Understanding the non-steady electrochemical mechanism on SCC of 304 SS under applied polarization potentials
Source abstract
Abstract
In this work, the non-steady electrochemical model on stress corrosion cracking (SCC) was established, which was verified by SCC of 304 SS with various microstructures. SCC mechanism depends on applied potentials including anodic dissolution (AD), hydrogen embrittlement (HE) and AD+HE, and the potential range for each mechanism was determined with the critical potentials on slow/fast scan potentiodynamic curves. The quantitative relationship of SCC susceptibility and applied potentials is acquired with the model, which is effective for assessing SCC. It was verified by 304 SS with various microstructures, which presents similar non-steady electrochemical characteristics and SCC susceptibility.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Concrete Corrosion and Durability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (62)
Show source-provided references
1. CO2 corrosion behavior of sensitized 304 and 316 austenitic stainless steels in 3.5 wt% NaCl solution and presence of H2S10.1016/j.corsci.2019.108230 ↗
2. Microstructure evolution and SSCC behavior of strain-strengthened 304 SS pre-strained at room temperature and cryogenic temperature10.1016/j.corsci.2022.110855 ↗
3. A new study for healing pitting defects of 316L stainless steel based on microarc technology10.1016/j.corsci.2021.109505 ↗
4. Influence of sensitization on microstructure and passive property of AISI 2205 duplex stainless steel10.1016/j.corsci.2015.12.005 ↗
5. Susceptibility to intergranular corrosion in sensitized austenitic stainless steel characterized via crystallographic characteristics of grain boundaries10.1016/j.corsci.2021.109946 ↗
6. Coupling effect of microstructure and hydrogen absorbed during service on pitting corrosion of 321 austenitic stainless steel weld joints10.1016/j.corsci.2019.108339 ↗
7. Eddy current technique as a nondestructive method for evaluating the degree of sensitization of 304 stainless steel10.1016/j.corsci.2020.108742 ↗
8. Pit initiation on sensitized Type 304 stainless steel under applied stress: Correlation of stress, Cr-depletion, and inclusion dissolution10.1016/j.corsci.2020.108506 ↗
9. Effect of hydrogen charging on SCC of 2205 duplex stainless steel with varying microstructures in simulated deep-sea environment10.1016/j.corsci.2021.110026 ↗
10. Stress corrosion cracking of E690 steel as a welded joint in a simulated marine atmosphere containing sulphur dioxide10.1016/j.corsci.2015.08.039 ↗
11. Correlation between grain boundaries, carbides and stress corrosion cracking of Alloy 690TT in a high temperature caustic solution with lead10.1016/j.corsci.2018.08.010 ↗
12. Stress corrosion cracking behavior and mechanism of Fe-Mn-Al-C-Ni high specific strength steel in the marine atmospheric environment10.1016/j.corsci.2021.109760 ↗
13. Effect of cathodic polarisation on stress corrosion cracking behaviour of a Ni(Fe, Al)-maraging steel in artificial seawater10.1016/j.corsci.2020.109176 ↗
14. Effect of cathodic potential on stress corrosion cracking behavior of different heat-affected zone microstructures of E690 steel in artificial seawater10.1016/j.jmst.2019.08.029 ↗
15. Hydrogen embrittlement under cathodic protection of friction stir welded UNS S32760 super duplex stainless steel10.1016/j.msea.2017.08.117 ↗
16. Hydrogen permeation and stress corrosion cracking of heat-affected zone of E690 steel under the combined effect of sulfur species and cathodic protection in artificial seawater10.1016/j.conbuildmat.2021.123721 ↗
17. Mechanistic Aspect of Non-Steady Electrochemical Characteristic During Stress Corrosion Cracking of an X70 Pipeline Steel in Simulated Underground Water10.5006/1153 ↗
18. Effect of cathodic potentials on the SCC behavior of E690 steel in simulated seawater10.1016/j.msea.2015.05.109 ↗
19. Improving the resistance of high-strength steel to SCC in a SO2-polluted marine atmosphere through Nb and Sb microalloying10.1016/j.corsci.2020.108693 ↗
20. Influence of mechanical surface treatments on oxide properties formed on 304L stainless steel in simulated BWR and PWR
21. Local additional potential model for effect of strain rate on SCC of pipeline steel in an acidic soil solution10.1016/j.corsci.2009.08.019 ↗
22. Effect of strain rate and sulfate reducing bacteria on stress corrosion cracking behaviour of X70 pipeline steel in simulated sea mud solution10.1016/j.engfailanal.2019.02.009 ↗
23. Effect of cold work and slow strain rate on 321SS stress corrosion cracking in abnormal conditions of simulated PWR primary environment
24. Corrosion of metals and alloys-Removal of corrosion products from corrosion test specimens, (2015).
25. Effect of machining on stress corrosion crack initiation in warm-forged type 304L stainless steel in high temperature water10.1016/j.actamat.2018.11.046 ↗
26. Effect of temperature on the stacking fault energy and deformation behaviour in 316L austenitic stainless steel10.1016/j.msea.2019.05.079 ↗
27. Intergranular corrosion behavior associated with delta-ferrite transformation of Ti-modified Super304H austenitic stainless steel10.1016/j.corsci.2014.10.031 ↗
28. Effects of thermal aging on the stress corrosion cracking behavior of cast stainless steel with different δ-ferrite levels in high temperature water environment10.1016/j.jnucmat.2022.153900 ↗
29. An electrochemical study on the effect of stabilization and sensitization heat treatments on the intergranular corrosion behaviour of AISI 321H austenitic stainless steel10.1016/j.corsci.2018.03.043 ↗
30. Predictive approaches to stress corrosion cracking failure10.1016/0010-938X(80)90128-6 ↗
31. Characteristics of hydrogen embrittlement in high-pH stress corrosion cracking of X100 pipeline steel in carbonate/ bicarbonate solution10.1016/j.conbuildmat.2020.120124 ↗
32. Hydrogen effects on passivation and SCC of 2205 DSS in acidified simulated seawater10.1016/j.corsci.2022.110640 ↗
33. The role of hydrogen in the corrosion and cracking of steels - a review10.1016/j.corcom.2021.10.005 ↗
34. The analysis of electrode impedances complicated by the presence of a constant phase element10.1016/S0022-0728(84)80324-1 ↗
35. Constant-phase-element behavior caused by resistivity distributions in films10.1149/1.3499565 ↗
36. Corrosion evolution and stress corrosion cracking behavior of a low carbon bainite steel in the marine environments: effect of the marine zones10.1016/j.corsci.2022.110490 ↗
37. Evolution of dissolution processes at the interface of carbon steel corroding in a CO2 environment studied by EIS10.1016/j.corsci.2009.10.007 ↗
38. Effects of testing parameters on the susceptibility to hydrogen embrittlement in precipitation-hardened nickel-based alloys: The role of continuous straining10.1016/j.corsci.2022.110171 ↗
39. Consequences of mobile and trapped hydrogen on the dissolution kinetics and pitting processes of an austenitic stainless steel10.1016/j.corsci.2022.110546 ↗
40. In-situ electrochemical impedance spectroscopy investigations on the early stage corrosion behavior of Zircaloy-4 in high-temperature lithiated water10.1016/j.corsci.2020.109223 ↗
41. Passivity of iron surface in curing cement paste environment investigated by electrochemical impedance spectroscopy and surface characterization techniques, Surf
42. Hydrogen-facilitated anodic dissolution of austenitic stainless steels10.5006/1.3284854 ↗
43. The mechanism of hydrogen-facilitated anodic-dissolution-type stress corrosion cracking: theories and experiments10.1080/01418610108216638 ↗
44. Effect of negative half-wave alternating current on stress corrosion cracking behavior and mechanism of X80 pipeline steel in near-neutral solution10.1016/j.conbuildmat.2017.07.076 ↗
45. Effect of B addition on the microstructure and corrosion resistance of S31254 super austenitic stainless steels after solid solution treatment10.1016/j.matlet.2019.05.107 ↗
46. Influence of sensitization on passive films in AISI 2205 duplex stainless steel10.1016/j.jallcom.2015.10.246 ↗
47. Near boundary gradient zone and sensitization control in austenitic stainless steel10.1016/j.corsci.2015.08.027 ↗
48. Performance of different microstructure on electrochemical behaviors of laser solid formed Ti–6Al–4V alloy in NaCl solution10.1016/j.corsci.2021.109392 ↗
49. Development of gradient microstructure in mild steel and grain size dependence of its electrochemical response10.1016/j.corsci.2018.04.009 ↗
50. Effect of annealing treatment on microstructure, mechanical property and anti-corrosion behavior of X2CrNi12 ferritic stainless steel10.1016/j.jmrt.2022.02.117 ↗
51. Temperature change induce crack mode transition of 316L stainless steel in H2S environment revealed by dislocation configurations10.1016/j.corsci.2021.109896 ↗
52. Hydrogen-assisted decohesion and localized plasticity in dual-phase steel10.1016/j.actamat.2014.01.048 ↗
53. Hydrogen-associated decohesion and localized plasticity in a high-Mn and high-Al two-phase lightweight steel10.1016/j.actamat.2022.118296 ↗
54. Stability, validity, and sensitivity to input parameters of the slip-dissolution model for stress-corrosion cracking10.1016/j.corsci.2007.05.001 ↗
55. Effect of plastic deformation on the electrochemical and stress corrosion cracking behavior of X70 steel in near-neutral pH environment10.1016/j.msea.2016.09.033 ↗
56. Study of the corrosion behaviour of sensitized 904L austenitic stainless steel in Cl- solution10.1016/j.corsci.2020.109234 ↗
57. Studies on the degree of sensitization of hyper-duplex stainless steel 2707 at 900℃ using a modified DL-EPR test10.1016/j.corsci.2021.109432 ↗
58. Combined effects of prior plastic deformation and sensitization on hydrogen embrittlement of 304 austenitic stainless steel10.1016/j.ijhydene.2019.01.122 ↗
59. Influence of pre-deformation, sensitization and oxidation in high temperature water on corrosion resistance of AISI 304 stainless steel10.1016/j.nucengdes.2016.09.004 ↗
60. Effect of strain-induced martensite on hydrogen embrittlement of austenitic stainless steels investigated by combined tension and hydrogen release methods10.1016/j.ijhydene.2013.01.198 ↗
61. Effect of solution annealing temperature on the localised corrosion behaviour of a modified super austenitic steel produced in an open-air atmosphere10.1016/j.matchemphys.2023.127498 ↗
62. Simultaneously enhanced strength-ductility synergy and corrosion resistance in liquid-solid bonded stainless steel cladding carbon steel plate by hot rolling and annealing treatment10.1016/j.msea.2023.144928 ↗