journal article·2024-03Open access

Electrochemical corrosion behaviour and corrosion mechanism of Sn-9Zn-xGe solder alloys in NaCl solution

Cunji Pu, Caiju Li, Yingde Miao, Qiong Lu, Jubo Peng, Zunyan Xu, Xin Zhang, Jianhong Yi

Corrosion Science· Volume 228

Abstract

The electrochemical corrosion behaviour and corrosion mechanism of Sn-9Zn-xGe alloy in 3.5 wt.% NaCl solution was investigated using electrochemical techniques combined with surface characterization techniques. The results showed that the alloy corrosion was mainly affected by the rupture of passivation film and Cl - migration along grain boundaries. Trace Germanium (Ge) addition refined the microstructure and improved the corrosion potential of the alloy. Solder alloys containing 0.6 wt.% Ge formed a uniform and dense passivation film on the corrosion surfaces , which reduced the corrosion rate and increased the corrosion resistance .
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Electronic Packaging and Soldering Technologies · Advanced Welding Techniques Analysis · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (56)

Show source-provided references
1. Significantly enhanced ductility of Sn–57Bi–1Ag alloy induced by microstructure modulation from in addition10.1007/s10854-023-10946-1 ↗
2. Morphologies and nucleus models of β-Sn grains in SAC305-xIn freestanding solder balls and solder joints10.1016/j.matchar.2023.112847 ↗
3. The effects of antimony additions on microstructures, thermal and mechanical properties of Sn-8Zn-3Bi alloys10.1016/j.matdes.2017.01.061 ↗
4. Hypo-eutectic microstructure formation and nanomechanical response in Sn-3.0Ag-0.5Cu solder balls: effects of undercooling10.1016/j.matchar.2023.112707 ↗
5. Tin whisker growth inhibition in RE-doped Sn-Zn soldered joints10.3390/app9071406 ↗
6. Physical and mechanical properties of synthesized low Ag/lead-free Sn-Ag-Cu-xBi (x = 0, 1, 2.5, 5 wt%) solders10.1016/j.msea.2018.08.071 ↗
7. Influences of Ag and In alloying on Sn-Bi eutectic solder and SnBi/Cu solder joints10.1007/s10854-019-02206-y ↗
8. Structure and properties of Sn-Cu lead-free solders in electronics packaging10.1080/14686996.2019.1591168 ↗
9. Study on characteristics of interfacial microstructure and electrical current mechanism in Sn-xZn/Al photovoltaic modules10.1016/j.solener.2018.06.002 ↗
10. Al-based metal printed circuit board with polyimide/Al2O3 composite dielectric layer for light-emitting diodes10.1166/jnn.2016.12530 ↗
11. Microstructure and interfacial reaction of Sn–Zn–x(Al,Ag) near-eutectic solders on Al and Cu substrates10.1007/s10854-014-1877-3 ↗
12. Mechanical properties and electrochemical corrosion behavior of Al/Sn-9Zn-xAg/Cu Joints10.1007/s11664-010-1459-y ↗
13. Ultrasonic soldering silica glass and 2024 alloy in low temperature10.1080/13621718.2022.2063567 ↗
14. Ultrasonic-assisted soldering of fine-grained 7034 aluminum alloy using Sn-Zn solders below 300 °C10.1016/j.ultsonch.2017.08.020 ↗
15. Study on low temperature brazing of magnesium alloy to aluminum alloy using Sn–xZn solders10.1016/j.matdes.2012.02.021 ↗
16. Low-temperature high-frequency induction brazing of 5052 aluminum alloy to stainless steel with Sn-Zn solder10.1007/s11837-018-3280-7 ↗
17. Atmospheric corrosion of tin coatings on H62 brass and T2 copper in an urban environment10.1016/j.engfailanal.2022.106735 ↗
18. Atmospheric corrosion maps as a tool for designing and maintaining building materials: a review10.1016/j.heliyon.2022.e10438 ↗
19. Effect of polyvinyl chloride fire smoke on the long-term corrosion kinetics and surface microstructure of tin–lead and lead-free solders
20. Understanding corrosion mechanism of Sn-Zn alloys in NaCl solution via corrosion products characterization10.1002/maco.201508605 ↗
21. Effect mechanism of Ag and Bi elements on the corrosion process in Sn–9Zn–1Ag and Sn–9Zn–3Bi solders10.1088/2053-1591/ab2663 ↗
22. Effects of Ga, Al, Ag, and Ce multi-additions on the properties of Sn–9Zn lead-free solder10.1007/s10854-009-9877-4 ↗
23. Corrosion behavior of Sn-based lead-free solder alloys: a review10.1007/s10854-020-03540-2 ↗
24. Effects of Bi addition on the solderability and mechanical properties of Sn-Zn-Cu lead-free solder10.1007/s11664-022-09732-2 ↗
25. Solderability and intermetallic compounds formation of Sn-9Zn-xAg lead-free solders wetted on Cu substrate10.1007/s12598-009-0125-0 ↗
26. Solidification behavior of Sn–9Zn–xAg lead-free solder alloys10.1016/j.msea.2005.08.185 ↗
27. Effect of Ag addition on the microstructure and corrosion properties of Sn–9Zn lead-free solder10.1016/j.jmrt.2023.11.123 ↗
28. Effect of Cu content on performance of Sn-Zn-Cu lead-free solder alloys designed by cluster-plus-glue-atom model10.3390/ma14092335 ↗
29. Effect of minor Cu addition on corrosion behavior of Sn-Zn-xCu touch-up solder alloys10.1002/maco.201609313 ↗
30. Effect of trace Mn modification on the microstructure and corrosion behavior of Sn−9Zn solder alloy
31. Effects of minor alloying with Ge and In on the interfacial microstructure between Zn–Sn solder alloy and Cu substrate10.1016/j.jallcom.2020.154812 ↗
32. Pb-free solder-alloy based on Sn–Zn–Bi with the addition of germanium10.1016/j.jallcom.2010.03.094 ↗
33. Electrochemical corrosion study of Pb-free solders10.1557/jmr.2006.0035 ↗
34. Effect of Zn incorporation on the electrochemical corrosion properties of SAC105 solder alloys10.1007/s10854-019-01055-z ↗
35. Effect of Nd addition on the corrosion behavior of SAC305 solder alloy10.1016/j.corsci.2023.111264 ↗
36. Corrosion behaviour of Sn-9Zn-xS solders in 3.5 wt% NaCl solution10.1080/02670836.2022.2159635 ↗
37. The role of Zn precipitates and Cl− anions in pitting corrosion of Sn–Zn solder alloys10.1016/j.corsci.2014.12.014 ↗
38. Effect of Al on the electrochemical corrosion behaviour of Pb free Sn–8.5 Zn–0.5 Ag–XAl–0.5 Ga solder in 3.5 % NaCl solution10.1016/j.apsusc.2005.08.020 ↗
39. Discussion and challenges concerning the elaboration of a dissolution reaction mechanism10.1016/j.electacta.2019.02.036 ↗
40. Effects of Ag contents in Sn–xAg lead-free solders on microstructure, corrosion behavior and interfacial reaction with Cu substrate10.1016/S1003-6326(19)65076-4 ↗
41. Enhancement on the high-temperature joint reliability and corrosion resistance of Sn–0.3Ag–0.7Cu low-Ag solder contributed by Al2O3 Nanoparticles (0.12 wt%)10.1007/s10854-018-0092-z ↗
42. Effects of nanoscale Sn segregation on corrosion behavior of laser powder bed fusion Cu-15Ni-8Sn alloy10.1016/j.jmst.2023.01.056 ↗
43. The analysis of electrode impedances complicated by the presence of a constant phase element10.1016/S0022-0728(84)80324-1 ↗
44. The analysis of electrode impedances complicated by the presence of a constant phase element10.1016/S0022-0728(84)80324-1 ↗
45. Electrochemical corrosion behaviour of Sn–Sb solder alloys: the roles of alloy Sb content and type of intermetallic compound10.1080/1478422X.2020.1791446 ↗
46. EIS analysis on chloride-induced corrosion behavior of reinforcement steel in simulated carbonated concrete pore solutions10.1016/j.jelechem.2012.09.012 ↗
47. Short-term deterioration of polymer-coated 55 % Al-Zn – part 1: behavior of thin polymer films10.5006/1.3280481 ↗
48. The semi-conductor property and corrosion resistance of passive film on electroplated Ni and Cu–Ni alloys10.1016/j.jelechem.2011.09.013 ↗
49. Ti addition to enhance corrosion resistance of Sn–Zn solder alloy by tailoring microstructure10.1016/j.jallcom.2015.04.168 ↗
50. Experimental Investigation of the Ternary Ge-Sn-In and Ge-Sn-Zn Systems10.1007/s11669-018-0696-2 ↗
51. Thermodynamic optimization of the Ge–Sb and Ge–Sb–Sn systems10.1016/j.tca.2011.03.008 ↗
52. Electrochemical behaviors of the Sn-9Zn-xAg lead-free solders in a 3.5 wt% NaCl solution10.1149/1.1756890 ↗
53. X-ray photoelectron spectroscopy investigation of argon ion sputtered tin oxides and solder alloy
54. XPS analysis of oxide films on lead-free solders with trace additions of germanium and gallium10.4028/www.scientific.net/MSF.857.63 ↗
55. XPS study of the surface chemistry of conventional hot-dip galvanised pure Zn, galvanneal and Zn–Al alloy coatings on steel10.1016/S1359-6454(03)00408-7 ↗
56. Electrochemical corrosion behaviour of Sn-Zn-xBi alloys used for miniature detonating cords