To mitigate interphase degradation and improve the mechanical and ablation properties of leading edge shaped C/C-ZrC-SiC composites fabricated by reactive melt infiltration, a tailored SiC-C interphase composed of SiC, gas pyrolysis carbon and phenolic resin pyrolysis char was introduced. The SiC-C interphase can effectively protect the carbon fiber from high-temperature melt erosion, improving the flexural strength of the composites by 98%. The mass and thickness change rates of the leading edge composites were 2.96 ± 0.04 µm/s and − 0.42 ± 0.04 mg/s, respectively. The better ablation performance was attributed to the synergistic effect of dense and stabilized Zr-Si-O oxide layer formation and heat transfer.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Diamond and Carbon-based Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (55)

Show source-provided references
1. Material property requirements for analysis and design of UHTC10.1016/j.jeurceramsoc.2010.01.026 ↗
2. Advanced structural ceramics in aerospace propulsion10.1038/nmat4687 ↗
3. UHTC composites for hypersonic applications
4. Arc-jet testing of ultra-high-temperature-ceramics10.1016/j.ast.2009.12.004 ↗
5. Oxidation behavior of aerospace materials in high enthalpy flows using an oxyacetylene torch10.1111/jace.13462 ↗
6. The future of carbon-carbon composites10.1016/0008-6223(87)90116-3 ↗
7. Effect of fiber architecture and density on the ablation behavior of carbon/carbon composites modified by Zr-Ti-C10.1016/j.carbon.2013.06.043 ↗
8. Recovery in oxidation behavior of damaged SiC-ZrB2/SiC coating of carbon/carbon composites
9. Oxidation behavior of SiC-HfB2-Si coating on C/C composites prepared by slurry dipping combined with gaseous Si infiltration
10. Self-healing improvement strategy of thermally sprayed MoSi2 coating at 1773 K: From calculation to experiment10.1016/j.corsci.2021.109599 ↗
11. Effect of temperature gradient on the ablation and flexural behavior of C/C-ZrC composites10.1016/j.corsci.2021.109736 ↗
12. Effect of loading spectrum with different single pulsing time on the cyclic ablation of C/C-SiC-ZrB2-ZrC composites in plasma10.1016/j.corsci.2021.109817 ↗
13. Novel one-step formed composite reinforcement of "Spider web like" SiCnw networks and "Z-pins like" SiC rods for ablation resistance improvement of C/C-ZrC-SiC10.1016/j.jeurceramsoc.2021.10.051 ↗
14. Quasi-static and dynamic compressive behaviors of porous ZrC ceramic reinforced pyrocarbon composites10.1016/j.compositesa.2021.106749 ↗
15. Sealing role of Ti-rich phase in HfC-ZrC-TiC coating for C/C composites during ablation above 2100℃10.1016/j.corsci.2022.110474 ↗
16. Influence of crystallite morphology on the ablative behaviors of CVD-TaC coatings prepared on C/C composites beyond 2100℃10.1016/j.corsci.2022.110426 ↗
17. Grain growth limitation in the monolayer ZrB2-SiC coating above 1700 °C10.1016/j.ceramint.2022.02.014 ↗
18. Domination of phononic scattering in solid solutioning and interfaces of HfB2-ZrB2-SiC -carbon nanotube based ultra high temperature composites10.1016/j.scriptamat.2022.114776 ↗
19. Dynamic oxidation protective ultrahigh temperature ceramic TaB2-20%wtSiC composite coating for carbon material10.1016/j.compositesb.2018.10.080 ↗
20. Microstructure and mechanical performance evolution of C/C-ZrC composites exposed to oxyacetylene flame10.1016/j.ceramint.2021.04.279 ↗
21. Preparation and ablation resistance of ZrC nanowires-reinforced CVD-ZrC coating on sharp leading edge C/C composites10.1016/j.apsusc.2022.152617 ↗
22. The ablation and mechanical behaviors of C/(SiC-ZrC)n multi-layer structure matrix composites by chemical vapor infiltration10.1016/j.jeurceramsoc.2022.04.026 ↗
23. High-aspect-ratio ZrC whiskers: synthesis, growth mechanism and electromagnetic wave absorption properties
24. Theoretical screening, intrinsic brittleness and thermal properties of the S-containing MAX carbides and borides
25. Mechanical properties and microstructure of Cf/ZrC-SiC and Cf/SiC composites produced by precursor infiltration and pyrolysis combined with gaseous silicon infiltration10.1016/j.jallcom.2022.164706 ↗
26. Effects of ZrC particle size on ablation behavior of C/C-SiC-ZrC composites prepared by chemical liquid vapor deposition10.1016/j.corsci.2022.110469 ↗
27. Starting from essence to reveal the ablation behavior and mechanism of 3D PyC Cf/ZrC-SiC composite10.1016/j.corsci.2022.110261 ↗
28. Microstructure and ablation behavior of SiC coated C/C-SiC-ZrC composites prepared by a hybrid infiltration process10.1016/j.carbon.2013.08.014 ↗
29. Cyclic ablation behavior of C/C-ZrC-SiC-ZrB2 composites under oxyacetylene torch with two heat fluxes at the temperatures above 2000 ºC10.1016/j.corsci.2020.109202 ↗
30. Microstructure and ablation behavior of carbon/carbon composites infiltrated with Zr-Ti10.1016/j.carbon.2012.11.042 ↗
31. Effect of PyC interface phase on the cyclic ablation resistance and flexural properties of two-dimensional Cf/HfC10.1016/j.jeurceramsoc.2020.08.049 ↗
32. A novel vibration-assisted slurry impregnation to fabricate Cf/ZrB2-SiC composite with enhanced mechanical properties10.1016/j.jeurceramsoc.2018.10.029 ↗
33. Advances in ultra-high temperature ceramics, composites, and coatings10.1007/s40145-021-0550-6 ↗
34. Reactive melt infiltration of silicon-molybdenum alloys into microporous carbon preforms
35. Interphase degradation of three-dimensional Cf/SiC-ZrC-ZrB2 composites fabricated via reactive melt infiltration10.1111/jace.14983 ↗
36. Reaction mechanism and microstructure development of ZrSi2 melt-infiltrated Cf/SiC-ZrC-ZrB2 composites: The influence of preform pore structures
37. Effects of the single layer CVD SiC interphases on mechanical properties of mullite fiber-reinforced mullite matrix composites fabricated via a sol-gel process10.1016/j.ceramint.2013.09.012 ↗
38. Effect of pyrolytic carbon interface on the properties of 3D C/ZrC-SiC composites fabricated by reactive melt infiltration10.1016/j.ceramint.2016.03.155 ↗
39. Effects of SiC interphase on the mechanical and ablation properties of C/C-ZrC-ZrB2-SiC composites prepared by precursor infiltration and pyrolysis10.1016/j.matdes.2017.02.086 ↗
40. Fabrication and properties of 3-D Cf/ZrB2–ZrC–SiC composites via polymer infiltration and pyrolysis10.1016/j.ceramint.2012.11.074 ↗
41. Ablative property of ZrC-SiC multilayer coating for PIP-C/SiC composites under oxy-acetylene torch10.1016/j.ceramint.2011.11.063 ↗
42. Study on factors affecting ablative performance of C/C composites
43. Influence of carbon-matrix structure on antiablative performances of C/C composites
44. Insights into service-derived Zr-Ta-O film: Morphology evolution, temperature resistance, and atomic bonding10.1016/j.jeurceramsoc.2023.09.008 ↗
45. Ablation behavior of sharp leading-edge C/C-ZrC-SiC composites using 3000 °C oxyacetylene torch10.1016/j.corsci.2022.110551 ↗
46. Reaction mechanism and microstructure development of Zr-Si alloyed melt-infiltrated ZrC-modified C/C composite10.1111/jace.13595 ↗
47. Comparative insights into C/C-ZrC-SiC composites with different substrate carbon on microstructures, mechanical properties, and ablation behaviors10.1016/j.jmrt.2021.06.089 ↗
48. Mechanical properties and ablation behavior of C/C-ZrC and C/C-ZrC-SiC composites prepared by precursor infiltration and pyrolysis combined with chemical vapor infiltration10.1016/j.ceramint.2018.09.131 ↗
49. The ablation behavior and mechanical property of C/C-SiC-ZrB2 composites fabricated by reactive melt infiltration10.1016/j.ceramint.2017.02.008 ↗
50. Ablation-resistant carbide Zr0.8Ti0.2C0.74B0.26 for oxidizing environments up to 3000 ℃10.1038/ncomms15836 ↗
51. Ablation behavior and mechanism of C/C-ZrC-SiC composites under an oxyacetylene torch at 3000 °C10.1016/j.ceramint.2012.10.273 ↗
52. Ablation behavior of sharp leading edge parts made of rare earth La-compound modified ZrB2 coated C/C composites10.1016/j.corsci.2020.108895 ↗
53. Construction of sandwich-structured C/C-SiC and C/C-SiC-ZrC composites with good mechanical and anti-ablation properties10.1016/j.jeurceramsoc.2021.12.006 ↗
54. Ablation behaviors and mechanism of ZrC-SiC-Si/SiC-Si double-layered coatings on C/C composite under plasma flame at 3000 ℃10.1016/j.corsci.2023.111200 ↗
55. Ablative property and mechanism of SiC-CuxSiy modified C/C-ZrC composites prepared by a rapid method10.1016/j.jeurceramsoc.2023.04.011 ↗