Microstructure and corrosion behaviour of wire arc additive manufactured AA2024 alloy thin wall structure
Source abstract
Abstract
In the present work, the microstructure and corrosion behaviour of wire arc additive manufactured (WAAM) AA2024 alloy thin wall structure are investigated. Three distinctive zones are present in the WAAM structure, including melt pool zone (MPZ), melt pool border (MPB) and heat affected zone (HAZ). Localized corrosion initiates at the multi-phase lamellar eutectic structure via de-alloying of S-phase (Al2CuMg) intermetallics. MPB is most susceptible to localized corrosion due to its relatively high volume fraction of eutectic S-phase resulted from alloying elements segregation during solidification.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (45)
Show source-provided references
1. Additive manufacturing of metals10.1016/j.actamat.2016.07.019 ↗
2. Corrosion behavior of alsi10mg alloy produced by additive manufacturing (am) vs. its counterpart gravity cast alloy10.3390/met6070148 ↗
3. Wire arc additive manufacturing of aluminium alloys: a review
4. Wire arc additive manufacturing10.1179/1743284715Y.0000000073 ↗
5. Effect of heat treatment on corrosion resistance of DMLS AlSi10Mg alloy10.1016/j.electacta.2016.04.157 ↗
6. Additive manufactured AlSi10Mg samples using Selective Laser Melting (SLM): microstructure, high cycle fatigue, and fracture behavior10.1016/j.matdes.2011.07.067 ↗
7. Influence of heat treatments on the corrosion mechanism of additive manufactured AlSi10Mg10.1016/j.corsci.2018.11.038 ↗
8. Oxides, porosity and fatigue performance of AlSi10Mg parts produced by selective laser melting10.1016/j.ijfatigue.2016.06.002 ↗
9. Inoculation treatment of an additively manufactured 2024 aluminium alloy with titanium nanoparticles10.1016/j.actamat.2020.06.026 ↗
10. 3D printing of Aluminium alloys: additive Manufacturing of Aluminium alloys using selective laser melting10.1016/j.pmatsci.2019.100578 ↗
11. Deformation-based additive manufacturing of 7075 aluminum with wrought-like mechanical properties10.1016/j.matdes.2020.109288 ↗
12. Welding and additive manufacturing with nanoparticle-enhanced aluminum 7075 wire10.1016/j.jallcom.2020.154987 ↗
13. 3D printing of high-strength aluminium alloys10.1038/nature23894 ↗
14. The status, challenges, and future of additive manufacturing in engineering
15. On the corrosion of additively manufactured aluminium alloy AA2024 prepared by selective laser melting10.1016/j.corsci.2018.08.019 ↗
16. Selective laser melting of high strength Al–Cu–Mg alloys: processing, microstructure and mechanical properties10.1016/j.msea.2015.12.101 ↗
17. Microstructure evolution of wire-arc additively manufactured 2319 aluminum alloy with interlayer hammering10.1016/j.msea.2020.140168 ↗
18. Laser welding introduced segregation and its influence on the corrosion behaviour of Al-Cu-Li alloy10.1016/j.corsci.2018.02.044 ↗
19. Sames · 2016
20. Grain morphology evolution behavior of titanium alloy components during laser melting deposition additive manufacturing10.1016/j.jallcom.2015.01.256 ↗
21. Corrosion of additively manufactured alloys: a review10.5006/2926 ↗
22. Localized corrosion in AA2024-T351 aluminium alloy: transition from intergranular corrosion to crystallographic pitting10.1016/j.matchar.2017.06.022 ↗
23. Intergranular corrosion of AA6082 Al–Mg–Si alloy extrusion: the influence of trace Cu and grain boundary misorientation10.1016/j.jallcom.2020.157228 ↗
24. Localized corrosion of 2024 T351 aluminium alloy in chloride media10.1016/S0010-938X(98)00116-4 ↗
25. Local dissolution phenomena associated with S phase (Al2CuMg) particles in aluminum alloy 2024-T310.1149/1.1837874 ↗
26. Corrosion behaviour of AA6082 Al-Mg-Si alloy extrusion: the influence of quench cooling rate10.1016/j.corsci.2019.01.030 ↗
27. Corrosion behaviour of 2A97-T6 Al-Cu-Li alloy: the influence of non-uniform precipitation10.1016/j.corsci.2017.12.010 ↗
28. Local corrosion behavior of additive manufactured AlSiMg alloy assessed by SEM and SKPFM10.1149/2.0461702jes ↗
29. On microstructure and early stage corrosion performance of heat treated direct metal laser sintered AlSi10Mg
30. Improved corrosion behavior of ultrafine-grained eutectic Al-12Si alloy produced by selective laser melting10.1016/j.matdes.2018.03.025 ↗
31. Abnormal corrosion behavior of selective laser melted AlSi10Mg alloy induced by heat treatment at 300 °C10.1016/j.jallcom.2019.06.274 ↗
32. Corrosion behavior of selective laser melted AlSi10Mg alloy in NaCl solution and its dependence on heat treatment10.1007/s40195-019-00903-5 ↗
33. Distinction of corrosion resistance of selective laser melted Al-12Si alloy on different planes10.1016/j.jallcom.2018.03.062 ↗
34. Effect of arc mode in cold metal transfer process on porosity of additively manufactured Al-6.3%Cu alloy10.1007/s00170-014-6346-x ↗
35. The influence of build parameters and wire batch on porosity of wire and arc additive manufactured aluminium alloy 231910.1016/j.jmatprotec.2018.07.030 ↗
36. Investigation of dealloying of S phase (Al2CuMg) in AA 2024-T3 aluminium alloy using high resolution 2D and 3D electron imaging10.1016/j.corsci.2015.11.013 ↗
37. Investigation of the de-alloying behaviour of θ-phase (Al2Cu) in AA2024-T351 aluminium alloy10.1016/j.corsci.2016.03.003 ↗
38. Study of localized corrosion in AA2024 aluminium alloy using electron tomography10.1016/j.corsci.2012.02.001 ↗
39. Stable pit formation on AA2024-T3 in a NaCl environment10.1016/j.corsci.2009.08.043 ↗
40. FIB/SEM study of AA2024 corrosion under a seawater drop: part I10.1016/j.corsci.2010.12.004 ↗
41. Effect of partition coefficient on microsegregation during solidification of aluminium alloys10.1007/s12613-014-0999-1 ↗
42. The effect of free-floating dendrites and convection on macrosegregation in direct chill cast aluminum alloys Part II: predictions for Al-Cu and Al-Mg alloys10.1016/S0017-9310(99)00175-1 ↗
43. Precipitates and intermetallic phases in precipitation hardening Al-Cu-Mg-(Li) based alloys10.1179/174328005X14357 ↗
44. Pitting corrosion of aluminium10.1016/S0010-938X(99)00012-8 ↗
45. Grain stored energy and the propagation of IGC in AA2xxx aluminium alloys10.1002/sia.5218 ↗