journal article·2021-05

A comparative study on liquid metal embrittlement susceptibility of three FeCrAl ferritic alloys in contact with liquid lead-bismuth eutectic at 350°C

Xing Gong, Jiajun Chen, Congying Xiang, Zhiyang Yu, Haoran Gong, Yuan Yin

Corrosion Science· Volume 183
Publisher page

Abstract

Abstract Liquid metal embrittlement (LME) susceptibility of three FeCrAl alloys (i.e., Fe10Cr4Al, Fe15Cr4Al and Fe10Cr6Al, wt%) was tested in oxygen-saturated and -depleted liquid lead-bismuth eutectic (LBE) at 350 °C using slow strain rate tensile tests. The results show that all three alloys are very susceptible to LME, manifested by a severe reduction in total elongation to failure and prevailing cleavage on fracture surfaces. LME is delayed in oxygen-saturated LBE, due to a dewetting effect of surface oxides. In three alloys, Fe10Cr6Al is most susceptible to LME, especially in presence of oxygen-depleted LBE.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Nuclear Materials and Properties · Nuclear reactor physics and engineering · Fusion materials and technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (62)

Show source-provided references
1. OECD/NEA · 2015
2. GEN-IV LFR development: status & perspectives10.1016/j.pnucene.2018.02.005 ↗
3. Overview of lead-cooled fast reactor activities10.1016/j.pnucene.2013.11.011 ↗
4. Multi-purpose hybrid research reactor for high-tech applications a multipurpose fast spectrum research reactor10.1002/er.1891 ↗
5. Opportunities for the LWR ATF materials development program to contribute to the LBE-cooled ADS materials qualification program10.1016/j.jnucmat.2016.10.012 ↗
6. Review of the studies on fundamental issues in LBE corrosion10.1016/j.jnucmat.2007.06.019 ↗
7. A review of steel corrosion by liquid lead and lead-bismuth10.1016/j.corsci.2009.03.013 ↗
8. Influence of temperature on the interaction mode of T91 and AISI 316L steels with Pb-Bi melt saturated by oxygen10.1016/j.corsci.2008.02.006 ↗
9. Long-term corrosion performance of T91 ferritic/martensitic steel at 400 °C in flowing Pb-Bi eutectic with 2x10−7mass% dissolved oxygen10.1016/j.corsci.2020.108852 ↗
10. Corrosion in iron and steel T91 caused by flowing lead-bismuth eutectic at 400 °C and 10−7 Mass% dissolved oxygen10.1115/1.4040937 ↗
11. Characterization of corrosion phenomena and kinetics on T91 ferritic/martensitic steel exposed at 450 and 550 °C to flowing Pb-Bi eutectic with 10−7 mass% dissolved oxygen10.1016/j.jnucmat.2017.07.031 ↗
12. A refined oxidation mechanism proposed for ferritic-martensitic steels exposed to oxygen-saturated liquid lead-bismuth eutectic at 400°C for 500 h10.1016/j.jnucmat.2021.152852 ↗
13. Influence of plastic deformation on dissolution corrosion of type 316L austenitic stainless steel in static, oxygen-poor liquid lead-bismuth eutectic at 500 °C10.5006/2400 ↗
14. Effect of lead-bismuth eutectic oxygen concentration on the onset of dissolution corrosion in 316L austenitic stainless steel at 450 °C10.1115/1.4039598 ↗
15. Effect of deformation twinning on dissolution corrosion of 316L stainless steels in contact with static liquid lead-bismuth eutectic (LBE) at 500 °C10.1016/j.jnucmat.2018.08.030 ↗
16. Dissolution corrosion of 316L austenitic stainless steels in contact with static liquid lead-bismuth eutectic (LBE) at 500 °C10.1016/j.jnucmat.2017.04.004 ↗
17. Transmission electron microscopy study of complex oxide scales on DIN 1.4970 steel exposed to liquid Pb-Bi eutectic10.1016/j.corsci.2018.10.018 ↗
18. Long-term corrosion of austenitic steels in flowing LBE at 400 °C and 10−7 mass% dissolved oxygen in comparison with 450 and 550 °C10.1016/j.jnucmat.2015.09.027 ↗
19. Selective leaching of nickel and chromium from Type 316 austenitic steel in oxygen-containing lead-bismuth eutectic (LBE)10.1016/j.corsci.2014.03.016 ↗
20. Corrosion behaviour of austenitic steels 1.4970, 316L and 1.4571 in flowing LBE at 450 and 550 °C with 10−7 mass% dissolved oxygen10.1016/j.jnucmat.2014.08.024 ↗
21. Corrosion scales on various steels after exposure to liquid lead–bismuth eutectic10.1016/j.jnucmat.2013.09.034 ↗
22. Corrosion Interaction of 9% Cr Ferritic/Martensitic steels at 450 and 550 °C with flowing Pb-Bi Eutectic Containing 10−7 Mass% dissolved oxygen10.1115/1.4041432 ↗
23. Influence of liquid lead and lead-bismuth eutectic on tensile, fatigue and creep properties of ferritic/martensitic and austenitic steels for transmutation system10.1016/j.jnucmat.2011.04.047 ↗
24. KINETICS AND MECHANISM OF CRACK INITIATION OF LIQUID METAL EMBRITTLEMENT
25. Environmentally assisted cracking of T91 ferritic-martensitic steel in heavy liquid metals10.1515/corrrev-2019-0035 ↗
26. Fracture mechanics behaviour of the T91 martensitic steel in contact with liquid lead-bismuth eutectic for application in an accelerator driven system10.1016/j.jnucmat.2011.04.021 ↗
27. Investigating liquid-metal embrittlement of T91 by fracture toughness tests10.1016/j.jnucmat.2015.12.019 ↗
28. Liquid metal embrittlement of the T91 steel in lead bismuth eutectic: the role of loading rate and of the oxygen content in the liquid metal10.1016/j.msea.2014.04.082 ↗
29. Fatigue behaviour of a martensitic and an austenitic steel in heavy liquid metals10.1016/j.proeng.2013.03.336 ↗
30. Investigation of liquid LBE embrittlement effects on irradiated ferritic/martensitic steels by slow-strain-rate tensile tests10.1016/j.jnucmat.2011.11.036 ↗
31. The role of oxide films in preventing liquid metal embrittlement of T91 steel exposed to liquid lead-bismuth eutectic10.1016/j.jnucmat.2018.07.018 ↗
32. Stability of fatigue cracks at 350 °C in air and in liquid metal in T91 martensitic steel10.1016/j.ijfatigue.2019.105265 ↗
33. Low cycle fatigue behaviour of a modified 9Cr-1Mo ferritic-martensitic steel in lead-bismuth eutectic at 350°C - effects of oxygen concentration in the liquid metal and strain rate10.1016/j.corsci.2015.02.022 ↗
34. Slow strain rate tensile tests on T91 in static lead-bismuth eutectic10.1016/j.jnucmat.2006.05.039 ↗
35. Liquid Pb-Bi embrittlement effects on the T91 after different heat treatments10.1016/j.jnucmat.2008.02.050 ↗
36. Influence of LBE long term exposure and simultaneous fast neutron irradiation on the mechanical properties of T91 and 316L10.1016/j.jnucmat.2016.02.008 ↗
37. Creep failure of a solution-annealed 15-15Ti steel exposed to stagnant lead-bismuth eutectic at 550 and 600°C10.1016/j.msea.2020.140230 ↗
38. T91 cladding tubes with and without modified FeCrAlY coatings exposed in LBE at different flow, stress and temperature conditions10.1016/j.jnucmat.2008.02.026 ↗
39. Oxide scales formed on Fe-Cr-Al-based model alloys exposed to oxygen containing molten lead10.1016/j.jnucmat.2013.02.044 ↗
40. Influence of composition and microstructure on the corrosion behaviour of different Fe-Cr-Al alloys in molten LBE10.1016/j.jnucmat.2011.11.049 ↗
41. Corrosion resistance and microstructural stability of austenitic Fe-Cr-Al-Ni model alloys exposed to oxygen-containing molten lead10.1016/j.jnucmat.2019.06.043 ↗
42. Corrosion behaviour of Al-added high Mn austenitic steels in molten lead bismuth eutectic with saturated and low oxygen concentrations at 450°C10.1016/j.corsci.2020.108864 ↗
43. Corrosion resistance of Si-and Al-rich steels in flowing lead-bismuth10.1016/j.jnucmat.2006.05.019 ↗
44. Design of alumina forming FeCrAl steels for lead or lead-bismuth cooled fast reactors10.1016/j.jnucmat.2012.04.006 ↗
45. Corrosion and radiation resistant nanoceramic coatings for lead fast reactors10.1016/j.corsci.2017.05.011 ↗
46. Oxidative passivation of Fe-Cr-Al steels in lead-bismuth eutectic under oxygen-controlled static conditions at 700 and 800°C10.1016/j.jnucmat.2019.06.004 ↗
47. Corrosion studies of a low alloyed Fe-10Cr-4Al steel exposed in liquid Pb at very high temperatures10.1016/j.jnucmat.2020.152022 ↗
48. Oxidation studies of Fe10CrAl-RE alloys exposed to Pb at 550°C for 10000h10.1016/j.jnucmat.2013.07.023 ↗
49. Liquid metal embrittlement of an Fe10Cr4Al ferritic alloy exposed to oxygen-depleted and -saturated lead-bismuth eutectic at 350°C10.1016/j.corsci.2019.108364 ↗
50. Effect of temperature on liquid metal embrittlement susceptibility of an Fe10Cr4Al ferritic alloy in contact with stagnant lead-bismuth eutectic10.1016/j.jnucmat.2020.152196 ↗
51. Liquid metal embrittlement susceptibility of a high-entropy alloy exposed to oxygen-depleted liquid lead-bismuth eutectic at 250 and 350 °C10.1016/j.jnucmat.2019.151859 ↗
52. Comparison of solid metal-metal oxide reference electrodes for potentiometric oxygen sensors in liquid lead-bismuth eutectic operating at low temperature ranges10.1016/j.snb.2015.03.004 ↗
53. Schroer · 2007
54. Oxidation mechanism of a Fe–9Cr–1Mo steel by liquid Pb–Bi eutectic alloy (Part I)10.1016/j.corsci.2008.06.050 ↗
55. A review of recent advances in the understanding of liquid metal embrittlement10.5006/2904 ↗
56. Crack propagation in a liquid metal environment10.1016/0001-6160(63)90180-9 ↗
57. Concerning liquid metal embrittlement, particularly of zinc monocrystals by mercury10.1080/14786436308213836 ↗
58. Multiscale investigation of quasi-brittle fracture characteristics in a 9Cr-1Mo ferritic-martensitic steel embrittled by liquid lead-bismuth under low cycle fatigue10.1016/j.corsci.2015.10.003 ↗
59. Failures of structures and components by metal-induced embrittlement10.1007/s11668-008-9124-y ↗
60. A short review of high-temperature wetting and complexion transitions with a critical assessment of their influence on liquid metal embrittlement and corrosion10.5006/1925 ↗
61. In situ investigation of liquid Ga penetration in Al bicrystal grain boundaries: grain boundary wetting or liquid metal embrittlement?10.1016/j.actamat.2004.09.012 ↗
62. Role of grain size in liquid-metal embrittlement of iron