Abstract

The initiation site of pitting corrosion on type 304 stainless steel was quantitatively analysed using an automatic inclusion analyser and electron backscatter diffraction. In a sample anodically polarised at 0.43 V SSE , the fraction of stable pits initiated from inclusions was only 23 %. Pits initiated from sites other than inclusions probably initiated from grain boundaries, strain-induced martensite and scratches. In mixed inclusions of MnS and oxides, the probability of pit initiation increased with the S concentration. The Ti concentration had no effect on the probability of pit initiation, suggesting that whether Ti exists as TiO 2 or TiN is important.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Welding Techniques and Residual Stresses

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (47)

Show source-provided references
1. The initiation of pitting corrosion on austenitic stainless steel: on the role and importance of sulphide inclusions10.1016/0010-938X(92)90074-D ↗
2. Pitting and sulphide inclusions in steel10.1016/S0010-938X(74)80047-8 ↗
3. The role of inclusions on initiation of crevice corrosion of stainless steel: I. Experimental studies10.1149/1.2096896 ↗
4. Occluded solution chemistry control and the role of alloy sulfur on the initiation of crevice corrosion in type 304ss10.1016/S0010-938X(98)00084-5 ↗
5. Pit initiation at single sulfide inclusions in stainless steel: I. Electrochemical microcell measurements10.1149/1.1474430 ↗
6. Microelectrochemical measurements of Dissolution of MnS inclusions and morphological observation of metastable and stable pitting on stainless steel10.1149/1.2745639 ↗
7. Why stainless steel corrodes10.1038/415770a ↗
8. Initiation of pitting at sulfide inclusions in stainless steel10.1149/1.2401840 ↗
9. Pit initiation mechanism at MnS inclusions in stainless steel: synergistic effect of elemental sulfur and chloride ions10.1149/2.081310jes ↗
10. Mechanism of (Mg, Al, Ca)-oxide inclusion-induced pitting corrosion in 316L stainless steel exposed to sulphur environments containing chloride ion10.1016/j.corsci.2012.09.044 ↗
11. Initiation of pitting at severe crevice of titanium carbonitride/matrix boundary on ferritic stainless steels10.3323/jcorr.63.325 ↗
12. Rust nucleation sites in 18Cr-Ti stainless steel10.2355/tetsutohagane1955.63.10_1719 ↗
13. The effect of retained ferrite on localized corrosion in duplex 304 L stainless steel
14. Effect of cold-working in the passive behavior of 304 stainless steel in sulfate media10.1149/1.1516774 ↗
15. The effects of morphology of ferrite and non-metallic inclusions on corrosion behavior of as-cast 304 stainless steel10.5006/3763 ↗
16. L. Peguet, B. Malki, B. Baroux, Influence of cold working on the pitting corrosion resistance of stainless steels, Corros. Sci., vol. 49, 2007, pp. 1993–48.10.1016/j.corsci.2006.08.021 ↗
17. Influence of the individual microstructural features on pitting corrosion in type 304 austenitic stainless steel10.1016/j.corsci.2019.108091 ↗
18. Transport processes and the mechanism of pitting of metals10.1149/1.2132857 ↗
19. Ghahari · Corros. Sci. · 2015 · 100 · 2310.1016/j.corsci.2015.06.023 ↗
20. X-Ray tomographic characterisation of pitting corrosion in lean duplex stainless steel10.1016/j.corsci.2019.108406 ↗
21. Mechanism of pit growth on aluminum under open circuit conditions10.5006/1.3593889 ↗
22. The mechanism of lacy cover formation in pitting10.1016/S0010-938X(97)00043-7 ↗
23. Pit growth studies in stainless steel foils. II. Effect of temperature, chloride concentration and sulphate addition10.1016/S0010-938X(01)00134-2 ↗
24. Pitting, lacy covers, and pit merger in stainless steel: 3D peridynamic models10.1016/j.corsci.2019.01.006 ↗
25. A new microelectrochemical method to study pit initiation on stainless steel10.1016/S0013-4686(70)01783-8 ↗
26. Roles of different components of complex inclusion in pitting of 321 stainless steel: induction effect of CaS and inhibition effect of TiN10.1016/j.corsci.2022.110692 ↗
27. Passivity of (Mn,Cr)S inclusions in type 304 stainless steel: the role of Cr and the critical concentration for preventing inclusion dissolution in NaCl solution10.1016/j.corsci.2020.109060 ↗
28. Initiation of corrosion pits at inclusions on 304 stainless steel10.1149/1.2048462 ↗
29. Operando electrochemical TEM, ex-situ SEM and atomistic modelling studies of MnS dissolution and its role in triggering pitting corrosion in 304L stainless steel10.1016/j.corsci.2022.110184 ↗
30. R.P.M. Procter, in: L.L. Shreir, R.A. Jarman, G.T. Burstein (eds.), Corrosion, 3rd ed., Vol. 1, Butterworth-Heinemann, Oxford, 1994, pp. 49–50.
31. Anomalous evolution of corrosion behaviour of warm-rolled type 304 austenitic stainless steel10.1016/j.corsci.2019.04.025 ↗
32. The effect of mechanical polishing and finishing on the corrosion resistance of AISI 304 stainless steel10.1080/1478422X.2015.1131493 ↗
33. Heinrich · 1991
34. Pitting at the δ/γ boundary of type 304 stainless steel in NaCl solution: the role of oxide inclusions and segregation10.1149/2.0561714jes ↗
35. Surface analysis of corrosion pits initiated at MnS inclusions in 304 stainless steel10.1149/1.2069458 ↗
36. On the mechanism of localized corrosion of iron and stainless steel: I. Electrochemical studies10.1149/1.2403982 ↗
37. On the mechanism of localized corrosion of iron and stainless steel: II. Morphological studies10.1149/1.2403983 ↗
38. Dependence of the critical pitting temperature of surface roughness10.1016/S0010-938X(02)00215-9 ↗
39. Statistical analysis of nonmetallic inclusions as initiation sites of pitting corrosion for stainless steel by all-surface survey10.3323/jcorr.71.46 ↗
40. Optimization of grain boundary character distribution for intergranular corrosion resistant 304 stainless steel by twin-induced grain boundary engineering10.1016/S1359-6454(02)00064-2 ↗
41. Twinning-related grain boundary engineering10.1016/j.actamat.2004.05.031 ↗
42. Sensitisation behaviour of grain boundary engineered austenitic stainless steel10.1016/j.msea.2010.03.058 ↗
43. Atomic force microscopy based approach to local impedance measurement of grain interiors and grain boundaries of sensitized AISI 304 stainless steel10.1016/j.electacta.2010.11.079 ↗
44. Stochastic theory of pitting corrosion10.5006/0010-9312-33.7.243 ↗
45. Further insights on the pitting corrosion of stainless steels
46. Cerium addition to CaS inclusions in stainless steel: insolubilizing water-soluble inclusions and improving pitting corrosion resistance10.1016/j.corsci.2020.109222 ↗
47. Thermodynamics of oxidation reduction equilibria in the TiN-H2O system