Corrosion mechanism of novel MgO–Al3BC3 refractories in contact with converter slag

Xuan Wang, Chengji Deng, Bo Dong, Jun Ding, Beiyue Ma, Zhoufu Wang, Hongxi Zhu, Pengcheng Gong, Chao Yu

Corrosion Science· Volume 228
Publisher page

Abstract

The corrosion mechanism of novel MgO–Al 3BC 3 refractories in contact with converter slag was investigated. Results demonstrated that refractories with an optimized Al 3BC 3 –Al composition exhibited significantly reduced corrosion index compared with low–carbon MgO–C refractories. The superior corrosion resistance was primarily attributed to the formation of a dense protective layer composed of MgO–MgAl 2O 4–Mg 3B 2O 6, which was achieved at 1100 °C by combining Al 3BC 3 –Al. These protective layers with enhanced diffusion barriers effectively impedes the penetration and solid solution of Ca and Fe ions, thereby also optimizing the slag viscosity. The self–healing capability of the novel MgO–Al 3BC 3 refractories further enhances their corrosion resistance.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnesium Oxide Properties and Applications · Advanced ceramic materials synthesis · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (48)

Show source-provided references
1. High temperature mechanical and corrosion resistance of Fe-containing MgO-C refractory in oxidizing atmosphere10.1016/j.ceramint.2019.06.306 ↗
2. Preparation and properties of porous MgO based ceramics from magnesite tailings and fused magnesia10.1016/j.ceramint.2023.03.034 ↗
3. Preparation and thermal shock behavior of nanoscale MgAl2O4 spinel-toughened MgO-based refractory aggregates10.1016/j.ceramint.2019.03.107 ↗
4. Current State of Application of Machine Learning for Investigation of MgO-C Refractories: A Review10.3390/ma16237396 ↗
5. Improvement in the properties of low carbon MgO-C refractories through the addition of graphite-SiC micro- composite10.1016/j.jeurceramsoc.2021.11.049 ↗
6. Effect of Al4SiC4 addition to carbon-containing refractories10.2109/jcersj.103.235 ↗
7. A novel strategy for the fabrication of AlN–AlON refractories: Nitrogen gas pressure sintering of Al4O4C10.1111/jace.18709 ↗
8. Oxidation mechanism of MAX phases (Ti3AlC2 powders) with and without Sn doping10.1016/j.corsci.2020.109197 ↗
9. Influence of Ti3AlC2 addition on water vapor resistance of low‐carbon Al2O3–C refractories10.1111/ijac.14219 ↗
10. Fabrication of novel AlN-SiC-C refractories by nitrogen gas-pressure sintering of Al4SiC410.1016/j.jeurceramsoc.2022.02.058 ↗
11. Synthesis of monophase Al4O4C and the effect of Al4O4C addition to MgO–C refractory10.1016/j.jallcom.2013.06.088 ↗
12. In-situ formation of plate-like Al4O4C and MWCNTs in Al2O3–C refractories with Al4SiC4 additives10.1016/j.matchemphys.2021.124363 ↗
13. Elucidating the role of Ti3AlC2 in low carbon MgO-C refractories: antioxidant or alternative carbon source?10.1016/j.jeurceramsoc.2018.03.035 ↗
14. Enhanced oxidation resistance of low-carbon MgO–C refractories with ternary carbides: a review10.1007/s42243-022-00804-5 ↗
15. Oxidation protection of MgO–C refractories by means of Al8B4C710.1111/j.1151-2916.2001.tb00701.x ↗
16. Enhanced oxidation resistance of low-carbon MgO–C refractories with Al3BC3–Al antioxidants: A synergistic effect10.1111/jace.19023 ↗
17. Comparative study of B4C, Mg2B2O5, and ZrB2 powder additions on the mechanical properties, oxidation, and slag corrosion resistance of MgO–C refractories10.1016/j.ceramint.2022.01.297 ↗
18. Corrosion mechanism of Al2O3–SiC–C refractory by SiO2–MgO-based slag10.1016/j.ceramint.2020.07.327 ↗
19. Interfacial phenomena and metallurgical processes10.1179/cmq.1982.21.2.111 ↗
20. Corrosion mechanism of Cr2O3-Al2O3-ZrO2 refractories in a coal-water slurry gasifier: A post-mortem analysis10.1016/j.corsci.2019.108250 ↗
21. Corrosion and penetration behaviors of slag/steel on the corroded interfaces of Al2O3-C refractories: Role of Ti3AlC210.1016/j.corsci.2018.08.022 ↗
22. Viscosities of the quaternary Al2O3-CaO-MgO-SiO2 slags10.1002/srin.201000150 ↗
23. Oxidation behavior of Al3BC3 powders at 800–1400 °C in ambient air10.1016/j.jmrt.2023.01.042 ↗
24. First-principles prediction of low shear-strain resistance of Al3BC3: a metal borocarbide containing short linear BC2 units10.1063/1.2220549 ↗
25. First-principles study of ternary metal boride compounds containing finite linear BC2 units10.1016/S0022-4596(03)00348-7 ↗
26. Mineralizing magnesium aluminate spinel formation with B2O310.1111/j.1551-2916.2006.01189.x ↗
27. Magnesium Aluminate Spinel: Structure, Properties, Synthesis and Applications10.1080/0371750X.2022.2137701 ↗
28. The influence of B2O3 on spinel formation in the Al2O3-MgO-B2O3 system
29. Influence of sintering temperature on the interfacial behavior of Ti3Al(Si)C2 ceramic and Ti6Al4V alloy10.1111/jace.18703 ↗
30. Rapidly quenched metastable iron–boron solid solutions10.1016/0038-1098(78)90561-6 ↗
31. Influence of microsilica content on the slag resistance of castables containing porous corundum–spinel aggregates10.1111/j.1744-7402.2008.02240.x ↗
32. Chemical corrosion behavior of chrome-free SiC-MgAl2O4 composites under simulated coal-water gasification conditions10.1016/j.corsci.2022.110560 ↗
33. The development of a thermodynamic model for Al2O3–MgO refractory castable corrosion by secondary metallurgy steel ladle slags10.1016/j.ceramint.2008.04.002 ↗
34. Solid precipitation behaviors in coal slag from different primary phases and their effects on slag viscosity from thermochemistry and experimental10.3390/pr11051522 ↗
35. Corrosion study of novel Cr-free alumina-spinel refractory material dedicated to the copper industry10.1016/j.jeurceramsoc.2022.08.038 ↗
36. Slag attack evaluation of in situ spinel-containing refractory castables via experimental tests and thermodynamic simulations10.1016/j.ceramint.2011.09.033 ↗
37. Corrosion of magnesium aluminate spinel-rich refractories by sulphur-containing slag10.1016/j.jeurceramsoc.2014.11.031 ↗
38. Densification mechanism of porous alumina plugs by molten steel with different oxygen levels10.1016/j.jeurceramsoc.2018.01.031 ↗
39. Influence of additives on corrosion resistance and corroded microstructures of MgO–C refractories10.1016/S0955-2219(01)00208-4 ↗
40. Calculation and analysis of the structure and viscosity of B2O3-regulated CaO-Al2O3-based mold fluxes
41. Influence of additives on slag resistance of Al2O3‐SiO2‐SiC‐C refractory bond phases under reducing atmosphere10.1111/j.1151-2916.1998.tb02754.x ↗
42. Influence of B2O3 on viscosity and structure of low MgO slag containing titanium10.1051/metal/2017103 ↗
43. Thermodynamic stability of spinel phase at the interface between alumina refractory and CaO–CaF2–SiO2–Al2O3–MgO–MnO slags10.1111/jace.13570 ↗
44. Slag resistance of Al2O3–MgO refractory castables in different environmental conditions10.1111/jace.12433 ↗
45. Microstructural analysis of corroded alumina-spinel castable refractories10.1016/S0955-2219(96)00073-8 ↗
46. Melt corrosion of oxide and oxide–carbon refractories10.1179/095066099101528234 ↗
47. Influence of FeO/SiO2 and CaO/SiO2 ratios in iron‐saturated ZnO-rich fayalite slags on the corrosion of MgO10.1111/jace.14379 ↗
48. Recycled magnesia-carbon aggregate as the component of new type of MgO-C refractories10.1016/j.conbuildmat.2020.121912 ↗