journal article·2022-06

Improvement mechanism in stress corrosion resistance of the X70 pipeline steel in hydrogen sulfide solution by massive laser shock peening treatment

Zhao Wang, Haifei Lu, Jie Cai, Liujun Wu, Kaiyu Luo, Jinzhong Lu

Corrosion Science· Volume 201
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Surface Treatment and Residual Stress · Erosion and Abrasive Machining · Diamond and Carbon-based Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (66)

Show source-provided references
1. Environment hydrogen embrittlement of pipeline steel X70 under various gas mixture conditions with in situ small punch tests10.1016/j.msea.2020.139114 ↗
2. Hydrogen embrittlement susceptibility of X70 pipeline steel weld under a low partial hydrogen environment10.1016/j.ijhydene.2020.06.199 ↗
3. Stress corrosion cracking behavior of rusted X100 steel under the combined action of Cl− and HSO3− in a wet–dry cycle environment10.1016/j.corsci.2019.108382 ↗
4. Effect of strain rate and sulfate reducing bacteria on stress corrosion cracking behaviour of X70 pipeline steel in simulated sea mud solution10.1016/j.engfailanal.2019.02.009 ↗
5. Electrochemical impedance spectroscopy analysis of X70 pipeline steel stress corrosion cracking in high pH carbonate solution10.1016/j.corsci.2012.04.024 ↗
6. Macro- and microscale investigations of hydrogen embrittlement in X70 pipeline steel by in-situ and ex-situ hydrogen charging tensile tests and in-situ electrochemical micro-cantilever bending test10.1016/j.msea.2019.138762 ↗
7. А. Lamikiz, Influence of combined laser heat treatment and ultrasonic impact treatment on microstructure and corrosion behavior of AISI 1045 steel10.1016/j.surfcoat.2020.126275 ↗
8. Effect of microstructural aspects in the heat-affected zone of high strength pipeline steels on the stress corrosion cracking mechanism: Part I. In acidic soil environment10.1016/j.corsci.2019.108167 ↗
9. Synergistic effects of corrosion and slow strain rate loading on the mechanical and electrochemical response of an aluminium alloy10.1016/j.corsci.2019.03.018 ↗
10. Role of texture and inclusions on the failure of an API X70 pipeline steel at different service environments10.1016/j.matchar.2020.110330 ↗
11. Stress-corrosion cracking of pipe steel under complex influence of factors10.1016/j.engfailanal.2020.104757 ↗
12. Study on the effect of multiple laser shock peening on residual stress and microstructural changes in modified 9Cr-1Mo (P91) steel10.1016/j.surfcoat.2018.11.027 ↗
13. Surface nanocrystallization of Ti–45Al–7Nb–0.3W intermetallics induced by surface mechanical grinding treatment10.1016/j.matlet.2015.12.025 ↗
14. Microstructure modification and improving corrosion resistance of laser surface quenched nickel–aluminum bronze alloy10.1016/j.corsci.2020.108744 ↗
15. Effect of shot peening coverage on residual stress and surface roughness of 18CrNiMo7-6 steel10.1016/j.ijmecsci.2020.105785 ↗
16. Microstructure and mechanical properties of CoCrFeMnNi high entropy alloy with ultrasonic nanocrystal surface modification process10.1016/j.jmst.2020.02.083 ↗
17. Effects of laser shock peening on the micro-hardness, tensile properties, and fracture morphologies of CP-Ti alloy at different temperatures10.1016/j.apsusc.2017.05.202 ↗
18. Wear behavior of Mg-3Al-1Zn alloy subjected to laser shock peening10.1016/j.surfcoat.2018.01.043 ↗
19. The compound process of laser shock peening and vibratory finishing and its effect on fatigue strength of Ti-3.5Mo-6.5Al-1.5Zr-0.25Si titanium alloy10.1016/j.jallcom.2018.12.294 ↗
20. Laser shock peening-induced surface gradient stress distribution and extension mechanism in corrosion fatigue life of AISI 420 stainless steel10.1016/j.corsci.2020.109027 ↗
21. Effects of service temperature on tensile properties and microstructural evolution of CP titanium subjected to laser shock peening10.1016/j.jallcom.2018.08.161 ↗
22. Effects of laser shock peening on SCC behavior of Alloy 600 in tetrathionate solution10.1016/j.corsci.2014.10.045 ↗
23. Laser shock peening (LSP): Electrochemical and hydrodynamic investigation of corrosion protection pre-treatment for a copper surface in 3.5% NaCl medium10.1016/j.corsci.2020.109156 ↗
24. Effect of laser shock peening on the stress corrosion cracking of AZ31B magnesium alloy in a simulated body fluid10.1016/j.surfcoat.2016.12.093 ↗
25. Effects of laser peening on stress corrosion cracking (SCC) of ANSI 304 austenitic stainless steel10.1016/j.corsci.2012.03.044 ↗
26. Electrochemical polarization behavior of X70 steel in thin carbonate/bicarbonate solution layers trapped under a disbonded coating and its implication on pipeline SCC10.1016/j.corsci.2010.03.019 ↗
27. Electrochemical characteristic and stress corrosion behavior of API X70 high-strength pipeline steel under a simulated disbonded coating in an artificial seawater environment10.1016/j.jelechem.2019.05.044 ↗
28. Stress corrosion cracking and fatigue crack growth of an API 5L X70 welded joint in an ethanol environment10.1016/j.ijpvp.2019.01.006 ↗
29. The effect of the initial microstructure of the X70 low-carbon microalloyed steel on the heat affected zone formation and the mechanical properties of laser welded joints10.1016/j.msea.2020.140075 ↗
30. Mechanical property-microstructure relationships of an X70 pipeline steel at elevated temperatures10.1016/j.msea.2020.140041 ↗
31. Microstructure evolution and electrochemical corrosion behaviour of API X70 linepipe steel in different environments10.1016/j.ijpvp.2019.01.013 ↗
32. Evaluation of the fracture toughness of X70 pipeline steel with ferrite-bainite microstructure10.1016/j.msea.2017.01.043 ↗
33. Effects of microstructure alteration on corrosion behavior of welded joint in API X70 pipeline steel10.1016/j.matdes.2012.09.051 ↗
34. Effect of solution pH on stress corrosion cracking behavior of modified AZ80 magnesium alloy in simulated body fluid10.1016/j.matchemphys.2021.124232 ↗
35. Quantitative study of the corrosion evolution and stress corrosion cracking of high strength aluminum alloys in solution and thin electrolyte layer containing Cl-10.1016/j.corsci.2020.109076 ↗
36. Near-neutral pH corrosion and stress corrosion crack initiation of a mill-scaled pipeline steel under the combined effect of oxygen and paint primer10.1016/j.corsci.2021.109511 ↗
37. Effects of dissolved hydrogen and surface condition on the intergranular stress corrosion cracking initiation and short crack growth behavior of non-sensitized 316 stainless steel in simulated PWR primary water10.1016/j.corsci.2017.02.003 ↗
38. Hydrogen atoms on the SCC behavior of SUS301L-MT stainless steel laser-arc hybrid welded joints10.1016/j.corsci.2018.12.023 ↗
39. Hydrogen damage and delayed fracture in bulk metallic glass10.1016/j.corsci.2004.07.045 ↗
40. Effect of hydrogen charging on SCC of 2205 duplex stainless steel with varying microstructures in simulated deep-sea environment10.1016/j.corsci.2021.110026 ↗
41. Effects of laser shock peening on the hot corrosion behaviour of the selective laser melted Ti6Al4V titanium alloy10.1016/j.corsci.2021.109558 ↗
42. Microstructural response and grain refinement mechanism of commercially pure titanium subjected to multiple laser shock peening impacts10.1016/j.actamat.2017.01.050 ↗
43. Revealing the deformation mechanisms of nanograins in gradient nanostructured Cu and CuAl alloys under tension10.1016/j.actamat.2019.09.021 ↗
44. Effect of microstructure and inclusions on hydrogen induced cracking susceptibility and hydrogen trapping efficiency of X120 pipeline steel10.1016/j.msea.2010.07.022 ↗
45. Effect of hydrogen-induced plasticity on the stress corrosion cracking of X70 pipeline steel in simulated soil environments10.1016/j.msea.2016.02.019 ↗
46. Stress corrosion cracking and hydrogen embrittlement of sensitized austenitic stainless steels in boiling saturated magnesium chloride solutions10.1016/j.corsci.2008.04.024 ↗
47. Effect of pH and hydrogen on the stress corrosion cracking behavior of duplex stainless steel in marine atmosphere environment10.1016/j.oceaneng.2017.10.002 ↗
48. Strain-shock-induced early stage high pH stress corrosion crack initiation and growth of pipeline steels10.1016/j.corsci.2020.109056 ↗
49. Grain boundary structure and intergranular stress corrosion crack initiation in high temperature water of a thermally sensitised austenitic stainless steel, observed in situ10.1016/j.corsci.2014.04.050 ↗
50. Characteristics of hydrogen embrittlement in high-pH stress corrosion cracking of X100 pipeline steel in carbonate/ bicarbonate solution10.1016/j.conbuildmat.2020.120124 ↗
51. Microstructure, microhardness and residual stress of laser additive manufactured CoCrFeMnNi high-entropy alloy subjected to laser shock peening10.1016/j.jmatprotec.2020.116806 ↗
52. Investigation and microstructural analyses of massive LSP impacts with coverage area on crack initiation location and tensile properties of AM50 magnesium alloy10.1016/j.msea.2015.10.036 ↗
53. Residual stress, phase, microstructure and mechanical property studies of ultrafine bainitic steel through laser shock peening10.1016/j.optlastec.2019.02.041 ↗
54. Formation of nano-laminated structure in nickel by means of surface mechanical grinding treatment10.1016/j.actamat.2015.06.014 ↗
55. Stress corrosion cracking behavior of LSP/MAO treated magnesium alloy during SSRT in a simulated body fluid10.1016/j.jallcom.2020.153707 ↗
56. Laser shock peening without coating induced residual stress distribution, wettability characteristics and enhanced pitting corrosion resistance of austenitic stainless steel10.1016/j.apsusc.2017.09.138 ↗
57. Hydrogen embrittlement of high-strength marine steel as a weld joint in artificial seawater under cathodic polarization10.1016/j.engfailanal.2022.106044 ↗
58. High-performance integrated additive manufacturing with laser shock peening –induced microstructural evolution and improvement in mechanical properties of Ti6Al4V alloy components10.1016/j.ijmachtools.2019.103475 ↗
59. Residual stresses induced by laser shock peening in orthopaedic Ti-6Al-7Nb alloy10.1016/j.optlastec.2020.106446 ↗
60. Effects of laser shock processing on electrochemical corrosion resistance of ANSI 304 stainless steel weldments after cavitation erosion10.1016/j.corsci.2012.08.034 ↗
61. Effect of laser shock peening on the hot corrosion behavior of Ni-based single-crystal superalloy at 750°C10.1016/j.corsci.2021.109419 ↗
62. LSP/MAO composite bio-coating on AZ80 magnesium alloy for biomedical application10.1016/j.msec.2017.03.003 ↗
63. Effect of cathodic potentials on the SCC behavior of E690 steel in simulated seawater10.1016/j.msea.2015.05.109 ↗
64. Effects of laser shock peening with different coverage layers on fatigue behaviour and fractural morphology of Fe-Cr alloy in NaCl solution10.1016/j.jallcom.2018.09.147 ↗
65. Corrosion behaviour of AISI 304 stainless steel subjected to massive laser shock peening impacts with different pulse energies10.1016/j.corsci.2013.11.003 ↗
66. Study on the effect of multiple laser shock peening on residual stress and microstructural changes in modified 9Cr-1Mo (P91) steel10.1016/j.surfcoat.2018.11.027 ↗