Enhanced corrosion resistance of 15–15Ti austenitic steel in liquid lead-bismuth eutectic at 550 ℃ by shot peening processing
Source abstract
Abstract
The effect of shot peening on microstructure and corrosion of 15–15Ti austenitic steel in liquid LBE at 550 ℃ was investigated. The nanocrystallization and preferential recrystallization were observed, improving the resistance to corrosion and intergranular cracking in LBE. The intensive grain boundaries and dislocations on steel surface improved the compactness and adhesion of the formed oxide scale, efficiently preventing LBE penetration into steel. The Cr-rich oxide formed in boundaries of the recrystallized grains is Fe-Cr spinel with porous structure, it significantly prohibited the counter diffusion of elements, suppressing the growth of outer magnetite layer and inner transgranular oxide.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Nuclear Materials and Properties · Thermodynamic and Structural Properties of Metals and Alloys · Fusion materials and technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (64)
Show source-provided references
1. Creep failure of a solution-annealed 15-15Ti steel exposed to stagnant lead-bismuth eutectic at 550 and 600 °C10.1016/j.msea.2020.140230 ↗
2. Thermal creep properties of Ti-stabilized DIN 1.4970 (15-15Ti) austenitic stainless steel pressurized cladding tubes10.1016/j.jnucmat.2017.06.013 ↗
3. Transmission electron microscopy study of complex oxide scales on DIN 1.4970 steel exposed to liquid Pb-Bi eutectic10.1016/j.corsci.2018.10.018 ↗
4. Liquid metal as a heat transport fluid for thermal solar power applications10.1016/j.egypro.2014.03.068 ↗
5. Overview of lead-cooled fast reactor activities10.1016/j.pnucene.2013.11.011 ↗
6. M. Utili, GEN-IV LFR development: status & perspectives10.1016/j.pnucene.2018.02.005 ↗
7. Microstructural stability of Fe-Cr-Al alloys at 450-550 degrees C10.1016/j.jnucmat.2014.11.101 ↗
8. A comparison of supercritical carbon dioxide power cycle configurations with an emphasis on CSP applications10.1016/j.egypro.2014.03.128 ↗
9. OECD, N.E.Agency, Handbook on Lead-bismuth Eutectic Alloy and Lead Properties, Materials Compatibility, Thermalhydraulics and Technologies, 2015.
10. Opportunities for the LWR ATF materials development program to contribute to the LBE-cooled ADS materials qualification program10.1016/j.jnucmat.2016.10.012 ↗
11. Influence of liquid lead and lead-bismuth eutectic on tensile, fatigue and creep properties of ferritic/martensitic and austenitic steels for transmutation systems10.1016/j.jnucmat.2011.04.047 ↗
12. Influence of LBE long term exposure and simultaneous fast neutron irradiation on the mechanical properties of T91 and 316L10.1016/j.jnucmat.2016.02.008 ↗
13. Study of Crack Initiation of 15-15Ti Austenitic Steel in Liquid PbBi10.1115/1.4041564 ↗
14. Selective leaching of nickel and chromium from Type 316 austenitic steel in oxygen-containing lead–bismuth eutectic (LBE)10.1016/j.corsci.2014.03.016 ↗
15. Corrosion behavior of austenitic steels in liquid lead bismuth containing 10−6wt% and 10−8wt% oxygen at 400–500°C10.1016/j.jnucmat.2014.01.046 ↗
16. Orientation relationship of the austenite-to-ferrite transformation in austenitic stainless steels due to dissolution corrosion in contact with liquid Pb-Bi eutectic10.1016/j.scriptamat.2019.03.035 ↗
17. Nanoscale corrosion investigation of surface nanocrystallized 7150 Al alloy in 3.5 wt% NaCl solution by using FIB-TEM techniques10.1016/j.corsci.2021.110021 ↗
18. Effect of shot-peening on corrosion behavior of austenitic steel in supercritical carbon dioxide at 700 °C10.1016/j.corsci.2022.110180 ↗
19. New insights into the effects of surface nanocrystallization on the oxidation of 321 austenitic stainless steel in a humid oxygen environment at 1000 °C10.1016/j.corsci.2018.11.024 ↗
20. Improving the fretting and corrosion fatigue performance of 300M ultra-high strength steel using the ultrasonic surface rolling process10.1016/j.ijfatigue.2018.11.017 ↗
21. Gradient nanostructure and residual stresses induced by Ultrasonic Nano-crystal Surface Modification in 304 austenitic stainless steel for high strength and high ductility10.1016/j.msea.2014.06.114 ↗
22. Fatigue behaviors of AISI 316L stainless steel with a gradient nanostructured surface layer10.1016/j.actamat.2014.12.057 ↗
23. Improving the oxidation resistance of SIMP steel to liquid Pb-Bi eutectic by shot peening treatments10.1016/j.apsusc.2021.151910 ↗
24. Effects of pre-formed nanostructured surface layer on oxidation behaviour of 9Cr2WVTa steel in air and liquid Pb-Bi eutectic alloy10.1016/j.corsci.2015.10.021 ↗
25. Enhanced oxidation resistance of a reduced activation ferritic/martensitic steel in liquid Pb-Bi eutectic alloy by preforming a gradient nanostructured surface layer10.1016/j.jnucmat.2018.04.042 ↗
26. Effect of nanostructured surface on the corrosion behavior of RAFM steels10.1007/s11085-019-09895-0 ↗
27. Alloy effects in nanostructures10.1016/0965-9773(93)90088-S ↗
28. Corrosion-induced hydrogen embrittlement of 2024 and 6013 aluminum alloys10.1016/j.tafmec.2003.11.014 ↗
29. Achieving excellent corrosion resistance properties of 7075 Al alloy via ultrasonic surface rolling treatment10.1016/j.jallcom.2022.165009 ↗
30. The Effect of Shot Peening on Steam Oxidation of 304H Stainless Steel10.1007/s11085-019-09951-9 ↗
31. Effect of high energy shot peening pressure on the stress corrosion cracking of the weld joint of 304 austenitic stainless steel10.1016/j.msea.2015.03.088 ↗
32. Improvement of corrosion resistance of AA2024-T3 using femtosecond laser peening without protective and confining medium10.1016/j.corsci.2018.08.030 ↗
33. Effect of warm shot peening treatments on surface properties and corrosion behavior of AZ31 magnesium alloy10.1016/j.surfcoat.2020.126285 ↗
34. Surface characteristics and stress corrosion behavior of AA 7075-T6 aluminum alloys after different shot peening processes10.1016/j.surfcoat.2022.128481 ↗
35. Oxidative passivation of Fe–Cr–Al steels in lead-bismuth eutectic under oxygen-controlled static conditions at 700° and 800 °C10.1016/j.jnucmat.2019.06.004 ↗
36. The effects of cold working on the corrosion behavior of an austenitic stainless steel in liquid lead-bismuth eutectic under vacuum at 873 K10.1016/j.jnucmat.2018.07.034 ↗
37. Intergranular precipitation-enhanced wetting and phase transformation in an Al0.4CoCrFeNi high-entropy alloy exposed to lead-bismuth eutectic10.1016/j.corsci.2021.110038 ↗
38. Effect of contact conditions on embrittlement of T91 steel by lead-bismuth10.1016/j.jnucmat.2004.07.025 ↗
39. Effects of constrained groove pressing, severe shot peening and ultrasonic nanocrystal surface modification on microstructure and mechanical behavior of S500MC high strength low alloy automotive steel
40. Localized corrosion behaviour of AA7150 after ultrasonic shot peening Corrosion depth vs impact energy10.1016/j.corsci.2017.11.008 ↗
41. Effects of ultrasonic surface rolling processing on microstructure and wear properties of high-carbon high-chromium steel10.1016/j.surfcoat.2021.127531 ↗
42. Long-term isothermal oxidation behavior of two industrial polycrystalline nickel base alloys in air at 700 °C – Evaluation of intergranular oxidation distribution and kinetic10.1016/j.corsci.2021.109500 ↗
43. Oxidation mechanism of an Fe–9Cr–1Mo steel by liquid Pb–Bi eutectic alloy at 470 °C (Part II)10.1016/j.corsci.2008.06.051 ↗
44. Environmental degradation of structural materials in liquid lead- and lead-bismuth eutectic-cooled reactors10.1016/j.pmatsci.2022.100920 ↗
45. Mechanical performance of ferritic martensitic steels for high dose applications in advanced nuclear reactors10.1007/s11661-012-1565-y ↗
46. Mechanical properties of 9Cr martensitic steels and ODS-FeCr alloys after neutron irradiation at 325 degrees C up to 42 dpa10.1016/j.jnucmat.2007.03.166 ↗
47. Local passivation of metals at grain boundaries: In situ scanning tunneling microscopy study on copper10.1016/j.corsci.2016.04.013 ↗
48. The effect of grain boundary structure on the intergranular degradation behavior of solution annealed alloy 690 in high temperature, hydrogenated water10.1016/j.actamat.2019.10.041 ↗
49. Intergranular oxidation of Ni-based Alloy 600 in a simulated PWR primary water environment10.1016/j.corsci.2016.02.040 ↗
50. Grain boundary depletion and migration during selective oxidation of Cr in a Ni–5Cr binary alloy exposed to high-temperature hydrogenated water10.1016/j.scriptamat.2014.06.022 ↗
51. Review of the studies on fundamental issues in LBE corrosion10.1016/j.jnucmat.2007.06.019 ↗
52. J. Lim, Thermodynamic Assessment of the Oxygen Control Boundary for the Operation of MYRRHA, SCK⋅CEN, 2011.
53. K.J. Schroer C., Physical chemistry of corrosion and oxygen control in liquid lead and lead bismuth eutectic, FZKA 7364, Karlsruhe, Germany, 2007.
54. Enhanced corrosion resistance of the surface modified Ti-13Nb-13Zr alloy by ultrasonic shot peening10.1016/j.corsci.2021.109597 ↗
55. Mechanism of electropulsing induced recrystallization in a cold-rolled Mg-9Al-1Zn alloy10.1016/j.jallcom.2012.05.014 ↗
56. Effect of cyclic oxidation on the tensile behavior of directionally solidified CM-247LC Ni-based superalloy at 870°C10.1016/j.msea.2010.06.046 ↗
57. Nanostructure formation mechanism of alpha-titanium using SMAT10.1016/j.actamat.2004.05.023 ↗
58. Microstructure–mechanical and chemical behavior relationships in passive thin films10.1016/j.tsf.2009.08.032 ↗
59. Effect of grain size on mechanical property and corrosion behavior of a metastable austenitic stainless steel10.1016/j.matchar.2022.112360 ↗
60. The role of cold work and applied stress on surface oxidation of 304 stainless steel10.1016/j.corsci.2011.11.021 ↗
61. Observations of intergranular corrosion in AA2024-T351: the influence of grain stored energy10.1016/j.corsci.2012.04.005 ↗
62. Influence of peening on the corrosion properties of AISI 304 stainless steel10.1016/j.corsci.2009.08.008 ↗
63. The effect of laser shock processing on the microstructures and properties of 2060 Al-Li alloys10.1016/j.surfcoat.2022.128208 ↗
64. Influence of surface roughness on the corrosion behaviour of magnesium alloy10.1016/j.matdes.2010.12.016 ↗