journal article·2023-07

A systematic analysis of the calcium-magnesium-aluminosilicate corrosion behavior of high-entropy (5Re0.2)2Si2O7 materials

Fushuang Wei, Dongxing Zhang, Xue Gong, Yong Liu, Binxin Li, Peng Hao, Feifei Zhou, Baosheng Xu, Xiaodong Zhang, You Wang

Corrosion Science· Volume 219
Publisher page

Abstract

The CaO-MgO-AlO 1.5-SiO 2 (CMAS) corrosion resistance of disilicates is an urgent task in environmental barrier coatings. Based on this, four high-entropy rare earth disilicates (Yb 0.2Y 0.2Lu 0.2Sc 0.2Gd 0.2) 2Si 2O 7, (Yb 0.2Tm 0.2Lu 0.2Sc 0.2Gd 0.2) 2Si 2O 7, (Yb 0.2Tm 0.2Lu 0.2Sc 0.2Er 0.2) 2Si 2O 7, and (Yb 0.2Y 0.2Lu 0.2Ho 0.2Er 0.2) 2Si 2O 7 and single-component Yb 2Si 2O 7 for comparison were investigated. Results showed that cyclosilicate Ca 3RE 2(Si 3O 9) 2 and apatite Ca 2RE 8(SiO 4) 6O 2 are formed sequentially at 1300 ℃ for 48 h, which can block the CMAS from infiltrating the ceramics. The corrosion resistance of the four high-entropy rare earth silicates varied depending on the average RE 3+ radius, but all performed better than Yb 2Si 2O 7.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · High Entropy Alloys Studies · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. CMAS degradation of environmental barrier coatings10.1016/j.surfcoat.2007.06.045 ↗
2. Progress in ceramic materials and structure design toward advanced thermal barrier coatings10.1007/s40145-022-0581-7 ↗
3. Current status of environmental barrier coatings for Si-based ceramics
4. Water vapor volatilization and oxidation induced surface cracking of environmental barrier coating systems: A numerical approach10.1016/j.ceramint.2021.02.225 ↗
5. Advanced structural ceramics in aerospace propulsion10.1038/nmat4687 ↗
6. A review on environmental barrier coatings: history, current state of the art and future developments10.1016/j.jeurceramsoc.2020.10.057 ↗
7. Thermal expansion of rare‐earth pyrosilicates10.1111/jace.12388 ↗
8. Corrosion of RE2Si2O7 (RE= Y, Yb, and Lu) environmental barrier coating materials by molten calcium-magnesium-alumino-silicate glass at high temperatures10.1016/j.jeurceramsoc.2019.05.036 ↗
9. Environmental-barrier coating ceramics for resistance against attack by molten calcia-magnesia-aluminosilicate (CMAS) glass: Part I, YAlO3 and γ-Y2Si2O710.1016/j.jeurceramsoc.2018.03.021 ↗
10. Environmental-barrier coating ceramics for resistance against attack by molten calcia-magnesia-aluminosilicate (CMAS) glass: Part II, β-Yb2Si2O7 and β-Sc2Si2O710.1016/j.jeurceramsoc.2018.03.010 ↗
11. A fracture-resistant high-entropy alloy for cryogenic applications10.1126/science.1254581 ↗
12. Strength-ductility synergy of Al0.1CoCrFeNi high-entropy alloys with gradient hierarchical structures10.1016/j.scriptamat.2019.04.002 ↗
13. Microstructure and mechanical properties of refractory HfMo0.5NbTiV0.5Six high-entropy composites10.1016/j.jallcom.2016.10.014 ↗
14. Microstructures and properties of high-entropy alloys
15. Thermal conductivity and hardness of three single-phase high-entropy metal diborides fabricated by borocarbothermal reduction and spark plasma sintering10.1016/j.ceramint.2019.11.186 ↗
16. A multicomponent γ-type (Gd1/6Tb1/6Dy1/6Tm1/6Yb1/6Lu1/6)2Si2O7 disilicate with outstanding thermal stability10.1080/21663831.2020.1783007 ↗
17. Technology, High-entropy (Y0.2Nd0.2Sm0.2Eu0.2Er0.2)AlO3: a promising thermal/environmental barrier material for oxide/oxide composites10.1016/j.jmst.2020.02.011 ↗
18. High-entropy ceramics10.1038/s41578-019-0170-8 ↗
19. Exploration of the mechanism of enhanced CMAS corrosion resistance at 1500 °C for multicomponent (Er0.25Tm0.25Yb0.25Lu0.25)2Si2O7 disilicate10.1016/j.corsci.2022.110343 ↗
20. Preparation and corrosion resistance of high-entropy disilicate (Y0.25Yb0.25Er0.25Sc0.25)2Si2O7 ceramics10.1016/j.corsci.2021.109786 ↗
21. Investigation on improving corrosion resistance of rare earth pyrosilicates by high-entropy design with RE-doping10.1016/j.corsci.2022.110217 ↗
22. High-entropy environmental barrier coating for the ceramic matrix composites10.1016/j.jeurceramsoc.2019.02.022 ↗
23. High-entropy rare-earth disilicate (Lu0.2Yb0.2Er0.2Tm0.2Sc0.2)2Si2O7: a potential environmental barrier coating material10.1016/j.jeurceramsoc.2022.03.006 ↗
24. Thermochemistry of calcium rare‐earth silicate oxyapatites10.1111/jace.16816 ↗
25. Effects of crystal structure and cation size on molten silicate reactivity with environmental barrier coating materials10.1111/jace.16694 ↗
26. Calcium-magnesium-aluminosilicate corrosion behaviors of rare-earth disilicates at 1400°C10.1016/j.jeurceramsoc.2013.05.030 ↗
27. High-Temperature thermochemical interactions of molten silicates with Yb2Si2O7 and Y2Si2O7 environmental barrier coating materials10.1016/j.jeurceramsoc.2019.06.051 ↗
28. General trend on the phase stability and corrosion resistance of rare earth monosilicates to molten calcium-magnesium-aluminosilicate at 1300 ℃10.1016/j.corsci.2018.12.032 ↗
29. Hot corrosion of RE2SiO5 with different cation substitution under calcium-magnesium-aluminosilicate attack10.1016/j.ceramint.2017.04.045 ↗
30. Corrosion of RE2Si2O7 (RE=Y, Yb, and Lu) environmental barrier coating materials by molten calcium-magnesium-alumino-silicate glass at high temperatures10.1016/j.jeurceramsoc.2019.05.036 ↗
31. Towards thermal barrier coating application for rare earth silicates RE2SiO5 (RE= La, Nd, Sm, Eu, and Gd)10.1016/j.jeurceramsoc.2018.12.015 ↗
32. Effects of cation substitution and temperature on the interaction between thermal barrier oxides and molten CMAS10.1016/j.jeurceramsoc.2014.09.006 ↗
33. Phase equilibria and crystal chemistry in the calcia-silica-yttria system10.1016/j.jeurceramsoc.2016.01.046 ↗
34. Synthesis and structural refinement of isomorphic cyclosilicate Ca3RE2(Si3O9)2 (RE = Nd, Sm, Gd, Dy, Yb)10.1016/j.jssc.2022.123312 ↗
35. Revised effective ionic radii and systematic studies of interatomic distances in halides and chalcogenides10.1107/S0567739476001551 ↗
36. Tailoring thermal and chemical properties of a multi-component environmental barrier coating candidate (Sc0.2Nd0.2Er0.2Yb0.2Lu0.2)2Si2O7
37. (La0.2Ce0.2Nd0.2Sm0.2Eu0.2)2Zr2O7: a novel high-entropy ceramic with low thermal conductivity and sluggish grain growth rate10.1016/j.jmst.2019.05.054 ↗
38. Sluggish diffusion in Co-Cr-Fe-Mn-Ni high-entropy alloys10.1016/j.actamat.2013.04.058 ↗