Corrosion characterization and ion release in SLM-manufactured and wrought Ti6Al4V alloy in an oral environment
Source abstract
Abstract
As-produced and heat-treated TiAlV samples were prepared by selective laser melting and compared to wrought samples of identical chemical composition. Microstructural, corrosion, and spectroscopic studies of additively manufactured samples in artificial saliva at 37 °C, with NaF and at pH 2.3 were as a novelty combined with metal ion release during 42 days immersion. In artificial saliva higher amount of ions was released on SLM specimen when compared to wrought alloy. The total amount of ions released from SLM specimen in AS containing NaF was 10-times higher than in AS, while in AS with lactic acid it was 100-times higher.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Titanium Alloys Microstructure and Properties · Dental materials and restorations
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (45)
Show source-provided references
1. Passive layers and corrosion resistance of biomedical Ti-6Al-4V and β-Ti alloys10.3390/coatings11050487 ↗
2. Synergistic interactions between corrosion and wear at titanium-based dental implant connections: a scoping review10.1111/jre.12469 ↗
3. Is there scientific evidence favoring the substitution of commercially pure titanium with titanium alloys for the manufacture of dental implants?10.1016/j.msec.2016.10.025 ↗
4. On the response of Ti–6Al–4V and Ti–6Al–7Nb alloys to a Nitron-100 treatment10.1016/j.surfcoat.2014.11.034 ↗
5. Can degradation products released from dental implants affect peri‐implant tissues?10.1111/jre.12479 ↗
6. Determinants of corrosion resistance of Ti-6Al-4V alloy dental implants in an In Vitro model of peri-implant inflammation
7. A comprehensive review on the corrosion pathways of titanium dental implants and their biological adverse effects10.3390/met10091272 ↗
8. Particle release from implantoplasty of dental implants and impact on cells10.1186/s40729-020-00247-1 ↗
9. Elucidating the corrosion-related degradation mechanisms of a Ti-6Al-4V dental implant10.1016/j.dental.2020.01.008 ↗
10. The effect of metal ions released from different dental implant-abutment couples on osteoblast function and secretion of bone resorbing mediators10.1016/j.jdent.2017.08.002 ↗
11. Potential causes of titanium particle and ion release in implant dentistry: a systematic review10.3390/ijms19113585 ↗
12. Fretting corrosion behavior of additive manufactured and cryogenic-machined Ti6Al4V for biomedical applications: fretting corrosion behavior of cryogenic machined Ti6Al4V10.1002/adem.201500629 ↗
13. A literature review study on atomic ions dissolution of titanium and its alloys in implant dentistry10.3390/ma12030368 ↗
14. Influence of the machining cooling strategies on the dental tribocorrosion behaviour of wrought and additive manufactured Ti6Al4V10.1016/j.biotri.2017.03.002 ↗
15. Development of an artificial saliva solution for studying the corrosion behavior of dental alloys10.5006/1.3287764 ↗
16. Microstructural examination and corrosion behavior of selective laser melted and conventionally manufactured Ti6Al4V for dental applications10.1016/j.msec.2020.110980 ↗
17. Passive film on orthopaedic TiAlV alloy formed in physiological solution investigated by X-ray photoelectron spectroscopy10.1016/S0142-9612(00)00145-9 ↗
18. Corrosion behavior of titanium in artificial saliva by lactic acid10.3390/ma7085528 ↗
19. Fabrication and characterization of selective laser melting printed Ti–6Al–4V alloys subjected to heat treatment for customized implants design10.1016/j.pnsc.2016.12.006 ↗
20. C.V. Funch, K. Somlo, K. Poulios, S. Mohanty, M.A.J. Somers, T.L. Christiansen, The influence of microstructure on mechanical properties of SLM 3D printed Ti-6Al-4V, MATEC Web Conf. 321 (2020) 03005. https://doi.org/10.1051/matecconf/202032103005.10.1051/matecconf/202032103005 ↗
21. Influence of material microstructures in micromilling of Ti6Al4V alloy10.3390/ma6094268 ↗
22. Corrosion evaluation of Ti–6Al–4V manufactured by electron beam melting in Ringer’s physiological solution: an in vitro study of the passive film10.1007/s10800-022-01683-0 ↗
23. Corrosion behavior of Ti-6Al-4V with different thermomechanical treatments and microstructures10.5006/1.3452400 ↗
24. Effect of surface powder particles and morphologies on corrosion of Ti-6Al-4 V fabricated with different energy densities in selective laser melting10.1016/j.matdes.2021.110184 ↗
25. Martensite formation and decomposition during traditional and AM processing of two-phase titanium alloys—an overview10.3390/met11030481 ↗
26. Microstructure and mechanical behavior of Ti–6Al–4V produced by rapid-layer manufacturing, for biomedical applications10.1016/j.jmbbm.2008.05.004 ↗
27. Corrosion behaviour of electron beam melted Ti6Al4V: effects of microstructural variation10.1149/1945-7111/abb9d1 ↗
28. Formation and control of martensite in Ti-6Al-4V alloy produced by selective laser melting10.1016/j.matdes.2016.06.117 ↗
29. Electrochemical studies on the stability and corrosion resistance of titanium-based implant materials10.1016/S0142-9612(00)00309-4 ↗
30. Electrochemical impedance spectroscopy characterization of passive film formed on implant Ti–6Al–7Nb alloy in Hank’s solution10.1023/B:JMSM.0000010097.86245.74 ↗
31. Study of the corrosion behavior of titanium and some of its alloys for biomedical and dental implant applications10.1016/S0022-0728(99)00260-0 ↗
32. Electrical properties of nanocrystalline CeO[sub 2] thin films deposited by in situ pulsed laser deposition10.1149/1.2165778 ↗
33. Broadband dielectric characterization of TiO2 ceramics sintered through microwave and conventional processes10.1016/j.ceramint.2012.06.025 ↗
34. Resolving surface chemical states in XPS analysis of first row transition metals, oxides and hydroxides: Sc, Ti, V, Cu and Zn10.1016/j.apsusc.2010.07.086 ↗
35. Corrosion behaviour and cell interaction of Ti-6Al-4V alloy prepared by two techniques of 3D printing10.1016/j.msec.2018.08.066 ↗
36. Physical electronics, incorporation
37. A methodology to systematically investigate the diffusion degradation of cemented carbide during machining of a titanium alloy10.3390/ma12142271 ↗
38. Physical characterization of 3 implant systems made of distinct materials with distinct surfaces
39. On the interactions of human bone cells with Ti6Al4V thermally oxidized by means of laser shock processing10.1088/1748-6041/11/1/015009 ↗
40. Surface (XPS, SIMS) chemical investigation on poly(pyrrole-3-acetic acid) films electrosynthesized on Ti and TiAlV substrates for the development of new bioactive substrates10.1002/sia.2053 ↗
41. Pourbaix · 1974
42. Evaluation of metal ion release from Ti6Al4V and Co-Cr-Mo casting alloys: in vivo and in vitro study: metal ion release from Ti6Al4V and Co-Cr-Mo casting alloys10.1111/jopr.12067 ↗
43. The effect of fluoride ions on the corrosion behaviour of Ti metal, and Ti6-Al-7Nb and Ti-6Al-4V alloys in artificial saliva
44. The corrosion behavior of Ti6Al4V fabricated by selective laser melting in the artificial saliva with different fluoride concentrations and pH values10.1016/j.corsci.2020.109097 ↗
45. Influence of fluoride ions in artificial saliva solution to corrosion behavior of Ti-6Al-4V and Ti-10Mo-4Zr titanium alloys