journal article·2020-04

Unlocking the impurity-induced pipeline corrosion based on phase behavior of impure CO2 streams

Chong Sun, Jianbo Sun, Jing-Li Luo

Corrosion Science· Volume 165
Publisher page

Abstract

Abstract This study explored the phase behavior of impure CO2 streams and further unmasked its effects on pipeline corrosion by combing thermodynamic calculation and corrosion test. Thermodynamically, H2S impurity promotes water precipitation via reducing the H2O solubility in CO2. H2S-induced phase distribution changes point to the root cause of H2S-enhanced corrosion. To mitigate the above effects from impure CO2 streams on pipeline steel, we prepared an amorphous Ni–P coating on steel and found that the formation of protective film endows the coating with good corrosion resistance. Hence, more than 80 % of corrosion effects and the localized corrosion are effectively prevented.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · High-Temperature Coating Behaviors · Hydrogen embrittlement and corrosion behaviors in metals

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (54)

Show source-provided references
1. Modern global climate change10.1126/science.1090228 ↗
2. Effective use of an idle carbon-deposited catalyst for energy storage applications10.1039/C6TA05082D ↗
3. An overview of current status of carbon dioxide capture and storage technologies10.1016/j.rser.2014.07.093 ↗
4. Dynamis CO2 quality recommendations10.1016/j.ijggc.2008.04.006 ↗
5. State-of-the-art overview of pipeline steel corrosion in impure dense CO2 for CCS transportation: mechanisms and models10.1080/1478422X.2017.1304690 ↗
6. Predicting possible effects of H2S impurity on CO2 transportation and geological storage10.1021/es301292n ↗
7. Electrochemical behaviour of martensitic stainless steel after immersion in a H2S-saturated solution10.1016/j.corsci.2017.10.015 ↗
8. Internal corrosion of carbon steel pipelines for dense-phase CO2 transport in carbon capture and storage (CCS) – a review10.1080/09506608.2016.1176306 ↗
9. Effect of H2S on the corrosion behavior of pipeline steels in supercritical and liquid CO2 environments10.5006/2026 ↗
10. Corrosion of low alloy steel and stainless steel in supercritical CO2/H2O/H2S systems10.1016/j.corsci.2016.06.003 ↗
11. The effect of O2 content on the corrosion behaviour of X65 and 5Cr in water-containing supercritical CO2 environments10.1016/j.apsusc.2015.08.116 ↗
12. Effect of O2 and H2S impurities on the corrosion behavior of X65 steel in water-saturated supercritical CO2 system10.1016/j.corsci.2016.02.017 ↗
13. Effect of impurities on the corrosion behavior of CO2 transmission pipeline steel in supercritical CO2–water environments10.1021/es102578c ↗
14. Assessment of general and localized corrosion behavior of X65 and 13Cr steels in water-saturated supercritical CO2 environments with SO2/O210.1016/j.ijggc.2017.07.012 ↗
15. Effect of small amount of H2S on the corrosion behavior of carbon steel in the dynamic supercritical CO2 environments10.1016/j.corsci.2015.11.009 ↗
16. Dugstad · 2014
17. Corrosion in supercritical CO2 by diffusion of flue gas acids and water10.1016/j.supflu.2012.04.015 ↗
18. Assessing the corrosion product scale formation characteristics of X80 steel in supercritical CO2–H2O binary systems with flue gas and NaCl impurities relevant to CCUS technology10.1016/j.supflu.2019.01.009 ↗
19. Effects of O2 and SO2 on water chemistry characteristics and corrosion behavior of X70 pipeline steel in supercritical CO2 transport system10.1021/acs.iecr.7b04870 ↗
20. State of the aqueous phase in liquid and supercritical CO2 as relevant to CCS pipelines10.1016/j.ijggc.2011.12.008 ↗
21. Impact of SO2 concentration on the corrosion rate of X70 steel an iron in water-saturated supercritical CO2 mixed with SO210.1016/j.supflu.2011.06.007 ↗
22. Effect of SO2 and NO2 on corrosion and solid formation in dense phase CO2 pipelines10.1016/j.egypro.2013.06.173 ↗
23. The upper limit of moisture content for supercritical CO2 pipeline transport10.1016/j.supflu.2012.03.006 ↗
24. Investigating the effect of water content in supercritical CO2 as relevant to the corrosion of carbon capture and storage pipelines10.5006/0944 ↗
25. The influence of SO2 on the tolerable water content to avoid pipeline corrosion during the transportation of supercritical CO210.1016/j.ijggc.2015.03.031 ↗
26. Effect of water content on the corrosion behavior of X65 pipeline steel in supercritical CO2–H2O–O2–H2S–SO2 environment as relevant to CCS application10.1016/j.corsci.2018.03.041 ↗
27. Inhibition of N80 steel corrosion in impure supercritical CO2 and CO2-saturated aqueous phases by using imino inhibitors10.1016/j.ijggc.2017.05.010 ↗
28. A review of the protection strategies against internal corrosion for the safe transport of supercritical CO2 via steel pipelines for CCS purposes10.1016/j.ijggc.2014.08.010 ↗
29. Hua · 2016
30. Corrosion behavior of various steels in a continuous flow of carbon dioxide containing impurities10.1016/j.ijggc.2012.03.005 ↗
31. Cross impact of CO2 phase and impurities on the corrosion behavior for stainless steel and carbon steel in water-containing dense CO2 environments10.1016/j.ijggc.2018.02.011 ↗
32. Yevtushenko · 2013
33. EIS as a means of evaluating electroless nickel deposits10.1016/0013-4686(93)80345-Z ↗
34. Electrochemical corrosion behavior of electroless Ni–P coating in NaCl and H2SO4 solutions10.1002/maco.200905575 ↗
35. Effect of defect on corrosion behavior of electroless Ni–P coating in CO2-saturated NaCl solution10.1016/j.corsci.2018.01.041 ↗
36. Characterization and corrosion behavior of electroless Ni–P/nano-SiC coating inside the CO2 containing media in the presence of acetic acid10.1016/j.matdes.2010.07.030 ↗
37. The corrosion behavior of electroless Ni–P coating in Cl–/H2S environment10.1016/j.apsusc.2012.05.094 ↗
38. Unraveling the effects of CO2 and H2S on the corrosion behavior of electroless Ni–P coating in CO2/H2S/Cl– environments at high temperature and high pressure10.1016/j.corsci.2018.12.022 ↗
39. Key issues related to modelling of internal corrosion of oil and gas pipelines – a review10.1016/j.corsci.2007.06.006 ↗
40. Marcus · 2012
41. An XPS investigation into the passivity of an amorphous Ni–20P alloy10.1149/1.2095880 ↗
42. Calculation of effective penetration depth in X-ray diffraction for pharmaceutical solids10.1002/jps.22202 ↗
43. Formation of iron oxide and iron sulfide at high temperature and their effects on corrosion10.1016/j.corsci.2018.02.045 ↗
44. Smith · 2002
45. Onsite substitution synthesis of ultrathin Ni nanofilms loading ultrafine Pt nanoparticles for hydrogen evolution10.1021/acsami.5b07472 ↗
46. Cliff-like NiO/Ni3S2 directly grown on Ni Foam for battery-type electrode with high area capacity and long cycle stability10.1016/j.electacta.2017.08.102 ↗
47. Synthesizing amorphous Ni–P micro-/nano-composites with perfect roundness or embryo-like structures10.1016/j.apt.2017.09.025 ↗
48. Insights into the interfacial process in electroless Ni–P coating on supercritical CO2 transport pipeline as relevant to carbon capture and storage10.1021/acsami.9b03623 ↗
49. Auger parameters for sulfur-containing compounds using a mixed aluminum-silver excitation source10.1016/0368-2048(90)87059-W ↗
50. Dissolution and passivation of nickel. An X-ray photoelectron spectroscopic study10.1039/f19777300327 ↗
51. Effect of CO2 and H2S on the composition and stability of passive film on iron alloys in geothermal water10.1016/j.electacta.2007.01.086 ↗
52. The effect of H2S on the performance of Ni–YSZ anodes in solid oxide fuel cells10.1016/j.jpowsour.2009.02.001 ↗
53. Effect of alloying elements and microstructure on stability of corrosion product in CO2 and/or H2S environments
54. Crystallisation and phase transformation behaviour of electroless nickel-phosphorus deposits and their engineering properties10.1179/026708402225010010 ↗