journal article·2018-08Open access

The effect of high-temperature water chemistry and dissolved zinc on the cobalt incorporation on type 316 stainless steel oxide

Samuel Holdsworth, Fabio Scenini, M. Grace Burke, Giacomo Bertali, Tsuyoshi Ito, Yoichi Wada, Hideyuki Hosokawa, Nobuyuki Ota, Makoto Nagase

Corrosion Science· Volume 140

Abstract

Oxidation tests on Type 316 stainless steel were performed under hydrogen water chemistry and normal water chemistry for 500 hours with continuous injection of a 59Co solution with and without 5 ppb of Zn injection. The present paper identifies the resultant oxides, analysed using analytical electron microscopy and complementary surface microstructural characterisation techniques. Zn injection has been shown to reduce Co incorporation in the inner oxide layer under both water chemistry conditions. The secondary effects of Zn injection on the oxide film growth have also been investigated and discussed.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Corrosion Behavior and Inhibition · Electronic and Structural Properties of Oxides

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (31)

Show source-provided references
1. In situ measurement of corrosion of type 316L stainless steel in 553 K pure water via the electrical resistance of a thin wire10.1080/00223131.2012.730899 ↗
2. On the interaction between fuel crud and water chemistry in nuclear power plants
3. A review of corrosion product transport and radiation field buildup in boiling water reactors10.1016/j.pnucene.2008.05.005 ↗
4. Ishida · 2010 · 1
5. Recent developments in LWR radiation field control10.1016/0149-1970(87)90021-7 ↗
6. Analyses of fuel crud and coolant-borne corrosion products in normal water chemistry BWRs10.1016/j.jnucmat.2011.08.032 ↗
7. Investigation of cobalt deposition behavior with zinc injection on stainless steel under BWR conditions10.1080/18811248.2004.9715533 ↗
8. The mechansim of high temperature aqueous corrosion of stainless steel10.1016/0010-938X(91)90125-9 ↗
9. Microstructural characterization of SCC crack tip and oxide film for SUS 316 stainless steel in simulated PWR primary water at 320°C10.1080/18811248.2005.9726383 ↗
10. Effect of surface preparation on the corrosion of austenitic stainless steel 304L in high temperature steam and simulated PWR primary water10.1016/j.corsci.2011.12.007 ↗
11. The radiation chemistry of nuclear reactor decontaminating reagents
12. The mechanisms of corrosion product transport and their investigation in high temperature water loops10.5006/0010-9312-35.3.89 ↗
13. effects of noble metal deposition upon corrosion behavior of structural materials in nuclear power plants, (I) effect of noble metal deposition with an oxide film on type 304 stainless steel10.1080/18811248.2004.9726449 ↗
14. Analysis of oxide film formed on type 304 stainless steel in 288 C water containing oxygen, hydrogen, and hydrogen peroxide10.5006/1.3283969 ↗
15. Characterization of the oxide film formed on type 316 stainless steel in 288°C water in cyclic normal and hydrogen water chemistries10.5006/1.3293562 ↗
16. Effects of hydrogen peroxide on corrosion of stainless steel, (V) characterization of oxide film with multilateral surface analyses10.1080/18811248.2006.9711173 ↗
17. A Raman study of the systems Fe3-xCrxO4 and Fe2-xCrxO310.1016/0022-4596(89)90245-4 ↗
18. Lister · 2012
19. Investigation of cobalt buildup behavior and suppression by zinc injection on stainless steel under HWC conditions using simultaneous continuous measurements of corrosion and cobalt buildup10.1080/00223131.2014.967323 ↗
20. The thermodynamics of cation distributions in simple spinels10.1016/0022-1902(67)80008-3 ↗
21. Influence of Zn injection on characteristics of oxide film on 304 stainless steel in borated and lithiated high temperature water10.1016/j.corsci.2011.06.011 ↗
22. T. Saito, K. Ichikawa, H. Ishimaru, M. Aizawa, Y. Sato, and S. Morita, Radiation exposure reduction technologies for a Japanese Advanced BWR (Dose Rate Reduction Experience in Shika Unit 2), Nucl. Plant Chem. Conferance.
23. Couvant · 2013
24. High temperature dissolution of oxide deposits formed over structural materials under PHWR and BWR chemistry conditions10.1016/j.pnucene.2012.04.003 ↗
25. Improving the oxidation resistance of 316L stainless steel in simulated pressurized water reactor primary water by electropolishing treatment10.1016/j.jnucmat.2015.09.029 ↗
26. Growth behavior of surface oxide layer on SUS316L stainless steel at the early stage of exposure to 288°C water10.2320/matertrans.M2011200 ↗
27. Development of an in situ Raman spectroscopic system for surface oxide films on metals and alloys in high temperature water10.1016/j.nucengdes.2004.12.002 ↗
28. Zinc treatment effects on corrosion behavior of 304 stainless steel in high temperature, hydrogenated water
29. Marble · 1994 · 1
30. Betova · 2011
31. Synergy effect of simultaneous zinc and nickel addition on cobalt deposition onto stainless steel in oxygenated high temperature water10.1080/18811248.2003.9715344 ↗