journal article·2023-07

CMAS + sea salt corrosion to thermal barrier coatings

Lei Guo, Xinmu Zhang, Mingguang Liu, Shuo Yang, JianWei Dai

Corrosion Science· Volume 218
Publisher page

Abstract

In marine environment, sea salt and calcium-magnesium-alumina-silicate (CMAS) coexist largely endangering thermal barrier coatings (TBCs) service safety. In this study, the corrosion behavior of synthetic sea salt and CMAS to TBCs was investigated. Sea salt changed the CMAS structure, thereby decreasing its melting temperature and high-temperature viscosity. At 1200 ℃, CMAS + sea salt completely melted but CMAS did not; at 1250 ℃, both melted while CMAS + sea salt had stronger penetration ability in TBCs than CMAS. Thus, TBCs which have not been or are less affected by CMAS may be damaged due to CMAS + sea salt attack.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Advanced ceramic materials synthesis · Magnesium Oxide Properties and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (49)

Show source-provided references
1. Thermal barrier coatings for high-temperature application on superalloy substrates - a review10.1016/j.matpr.2021.12.223 ↗
2. Progress update on failure mechanisms of advanced thermal barrier coatings: a review10.1016/j.porgcoat.2015.09.019 ↗
3. Present status and future prospects of plasma sprayed multilayered thermal barrier coating systems10.1016/j.jeurceramsoc.2020.03.016 ↗
4. Thermal barrier coatings for more efficient gas-turbine engines10.1557/mrs.2012.232 ↗
5. Progress in ceramic materials and structure design toward advanced thermal barrier coatings10.1007/s40145-022-0581-7 ↗
6. Overview on advanced thermal barrier coatings, Surf. Coatings Technol
7. Key influencing factors for the thermal shock resistance of La2Zr2O7-based multilayer TBCs10.1016/j.surfcoat.2020.125951 ↗
8. Thermal barrier coatings-a state of the art review10.1007/s12540-020-00705-w ↗
9. Zirconates as new materials for thermal barrier coatings10.1111/j.1151-2916.2000.tb01506.x ↗
10. Surface roughness affects metastable non-wetting behavior of silicate melts on thermal barrier coatings10.1007/s12598-021-01773-6 ↗
11. Comparison of CMAS corrosion and sintering induced microstructural characteristics of APS thermal barrier coatings10.1016/j.jmst.2018.09.046 ↗
12. Molten-volcanic-ash-phobic thermal barrier coating based on biomimetic structure10.1002/advs.202205156 ↗
13. A review on failure mechanism of thermal barrier coatings and strategies to extend their lifetime10.1016/j.ceramint.2019.12.200 ↗
14. Corrosion resistance of non-stoichiometric gadolinium zirconate fabricated by laser-enhanced chemical vapor deposition10.1007/s40145-020-0454-x ↗
15. Erosion behavior of EB-PVD 7YSZ coatings under corrosion/erosion regime: effect of TBC microstructure and the CMAS10.1016/j.jeurceramsoc.2018.06.039 ↗
16. Corrosiveness of CMAS and CMAS + salt (NaVO3, Na2SO4 and NaCl) to YSZ thermal barrier coating materials10.1016/j.corsci.2022.110738 ↗
17. Role of environmental deposits and operating surface temperature in spallation of air plasma sprayed thermal barrier coatings10.1016/S0257-8972(96)02994-5 ↗
18. Finite element analysis on temperature field and stress distribution of thermal barrier coatings by laser modification and CMAS corrosion10.1016/j.corcom.2021.12.002 ↗
19. Zirconium silicate growth induced by the thermochemical interaction of yttria-stablized zirconia coatings with molten CMAS deposits10.1016/j.corsci.2019.01.011 ↗
20. Advanced structural ceramics in aerospace propulsion10.1038/nmat4687 ↗
21. Dynamic spreading of re-melted volcanic ash bead on thermal barrier coatings10.1016/j.corsci.2020.108659 ↗
22. Step-by-step investigation of degradation mechanisms induced by CMAS attack on YSZ materials for TBC applications10.1016/j.surfcoat.2013.08.055 ↗
23. CMAS corrosion behavior of Sc doped Gd2Zr2O7 /YSZ thermal barrier coatings and their corrosion resistance mechanisms10.1016/j.corsci.2021.109899 ↗
24. Calcia–magnesia–alumina–silicate (CMAS) attack mechanisms and roadmap towards sandphobic thermal and environmental barrier coatings10.1080/09506608.2020.1824414 ↗
25. Calcia-magnesia-alumino-silicate (CMAS)-induced degradation and failure of air plasma sprayed yttria-stabilized zirconia thermal barrier coatings10.1016/j.actamat.2015.12.044 ↗
26. Mechanisms of cracking and delamination within thick thermal barrier systems in aero-engines subject to calcium-magnesium-alumino-silicate (CMAS) penetration10.1016/j.msea.2008.01.006 ↗
27. CMAS corrosion behavior and protection method of thermal barrier coatings for aeroengine
28. Silicate deposit degradation of engineered coatings in gas turbines: progress toward models and materials solutions10.1146/annurev-matsci-010917-105000 ↗
29. Experimental and numerical investigation on the thermal and mechanical behaviours of thermal barrier coatings exposed to CMAS corrosion10.1007/s40145-021-0457-2 ↗
30. Some aspects of the hot corrosion of thermal barrier coatings10.1007/BF02646315 ↗
31. Comparison of hot corrosion behaviors of plasma-sprayed nanostructured and conventional YSZ thermal barrier coatings exposure to molten vanadium pentoxide and sodium sulfate10.1016/j.jeurceramsoc.2013.08.006 ↗
32. Hot corrosion behavior of YSZ, Gd2Zr2O7 and YSZ/Gd2Zr2O7 thermal barrier coatings exposed to molten sulfate and vanadate salt10.1016/j.apsusc.2017.09.047 ↗
33. Femtosecond laser polishing yttria-stabilized zirconia coatings for improving molten salts corrosion resistance10.1016/j.corsci.2021.109367 ↗
34. Hot corrosion behavior of NdYb Zr2O7 exposed to V2O5 and Na2SO4 + V2O5 molten salts10.1016/j.ceramint.2019.12.083 ↗
35. Phase stability and thermal conductivity of RE2O3 (RE = La, Nd, Gd, Yb) and Yb2O3 co-doped Y2O3 stabilized ZrO2 ceramics10.1016/j.ceramint.2016.01.138 ↗
36. Hot corrosion behavior of rare earth zirconates and yttria partially stabilized zirconia thermal barrier coatings, Surf. Coatings Technol
37. Rodriguez, The accelerating effect of CaSO4 within CMAS (CaO-MgO-Al2O3-SiO2) and its effect on the infiltration behavior in EB-PVD 7YSZ10.1111/jace.14077 ↗
38. CMAS effects on ship gas-turbine components/materials
39. Comparison of NaVO3+CMAS mixture and CMAS corrosion to thermal barrier coatings10.1016/j.corsci.2020.108968 ↗
40. Thermochemical interaction of thermal barrier coatings with molten CaO-MgO-Al2O3-SiO2 (CMAS)10.1111/j.1551-2916.2006.01209.x ↗
41. Effects of pellet surface roughness and pre-oxidation temperature on CMAS corrosion behavior of Ti2AlC10.1007/s40145-022-0588-0 ↗
42. Self-crystallization characteristics of calcium-magnesium-alumina-silicate (CMAS) glass under simulated conditions for thermal barrier coating applications10.1016/j.jeurceramsoc.2020.07.025 ↗
43. The structure of silicate melts: a glass perspective10.2113/gscanmin.43.6.1921 ↗
44. The structure of lithium-containing silicate and germanate glasses10.2113/gscanmin.43.5.1643 ↗
45. Raman spectroscopic investigation of the structure of silicate glasses. III. Raman intensities and structural units in sodium silicate glasses10.1063/1.442472 ↗
46. structural, optical, and nuclear magnetic resonance studies of V2O5 - doped lead calcium titanate borosilicate glasses10.1016/j.jpcs.2018.10.030 ↗
47. Fourier analysis of X-ray patterns of soda–silica glass10.1111/j.1151-2916.1938.tb15774.x ↗
48. The atomic arrangement in glass10.1021/ja01349a006 ↗
49. Evolution of porosity, crack density, and CMAS penetration in thermal barrier coatings subjected to burner rig testing10.1111/jace.16465 ↗