An investigation of oxidation/hot corrosion-creep interaction at 800 °C in a Ni-base superalloy coated with salt mixture deposits of Na2SO4-NaCl-NaVO3
Source abstract
Abstract
Abstract Creep-rupture behaviour of Nimonic263 alloy coated with 87.5 wt.%Na2SO4+5 wt.%NaCl +7.5 wt.%NaVO3(3SM) and 74 wt.%Na2SO4+21.7 wt.%NaCl+4.3 wt.%NaVO3(3SM-A) was investigated in the stress range of 180–350 MPa at 800 °C. The 3SMs are responsible for the reduction in creep-rupture life. Hot corrosion products found in the crack regions of the crept specimens deformed under the influence of 3SMs. Sulphidation followed by oxidation was dominant at 250 MPa, whereas oxidation was dominant at 215 and 180 MPa. Comprehensive microstructural characterization and analysis suggest that three-salt mixtures(3SMs) accelerate oxygen and sulphur penetration along the grain boundaries during creep, and enhance the stress assisted grain boundary oxidation resulting in a reduction in creep-rupture life.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High Temperature Alloys and Creep · High-Temperature Coating Behaviors · Nuclear Materials and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (51)
Show source-provided references
1. Nickel-base superalloys : current status and potential10.1098/rsta.1995.0044 ↗
2. Nickel-based superalloys for advanced turbine engines: chemistry, microstructure and properties10.2514/1.18239 ↗
3. Mechanism of intermediate temperature embrittlement of Ni and Ni-based superalloys10.1080/10408436.2011.613492 ↗
4. Carpenter · 1997 · 679
5. Environmental effects on the creep behavior of a nickel-base superalloy10.1007/BF02648351 ↗
6. Effet of environment on mechanical properties of coated superalloys and gas turbine blades
7. Effect of hot corrosion on the the mechanical performances of superalloys and coating systems10.1016/0010-938X(93)90331-A ↗
8. A mechanism for stress-aided grain boundary oxidation ahead of cracks10.1016/j.scriptamat.2013.03.026 ↗
9. Effects of oxygen on creep performance: mechanisms and predictive modelling10.1179/mst.1990.6.1.2 ↗
10. Effects of the environment on the crack propagation behavior of IN718 in the temperature range of the dynamic embrittlement10.1520/JAI103569 ↗
11. Oxygen-induced intergranular cracking of a Ni-base alloy elevated temperatures-an example of dynamic embrittlement10.1016/S1359-6454(01)00005-2 ↗
12. The effect of prior exposure-time on air-environment/creep interactions10.1016/0001-6160(86)90168-9 ↗
13. Influence of sulphidation and carburisation on creep10.1179/mst.1990.6.1.9 ↗
14. Creep-fatigue failure of SAF 2205 and 316 stainless steels in Ar + 3 % SO2 environment at 700 °C10.1007/BF00351293 ↗
15. Penetration and embrittlement of grain boundaries by sulphur and chlorine – preliminary observations in nickel and a nickel base superalloys10.1016/0036-9748(83)90229-6 ↗
16. The environmental-effect of SO2-bearing atmosphere on the creep-fatigue failure of aluminide-coated MM-002 nickel-base superalloy at 870 °C10.1007/BF00353050 ↗
17. Hot corrosion in gas turbine components10.1016/S1350-6307(00)00035-2 ↗
18. Impurity deposits in gas turbines from fuels containing sodium and vanadium10.1149/1.2123941 ↗
19. The effect of hot corrosion on creep and fracture behaviour of cast nickel-based superalloy IN738LC
20. Influence of hot corrosion on the creep strength of the nickel-base superalloy10.1016/0025-5416(84)90262-3 ↗
21. Balsone · 1985
22. Effect of creep or low cycle fatigue on the oxidation or hot corrosion behaviour of nickel-base superalloys10.1016/0025-5416(87)90085-1 ↗
23. Effect of environmental factors on the creep rupture properties of a Nickel base superalloys subjected to hot corrosion10.2320/matertrans1960.29.26 ↗
24. Interaction of low temperature hot corrosion and creep10.1016/0921-5093(89)90349-3 ↗
25. Effect of vanadic corrosion on creep-rupture properties of Superni-600 at 650–750 °C10.1080/09603409.1992.11689425 ↗
26. Creep rupture behaviour of 2.25Cr-1Mo steel in sulphate-pyrosulphate mixture10.1007/BF00882544 ↗
27. Vanadic hot corrosion - creep interaction of superni - C276 in the temperature range 650-750 °C10.1515/HTMP.1994.13.4.277 ↗
28. Effect of salt induced high temperature corrosion on creep rupture properties on AISI316 stainless steel
29. Effect of hot corrosion on the creep properties of types 321 and 347 stainless steels10.1361/105994999770347223 ↗
30. Creep rupture of Nimonic-90 under salt-induced high temperature corrosion
31. Interaction of hot corrosion and creep in Alloy 61710.1016/j.engfailanal.2016.03.012 ↗
32. Effect of salt-deposit hot corrosion on creep rupture behaviors of DZ466 superalloy10.4028/www.scientific.net/MSF.850.56 ↗
33. Physically-based model for creep in nickel-base superalloy C263 both above and below the gamma solvus10.1016/S1359-6454(02)00119-2 ↗
34. Phase precipitation and phase stability in nimonic 26310.1007/s11661-001-0217-4 ↗
35. Analysis of creep curves of a nickel base superalloy in a wide stress/temperature range10.1016/j.msea.2005.11.084 ↗
36. Mechanism of dislocation shearing of gamma prime in fine precipitate strengthened superalloy10.1179/026708301101509818 ↗
37. Prestraining effect on creep behaviour of nickel base C263 superalloy10.1179/026708302225004838 ↗
38. Air-environment-creep interaction in a nickel base superalloy10.1016/1350-6307(95)00019-M ↗
39. Effect of prior oxidation on the creep behaviour of nickel and iron based superalloys
40. The role of particle ripening on the creep acceleration of Nimonic 263 superalloy
41. Influence of saline environment on creep rupture life of Nimonic-263 for marine turbine application10.1016/j.msea.2012.12.081 ↗
42. Corrosion resistance of superalloys in the temperature range 800-1300 ºF10.1007/BF02833378 ↗
43. Hot corrosion studies on Ni-base superalloy at 650 °C under marine-like environment conditions using three salt mixture (Na2SO4+NaCl+NaVO3)10.1016/j.corsci.2016.01.008 ↗
44. Influence of two different salt mixture combinations of Na2SO4-NaCl-NaVO3 on hot corrosion behavior of Ni-base superalloy at 800 °C
45. Isothermal high temperature low cycle fatigue behavior of Nimonic-263 : Influence of type I and type II hot corrosion10.1016/j.msea.2014.11.016 ↗
46. An innovative spraying setup to obtain uniform salt(s) mixture deposition to investigate hot corrosion10.1063/1.4941779 ↗
47. The influence of oxidation on the high temperature tensile creep of iron10.1179/030634571790439603 ↗
48. The influence of oxidation on the steady state creep of iron at 823–1023K10.1080/01418618108239559 ↗
49. Role of metal-oxide interfacial reactions on the interactions between oxidation and deformation10.1016/S1359-6462(98)00202-4 ↗
50. Hot corrosion behavior of CM 247 LC alloy in Na2SO4 and NaCl environments10.1023/A:1018831025272 ↗
51. Static and dynamic aspects of coupling between creep behavior and oxidation on MC2 single crystal superalloy at 1150 °C10.1016/j.actamat.2005.05.018 ↗