journal article·2021-08

Ablation behavior of ZrC-SiC-ZrB2 and ZrC-SiC inhibited carbon/carbon composites components under ultrahigh temperature conditions

Zhigang Zhao, Kezhi Li, Wei Li

Corrosion Science· Volume 189
Publisher page

Abstract

Abstract The ZrC-SiC-ZrB2 and ZrC-SiC inhibited carbon/carbon composites wedge shaped components were fabricated by reactive melt infiltration and tested on an oxyacetylene torch at the heat flux of 2.38 MW/m2 for 120 s. Compared with C/C composites, both of the inhibited composites components exhibited better ablation resistance. The tip temperatures of the composites components reached about 2500 °C. A structure evolution on the surfaces of the inhibited composites components included the porous ZrO2 layer near the tip, the layered structure of the outer ZrO2 layer and the subsurface ZrO2-SiO2 layer in the intermediate region and the SiO2 layer in the tail.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Diamond and Carbon-based Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. Advanced structural ceramics in aerospace propulsion10.1038/nmat4687 ↗
2. Oxidation behavior of aerospace materials in high enthalpy flows using an oxyacetylene torch facility10.1111/jace.13462 ↗
3. Ultra-high temperature ceramics: materials for extreme environments10.1016/j.scriptamat.2016.10.018 ↗
4. Thermal and oxidation response of UHTC leading edge samples exposed to simulated hypersonic flight conditions10.1111/jace.12180 ↗
5. Savage · 1993 · 323
6. Arc-jet testing of ultra-high-temperature-ceramics10.1016/j.ast.2009.12.004 ↗
7. Resistance to thermal shock and to oxidation of metal diborides–SiC ceramics for aerospace application10.1111/j.1551-2916.2007.01589.x ↗
8. SiC Depletion in ZrB2–30 vol% SiC at ultrahigh temperatures10.1111/jace.13519 ↗
9. Ceramic matrix composite (CMC) thermal protection systems (TPS) and hot structures for hypersonic vehicles
10. Fitzer · 1998 · 310
11. Ablation mechanism of C/C–ZrB2–ZrC–SiC composite fabricated by polymer infiltration and pyrolysis with preform of Cf/ZrB210.1016/j.corsci.2015.05.064 ↗
12. Ablation resistance of wedge-shaped C/C-ZrB2-ZrC-SiC composites exposed to an oxyacetylene torch10.1016/j.corsci.2016.08.010 ↗
13. Effect of reaction melt infiltration temperature on the ablation properties of 2D C/C–SiC–ZrC composites10.1016/j.corsci.2012.01.001 ↗
14. Microstructures and ablation properties of C/C−SiC−ZrC composites prepared using C/C skeletons with various densities10.1016/j.ceramint.2013.03.093 ↗
15. Erosion resistance of C/C-SiC-ZrB2 composites exposed to oxyacetylene torch10.1016/j.jeurceramsoc.2016.04.007 ↗
16. Ablation behavior of sharp-shape C/C-SiC-ZrB2 composites under oxyacetylene flame10.1016/j.jallcom.2017.04.188 ↗
17. Carbon fibre reinforced CMC for high performance structures10.1111/j.1744-7402.2004.tb00169.x ↗
18. Heat flux mapping of oxyacetylene flames and their use to characterise Cf-HfB2 composites10.1080/17436753.2015.1104050 ↗
19. Thermoablative resistance of ZrB2-SiC-WC ceramics at 2400 °C10.1016/j.actamat.2017.05.033 ↗
20. Ablation behaviors of ultra-high temperature ceramic composites10.1016/j.msea.2007.02.040 ↗
21. Ablation behavior of ZrB2–SiC ultra high temperature ceramics under simulated atmospheric re-entry conditions10.1016/j.compscitech.2008.02.009 ↗
22. Aerothermal behaviour of a SiC fibre-reinforced ZrB2 sharp component in supersonic regime10.1016/j.jeurceramsoc.2012.01.019 ↗
23. Cyclic ablation behavior of C/C-ZrC-SiC-ZrB2 composites under oxyacetylene torch with two heat fluxes at the temperatures above 2000 ºC10.1016/j.corsci.2020.109202 ↗
24. Effect of heat flux on ablation behaviour and mechanism of C/C-ZrB2-SiC composite under oxyacetylene torch flame10.1016/j.corsci.2013.04.052 ↗
25. Zhang · 2014 · 33
26. Microstructure and mechanical properties of three dimensional Cf/SiC-ZrC-ZrB2 composites prepared by reactive melt infiltration method10.1016/j.jeurceramsoc.2016.07.002 ↗
27. Chase · 1998
28. Kalpakjian · 2009 · 865
29. Material property requirements for analysis and design of UHTC components in hypersonic applications10.1016/j.jeurceramsoc.2010.01.026 ↗
30. Oxidation microstructure studies of reinforced carbon/carbon10.1016/j.carbon.2005.11.013 ↗
31. UHTC–carbon fibre composites: preparation, oxyacetylene torch testing and characterisation10.1016/j.jeurceramsoc.2012.08.018 ↗
32. Microstructure and ablation properties of zirconium carbide doped carbon/carbon composites10.1016/j.carbon.2009.09.035 ↗
33. Oxidation-resistant ZrB2-SiC composites at 2200 °C10.1016/j.compscitech.2007.08.017 ↗
34. The ZrB2 volatility diagram10.1111/j.1551-2916.2005.00599.x ↗
35. Thermodynamic analysis of ZrB2-SiC oxidation: formation of a SiC-depleted region10.1111/j.1551-2916.2006.01329.x ↗
36. Oxidation-based materials selection for 2000 ºC + hypersonic aerosurfaces: theoretical considerations and historical experience10.1023/B:JMSC.0000041686.21788.77 ↗
37. Plasma wind tunnel testing of ultra-high temperature ZrB2-SiC composites under hypersonic re-entry conditions10.1016/j.jeurceramsoc.2010.01.029 ↗
38. Dynamic oxidation of ultra-high temperature ZrB2–SiC under high enthalpy supersonic flows10.1016/j.corsci.2010.11.018 ↗