An electro-chemo-mechanical framework for predicting hydrogen uptake in metals due to aqueous electrolytes
Source abstract
Abstract
We present a theoretical and numerical scheme that enables quantifying hydrogen ingress in metals for arbitrary environments and defect geometries. This is achieved by explicitly resolving the electrochemical behaviour of the electrolyte, the hydrogen and corrosion reactions, the kinetics of surface adsorption, and hydrogen uptake, diffusion and trapping in mechanically-deforming solids. This new framework is used to produce maps that relate the absorbed hydrogen with the applied potential, specimen geometry and fluid velocity. We also present simplified versions of our generalised model, and benchmark predictions of these and other existing models against the generalised electro-chemo-mechanical results, establishing regimes of validity.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · Concrete Corrosion and Durability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (59)
Show source-provided references
1. Hydrogen-assisted Cracking
2. Gangloff · 2012 · 520
3. The synergistic action and interplay of hydrogen embrittlement mechanisms in steels and iron: Localized plasticity and decohesion10.1016/j.engfracmech.2019.106528 ↗
4. Progress and opportunities in modelling environmentally assisted cracking10.21809/rilemtechlett.2021.145 ↗
5. A uniform hydrogen degradation law for high strength steels10.1016/j.engfracmech.2016.02.001 ↗
6. Hydrogen-enhanced-plasticity mediated decohesion for hydrogen-induced intergranular and “quasi-cleavage” fracture of lath martensitic steels10.1016/j.jmps.2017.12.016 ↗
7. A phase field formulation for hydrogen assisted cracking10.1016/j.cma.2018.07.021 ↗
8. On modeling fracture of ferritic steels due to hydrogen embrittlement10.1016/j.jmps.2018.09.012 ↗
9. Hydrogen induced fast-fracture10.1016/j.jmps.2019.103740 ↗
10. A mechanism-based multi-trap phase field model for hydrogen assisted fracture10.1016/j.ijplas.2021.103044 ↗
11. Marcus · 2012
12. Perspectives on hydrogen uptake, diffusion and trapping10.1016/j.ijhydene.2015.06.147 ↗
13. Cohesive zone modeling of fatigue crack propagation assisted by gaseous hydrogen in metals10.1016/j.ijfatigue.2014.06.007 ↗
14. A phase-field model for solute-assisted brittle fracture in elastic-plastic solids10.1016/j.ijplas.2017.11.004 ↗
15. Generalised boundary conditions for hydrogen transport at crack tips10.1016/j.corsci.2020.108698 ↗
16. A phase-field regularized cohesive zone model for hydrogen assisted cracking10.1016/j.cma.2019.112614 ↗
17. Sensitivity to hydrogen embrittlement of AISI 4140 steel: A numerical study on fracture toughness10.1016/j.tafmec.2020.102810 ↗
18. Hydrogen in metals: A coupled theory for species diffusion and large elastic-plastic deformations10.1016/j.ijplas.2012.11.005 ↗
19. Strain gradient plasticity modeling of hydrogen diffusion to the crack tip10.1016/j.ijhydene.2016.05.014 ↗
20. Coupled hydrogen diffusion simulation using a heat transfer analogy10.1016/j.ijmecsci.2016.07.020 ↗
21. A modelling framework for coupled hydrogen diffusion and mechanical behaviour of engineering components10.1007/s00466-020-01847-9 ↗
22. Analysis of the influence of microstructural traps on hydrogen assisted fatigue10.1016/j.actamat.2020.08.030 ↗
23. Determination of the hydrogen fugacity during electrolytic charging of steel10.1016/j.corsci.2014.06.033 ↗
24. Determination of the equivalent hydrogen fugacity during electrochemical charging of 3.5NiCrMoV steel10.1016/j.corsci.2017.12.018 ↗
25. Modelling of the hydrogen distribution at a crack tip10.1016/0921-5093(95)09897-6 ↗
26. On the suitability of slow strain rate tensile testing for assessing hydrogen embrittlement susceptibility10.1016/j.corsci.2019.108291 ↗
27. Predicting the effect of applied potential on crack tip hydrogen concentration in low-alloy martensitic steels10.5006/1.3278484 ↗
28. Mccafferty · 2004
29. Simulation of interfacial pH changes during hydrogen evolution reaction10.1016/j.jelechem.2015.09.029 ↗
30. An extended finite element method based approach for modeling crevice and pitting corrosion10.1115/1.4033379 ↗
31. Hydrogen embrittlement risk of high strength galvanized steel in contact with alkaline media10.1016/j.corsci.2011.05.023 ↗
32. Effect of pH on hydrogen absorption into steel in neutral and alkaline solutions10.2320/matertrans.M2016360 ↗
33. Crack tip chemistry and electrochemistry of environmental cracks in AA 705010.1016/j.corsci.2006.12.001 ↗
34. Hydrogen interaction with multiple traps: Can it be used to mitigate embrittlement?10.1016/j.ijhydene.2011.05.027 ↗
35. Cohesive zone modelling of hydrogen assisted fatigue crack growth: The role of trapping10.1016/j.ijfatigue.2022.106935 ↗
36. A new analysis of the diffusion of hydrogen in iron and ferritic steels
37. Modelling of thermal desorption of hydrogen from metals10.1016/S0921-5093(97)00426-7 ↗
38. The diffusion and trapping of hydrogen in steel10.1016/0001-6160(70)90078-7 ↗
39. Analysis of hydrogen permeation tests considering two different modelling approaches for grain boundary trapping in iron
40. Electroneutrality and ionic interactions in the modeling of mass transport in dilute electrochemical systems10.1016/j.electacta.2011.07.128 ↗
41. Calculation of the hydrogen surface coverage and rate constants of the hydrogen evolution reaction from polarization data10.1149/1.1393500 ↗
42. Kinetics of the hydrogen evolution reaction on NiMn graphite modified electrode10.1016/j.ijhydene.2011.06.106 ↗
43. A mechanistic analysis of hydrogen entry into metals during cathodic hydrogen charging10.1016/S0036-9748(88)80074-7 ↗
44. Analysis of hydrogen evolution and entry into metals for the discharge-recombination process10.1149/1.2097429 ↗
45. A new method for determining kinetic parameters by simultaneously considering all the independent conditions at an overpotential in case of hydrogen evolution reaction following Volmer–Heyrovsky–Tafel mechanism10.1016/j.ijhydene.2007.09.017 ↗
46. Modelling of hydrogen permeation experiments in iron alloys: Characterization of the accessible parameters – Part II – The exit side10.1016/j.electacta.2017.12.173 ↗
47. Determination of the rate constants of hydrogen absorption into metals10.1149/1.1393631 ↗
48. Determination of the kinetics of the hydrogen evolution reaction by the galvanostatic step technique10.1016/S0022-0728(02)00760-X ↗
49. Hydrogen over potential on pure metals in alkaline solution10.1149/1.2408305 ↗
50. Modelling of hydrogen permeation experiments in iron alloys: Characterization of the accessible parameters – Part I – The entry side10.1016/j.electacta.2017.12.172 ↗
51. Mechanism and kinetics of the hydrogen evolution reaction10.1016/j.ijhydene.2019.05.183 ↗
52. First-principles modeling of the hydrogen evolution reaction and its application in electrochemical corrosion of Mg10.1016/j.actamat.2019.11.025 ↗
53. A sequential non-iterative approach for modeling multi-ionic species reactive transport during localized corrosion10.1016/j.finel.2019.103318 ↗
54. Modeling hydrogen evolution reaction kinetics through explicit water-metal interfaces10.1021/acs.jpcc.0c08310 ↗
55. COMSOL · 2020
56. COMSOL Multiphysics®: Finite element software for electrochemical analysis. A mini-review10.1016/j.elecom.2013.12.020 ↗
57. Measurement and modeling of hydrogen environment-assisted cracking in monel K-50010.1007/s11661-014-2324-z ↗
58. Strain gradient plasticity-based modeling of hydrogen environment assisted cracking10.1016/j.actamat.2016.07.022 ↗
59. Applications of phase field fracture in modelling hydrogen assisted failures10.1016/j.tafmec.2020.102837 ↗