Abstract In this study, we performed three surface modifications for AISI H13 steel to study their protective effects in 1023 K molten aluminum. Results showed that air oxidation can produce a thin film of Fe2O3 and little FeO, and the liquid-nitriding formed a surface of iron nitrides and oxides (Fe2O3 + Fe3O4). While liquid-nitriding with post-oxidation can form a surface of Fe3O4 and little Fe2O3 by oxidizing the nitrides into Fe3O4 on the liquid-nitriding samples. The Fe3O4 has low wettability and good chemical stability against molten aluminum, thus the corrosion behaviors of molten aluminum to the samples change from dissolution to oxidation.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Semiconductor materials and devices · Advanced ceramic materials synthesis · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (55)
Show source-provided references
1. Corrosion resistance properties of enamels with high B2O3–P2O5 content to molten aluminum10.1016/S0921-5093(02)00527-0 ↗
2. Microstructural evolution of intermetallic layer in hot-dipped aluminide mild steel with silicon addition10.1016/j.surfcoat.2011.04.061 ↗
3. Laboratory assessment of wear on nitrided surfaces of dies for hot extrusion of aluminium10.1016/j.triboint.2005.09.032 ↗
4. Influence of the nitriding time in the wear behaviour of an AISI H13 steel during a crankshaft forging process10.1016/j.wear.2007.02.007 ↗
5. Effect of chromium on the formation of intermetallic phases in hot-dipped aluminide Cr–Mo steels10.1016/j.apsusc.2013.04.015 ↗
6. Microstructure and corrosion behaviour of pulsed plasma-nitrided AISI H13 tool steel10.1016/j.corsci.2010.05.036 ↗
7. THE EFFECT OF DOUBLE SHOT PEENING AND NITRIDING ON THE DIE SOLDERING BEHAVIOUR OF H13 AND Cr-Mo-v TOOL STEEL10.14716/ijtech.v7i3.2964 ↗
8. Effect of micro alloying elements on the interfacial reactions between molten aluminum alloy and tool steel10.1016/j.jallcom.2008.11.127 ↗
9. A study of PVD coatings and die materials for extended die-casting die life10.1016/S0257-8972(97)00476-3 ↗
10. Corrosion behavior of zirconium diboride coated stainless steel in molten 6061 aluminum alloy10.1016/j.surfcoat.2017.01.069 ↗
11. Evaluation of DC-MS and HiPIMS TiB2 and TaN coatings as diffusion barriers against molten aluminum: an insight into the wetting mechanism10.1016/j.surfcoat.2019.06.031 ↗
12. Study of protective coatings for aluminum die casting molds10.1016/j.apsusc.2015.08.013 ↗
13. Surface modification of steel and cast iron to improve corrosion resistance in molten aluminium10.1016/j.surfcoat.2005.06.026 ↗
14. The mechanism of surface nanocrystallization during plasma nitriding10.1016/j.apsusc.2019.05.164 ↗
15. Low-temperature gas nitriding of AISI 4140 steel accelerated by LaFeO3 perovskite oxide10.1016/j.apsusc.2018.10.111 ↗
16. Precipitation of γ′ nitrides in N-saturated ferrite at high temperature and its effect on nitriding10.1016/j.jallcom.2019.04.099 ↗
17. Corrosion properties of plasma nitrided AISI 410 martensitic stainless steel in 3.5% NaCl and 1% HCl aqueous solutions10.1016/j.corsci.2005.08.011 ↗
18. Combat molten aluminum corrosion of AISI H13 steel by low-temperature liquid nitrocarburizing10.1016/j.jallcom.2018.10.298 ↗
19. High temperature solution-nitriding and low-temperature nitriding of AISI 316: effect on pitting potential and crevice corrosion performance10.1016/j.apsusc.2017.06.094 ↗
20. The use of navy C-ring specimens to study distortion in ferritic nitrocarburized 1010 steel
21. The effect of gas mixture of post-oxidation on structure and corrosion behavior of plasma nitrided AISI 316 stainless steel10.1016/j.apsusc.2013.06.152 ↗
22. Effect of high temperature post-oxidizing on tribological and corrosion behavior of plasma nitrided AISI 316 austenitic stainless steel10.1016/j.vacuum.2010.08.008 ↗
23. Enhancement of Erosion resistance on AISI H13 tool steel by oxynitriding treatment10.2355/isijinternational.49.421 ↗
24. Effects of post-oxidizing treatment on melting loss and corrosion resistance of gas nitrided AISI H13 tool steel10.2355/isijinternational.52.499 ↗
25. Interfacial reactions between molten Al and a Co–Cr–Mo alloy with and without oxidation treatment10.1016/j.corsci.2011.08.015 ↗
26. Enhancement of corrosion resistance of Fe–Cr–Mo alloy to molten Al by thermal oxidation in air10.1016/j.corsci.2013.07.031 ↗
27. Influence of time on the microstructure of AISI 321 austenitic stainless steel in salt bath nitriding10.1016/j.surfcoat.2012.01.063 ↗
28. Applied stress-assisted growth of single crystal gamma-Fe2O3 nanowires10.3390/nano8121037 ↗
29. Mechanism of Al on FeCrAl steam oxidation behavior and molecular dynamics simulations10.1016/j.jallcom.2020.154310 ↗
30. Oxide layer formed on AISI 5140 steel by plasma nitriding and post-oxidation in a mixture of air and ammonia10.1016/j.jallcom.2019.07.314 ↗
31. The iron oxides: structure, properties, reactions, occurrence and uses: R. M. Cornell and U. Schwertmann. 573 pp. VCH, Weinheim and New York, 1996. ISBN: 3-527-28576-810.1016/S0010-938X(97)00096-6 ↗
32. 6 - Salt Bath thermal treating and nitriding
33. Sensitization of high-nitrogen austenitic stainless steels by dichromium nitride precipitation10.5006/1.3294349 ↗
34. Well-ordered oxygen-deficient CoMoO 4 and Fe 2 O 3 nanoplate arrays on 3D graphene foam: toward flexible asymmetric supercapacitors with enhanced capacitive properties10.1021/acsami.6b14810 ↗
35. 3D ordered macro-mesoporous indium doped Al2O310.1039/c3ce40562a ↗
36. Novel visible-light-driven Fe2O3/Ag3VO4 composite with enhanced photocatalytic activity toward organic pollutants degradation10.1039/C5RA22912J ↗
37. Surface properties of nitrided layer on AISI 316L austenitic stainless steel produced by high temperature plasma nitriding in short time10.1016/j.apsusc.2014.01.177 ↗
38. Analysis of XPS spectra of Fe2+ and Fe3+ ions in oxide materials10.1016/j.apsusc.2007.09.063 ↗
39. Low-temperature oxidation of nitrided Iron surfaces10.1021/jp027802w ↗
40. Crystallography of Fe2Al5 phase at the interface between solid Fe and liquid Al10.1016/j.intermet.2015.07.011 ↗
41. Growth kinetics and thickness prediction of interfacial intermetallic compounds between solid steel and molten aluminum based on thermophysical simulation in a few seconds10.1016/j.matchar.2017.09.012 ↗
42. Influence of intermetallic phases and Kirkendall-porosity on the mechanical properties of joints between steel and aluminium alloys10.1016/j.msea.2011.02.057 ↗
43. Effects of interfacial layers fracture on the dissolution mechanism of solid Fe in liquid Al10.1007/s11837-015-1435-3 ↗
44. Microstructural evolution and growth behavior of intermetallic compounds at the liquid Al/solid Fe interface by synchrotron X-ray radiography10.1016/j.matchar.2017.12.024 ↗
45. Interaction between the growth and dissolution of intermetallic compounds in the interfacial reaction between solid Iron and liquid aluminum10.1007/s11661-016-3667-4 ↗
46. Growth behavior of Fe2Al5 during reactive diffusion between Fe and Al at solid-state temperatures10.1016/j.msea.2007.01.099 ↗
47. Chemical interaction between SrAl2Si2O8 and molten aluminum10.1016/j.jeurceramsoc.2015.07.022 ↗
48. Effects of AlPO4 addition on the corrosion resistance of andalusite-based low-cement castables with molten Al-alloy10.1016/j.jeurceramsoc.2012.11.005 ↗
49. Corrosion of enamel with and without CaF2 in molten aluminum at 750 °C10.1016/j.corsci.2018.12.016 ↗
50. Effects of V2O5 addition on the corrosion resistance of andalusite-based low-cement castables with molten Al-alloy10.1016/j.jeurceramsoc.2012.01.023 ↗
51. The effect of SrSO4 and BaSO4 on the corrosion and wetting by molten aluminum alloys of mullite ceramics10.1016/j.ceramint.2010.01.015 ↗
52. Evaluation of adhesion and erosion/corrosion resistance of nano-composite and nano-multilayer thin films in molten aluminum alloy10.1007/s42452-019-1299-1 ↗
53. Synthesis and characterization of nanocrystalline α-Al2O3 using Al and Fe2O3 (hematite) through mechanical alloying10.1016/j.solidstatesciences.2008.06.021 ↗
54. Investigation of dissolution resistance of blank and GAS-NITRIDED carbon steels in stationary SAC305 SOLDER ALLOY MELT10.2298/JMMB170918019B ↗
55. Interfacial reactions of solid Co and solid Fe with liquid Al10.1016/j.corsci.2012.04.015 ↗