The coupling mechanism of shrinkage defects and graphite on the corrosion resistance of ductile iron
Source abstract
Abstract
This study investigated the coupling mechanism of shrinkage defects and graphite on the corrosion resistance of ductile iron by electrochemical measurements, quasi-in-situ immersion tests and numerical simulations. The detrimental impact of shrinkage defects was confirmed by elevated corrosion current density and the formation of a porous corrosion product layer. Multiple-galvanic coupling effect among the matrix, graphite, and shrinkage defects serves as corrosion triggers, which is verified by scanning Kelvin probe force microscopy (SKPFM) and numerical simulations. Additionally, quasi-in-situ observations corroborate the deposition of corrosion products and Cl enrichment at defect bottoms, expediting occluded cell formation and corrosion propagation.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · Microstructure and Mechanical Properties of Steels
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (57)
Show source-provided references
1. A review on heat treatment of cast iron: phase evolution and mechanical characterization10.3390/ma15207109 ↗
2. Electron microscopy of carbides in annealed 28 wt% Cr - 1 wt% (Mo/W) cast irons10.1016/j.matchar.2023.112723 ↗
3. Cyclic oxidation of high-silicon spheroidal graphite iron10.1016/j.corsci.2021.109854 ↗
4. In situ synchrotron investigation of degenerate graphite nodule evolution in ductile cast iron10.1016/j.actamat.2021.117367 ↗
5. Effect of selective pre-oxidation on the growth and corrosion resistance of hot-dip zinc coating of nodular cast iron10.1016/j.corsci.2021.109463 ↗
6. Thermal and mechanical behaviour of grey cast iron and ductile iron castings using magnetic molding and lost foam processes10.1016/j.jmatprotec.2008.10.002 ↗
7. Analysis of ductile cast iron tensile tests to relate ductility variation to casting defects and material microstructure10.1016/j.msea.2008.09.082 ↗
8. Fatigue strength optimization of gray cast iron processed by different austempering temperatures10.1016/j.ijfatigue.2023.107831 ↗
9. Microstructural, multilevel simulation of notch effect in ferritic ductile cast iron under low cycle fatigue10.1016/j.ijfatigue.2022.106993 ↗
10. Mechanical and tribological behavior of dual-phase ductile iron with different martensite amounts10.1016/j.jmrt.2023.03.210 ↗
11. Effect of austempering temperature on microstructure and mechanical properties of ductile cast iron modified by niobium10.1016/j.jmrt.2021.04.041 ↗
12. Effect of mechanically imposed stresses on the contact fatigue resistance of two cast irons with high hardness matrix10.1016/j.wear.2007.01.084 ↗
13. Comparison of the tribological behavior of quench-tempered ductile iron and austempered ductile iron with similar hardness
14. Wear Behavior of Nb Alloyed Gray Cast Iron for Automotive Brake Disc Application10.3390/met13020365 ↗
15. Long solidification time effect on solution strengthened ferritic ductile iron fatigue properties10.1016/j.ijfatigue.2020.106137 ↗
16. A strain energy density design approach for large cast iron components: From microstructural analysis to multiaxial fatigue response10.1016/j.ijfatigue.2023.107824 ↗
17. Effect of the Type of Inoculant on the Shrinkage Porosity of High-Silicon SG Iron
18. Study on the Austemperability of Thin-wall Ductile Cast Iron Produced by High-Pressure Die-casting10.1007/s11665-021-06252-8 ↗
19. Influence of Chemical Composition and Cooling Rate on Chunky Graphite Formation in Thick-Walled Ductile Iron Castings
20. Effect of Elemental Segregation on the Microstructure and Mechanical Properties of Heavy Section Compacted Graphite Iron
21. The Effects of Holding Time in the Heating/Pouring Unit on the Metallurgical Quality of Spheroidal Graphite Iron
22. Mechanical and fatigue properties of pearlitic ductile iron castings characterized by long solidification times10.1016/j.engfailanal.2017.06.007 ↗
23. Microscopic Characterization of Different Shrinkage Defects in Ductile Irons and their Relation with Composition and Inoculation Process
24. A new energy based highly stressed volume concept to investigate the notch-pores interaction in thick-walled ductile cast iron subjected to uniaxial fatigue10.1016/j.ijfatigue.2022.107491 ↗
25. A Study of the Mechanisms and Kinetics of the Localized Corrosion Aggravation of Ductile Iron in a Harsh Water Quality Environment10.3390/met12122103 ↗
26. Towards a better understanding of localised corrosion induced by typical non-metallic inclusions in low-alloy steels10.1016/j.corsci.2020.109150 ↗
27. New insights into the mechanism of localised corrosion induced by TiN-containing inclusions in high strength low alloy steel10.1016/j.jmst.2021.12.075 ↗
28. Corrosion behavior of nickel alloyed and austempered ductile irons in 3.5% sodium chloride10.1016/j.corsci.2010.05.006 ↗
29. Improved corrosive wear resistance of carbidic austempered ductile iron by addition of Cu10.1016/j.matchar.2020.110577 ↗
30. Pseudo-passive films on cast irons: A strategy to mitigate corrosion by acting directly on microstructure10.1016/j.corsci.2022.110480 ↗
31. Corrosion behavior of Cu–Al–Be shape memory alloys with different compositions and microstructures10.1016/j.corsci.2013.05.012 ↗
32. H. Natter, D. Bähre, Electrochemical dissolution of cast iron in NaNO3 electrolyte10.1007/s10800-015-0809-0 ↗
33. Eco-friendly approach to corrosion inhibition of AA5083 aluminum alloy in HCl solution by the expired Vitamin B1 drugs10.1016/j.molstruc.2021.130881 ↗
34. Liu · Influ. Cem. Coarse Corros. Resist. High. Strength Low. Alloy Steel, npj Mater. Degrad. · 2023 · 7 · 43
35. Comprehensive investigation of modified polyethyleneimine as an efficient polymeric corrosion inhibitor in neutral medium: Synthesis, experimental and theoretical assessments10.1016/j.molliq.2021.116803 ↗
36. Self-assembly anchored film of two modified polyamide as promising cost-effective inhibitor for protecting carbon steel in neutral medium, Materials Today
37. Mechanism of corrosion of cast iron covered by aged corrosion products: Application of electrochemical impedance spectrometry10.1016/j.corsci.2009.12.026 ↗
38. In-situ monitoring of the corrosion behaviour of austempered ductile iron (ADI) under cyclic salt spray exposure10.1016/j.corsci.2021.109437 ↗
39. Study on Growth of Corrosion Scale on Various Iron Based Materials (Grey cast iron/Carbon steel/Ductile Iron) in Water Distribution Systems10.20964/2020.09.80 ↗
40. Effects of chloride ions on corrosion of ductile iron and carbon steel in soil environments10.1038/s41598-017-07245-1 ↗
41. Mechano-electrochemical interaction of high-strength pipeline steels with Al-Ti deoxidization and Mg-Ca compound treatment10.1016/j.corsci.2023.111534 ↗
42. Understanding the galvanic corrosion of Cu-Ni alloy/2205 DSS couple using electrochemical noise and microelectrochemical studies10.1016/j.corsci.2023.111512 ↗
43. Influence of multispecies biofilms of Pseudomonas aeruginosa and Desulfovibrio vulgaris on the corrosion of cast iron10.1016/j.corsci.2017.03.008 ↗
44. Failure analysis in buried ductile iron pipelines: A study of leakage in drinking water distribution systems10.1016/j.engfailanal.2023.107361 ↗
45. Measurement of local galvanic surface corrosion using scanning electrochemical microscopy on ductile cast iron10.1007/s10853-019-03506-8 ↗
46. Effects of microbial cycling of Fe(II)/Fe(III) and Fe/N on cast iron corrosion in simulated drinking water distribution systems10.1016/j.corsci.2015.08.037 ↗
47. A finite element based model for prediction of corrosion defect growth on pipelines10.1016/j.ijpvp.2017.05.002 ↗
48. Experimental and numerical studies of effectiveness of cathodic protection at corrosion defects on pipelines10.1016/j.corsci.2013.09.011 ↗
49. Determination of pitting sensitivity of the aluminium alloy EN AW-6060-T6 in a carbon-fibre reinforced plastic/aluminium rivet joint by finite element simulation of the galvanic corrosion process10.1016/j.corsci.2013.03.033 ↗
50. Local scanning electrochemical microscopy analysis of a lithium-based conversion layer on AA2024-T3 at progressive stages of formation10.1016/j.electacta.2023.143270 ↗
51. Noell · Evol. Pit. Morphol. Growth Kinet. Alum. Atmos. Corros., npj Mater. Degrad. · 2023 · 7 · 12
52. Microstructure and corrosion behavior of welded joint between 2507 super duplex stainless steel and E690 low alloy steel, Corrosion
53. Discovering the nanoscale origins of localized corrosion in additive manufactured stainless steel 316L by liquid cell transmission electron microscopy10.1016/j.corsci.2022.110659 ↗
54. Role of gradient nano-structured surface in collapsed pitting corrosion on AISI 316L stainless steel during tribocorrosion10.1016/j.corsci.2021.110043 ↗
55. Research into water-soluble salts in efflorescent pottery during long-term storage in a museum10.1016/j.corsci.2014.09.003 ↗
56. Nodular corrosion inside the crevice of Alloy 690 in deaerated high-temperature chloride solution10.1016/j.corsci.2021.109442 ↗
57. Study on corrosion, hydrogen permeation, and stress corrosion cracking behaviours of AISI 4135 steel in the tidal zone10.1038/s41529-022-00309-2 ↗