead-bismuth eutectic at 550 °C
Source abstract
Abstract
Abstract Corrosion in static liquid lead–bismuth eutectic (LBE) with varying oxygen content is investigated at 550 °C on an alumina-forming duplex steel which contains both austenite and ferrite phases. The duration of the tests is about 1000 h. For oxygen concentration ranging from 10−12 to 10-8 % by mass, the steel shows preferential nickel dissolution and LBE penetration. The degradation of the ferrite is delayed in contrast to the austenitic part of the duplex microstructure. At 10-6 % oxygen, the steel is protected from LBE attack due to the formation of a thin oxide layer rich in aluminum. The precipitation of NiAl in the steel does not compromise the formation of Al-rich oxide at this oxygen concentration.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Nuclear materials and radiation effects · Nuclear Materials and Properties · Nuclear reactor physics and engineering
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. Materials challenges in nuclear energy10.1016/j.actamat.2012.11.004 ↗
2. Heavy liquid metal corrosion of structural materials in advanced nuclear systems
3. Assessment of liquid metal technology status and research paths for their use as efficient heat transfer fluids in solar central receiver systems10.1016/j.solener.2013.03.025 ↗
4. 2017 · 1
5. Investigation on oxygen controlled liquid lead corrosion of surface treated steels10.1016/S0022-3115(99)00211-1 ↗
6. Corrosion behavior of Fe-14Cr-2W and Fe-9Cr-2W ODS steels in stagnant liquid Pb with different oxygen concentration at 550 and 650°C10.1016/j.jnucmat.2013.07.040 ↗
7. Influence of composition and microstructure on the corrosion behavior of different Fe-Cr-Al alloys in molten LBE10.1016/j.jnucmat.2011.11.049 ↗
8. Corrosion in iron and Steel T91 caused by flowing lead–bismuth eutectic at 400 °C and 10−7 mass% dissolved oxygen10.1115/1.4040937 ↗
9. Behaviour of pre-stressed T91 and ODS steels exposed to liquid lead-bismuth eutectic10.1016/j.corsci.2017.12.005 ↗
10. Corrosion resistance of Si- and Al-rich steels in flowing lead–bismuth10.1016/j.jnucmat.2006.05.019 ↗
11. Silicon-containing ferritic/martensitic steel after exposure to oxygen-containing flowing lead–bismuth eutectic at 450 and 550 °C10.1016/j.jnucmat.2015.11.058 ↗
12. Development of Al added high-Cr ODS steels for fuel cladding of next generation nuclear systems10.1016/j.jnucmat.2010.12.300 ↗
13. Evaluation of Pb-17Li compatibility of ODS Fe-12Cr-5Al alloys10.1016/j.jnucmat.2016.07.017 ↗
14. Effects of minor alloy additions and oxidation temperature on protective alumina scale formation in creep-resistant austenitic stainless steels10.1016/j.scriptamat.2007.08.032 ↗
15. Co-optimization of wrought alumina-forming austenitic stainless steel composition ranges for high-temperature creep and oxidation/corrosion resistance10.1016/j.msea.2013.10.014 ↗
16. Evaluation of Mn substitution for Ni in alumina-forming austenitic stainless steels10.1016/j.msea.2009.06.043 ↗
17. Co-optimization of wrought alumina-forming austenitic stainless steel composition ranges for high-temperature creep and oxidation/corrosion resistance10.1016/j.msea.2013.10.014 ↗
18. Research progress on compatibility of liquid metal and iron-based alloy in lead cooled energy systems
19. Corrosion behavior of austenitic steels 1.4970, 316L and 1.4571 in flowing LBE at 450 and 550 °C with 10−7 mass% dissolved oxygen10.1016/j.jnucmat.2014.08.024 ↗
20. Long term corrosion on T91 and AISI1 316L steel in flowing lead alloy and corrosion protection barrier development: experiments and models10.1016/j.jnucmat.2011.04.028 ↗
21. Long term corrosion resistance of alumina forming austenitic stainless steels in liquid lead10.1016/j.jnucmat.2015.03.011 ↗
22. Dissolution and oxidation behaviour of various austenitic steels and Ni rich alloys in lead-bismuth eutectic at 520 °C10.1016/j.jnucmat.2015.11.005 ↗
23. Microstructural evolution and mechanical properties of an Fe-18Ni-16Cr-4Al base alloy during aging at 950°C10.1007/s12613-016-1240-1 ↗
24. Aspects of minimizing steel corrosion in liquid lead-alloys by addition of oxygen10.1016/j.nucengdes.2011.09.002 ↗
25. Schroer · 2007
26. Selective leaching of nickel and chromium from Type 316 austenitic steel in oxygen-containing lead-bismuth eutectic (LBE)10.1016/j.corsci.2014.03.016 ↗
27. Long-term service of austenitic steel 1.4571 as a container material for flowing lead-bismuth eutectic10.1016/j.jnucmat.2011.07.026 ↗
28. Quantification of the long-term performance of steels T91 and 316L in oxygen-containing flowing lead-bismuth eutectic at 550°C10.1115/1.4000364 ↗
29. Effect of oxygen concentration in static Pb–Bi eutectic on corrosion mode of aluminum-alloyed austenitic steels at 550 °C for 1000 h10.4028/www.scientific.net/MSF.1024.79 ↗
30. Oxidation and dissolution of iron in flowing lead-bismuth eutectic at 450°C10.1016/j.corsci.2012.04.022 ↗
31. Oxidation studies of Fe10CrAl-RE alloys exposed to Pb at 550°C for 10,000h10.1016/j.jnucmat.2013.07.023 ↗
32. Oxide scales formed on Fe-Cr-Al-based model alloys exposed to oxygen containing molten lead10.1016/j.jnucmat.2013.02.044 ↗
33. Oxide scale formation on 316L and FeCrAl steels exposed to oxygen controlled static LBE at temperatures up to 800°C10.1016/j.solmat.2015.09.007 ↗
34. Composition, microstructure, and water vapor effects on internal/external oxidation of alumina-forming austenitic stainless steel10.1007/s11085-009-9161-2 ↗
35. Increasing the upper temperature oxidation limit of alumina forming austenitic stainless steels in air with water vapor10.1007/s11085-011-9237-7 ↗
36. NiAl alloys for turbine airfoils