Revealing the oxidation mechanism of 310S stainless steel in supercritical water via high-resolution characterization
Source abstract
Abstract
This work studied the surface oxide scale of 310S stainless steel exposed to 650 °C supercritical water for 1000 h. The oxide scale showed a complex structure with an outer oxide layer, an inner oxide layer, and a much thinner Cr2O3 layer. The outer oxide layer consisted of Fe2O3, NiFe2O4 and NiO. Fe-Cr-Ni spinel was identified in the inner oxide layer due to internal oxidation. Transition from internal to external oxidation occurred at the metal-oxide interface, resulting in the formation of a protective Cr2O3 layer. The formation mechanisms of each oxide layer were discussed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Nuclear Materials and Properties · Subcritical and Supercritical Water Processes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (49)
Show source-provided references
1. Corrosion and stress corrosion cracking in supercritical water10.1016/j.jnucmat.2007.05.017 ↗
2. Corrosion issues in current and next generation nuclear reactors
3. Selection and corrosion evaluation tests of candidate SCWR fuel cladding materials10.1016/j.nucengdes.2011.08.086 ↗
4. Corrosion resistance of candidate cladding materials for supercritical water reactor10.1016/j.anucene.2018.12.007 ↗
5. Characterization of oxide scales grown on alloy 310S stainless steel after long term exposure to supercritical water at 500 °C10.1016/j.matchar.2016.09.013 ↗
6. A study on the corrosion and stress corrosion cracking susceptibility of 310-ODS steel in supercritical water10.1016/j.jnucmat.2018.11.016 ↗
7. Oxidation behavior of UHP Fe-based model alloy and SUS310S steel in superheated steam and supercritical water conditions
8. Internal oxidation and crack susceptibility of alloy 310S stainless steel after long term exposure to supercritical water at 500 degrees C10.1016/j.supflu.2016.09.007 ↗
9. Supercritical water-cooled reactor materials – summary of research and open issues10.1016/j.pnucene.2014.02.008 ↗
10. Materials assessment for the Canadian SCWR core concept10.1007/s11837-015-1758-0 ↗
11. Microstructural changes and corrosion resistance of AISI 310S steel exposed to 600–800 °C10.1016/j.matchar.2008.12.005 ↗
12. Time–temperature-sensitization diagrams and critical cooling rates of different nitrogen containing austenitic stainless steels10.1016/j.jnucmat.2010.01.003 ↗
13. Stress corrosion crack growth behavior of type 310S stainless steel in supercritical water10.5006/2775 ↗
14. Corrosion of austenitic alloys in supercritical water10.5006/1.3278237 ↗
15. Effect of Fe on corrosion of Ni-20Cr and Ni-30Cr alloys in wet CO2 gas at 650 and 700 degrees C10.1016/j.corsci.2019.04.007 ↗
16. Corrosion properties of candidate materials in supercritical water oxidation process
17. Oxidation of ferritic and ferritic-martensitic steels in flowing and static supercritical water10.1016/j.corsci.2015.10.017 ↗
18. Understanding the surface oxide evolution of T91 ferritic-martensitic steel in supercritical water through advanced characterization10.1016/j.actamat.2020.05.016 ↗
19. Influence of temperature on the oxidation behaviour of a ferritic-martensitic steel in supercritical water10.1016/j.corsci.2016.10.020 ↗
20. EFTEM and EELS analysis of the oxide layer formed on HCM12A exposed to SCW10.1016/j.jnucmat.2012.06.017 ↗
21. Effect of alloy composition and exposure conditions on the selective oxidation behavior of ferritic Fe-Cr and Fe-Cr-X alloys10.1007/s11085-010-9215-5 ↗
22. High-resolution characterization of the internal and external oxidation of austenitic alloys in supercritical water10.1016/j.scriptamat.2021.113814 ↗
23. Effect of exposure temperature on oxidation of austenitic steel HR3C in supercritical water10.1007/s11085-018-9879-9 ↗
24. Oxidation behavior of ferritic-martensitic and ODS steels in supercritical water10.1016/j.jnucmat.2012.03.009 ↗
25. The mechanism of high-temperature aqueous corrosion of stainless-steels10.1016/0010-938X(91)90125-9 ↗
26. The mechanism of oxide film formation on austenitic stainless steels in high temperature water10.1016/S0010-938X(97)00140-6 ↗
27. Corrosion behavior of Alloy 690 in aerated supercritical water10.1016/j.corsci.2012.10.001 ↗
28. Corrosion behavior of Alloy 690 in aerated supercritical water10.1016/j.corsci.2012.10.001 ↗
29. Effect of exposure temperature on the corrosion behaviors of TP347H austenitic stainless steel in supercritical water10.1016/j.corsci.2019.108188 ↗
30. Microstructural investigation of the nodular corrosion of 304NG stainless steel in supercritical water10.1016/j.corsci.2020.108652 ↗
31. A research on the corrosion and stress corrosion cracking susceptibility of 316L stainless steel exposed to supercritical water10.1016/j.corsci.2017.08.027 ↗
32. Corrosion behavior of alloy 316L stainless steel after exposure to supercritical water at 500 degrees C for 20,000h10.1016/j.supflu.2017.03.022 ↗
33. Diffusion in Fe·Ni·Cr alloys with an F.C.C. lattice10.1016/0025-5416(85)90069-2 ↗
34. Ternary diffusion in FCC phase of Fe-Ni-Cr alloy system at 1223 K10.2320/matertrans1989.32.1034 ↗
35. L. Tan, T.R. Allen, Y. Yang, Corrosion of austenitic stainless steels and nickel-base alloys in supercritical water and novel control methods, in: Green Corrosion Chemistry and Engineering, 2011, pp. 211–242.10.1002/9783527641789.ch8 ↗
36. The nature of high temperature oxidation
37. Rapid nickel diffusion in cold-worked carbon steel at 320–450 °C10.1080/14786435.2015.1091108 ↗
38. Acceleration of nickel diffusion by high tensile stress in cold-worked type 316 stainless steel at 450°C10.1080/14786435.2018.1495852 ↗
39. Water vapor effects on corrosion of Fe-Cr and Fe-Cr-Ni alloys containing silicon in CO2 gas at 818 A degrees C10.1007/s11085-015-9536-5 ↗
40. Internal oxidation of Ni-Al and Ni-Al-Si alloys at the dissociation pressure of Nio10.1016/0956-7151(94)90292-5 ↗
41. Accelerated stress corrosion crack initiation of alloys 600 and 690 in hydrogenated supercritical water10.1007/s11661-016-3898-4 ↗
42. Characteristics of oxidation and oxygen penetration of alloy 690 in 600 degrees C aerated supercritical water10.1016/j.jmst.2016.11.001 ↗
43. Corrosion mechanism of a Ni-based alloy in supercritical water: impact of surface plastic deformation10.1016/j.corsci.2015.06.032 ↗
44. L.Z. Tan, T.R. Allen, Y. Yang, Corrosion of austenitic stainless steels and nickel-base alloys in supercritical water and novel control methods, in: Green Corrosion Chemistry and Engineering: Opportunities and Challenges, 2012, pp. 211–242.10.1002/9783527641789.ch8 ↗
45. Corrosion behavior of alloy C-276 in supercritical water
46. New insights into the oxidation mechanisms of a Ferritic-Martensitic steel in high-temperature steam10.1016/j.actamat.2020.05.052 ↗
47. Microstructural understanding of the oxidation of an austenitic stainless steel in high-temperature steam through advanced characterization10.1016/j.actamat.2020.05.010 ↗
48. Theoretical analysis of the diffusion processes determining the oxidation rate of alloys10.1149/1.2779605 ↗
49. Competition between thermodynamics, kinetics and growth mode in the early-stage oxidation of an equimolar CoCrFeNi alloy10.1016/j.actamat.2020.06.056 ↗