journal article·2022-01

The effect of carboxylate compounds on Volta potential and corrosion inhibition of Mg containing different levels of iron

K.A. Yasakau, A. Maltseva, S.V. Lamaka, Di Mei, H. Orvi, P. Volovitch, M.G.S. Ferreira, M.L. Zheludkevich

Corrosion Science· Volume 194
Publisher page

Abstract

Abstract Corrosion protection and surface properties of Magnesium (Mg) containing 51 ppm Fe (HP-Mg) and 341 ppm Fe (CP-Mg) were assessed by EIS, AFM/SKPFM, and photoluminescence spectroscopy in NaCl solutions with/without fumarate (Fum), 2,5-pyridinedicarboxylate (PDCA) and salicylate (Sal) carboxylates. The PDCA was effective in corrosion inhibition of HP-Mg and CP-Mg, while the Sal was efficient in inhibition of CP-Mg only. Volta potential (VPD) changes on Mg were evaluated considering the contribution of molecular dipoles and chemical dipoles due to interaction of carboxylate groups present in carboxylates with Mg. VPD of CP-Mg increased due to adsorption of Fe(III)-salicylate complexes and salicylate molecules.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Magnesium Alloys: Properties and Applications · Concrete Corrosion and Durability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (98)

Show source-provided references
1. Magnesium: industrial and research developments over the last 15 years10.5006/1474 ↗
2. Biodegradable magnesium alloys: a review of material development and applications10.4028/www.scientific.net/JBBTE.12.25 ↗
3. Review of recent developments in the field of magnesium corrosion10.1002/adem.201400434 ↗
4. Assessing the corrosion of biodegradable magnesium implants: a critical review of current methodologies and their limitations10.1016/j.actbio.2011.11.014 ↗
5. Fundamentals and advances in magnesium alloy corrosion10.1016/j.pmatsci.2017.04.011 ↗
6. Comprehensive screening of Mg corrosion inhibitors10.1016/j.corsci.2017.07.011 ↗
7. Correlation between electrochemical impedance measurements and corrosion rate of magnesium investigated by real-time hydrogen measurement and optical imaging10.1016/j.electacta.2015.03.050 ↗
8. Accurate electrochemical measurement of magnesium corrosion rates; a combined impedance, mass-loss and hydrogen collection study10.1016/j.electacta.2013.12.124 ↗
9. The effect of iron re-deposition on the corrosion of impurity-containing magnesium10.1039/C5CP05577F ↗
10. Poisoning the corrosion of magnesium10.1016/j.elecom.2013.07.021 ↗
11. A high-specific-strength and corrosion-resistant magnesium alloy10.1038/nmat4435 ↗
12. Introductory lecture on corrosion chemistry: a focus on anodic hydrogen evolution on Al and Mg10.1039/C5FD00066A ↗
13. The negative difference effect and unipositive Mg10.1002/adem.200600275 ↗
14. The behaviour of magnesium during free corrosion and potentiodynamic polarization investigated by real-time hydrogen measurement and optical imaging10.1016/j.electacta.2013.12.109 ↗
15. Effect of impurities on the enhanced catalytic activity for hydrogen evolution in high purity magnesium10.1016/j.electacta.2015.03.021 ↗
16. Enhanced hydrogen evolution on Mg (OH)2 covered Mg surfaces10.1016/j.electacta.2015.02.079 ↗
17. The source of anodic hydrogen evolution on ultra high purity magnesium10.1016/j.electacta.2016.07.018 ↗
18. Corrosion mechanism and hydrogen evolution on Mg10.1016/j.cossms.2014.09.005 ↗
19. Electrochemical behavior of the magnesium anode10.1149/1.2428007 ↗
20. Potentiostatic study of the magnesium electrode in aqueous solution10.1016/S0022-0728(70)80201-7 ↗
21. Physical and electrochemical evidence for the role of a Mg hydride species in Mg alloy corrosion10.5006/2918 ↗
22. Corrosion mechanisms of magnesium alloys10.1002/(SICI)1527-2648(199909)1:1<11::AID-ADEM11>3.0.CO;2-N ↗
23. The source of hydrogen evolved from a magnesium anode10.1016/j.elecom.2013.08.023 ↗
24. A novel approach to on-line measurement of gas evolution kinetics: application to the negative difference effect of Mg in chloride solution10.1016/j.electacta.2013.07.131 ↗
25. Evidence of the enrichment of transition metal elements on corroding magnesium surfaces using rutherford backscattering spectrometry10.1149/2.0541506jes ↗
26. The pH dependence of magnesium dissolution and hydrogen evolution during anodic polarization10.1149/2.0621507jes ↗
27. On the Fe enrichment during anodic polarization of Mg and its impact on hydrogen evolution10.1149/2.0251508jes ↗
28. A new concept for corrosion inhibition of magnesium: suppression of iron re-deposition10.1016/j.elecom.2015.10.023 ↗
29. In situ surface film evolution during Mg aqueous corrosion in presence of selected carboxylates10.1016/j.corsci.2020.108484 ↗
30. ATR-FTIR in Kretschmann configuration integrated with electrochemical cell as in situ interfacial sensitive tool to study corrosion inhibitors for magnesium substrates10.1016/j.electacta.2020.136166 ↗
31. Corrosion inhibition of pure Mg containing a high level of iron impurity in pH neutral NaCl solution10.1016/j.corsci.2018.07.027 ↗
32. Investigating the effect of ferrous ions on the anomalous hydrogen evolution on magnesium in acidic ferrous chloride solution10.1149/2.0951813jes ↗
33. Impact of microgalvanic corrosion on the degradation morphology of WE43 and pure magnesium under exposure to simulated body fluid10.1016/j.corsci.2011.12.026 ↗
34. Characterization of AA2024–T3 by scanning Kelvin probe force microscopy10.1149/1.1838633 ↗
35. Calibration of the scanning Kelvin probe force microscope under controlled environmental conditions10.1016/j.electacta.2012.01.054 ↗
36. High-resolution Kelvin probe microscopy in corrosion science: scanning Kelvin probe force microscopy (SKPFM) versus classical scanning Kelvin probe (SKP)10.1016/j.electacta.2007.03.016 ↗
37. Volta potentials measured by scanning Kelvin probe force microscopy as relevant to corrosion of magnesium alloys10.5006/1432 ↗
38. Volta potential of oxidized aluminum studied by scanning Kelvin probe force microscopy10.1021/jp1011044 ↗
39. Sacrificial protection of Mg-based resorbable implant alloy by magnetron sputtered Mg5Gd alloy coating: a short-term study10.1016/j.corsci.2021.109590 ↗
40. The physical meaning of electrode potentials at metal surfaces and polymer/metal interfaces: consequences for delamination10.1149/1.2926589 ↗
41. Volta potential evolution of intermetallics in aluminum alloy microstructure under thin aqueous adlayers: a combined DFT and experimental study10.1007/s11244-018-0939-9 ↗
42. Kelvin microprobe analytics on iron-enriched corroded magnesium surface10.5006/2260 ↗
43. Resolution and contrast in Kelvin probe force microscopy10.1063/1.368181 ↗
44. Surface potential mapping: a qualitative material contrast in SPM10.1016/S0304-3991(97)00027-2 ↗
45. Kelvin probe force microscopy of nanocrystalline TiO2 photoelectrodes10.3762/bjnano.4.49 ↗
46. Scanning Kelvin probe study of metal/polymer interfaces10.1016/j.electacta.2004.01.054 ↗
47. Tuning the surface potential of Ag surfaces by chemisorption of oppositely-oriented thiolated carborane dipoles10.1016/j.jcis.2010.10.052 ↗
48. Effects of surface treatment and carboxylic acid and anhydride molecular dipole moments on the volta potential values of zinc surfaces10.1021/jp3096049 ↗
49. The role of intermetallics on the corrosion initiation of twin roll cast AZ31 Mg alloy10.1149/2.0291509jes ↗
50. On the volta potential measured by SKPFM – fundamental and practical aspects with relevance to corrosion science10.1080/1478422X.2019.1583436 ↗
51. Application of AFM-based techniques in studies of corrosion and corrosion inhibition of metallic alloys10.3390/cmd1030017 ↗
52. Insight into physical interpretation of high frequency time constant in electrochemical impedance spectra of Mg10.1016/j.corsci.2021.109501 ↗
53. On the corrosion mechanism of Mg investigated by electrochemical impedance spectroscopy10.1016/j.electacta.2019.03.080 ↗
54. An impedance investigation of the mechanism of pure magnesium corrosion in sodium sulfate solutions10.1149/1.2401056 ↗
55. The anodic surface film and hydrogen evolution on Mg10.1016/j.corsci.2015.05.047 ↗
56. Effect of pH on Mg(OH)2 film evolution on corroding Mg by in situ kinetic Raman mapping (KRM)10.1016/j.corsci.2019.03.024 ↗
57. Recent progress in the synthesis of nanostructured magnesium hydroxide10.1039/C7CE01570D ↗
58. On the in-situ aqueous stability of an Mg-Li-(Al-Y-Zr) alloy: role of Li10.1016/j.corsci.2019.108342 ↗
59. Luminescence of F and F+ centers in magnesium oxide10.1103/PhysRevB.39.10309 ↗
60. Blue and orange photoluminescence and surface band-gap narrowing in lithium-doped MgO microcrystals10.1021/acs.jpcc.6b12177 ↗
61. Electron transfer at oxide surfaces. The MgO paradigm: from defects to ultrathin films10.1021/cr3002017 ↗
62. Luminescence from oxygen vacancies in MgO crystals thermochemically reduced at high temperatures10.1103/PhysRevB.27.1283 ↗
63. Physicochemical and in situ photoluminescence study of the reversible transformation of oxide ions of low coordination into hydroxyl groups upon interaction of water and methanol with MgO10.1021/jp048760+ ↗
64. O2 adsorption dependent photoluminescence emission from metal oxide nanoparticles10.1039/C4CP03080J ↗
65. Photoluminescence quenching in compressed MgO nanoparticle systems10.1039/c3cp54582b ↗
66. The electrochemical corrosion of pure magnesium in 1 N NaCl10.1016/S0010-938X(96)00172-2 ↗
67. Analysis of the surface film formed on Mg by exposure to water using a FIB cross-section and STEM–EDS10.1016/j.corsci.2012.03.001 ↗
68. Initial surface film on magnesium metal: a characterization by X-ray photoelectron spectroscopy (XPS) and photocurrent spectroscopy (PCS)10.1016/j.electacta.2007.03.019 ↗
69. Novel electrochemical techniques in corrosion research, In: M. Schutze (Ed.) materials science and technology
70. Influence of oxygen and argon plasma treatments on the chemical structure and redox state of oxide covered iron10.1016/S0169-4332(98)00617-5 ↗
71. Imaging for uniformity of lithium metal surface using tapping mode-atomic force and surface potential microscopy10.1021/jp002014x ↗
72. Application of Volta potential mapping to determine metal surface defects10.1016/j.electacta.2007.05.077 ↗
73. Exciton thermoreflectance of MgO and CaO10.1016/0038-1098(73)90754-0 ↗
74. Semiempirical correlation between optical band gap values of oxides and the difference of electronegativity of the elements. Its importance for a quantitative use of photocurrent spectroscopy in corrosion studies10.1021/jp970046n ↗
75. Semiempirical correlation between the optical band gap of oxides and hydroxides and the electronegativity of their constituents10.1557/PROC-654-AA4.8.1 ↗
76. Investigation of Mg(O,OH) films prepared by chemical bath deposition as buffer layers for Cu(In,Ga)Se2 solar cells10.1149/1.3609047 ↗
77. Disorder, defects, and band gaps in ultrathin (001) MgO tunnel barrier layers10.1103/PhysRevB.73.205412 ↗
78. The initial oxidation of magnesium: an in situ study with XPS, HERDA and ellipsometry10.1002/sia.2349 ↗
79. Work function changes induced by deposition of ultrathin dielectric films on metals: a theoretical analysis10.1103/PhysRevB.78.235423 ↗
80. Oxide films at the nanoscale: new structures, new functions, and new materials10.1021/ar200139y ↗
81. Work function shifts, Schottky barrier height, and ionization potential determination of thin MgO films on Ag(001)10.1063/1.3525159 ↗
82. Work function measurements of thin oxide films on metals—MgO on Ag(001)10.1021/jp901226q ↗
83. Defects on bulk MgO(001) imaged by nc-AFM
84. Reactivity of (H+)(e−) color centers at the MgO surface: formation of O2− and N2− radical anions10.1016/S0039-6028(03)01000-8 ↗
85. Kelvin probe force microscopy on MgO(001) surfaces and supported Pd nanoclusters10.1021/jp807340k ↗
86. Surface dipoles and work functions of alkylthiolates and fluorinated alkylthiolates on Au(111)10.1021/jp0642847 ↗
87. Estimation of group dipole moments from surface potential measurements on Langmuir monolayers10.1039/f19898501009 ↗
88. Birdi · 2002
89. Surface photovoltage phenomena: theory, experiment, and applications10.1016/S0167-5729(99)00002-3 ↗
90. Cooperative effects and dipole formation at semiconductor and self-assembled-monolayer interfaces10.1103/PhysRevB.73.193310 ↗
91. Work function on dye-adsorbed TiO2 surfaces measured by using a Kelvin probe force microscope10.1021/jp077065+ ↗
92. Influence of the sensitizer adsorption mode on the open-circuit potential of dye-sensitized solar cells10.1021/nl071835b ↗
93. Development of stabilized magnetite nanoparticles for medical applications10.1155/2017/6514659 ↗
94. New copper(II) complexes including pyridine-2,5-dicarboxylic acid: synthesis, spectroscopic, thermal properties, crystal structure and how these complexes interact with purified PON 1 enzyme10.1080/00958972.2016.1188295 ↗
95. Ab initio modeling of the bonding of benzotriazole corrosion inhibitor to reduced and oxidized copper surfaces10.1039/C4FD00257A ↗
96. Binuclear complexes of iron(III) with salicylate ligands10.1080/00958977708073022 ↗
97. Salicylate coordination compounds of iron, models of their formation
98. Dean · 1978