Abstract ZrB2-SiC based composite coatings with different tungsten-containing additives (WB/WSi2/W) were prepared by vacuum plasma spray. The ablation resistance of the coatings was evaluated by a plasma flame. The phase composition and microstructure evolution of the composite coatings during ablation were characterized and the function of tungsten-containing additives was focused on. The results showed that the introduction of tungsten-containing additives could obviously reduce the surface temperature by about 300 °C during the ablation processes. Based on microstructure observation and thermodynamic calculations, it was considered that the evaporation of WO3 and formation/existence of pure W with high thermal conductivity contributed a lot to the reduction of the surface temperature.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. Ultra-high temperature ceramics: materials for extreme environments10.1016/j.scriptamat.2016.10.018 ↗
2. Refractory diborides of zirconium and hafnium10.1111/j.1551-2916.2007.01583.x ↗
3. Advances in oxidation and ablation resistance of high and ultra-high temperature ceramics modified or coated carbon/carbon composites10.1016/j.jeurceramsoc.2017.08.013 ↗
4. Processing and properties of ultra-high temperature ceramics for space applications10.1016/j.msea.2007.08.054 ↗
5. Laboratory, on-ground and in-flight investigation of ultra high temperature ceramic composite materials10.1016/j.ast.2016.09.004 ↗
6. Microstructure evolution of ZrB2–MoSi2 composite coatings at middle and high temperatures10.1016/j.surfcoat.2015.03.029 ↗
7. The oxidation behaviors of a ZrB2–SiC–ZrC ceramic10.1016/j.solidstatesciences.2010.12.022 ↗
8. Improved processing and oxidation-resistance of ZrB2 ultra-high temperature ceramics containing SiC nanodispersoids10.1016/j.msea.2007.03.002 ↗
9. In situ studies of oxidation of ZrB2 and ZrB2–SiC composites at high temperatures10.1016/j.jeurceramsoc.2010.03.009 ↗
10. Thermodynamic analysis of ZrB2-SiC oxidation: formation of a SiC-Depleted region10.1111/j.1551-2916.2006.01329.x ↗
11. SiC depletion in ZrB2-30 vol% SiC at ultrahigh temperatures10.1111/jace.13519 ↗
12. Ablation behavior of ZrB2–SiC protective coating for carbon/carbon composites10.1016/j.ceramint.2015.02.096 ↗
13. Dynamic oxidation of ultra-high temperature ZrB2–SiC under high enthalpy supersonic flows10.1016/j.corsci.2010.11.018 ↗
14. In-situ fabrication of ZrB2 –SiC/SiC gradient coating on C/C composites10.1016/j.jallcom.2015.05.205 ↗
15. Thermoablative resistance of ZrB2 -SiC-WC ceramics at 2400 °C10.1016/j.actamat.2017.05.033 ↗
16. Strong ZrB2-SiC-WC ceramics at 1600°C10.1111/j.1551-2916.2011.05062.x ↗
17. Effect of WB on oxidation behavior and microstructure evolution of ZrB2-SiC coating10.1016/j.corsci.2019.04.034 ↗
18. Effects of temperature and the incorporation of W on the oxidation of ZrB2 ceramics10.1016/j.corsci.2013.11.030 ↗
19. Improved oxidation resistance of zirconium diboride by tungsten carbide additions10.1111/j.1551-2916.2008.02713.x ↗
20. Oxidation of zirconium diboride with tungsten carbide additions10.1111/j.1551-2916.2010.04216.x ↗
21. Influence of Al2O3 addition on the ablation behavior of SiC coatings fabricated on C/C composites10.1016/j.surfcoat.2012.11.080 ↗
22. Oxidation and volatilization of silica formers in water vapor10.1111/j.1151-2916.2003.tb03459.x ↗
23. First-principles study of enhancement of transport properties of silica melt by water
24. Degradation of CVD-SiC coated C/SiC composites exposed to the monopropellant combustion products based on Hydroxylammonium nitrate (HAN)10.1016/j.corsci.2013.04.036 ↗
25. Oxidation behavior of 3D Hi-Nicalon/SiC composite exposed in wet and simulated air environments10.1016/j.corsci.2012.09.008 ↗
26. Paralinear oxidation of Cr-Si-C-Coated C/SiC at 1300°C in wet and dry air environments
27. Silicon oxidation studies: the role of H2O10.1149/1.2133151 ↗
28. Low-temperature electrical and thermal resistivities of tungsten10.1103/PhysRevB.3.3141 ↗
29. Thermophysical properties of transition metal carbides and diborides
30. Carbon-carbon composites10.1146/annurev.ms.24.080194.000315 ↗
31. A model to calculate the viscosity of silicate melts Part IV10.3139/146.110638 ↗
32. Condensed phase relations in the systems ZrO2-WO2-WO3 and HfO2-WO2-WO310.1111/j.1151-2916.1967.tb15084.x ↗
33. Negative thermal expansion from 0.3 to 1050 Kelvin in ZrW2O810.1126/science.272.5258.90 ↗