journal article·2021-01

Oxidation behaviour and related microstructural changes of two β0–phase containing TiAl alloys between 600 °C and 900 °C

L. Mengis, A.S. Ulrich, P. Watermeyer, C.H. Liebscher, M.C. Galetz

Corrosion Science· Volume 178
Publisher page

Abstract

Abstract A comparative study on the isothermal oxidation behaviour of the two β0–containing titanium aluminide alloys GE 4822 and TNM-B1 in the HIPed condition has been conducted at temperatures between 600 °C and 900 °C for up to 1000 h in air. The two alloys exhibit clear differences in their oxidation behaviour, however, both suffer from undesirable embrittlement due to oxidation after exposure for 100 h even at 600 °C. Phase transformations in the subsurface zone were shown to have a strong impact on the mechanical properties at room temperature.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Intermetallics and Advanced Alloy Properties · MXene and MAX Phase Materials · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (37)

Show source-provided references
1. Design, processing, microstructure properties, and applications of advanced intermetallic TiAl alloys10.1002/adem.201200231 ↗
2. TiAl alloys in commercial aircraft engines10.1080/09603409.2016.1183068 ↗
3. Advances in gammalloy materials–processes–application technology: successes, dilemmas, and future10.1007/s11837-018-2747-x ↗
4. Fundamentals of TiAl oxidation - a critical review
5. Oxidation behavior of intermetallic titanium aluminide alloys
6. Effect of elevated temperature exposure on cast gamma titanium aluminide (Ti-48A1-2Cr-2Nb)10.1016/0956-716X(94)90322-0 ↗
7. Modelling thermal exposure effects on fatigue of gamma titanium aluminides10.1016/S0921-5093(01)01556-8 ↗
8. Oxidation-induced embrittlement of TiAl alloys10.1016/j.intermet.2009.01.010 ↗
9. Effects of oxygen, water vapor, argon, air and exposure history on fracture strength of Ti-48Al-2Nb-2Cr notched tensile specimens10.1016/S0921-5093(97)00600-X ↗
10. Environmental embrittlement of a third generation γ TiAl alloy10.1016/j.intermet.2011.10.006 ↗
11. In situ X-ray tomography investigation of the crack formation in an intermetallic beta-stabilized TiAl-alloy during a stepwise tensile loading10.1016/j.ijfatigue.2019.02.035 ↗
12. Effects of thermal exposure on the properties of two y alloys10.1016/0921-5093(94)03331-5 ↗
13. The influence of high temperature exposure on the mechanical performance of a γ titanium aluminide alloy10.1016/S0921-5093(01)01470-8 ↗
14. Effect of exposure on the mechanical properties of Gamma MET PX10.1016/j.intermet.2004.12.015 ↗
15. Galetz · Intermetallics · 2020 · 12310.1016/j.intermet.2020.106830 ↗
16. Study of alpha-case depth in Ti-6Al-2Sn-4Zr-2Mo and Ti-6Al-4V10.1088/1757-899X/48/1/012002 ↗
17. Impact of β-phase in TiAl alloys on mechancial properties after high temperature air exposure10.1016/j.intermet.2020.106729 ↗
18. Influence of heat treatments on the microstructure of a multi-phase titanium aluminide alloy10.3139/147.110142 ↗
19. Alloying mechanism of beta stabilizers in a TiAl alloy10.1007/s11661-001-0136-4 ↗
20. The effect of nitrogen on the oxidation of γ-TiAl10.1016/0956-716X(95)00312-J ↗
21. Studies concerning the effect of nitrogen on the oxidation behavior of TiAl-based intermetallics at 900°C10.1007/BF01051039 ↗
22. Beneficial and detrimental Effects of Nitrogen on the oxidation behaviour of TiAl‐based intermetallics
23. Effect of ternary elements on the oxidation behavior of aluminized TiAl alloys10.1023/A:1016024810408 ↗
24. The influence of ternary element addition on the oxidation behaviour of TiAl intermetallic compound in high temperature air10.1016/0010-938X(93)90313-6 ↗
25. Oxidation of TiAl based intermetallics10.1023/A:1018529829167 ↗
26. The Effect of various ternary additives on the oxidation behavior of TiAl in high-temperature air10.1007/BF01046826 ↗
27. Review of the effect of alloy composition on the growth rates of scales formed during oxidation of gamma titanium aluminide alloys10.1016/S0921-5093(02)00064-3 ↗
28. Very long term oxidation of Ti-48Al-2Cr-2Nb at 704 ° C in air10.1016/S1359-6462(97)00178-4 ↗
29. The oxidation behaviour of aluminium-rich coatings on the TiAl alloy TNM-B110.1080/09603409.2017.1389097 ↗
30. The initial stages of oxidation of TiAl
31. Microstructural Study of oxidized γ-TiAl10.1023/A:1018892422121 ↗
32. A review of metastable Beta titanium alloys10.3390/met8070506 ↗
33. On the eutectoid transformation behavior of the Ti-Zn system and its metastable phases10.1016/j.jallcom.2017.05.103 ↗
34. The Cr-Ti (Chromium-Titanium) System10.1007/BF02881474 ↗
35. Modeling of alpha-case formation and its effects on the mechanical properties of titanium alloy castings10.1007/s11661-007-9406-0 ↗
36. Fracture mechanisms of γ–TiAl Alloys investigated by in-situ experiments in a scanning electron and atomic force microscope
37. Oxygen-dislocation interaction in titanium from first principles10.1016/j.scriptamat.2018.11.025 ↗