journal article·2024-06

In-depth understanding in the effect of hydrogen on microstructural evolution, mechanical properties and fracture micro-mechanisms of advanced high-strength steels welded joints

Junliang Xue, Wei Guo, Mingsheng Xia, Yongxin Zhang, Caiwang Tan, Jiaxin Shi, Xiang Li, Ying Zhu, Hongqiang Zhang

Corrosion Science· Volume 233
Publisher page

Abstract

The hydrogen embrittlement (HE) mechanism of QP980 steels laser welded joints with complex microstructures is unclear. The joint with hydrogen pre-charging fractured at the inter-critical heat affected zone (ICHAZ) in slow strain rate tensile test, and the relative loss of elongation amounted to 84.8 %. Hydrogen-induced microcracks mainly initiated inside martensite (∼ 60 %). Hydrogen-induced crack propagation paths of the joint were transgranular propagation of martensite and intergranular propagation of ferrite/martensite interface. The HE mechanism of the joint was the combination of the effects in hydrogen-enhanced localized plasticity (HELP) and hydrogen-enhanced decohesion (HEDE).
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Microstructure and Mechanical Properties of Steels · Material Properties and Failure Mechanisms

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (68)

Show source-provided references
1. Carbon-induced negative strain-rate sensitivity in a quenching and partitioning steel10.1016/j.actamat.2023.119099 ↗
2. Carbon partitioning into austenite after martensite transformation10.1016/S1359-6454(03)00059-4 ↗
3. A comparative study on the wear behavior of dual phase (DP) steel and quenching and partitioning (QP) steel10.1016/j.triboint.2024.109445 ↗
4. A mesoscale crystal plasticity model to predict room-temperature deformation and martensitic transformation of high-strength Quenching and Partitioning (Q&P) Steels and validation with synchrotron X-ray diffraction10.1016/j.ijplas.2023.103833 ↗
5. Interaction of carbon partitioning, carbide precipitation and bainite formation during the Q&P process in a low C steel10.1016/j.actamat.2015.11.032 ↗
6. An in situ investigation of neighborhood effects in a ferrite-containing quenching and partitioning steel: mechanical stability, strain partitioning, and damage10.1016/j.actamat.2023.118985 ↗
7. A comprehensive overview of high strength and toughness steels for automobile based on QP process10.1016/j.jmrt.2023.09.210 ↗
8. Keyhole threshold and morphology in laser melting revealed by ultrahigh-speed x-ray imaging10.1126/science.aav4687 ↗
9. Keyhole formation and thermal fluid flow-induced porosity during laser fusion welding in titanium alloys: experimental and modelling10.1016/j.actamat.2016.12.062 ↗
10. Microstructure and mechanical properties of fiber laser welded QP980 steel10.1016/j.jmatprotec.2018.02.015 ↗
11. Local microstructure and mechanical characteristics of HAZ and tensile behavior of laser welded QP980 joints10.1016/j.msea.2022.143862 ↗
12. Evaluation of hydrogen diffusion and trapping in AHSS and effects of laser-welding
13. Effect of hydrogen in advanced high strength steel materials10.1016/j.ijhydene.2019.08.149 ↗
14. The effect of hydrogen content and yield strength on the distribution of hydrogen in steel: a diffusion coupled micromechanical FEM study10.1016/j.actamat.2021.116799 ↗
15. Effect of plastic strain on corrosion-induced hydrogen infusion and embrittlement behaviors of Zn-coated ultra-high strength steel sheet10.1016/j.surfcoat.2023.130335 ↗
16. In-situ measurement of hydrogen entry and hydrogen embrittlement of steel by atmospheric corrosion10.1016/j.corsci.2023.111212 ↗
17. Hydrogen embrittlement in high strength fasteners: comparison between bainitic and tempered martensitic steels10.1016/j.engfailanal.2023.107474 ↗
18. Effects of heterogeneous plastic strain on hydrogen-induced cracking of twinning-induced plasticity steel: a quantitative approach10.1016/j.corsci.2022.110782 ↗
19. Critical role of Lüders banding in hydrogen embrittlement susceptibility of medium Mn steels10.1016/j.scriptamat.2020.08.025 ↗
20. Hydrogen trapping ability of steels with different microstructures10.1080/02533839.1999.9670440 ↗
21. Thermal desorption spectroscopy study of the interaction between hydrogen and different microstructural constituents in lab cast Fe–C alloys10.1016/j.corsci.2012.08.017 ↗
22. The influence of hydrogen on the mechanical and fracture properties of some martensitic advanced high strength steels studied using the linearly increasing stress test10.1016/j.corsci.2015.06.038 ↗
23. Proposal of a hydrogen embrittlement index for a martensitic advanced high-strength steel10.1016/j.corsci.2023.111357 ↗
24. Hydrogen-induced fast fracture in notched 1500 and 1700 MPa class automotive martensitic advanced high-strength steel10.1016/j.corsci.2021.109550 ↗
25. Comparing hydrogen embrittlement behaviors of two press hardening steels: 2 GPa vs. 1.5 GPa grade10.1016/j.jmst.2022.02.020 ↗
26. Hydrogen blistering and hydrogen-induced cracking in amorphous nickel phosphorus coating10.1016/j.jnoncrysol.2007.06.037 ↗
27. Enumeration of the hydrogen-enhanced localized plasticity mechanism for hydrogen embrittlement in structural materials10.1016/j.actamat.2018.12.014 ↗
28. Hydrogen-enhanced localized plasticity—a mechanism for hydrogen-related fracture10.1016/0921-5093(94)90975-X ↗
29. Equilibrium aspects of hydrogen-induced cracking of steels10.1016/0001-6160(74)90061-3 ↗
30. Hydrogen behavior in high strength steels during various stress applications corresponding to different hydrogen embrittlement testing methods10.1016/j.msea.2018.08.002 ↗
31. Atomistic investigation of hydrogen induced decohesion of Ni grain boundaries10.1016/j.mechmat.2020.103586 ↗
32. The predominant role of strain-induced vacancies in hydrogen embrittlement of steels: overview10.1016/j.actamat.2018.12.013 ↗
33. Hydrogen related failure of steels – a new aspect10.1179/026708304225019687 ↗
34. The synergistic action and interplay of hydrogen embrittlement mechanisms in steels and iron: Localized plasticity and decohesion10.1016/j.engfracmech.2019.106528 ↗
35. Hydrogen embrittlement of ferritic steels: observations on deformation microstructure, nanoscale dimples and failure by nanovoiding10.1016/j.actamat.2012.06.014 ↗
36. Pre-strain and hydrogen charging effect on the plastic and fracture behavior of quenching and partitioning (Q&P) steel10.1016/j.actamat.2023.119524 ↗
37. Mitigation of hydrogen embrittlement in ultra-high strength lath martensitic steel via Ta microalloying10.1016/j.matdes.2021.110090 ↗
38. The mechanism of hydrogen embrittlement in intercritically annealed medium Mn TRIP steel10.1016/j.actamat.2016.04.038 ↗
39. Effect of heat treatment processes on hydrogen embrittlement in hot-rolled medium Mn steels10.1016/j.ijhydene.2020.04.241 ↗
40. Revealing hydrogen-induced delayed fracture in ferrite-containing quenching and partitioning steels10.1016/j.mtla.2018.09.022 ↗
41. Investigation for enhancing the resistance of H-induced delayed cracking for martensitic steel by quenching tempering and quenching partitioning: influence of microstructure on hydrogen embrittlement and cracking behavior10.1016/j.ijhydene.2022.06.059 ↗
42. Hydrogen embrittlement of a quenching and partitioning steel during corrosion and zinc electroplating10.1016/j.msea.2018.12.022 ↗
43. Effect of plastic strain damage on the hydrogen embrittlement of a dual-phase (DP) and a quenching and partitioning (Q&P) advanced high-strength steel10.1016/j.msea.2020.139343 ↗
44. Analysis of hydrogen trapping behaviour in plastically deformed quenching and partitioning steel in relation to microstructure evolution by phase transformation10.1016/j.jallcom.2022.164018 ↗
45. Simultaneous improvement of hydrogen embrittlement resistance and tensile strength of quenching and partitioning steel through dense multiple interfaces10.1016/j.ijhydene.2024.01.270 ↗
46. Effect of retained austenite stability and morphology on the hydrogen embrittlement susceptibility in quenching and partitioning treated steels10.1016/j.msea.2016.02.026 ↗
47. Hydrogen embrittlement and fracture mechanism of friction stir welded quenching and partitioning 980 steel10.1016/j.msea.2020.140683 ↗
48. Hydrogen embrittlement mechanisms in advanced high strength steel10.1016/j.actamat.2021.117488 ↗
49. Statistical study on the effects of heterogeneous deformation and grain boundary character on hydrogen-induced crack initiation and propagation in twining-induced plasticity steels10.1016/j.corsci.2021.109796 ↗
50. Equivalent hydrogen fugacity during electrochemical charging of some martensitic advanced high-strength steels10.1016/j.corsci.2017.08.011 ↗
51. Effects of the microstructure and reversed austenite on the hydrogen embrittlement susceptibility of Ni-Cr-Mo-V/Nb high-strength steel10.1016/j.corsci.2023.111164 ↗
52. Hydrogen trapping sites and hydrogen-induced cracking in high strength quenching & partitioning (Q&P) treated steel10.1016/j.ijhydene.2014.06.079 ↗
53. Mesoscopic origin of damage nucleation in dual-phase steels10.1016/j.ijplas.2020.102920 ↗
54. A review of strain analysis using electron backscatter diffraction10.1017/S1431927611000055 ↗
55. HAZ Characterization and mechanical properties of QP980-DP980 laser welded joints10.1186/s10033-021-00596-x ↗
56. Microstructural evolution and mechanical behaviors of the third–generation automobile QP980 steel under continuous tension and compression loads10.1016/j.msea.2023.145533 ↗
57. Hydrogen diffusion and hydrogen embrittlement of a 1500 MPa hot-stamped steel 22MnB5 in different austenitizing conditions10.1016/j.msea.2024.146349 ↗
58. Effect of microstructure on the hydrogen embrittlement, diffusion, and uptake of dual-phase low alloy steels with varying ferrite-martensite ratios10.1016/j.ijhydene.2023.07.061 ↗
59. Twinning behavior and hydrogen embrittlement of a pre-strained twinning-induced plasticity (TWIP) steel10.1016/j.corsci.2021.109791 ↗
60. Spatially and kinetically resolved mapping of hydrogen in a twinning-induced plasticity steel by use of scanning kelvin probe force microscopy10.1149/2.0131512jes ↗
61. Hydrogen-assisted failure in a twinning-induced plasticity steel studied under in situ hydrogen charging by electron channeling contrast imaging10.1016/j.actamat.2013.04.030 ↗
62. Hydrogen-induced cracking at grain and twin boundaries in an Fe–Mn–C austenitic steel10.1016/j.scriptamat.2011.12.015 ↗
63. Characteristics and mechanisms of hydrogen-induced quasi-cleavage fracture of lath martensitic steel10.1016/j.actamat.2021.116635 ↗
64. Investigation of quasi-cleavage in a hydrogen charged maraging stainless steel10.1016/j.corsci.2023.111163 ↗
65. In-situ observation of microcrack initiation and damage nucleation modes on the HAZ of laser-welded DP1180 joint10.1016/j.jmst.2023.01.001 ↗
66. Recent advances in the study of structural materials compatibility with hydrogen10.1002/adma.200904354 ↗
67. Hydrogen-induced intergranular failure of iron10.1016/j.actamat.2014.01.060 ↗
68. Improved rotating bending fatigue performance of laser directed energy deposited Ti6Al4V alloys by laser shock peening10.1016/j.jallcom.2024.173664 ↗