Effect of variation in oxygen concentration in static Pb–Bi eutectic on long-term corrosion performance of Al-alloyed austenitic steels at 500 °C

Valentyn Tsisar, Erich Stergar, Serguei Gavrilov, Wouter Van Renterghem, Pierre Louette, Stéphane Lucas

Corrosion Science· Volume 195

Abstract

Aluminium-alloyed austenitic steels Fe-14Cr-2Mn-20Ni-0.5Cu-3Al and Fe-14Cr-5Mn-12Ni-3Cu-2.5Al were tested at 500 °C in static Pb-Bi eutectic for 10,000 h. The concentration of oxygen in the liquid metal was changed in a controlled way over the course of the test from ∼10−6 to ∼10−9 mass% which provided conditions for oxidation and dissolution, respectively. Both steels showed slight oxidation of surface. Steel with higher Ni content revealed also initiation of dissolution corrosion in the view of rare pit-type damages. The structural and compositional features of oxide films, sub-oxide zones and corrosion damages are discussed.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Metallurgical Processes and Thermodynamics · Hydrogen embrittlement and corrosion behaviors in metals

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (46)

Show source-provided references
1. The development of alumina-forming austenitic stainless steels for high-temperature structural use10.1007/s11837-008-0083-2 ↗
2. Overview of strategies for high-temperature creep and oxidation resistance of alumina-forming austenitic stainless steels10.1007/s11661-010-0295-2 ↗
3. Co-optimization of wrought alumina-forming austenitic stainless steel composition ranges for high-temperature creep and oxidation/corrosion resistance10.1016/j.msea.2013.10.014 ↗
4. Development of 1100 °C Capable Alumina-Forming Austenitic Alloys
5. A phenomenological model of embrittlement of metals under conditions of the adsorption action of liquid metal media
6. Handbook on lead-bismuth eutectic alloy and lead properties, materials compatibility, thermal-hydraulics and technologies
7. Selective leaching of nickel and chromium from Type 316 austenitic steel in oxygen-containing lead–bismuth eutectic (LBE)10.1016/j.corsci.2014.03.016 ↗
8. Oxide protection of materials in melts of lead and Bismuth10.1023/A:1011307907891 ↗
9. Structural materials for atomic reactors with liquid metal heat-transfer agents in the form of lead or lead—bismuth alloy10.1007/BF02469876 ↗
10. Influence of temperature on the interaction mode of T91 and AISI 316L steels with Pb–Bi melt saturated by oxygen10.1016/j.corsci.2008.02.006 ↗
11. Transmission electron microscopy (TEM) on oxide layers formed on D9 stainless steel in lead bismuth eutectic (LBE)10.1016/j.corsci.2012.09.019 ↗
12. Transmission electron microscopy study of complex oxide scales on DIN 1.4970 steel exposed to liquid Pb–Bi eutectic10.1016/j.corsci.2018.10.018 ↗
13. Quantification of the Long-Term Performance of Steels T91 and 316L in Oxygen-Containing Flowing Lead-Bismuth Eutectic at 550 °C10.1115/1.4000364 ↗
14. Long-term corrosion of austenitic steels in flowing LBE at 400 °C and 10−7 mass% dissolved oxygen in comparison with 450 and 550 °C10.1016/j.jnucmat.2015.09.027 ↗
15. Long-term service of austenitic steel 1.4571 as a container material for flowing lead–bismuth eutectic10.1016/j.jnucmat.2011.07.026 ↗
16. Corrosion behavior of austenitic steels 1.4970, 316L and 1.4571 in flowing LBE at 450 and 550 °C with 10−7mass% dissolved oxygen10.1016/j.jnucmat.2014.08.024 ↗
17. Long term corrosion on T91 and AISI1 316L steel in flowing lead alloy and corrosion protection barrier development: experiments and models10.1016/j.jnucmat.2011.04.028 ↗
18. Oxidation of Armco-Fe and steels in oxygensaturated liquid lead10.3184/096034007X220034 ↗
19. Silicon-containing ferritic/martensitic steel after exposure to oxygen-containing flowing lead–bismuth eutectic at 450 and 550 °C10.1016/j.jnucmat.2015.11.058 ↗
20. Excellent corrosion resistance of 18Cr–20Ni–5Si steel in liquid Pb–Bi10.1016/j.jnucmat.2003.12.009 ↗
21. Dissolution and oxidation behaviour of various austenitic steels and Ni rich alloys in lead-bismuth eutectic at 520 °C10.1016/j.jnucmat.2015.11.005 ↗
22. Corrosion resistance and microstructural stability of austenitic Fe–Cr–Al–Ni model alloys exposed to oxygen-containing molten lead10.1016/j.jnucmat.2019.06.043 ↗
23. Long term corrosion resistance of alumina forming austenitic stainless steels in liquid lead10.1016/j.jnucmat.2015.03.011 ↗
24. Effect of Oxygen Concentration in Static Pb-Bi Eutectic on Corrosion Mode of Aluminum-Alloyed Austenitic Steels at 550 °C for 1000 h10.4028/www.scientific.net/MSF.1024.79 ↗
25. Aspects of minimizing steel corrosion in liquid lead-alloys by addition of oxygen10.1016/j.nucengdes.2011.09.002 ↗
26. Long-term corrosion performance of T91 ferritic/martensitic steel at 400 °C in flowing Pb-Bi eutectic with 2 × 10−7 mass% dissolved oxygen10.1016/j.corsci.2020.108852 ↗
27. Gas/liquid oxygen-transfer to flowing lead alloys10.1016/j.nucengdes.2010.06.047 ↗
28. Accuracy of potentiometric oxygen sensors with Bi/Bi2O3 reference electrode for use in liquid LBE10.1016/j.jnucmat.2012.06.011 ↗
29. Performance of electrochemical oxygen pump in a liquid lead-bismuth eutectic loop10.1149/2.0711906jes ↗
30. Control of dissolved oxygen in liquid LBE by electrochemical oxygen pumping10.1016/j.snb.2014.07.117 ↗
31. Resolving surface chemical states in XPS analysis of first row transition metals, oxides and hydroxides: Cr, Mn, Fe, Co and Ni10.1016/j.apsusc.2010.10.051 ↗
32. A study of a number of mixed transition metal oxide spinels using X-ray photoelectron spectroscopy10.1016/0169-4332(89)90977-X ↗
33. Nature of oxygen at rocksalt and spinel oxide surfaces10.1116/1.1349194 ↗
34. The mechanism of lacy cover formation in pitting10.1016/S0010-938X(97)00043-7 ↗
35. Pit growth studies in stainless steel foils. I. Introduction and pit growth kinetics10.1016/S0010-938X(01)00133-0 ↗
36. Application of EBSD Methods to Severe Plastic Deformation (SPD) and Related Processing Methods
37. Effects of grain size, cold working, and surface finish on the metal-dusting resistance of steels10.1023/A:1018888321213 ↗
38. Effect of structural state and surface finishing on corrosion behavior of 1.4970 austenitic steel at 400 and 500 °C in flowing Pb–Bi eutectic with dissolved oxygen10.1115/1.4040422 ↗
39. Twin boundary-accelerated ferritization of austenitic stainless steels in liquid lead–bismuth eutectic10.1016/j.scriptamat.2016.02.029 ↗
40. Influence of plastic deformation on dissolution corrosion of 316L austenitic stainless steel in static, oxygen-poor liquid lead-bismuth eutectic at 500 °C10.5006/2400 ↗
41. Corrosion behavior of cold-worked austenitic stainless steels in liquid lead–bismuth eutectic10.1016/j.jnucmat.2014.02.006 ↗
42. Dissolution corrosion of 316L austenitic stainless steels in contact with static liquid lead-bismuth eutectic (LBE) at 500 °C10.1016/j.jnucmat.2017.04.004 ↗
43. Effect of Grain Size on Corrosion: A Review10.5006/1.3462912 ↗
44. Sensitivity of stress corrosion cracking of stainless steel to surface machining and grinding procedure10.1016/j.corsci.2011.06.020 ↗
45. Understanding the effect of surface finish on stress corrosion crack initiation in warm-forged stainless steel 304L in high-temperature water10.1016/j.scriptamat.2019.01.032 ↗
46. Effect of machining-induced surface residual stress on initiation of stress corrosion cracking in 316 austenitic stainless steel10.1016/j.corsci.2016.03.008 ↗