journal article·2023-07

Effects of the microstructure and reversed austenite on the hydrogen embrittlement susceptibility of Ni-Cr-Mo-V/Nb high-strength steel

Chao Hai, Yuetong Zhu, Endian Fan, Cuiwei Du, Xuequn Cheng, Xiaogang Li

Corrosion Science· Volume 218
Publisher page

Abstract

The effects of the microstructure and reversed austenite (RA) on the hydrogen embrittlement (HE) behavior were investigated in NiCrMoV/Nb high-strength steel prepared using three different heat treatments. The quenching and tempering (QT) steel showed a noble HE resistance for the lowest hydrogen diffusion and maximum apparent hydrogen concentration compared to quenching (Q) steel and quenching, lamellarizing, and tempering (QLT) steel. Thermal desorption spectroscopy (TDS) analysis confirmed that RA had an activation energy of 32.5 kJ/mol which indicates a stable trapping site. The QLT steel containing more RA exhibited a higher HE susceptibility, suggesting that RA degrades the HE resistance.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · High Temperature Alloys and Creep

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (68)

Show source-provided references
1. Analysis of intercritical heat treatment of cast steels10.1007/BF02833194 ↗
2. Quenching and partitioning martensite—a novel steel heat treatment10.1016/j.msea.2006.02.133 ↗
3. Hydrogen trapping sites and hydrogen-induced cracking in high strength quenching & partitioning (Q&P) treated steel10.1016/j.ijhydene.2014.06.079 ↗
4. The influence of tempering temperature on the reversed austenite formation and tensile properties in Fe–13%Cr–4%Ni–Mo low carbon martensite stainless steels10.1016/j.msea.2011.01.078 ↗
5. Carbon partitioning during quenching and partitioning heat treatment accompanied by carbide precipitation10.1016/j.actamat.2014.11.049 ↗
6. Carbon partitioning into austenite after martensite transformation10.1016/S1359-6454(03)00059-4 ↗
7. The role of reversed austenite in hydrogen embrittlement fracture of S41500 martensitic stainless steel10.1016/j.actamat.2017.08.011 ↗
8. Microstructure and mechanical properties of 06Cr13Ni4Mo steel treated by quenching-tempering-partitioning process10.1016/j.jmst.2015.10.004 ↗
9. Improvement of cryogenic toughness for 9% Ni steel keyhole TIG butt-welded joints with a Ni interlayer10.1016/j.msea.2022.142661 ↗
10. Microstructure understanding of high Cr-Ni austenitic steel corrosion in high-temperature steam10.1016/j.actamat.2022.117634 ↗
11. The influence of hydrogen on the mechanical and fracture properties of some martensitic advanced high strength steels studied using the linearly increasing stress test10.1016/j.corsci.2015.06.038 ↗
12. Hydrogen embrittlement of an automotive 1700 MPa martensitic advanced high-strength steel10.1016/j.corsci.2020.108726 ↗
13. Further study of the hydrogen embrittlement of martensitic advanced high-strength steel in simulated auto service conditions10.1016/j.corsci.2018.02.037 ↗
14. Hydrogen embrittlement of a medium carbon Q&P steel
15. Embrittlement of T-200 maraging steel in a hydrogen sulfide solution10.1016/j.corsci.2004.06.017 ↗
16. Hydrogen-assisted failure in a twinning-induced plasticity steel studied under in situ hydrogen charging by electron channeling contrast imaging10.1016/j.actamat.2013.04.030 ↗
17. Effect of microstructure and composition on hydrogen permeation in X70 pipeline steels10.1016/j.ijhydene.2012.11.127 ↗
18. Modelling of hydrogen diffusion and hydrogen induced cracking in supermartensitic and duplex stainless steels10.1016/j.matdes.2008.04.026 ↗
19. Hydrogen trapping phenomena in metals with B.C.C. and F.C.C. crystals structures by the desorption thermal analysis technique10.1016/0257-8972(86)90087-3 ↗
20. Effect of retained austenite stability and morphology on the hydrogen embrittlement susceptibility in quenching and partitioning treated steels10.1016/j.msea.2016.02.026 ↗
21. Effect of retained austenite on the hydrogen embrittlement of a medium carbon quenching and partitioning steel with refined microstructure10.1016/j.msea.2016.04.025 ↗
22. Embrittlement of welds10.1016/B978-0-12-341825-8.50017-9 ↗
23. Effect of aging treatment on hydrogen embrittlement of PH 13-8 Mo martensite stainless steel10.1016/j.msea.2015.09.116 ↗
24. The role of hydrogen in hydrogen embrittlement fracture of lath martensitic steel10.1016/j.actamat.2012.06.040 ↗
25. Influence of tempering process on mechanical properties of 00Cr13Ni4Mo supermartensitic stainless steel10.1016/S1006-706X(10)60128-8 ↗
26. Influence of hydrogen on the stacking-fault energy of an austenitic stainless steel
27. Hydrogen-enhanced lattice defect formation and hydrogen embrittlement of cyclically prestressed tempered martensitic steel
28. The effect of morphology on the stability of retained austenite in a quenched and partitioned steel10.1016/j.scriptamat.2012.11.003 ↗
29. Effect of tempering temperature on the microstructure and mechanical properties in mooring chain steel10.1016/j.msea.2015.03.102 ↗
30. The morphology and crystallography of lath martensite in Fe-C alloys10.1016/S1359-6454(02)00577-3 ↗
31. The effects of carbon contents and Ms temperatures on the hardness of martensitic Fe-Ni-C alloys10.2355/isijinternational1966.12.16 ↗
32. Evaluation of the dislocation density and dislocation character in cold rolled Type 304 steel determined by profile analysis of X-ray diffraction10.1016/j.actamat.2011.03.055 ↗
33. X-ray line broadening from filed aluminium and wolfram10.1016/0001-6160(53)90006-6 ↗
34. Effect of microstructure on the hydrogen trapping efficiency and hydrogen induced cracking of linepipe steel10.1016/j.corsci.2008.03.007 ↗
35. Quantitative investigation on deep hydrogen trapping in tempered martensitic steel10.1016/j.jallcom.2020.157218 ↗
36. Characterization of inclusions of X80 pipeline steel and its correlation with hydrogen-induced cracking10.1016/j.corsci.2010.12.011 ↗
37. Determination of the hydrogen fugacity during electrolytic charging of steel10.1016/j.corsci.2014.06.033 ↗
38. Effect of hydrogen on ductility of high strength quenched and tempered (QT) Cr-Ni-Mo steels10.1016/j.msea.2014.12.013 ↗
39. Atomic-scale investigation of deep hydrogen trapping in NbC/alpha-Fe semi-coherent interfaces10.1016/j.actamat.2020.09.031 ↗
40. Direct observation of hydrogen trapped by NbC in steel using small-angle neutron scattering10.1016/j.scriptamat.2007.09.026 ↗
41. Thermal analysis of trapped hydrogen in pure iron10.1007/BF02642424 ↗
42. Trap-governed hydrogen diffusivity and uptake capacity in ultrahigh-strength AERMET 100 steel10.1007/s11661-002-0032-6 ↗
43. Effects of internal hydrogen and surface-absorbed hydrogen on the hydrogen embrittlement of X80 pipeline steel10.1016/j.ijhydene.2019.04.239 ↗
44. The detrimental effect of hydrogen at dislocations on the hydrogen embrittlement susceptibility of Fe-C-X alloys: an experimental proof of the HELP mechanism10.1016/j.ijhydene.2017.12.109 ↗
45. Hydrogen-enhanced-plasticity mediated decohesion for hydrogen-induced intergranular and ``quasi-cleavage'' fracture of lath martensitic steels10.1016/j.jmps.2017.12.016 ↗
46. Effects of hydrogen on the properties of iron and steel10.1007/BF02654700 ↗
47. The effect of grain size and aging on hydrogen embrittlement of a maraging steel10.1016/j.corsci.2008.06.044 ↗
48. Retained austenite as a hydrogen trap in steel welds
49. M. De Sanctis, G. Lovicu, R. Ishak, M. Richetta, A. Varone, Novel methodology for the selection, dosing and nn-line control of corrosion inhibitors for industrial acid pickling, in: 10th International Conference on Processing and Manufacturing of Advanced Materials Processing, Fabrication, Properties, Applications (THERMEC), Cite Sci Paris, Paris, FRANCE, 2018, pp. 1698–1704.10.4028/www.scientific.net/MSF.941.1698 ↗
50. Effect of microstructure and temperature on hydrogen diffusion and trapping in X70 grade pipeline steel and its weldments
51. Hydrogen-induced cracking and healing behaviour of X70 steel10.1016/j.jallcom.2009.05.085 ↗
52. Effects of hydrogen-charging on the susceptibility of X100 pipeline steel to hydrogen-induced cracking10.1016/j.ijhydene.2009.09.090 ↗
53. Effect of line pipe steel microstructure on susceptibility to sulfide stress cracking10.5006/1.3287728 ↗
54. Hydrogen induced plasticity in stress corrosion cracking of engineering systems10.1016/S0013-7944(00)00121-1 ↗
55. Comparative study on the stress corrosion cracking of a new Ni-advanced high strength steel prepared by TMCP, direct quenching, and quenching & tempering10.1016/j.msea.2021.141854 ↗
56. Electrochemical investigation of hydrogen absorption in a duplex stainless steel10.1016/S1359-6454(02)00105-2 ↗
57. Turnbull · Hydrogen transport in SAF2205 and SAF2507 duplex stainless steels · 1994 · 268
58. Hydrogen transport in a duplex stainless steel10.1016/S1359-6454(00)00122-1 ↗
59. Effect of alloying elements on the hydrogen diffusion and trapping in high entropy alloys10.1016/j.scriptamat.2021.113957 ↗
60. Effect of vanadium content on hydrogen embrittlement of 1400 MPa grade high strength bolt steels10.1016/j.ijhydene.2021.08.060 ↗
61. Effect of nanosized NbC precipitates on hydrogen-induced cracking of high-strength low-alloy steel10.1007/s12613-020-2167-0 ↗
62. Effect of Nb on the hydrogen-induced cracking of high-strength low-alloy steel10.1016/j.corsci.2018.04.041 ↗
63. Hydrogen trapping behavior in vanadium-added steel10.2355/isijinternational.43.527 ↗
64. A new effect of retained austenite on ductility enhancement in high-strength quenching–partitioning–tempering martensitic steel10.1016/j.msea.2011.07.049 ↗
65. A statistical, physical-based, micro-mechanical model of hydrogen-induced intergranular fracture in steel10.1016/j.jmps.2009.10.005 ↗
66. Effect of post-weld heat treatment on the microstructure and hydrogen permeation of 13CrNiMo steels10.1016/j.corsci.2003.10.006 ↗
67. Formation of shear bands and strain-induced martensite during plastic deformation of metastable austenitic stainless steels10.1016/j.actamat.2007.07.015 ↗
68. P.J. Ferreira, I.M. Robertson, H.K. Birnbaum, Influence of hydrogen on the stacking-fault energy of an austenitic stainless steel, in: Intergranular and Interphase Boundaries in Materials, Pt 1, 1996, pp. 93–96.10.4028/www.scientific.net/MSF.207-209.93 ↗