Abstract

Abstract The corrosion behaviour of sputter-deposited, Al–W coatings with three different concentrations of tungsten (0.6, 3.5 and 11 at.% W) on AA7075 aluminium alloy substrates was investigated in chloride media using EIS, salt-fog tests and surface analyses. The surface analyses were performed with XPS/AES, SEM/EDS and TEM microscopy. The presence of W reduces the thickness of the oxide layer formed after the EIS test, as proved by the compositional depth profile. From the EIS data of the investigated Al–W x coatings, the polarisation resistance ( R p ) and the capacitive behaviour as a function of the immersion time were obtained. A small increase in R p suggested improved corrosion properties over time. However, the extent of the improvement depends on the content of W and the coating-surface morphology (the presence of growth defects on the coating surface). The capacitive behaviour observed at high frequencies was related to the dielectric properties and the thickness of the barrier oxide film formed. The salt-fog tests to some extent supported the results from the EIS measurements. However, there was a difference between the corrosion EIS and salt-fog test results in the case of the Al 89 W 11 coatings. The thickest oxide layer and the “layering” into the three regions (porous, semi-porous and intact) were observed when the salt-fog corrosion test was performed on the Al 89 W 11 coating. Galvanic corrosion, probably due to the local compositional and structural inhomogeneities, takes place. However, this was not unambiguously observed during the EIS corrosion test.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Corrosion Behavior and Inhibition · Copper Interconnects and Reliability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (44)

Show source-provided references
1. Fitting corrosion of aluminum10.1016/S0010-938X(99)00012-8 ↗
2. Pitting in aluminum thin films – supersaturation and effects of dichromate ions10.1149/1.1838722 ↗
3. Determination of pit growth-rates on aluminum using a metal foil technique10.5006/1.3577553 ↗
4. On the pitting resistance of sputter-deposited aluminum-alloys10.1149/1.2220794 ↗
5. Impedance spectra for aluminum-7075 during the early stages of immersion in sodium-chloride10.1016/0010-938X(93)90063-M ↗
6. Repassivation and pitting of freshly generated aluminium surfaces in acidic nitrate solution10.1016/j.corsci.2005.05.054 ↗
7. Study of Al alloy corrosion in neutral NaCl by the pitting scan technique10.1016/j.matchemphys.2010.02.022 ↗
8. Metastable pitting characteristics of aluminium alloys measured using current transients during potentiostatic polarisation10.1016/j.electacta.2012.01.090 ↗
9. Metastable pitting of aluminum and criteria for the transition to stable pit growth10.1149/1.2059275 ↗
10. Role of nanostructure in pitting of Al–Cu–Mg alloys10.1016/j.electacta.2010.02.001 ↗
11. Combined anodic/cathodic transient currents within nucleating pits on Al–Fe alloy surfaces10.1016/j.corsci.2010.11.008 ↗
12. Mechanisms of passivity of nonequilibrium Al–W alloys10.1149/1.2056234 ↗
13. Pitting of sputtered aluminum-alloy thin-films10.1149/1.2096864 ↗
14. Dependence of the pitting potential of Al-alloys on solubility of alloying element oxides10.1016/0010-938X(93)90282-L ↗
15. The influence of tungsten on the pitting of aluminum films10.1149/1.2086658 ↗
16. Chromium ion implantation for inhibition of corrosion of aluminium10.1016/0257-8972(95)02822-6 ↗
17. On some fundamental factors in the effect of alloying elements on passivation of alloys10.1016/0010-938X(94)90013-2 ↗
18. Corrosion behaviour of amorphous Al–Cr and Al–Cr–(N) coatings deposited by dc magnetron sputtering on mild steel substrate10.1016/j.tsf.2003.11.315 ↗
19. Correlation between hardness and stress in Al-(Nb, Mo, Ta) thin films10.1016/j.tsf.2009.03.172 ↗
20. Formation and physical properties of Al base alloys by sputtering10.1016/S0042-207X(00)00277-3 ↗
21. An Xps study of the corrosion behavior of sputter-deposited amorphous Al–W alloys in 1-M Hcl10.1016/0010-938X(91)90076-2 ↗
22. Stability of the passive state of Al–W sputter deposited amorphous alloys10.1016/S0254-0584(97)01883-X ↗
23. The corrosion behavior of Cr-(C, N) PVD hard coatings deposited on various substrates10.1016/j.electacta.2003.11.012 ↗
24. Electrical properties of nanocrystalline CeO2 thin films deposited by in situ pulsed laser deposition10.1149/1.2165778 ↗
25. Evaluation of anodized aluminum surfaces with electrochemical impedance spectroscopy10.1149/1.2095786 ↗
26. Impedance studies of the passive film on aluminium10.1016/j.corsci.2005.05.058 ↗
27. Assessing the corrosion of biodegradable magnesium implants: a critical review of current methodologies and their limitations10.1016/j.actbio.2011.11.014 ↗
28. The corrosion behavior of sputter-deposited aluminum-tungsten alloys10.1016/S0013-4686(02)00040-3 ↗
29. Corrosion resistance of amorphous aluminium–molybdenum alloys in an acidic chloride environment10.1016/j.corsci.2009.09.021 ↗
30. Role of oxide/metal interface in corrosion resistance. Al–W and Al–Mo systems10.5006/1.3277562 ↗
31. Recent progress in corrosion-resistant metastable alloys10.1016/0921-5093(95)80052-V ↗
32. Corrosion and related mechanical properties of bulk metallic glasses10.1557/jmr.2007.0051 ↗
33. D.K. Merl, P. Panjan, I. Milosev, Surface Engineering, in press.
34. W.F.S.J. F. Moulder, P.E. Sobol, K.D. Bomben, Handbook of X-ray Photoelectron Spectroscopy, Physical Electronics Inc., Eden Prairie, Minnesota, USA, 1995.
35. N.C.M.L.E. Davis, P.W. Palmberg, G.E. Riach, R.E. Weber, Handbook of Auger Electron Spectroscopy, second ed., Physical Electronics Industries Inc., Eden Prairie, Minnesota, 1976.
36. The corrosion behaviour of austenitic and duplex stainless steels in artificial saliva with the addition of fluoride10.1016/j.corsci.2010.11.010 ↗
37. On the interpretation of measured impedance spectra of insertion cathodes for lithium-ion batteries10.1149/1.3489353 ↗
38. Electrochemical impedance spectroscopy as a tool for materials selection: water for haemodialysis10.1016/j.electacta.2011.03.055 ↗
39. Raistrick · 2005
40. The Nucleation, Growth and Stability of Micropits in Stainless-Steel10.1016/0010-938X(94)90145-7 ↗
41. A review of the probabilistic aspects of localized corrosion10.5006/1.3585102 ↗
42. An eis study of aluminum barrier-type oxide-films formed in different media10.1016/0013-4686(92)85124-4 ↗
43. An ESCA method for determining the oxide thickness on aluminum alloys10.1002/sia.740150109 ↗
44. Measurement of oxide film growth on Mg and A1 surfaces over extended periods using XPS10.1016/S0039-6028(97)00054-X ↗