Abstract

The local corrosion behaviour and mechanism of welded joints were studied. The results show that the corrosion was caused by the distribution of microstructure defects in different areas of the weld. In the early stage, the potential difference between the base metal and the heat affected zone was less than 50 mV, so there would be no galvanic effect. As the corrosion progressed, the potential difference increased gradually, and the maximum value exceeded 160 mV. During this period, the corrosion rate was mainly affected by galvanic effect, and the order was weld seam > base metal > heat affected zone.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · Structural Integrity and Reliability Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (57)

Show source-provided references
1. Weatherability of 09CuPCrNi steel in a tropical marine environment10.1016/j.corsci.2009.04.024 ↗
2. Influence of alloyed chromium on the atmospheric corrosion resistance of weathering steels10.1016/j.corsci.2013.05.008 ↗
3. The mechanism of atmospheric rusting and the protective amorphous rust on low alloy steel10.1016/S0010-938X(74)80037-5 ↗
4. Five-year atmospheric corrosion of Cu, Cr and Ni weathering steels in a wide range of environments10.1016/j.corsci.2018.06.039 ↗
5. Initial microzonal corrosion mechanism of inclusions associated with the precipitated (Ti, Nb)N phase of Sb-containing weathering steel10.1016/j.corsci.2019.108232 ↗
6. Atmospheric corrosion behavior of low-alloy steels in a tropical marine environment10.1007/s42243-019-00316-9 ↗
7. Effect of concentrations of Fe2+ and Fe3+ on the corrosion behavior of carbon steel in Cl− and SO42− aqueous environments10.1007/s12540-019-00590-y ↗
8. Correlation between indoor and outdoor corrosion tests for coal train body steel in a coal medium environment10.1007/s42243-022-00758-8 ↗
9. Studies on effects of welding parameters on the mechanical properties of welded low-carbon steel
10. Corrosion behavior of SMA490BW steel and welded joints for high-speed trains in atmospheric environments10.3390/ma12183043 ↗
11. Analysis of the effects of vibration modes on fatigue damage in high-speed train bogie frames10.1016/j.engfailanal.2018.02.025 ↗
12. Effects of cerium on resistance to pitting corrosion of spring steel used in fasteners of high-speed railway10.1002/srin.201300438 ↗
13. Uniaxial behaviour and corrosion-welding-based constitutive model of marine structural steel10.1016/j.oceaneng.2021.109370 ↗
14. Tensile strength assessment of corroded small scale specimens10.1016/j.corsci.2014.04.031 ↗
15. Macrosegregation in dissimilar-metal fusion welding10.1016/j.actamat.2016.03.004 ↗
16. Nature and evolution of the fusion boundary in ferritic-austenitic dissimilar weld metals. Part 1 – Nucleation and growth
17. The galvanic corrosion of welded ultra-high strength steels used for automotive applications10.1016/j.corsci.2018.03.025 ↗
18. Correlation between the microstructure and corrosion behaviour of copper/316 L stainless-steel dissimilar-metal welded joints10.1016/j.corsci.2021.109729 ↗
19. Characterization of microstructure, mechanical properties and corrosion resistance of dissimilar welded joint between 2205 duplex stainless steel and 16MnR10.1016/j.matdes.2010.07.012 ↗
20. Influence of carbon content on corrosion resistance performance of weathering steel10.4028/www.scientific.net/AMR.580.465 ↗
21. Approach for fatigue damage assessment of welded structure considering coupling effect between stress and corrosion10.1016/j.ijfatigue.2016.03.024 ↗
22. Ultimate strength analysis of aged steel-plated structures exposed to marine corrosion damage: a review10.1016/j.corsci.2014.04.043 ↗
23. Microscale investigation of the correlation between microstructure and galvanic corrosion of low alloy steel A508 and its welded 309/308L stainless steel overlayer10.1016/j.corsci.2019.03.027 ↗
24. Micro-electrochemical characterization and Mott–Schottky analysis of corrosion of welded X70 pipeline steel in carbonate/bicarbonate solution10.1016/j.electacta.2009.09.001 ↗
25. The electrochemical study on mechanical and hydrogen embrittlement properties of HAZ part as a function of post-weld heat treatment in SMAW10.1016/S0257-8972(03)00219-6 ↗
26. The influence of electrolyte reduction potential on weld corrosion10.1016/S0013-4686(02)00366-3 ↗
27. The effect of post-weld heat treatment affecting corrosion resistance and hydrogen embrittlement of HAZ part in FCAW10.1016/S0257-8972(03)00060-4 ↗
28. Effect of TIG welding on corrosion behavior of 316L stainless steel10.1016/j.matlet.2006.09.008 ↗
29. A review of stress corrosion cracking of welded stainless steels10.4236/oalib.1104568 ↗
30. Influence of Creq/Nieq on pitting corrosion resistance and mechanical properties of UNS S32304 duplex stainless steel welded joints10.1016/j.corsci.2013.01.037 ↗
31. Thermal cycle simulation of welding process in low carbon steel10.1016/j.msea.2011.09.073 ↗
32. Welding thermal simulation and metallurgical characteristics analysis in WAAM for 5CrNiMo hot forging die remanufacturing10.1016/j.proeng.2017.10.982 ↗
33. Effect of weld thermal cycle on microstructure and fracture toughness of simulated heat-affected zone for a 800MPa grade high strength low alloy steel10.1016/j.jmatprotec.2007.12.049 ↗
34. Galvanic corrosion behavior of microwave welded and post-weld heat-treated inconel-718 joints10.1007/s11665-017-2665-z ↗
35. Galvanic corrosion of laser weldments of AA6061 aluminium alloy10.1016/j.corsci.2007.04.010 ↗
36. Galvanic corrosion of a welded joint in 3Cr low alloy pipeline steel10.1016/j.corsci.2016.05.032 ↗
37. Laser-arc hybrid welding of thick HSLA steel10.1016/j.jmatprotec.2018.04.019 ↗
38. Microstructural aspects of TIG and A-TIG welding process of dissimilar steel grades and correlation to mechanical behavior10.1007/s12666-016-0836-5 ↗
39. Fracture behavior of heat-affected zone in low alloy steels10.1016/S0022-3115(01)00688-2 ↗
40. Effect of Nb on the hydrogen-induced cracking of high-strength low-alloy steel10.1016/j.corsci.2018.04.041 ↗
41. Correlation of surface Volta potential with galvanic corrosion initiation sites in solid-state welded Ti-Cu bimetal using AFM-SKPFM10.1016/j.corsci.2018.06.026 ↗
42. Investigating accuracy of the Tafel extrapolation method in HCl solutions10.1016/j.corsci.2009.03.001 ↗
43. Influence of cold working on the pitting corrosion resistance of stainless steels10.1016/j.corsci.2006.08.021 ↗
44. Interface control for resistance to intergranular cracking10.1016/0921-5093(94)90995-4 ↗
45. Local additional potential model for effect of strain rate on SCC of pipeline steel in an acidic soil solution10.1016/j.corsci.2009.08.019 ↗
46. Sustained effect of remaining cementite on the corrosion behavior of ferrite-pearlite steel under the simulated bottom plate environment of cargo oil tank10.1016/j.corsci.2016.04.042 ↗
47. Sulphuric acid corrosion of ultrafine-grained mild steel processed by equal-channel angular pressing10.1016/j.corsci.2013.06.028 ↗
48. Mechanism of MnS-mediated pit initiation and propagation in carbon steel in an anaerobic sulfidogenic media10.1016/j.corsci.2013.06.049 ↗
49. The effect of microstructure and non-metallic inclusions on corrosion behavior of low carbon steel in chloride containing solutions10.1016/j.corsci.2013.11.038 ↗
50. Cao · 2008
51. Li · 2017
52. Crystallization of FeOOH via iron salts: an anion-chemoaffinity controlled hydrolysis toward high performance inorganic pseudocapacitor materials10.1039/C4CE02543A ↗
53. Corrosion behavior of extrusion, under-aged, peaked-aged and over-aged WE93 alloys in NaHSO3 solutions10.1016/S1002-0721(14)60199-X ↗
54. pH microelectrodes for use near corroding metal surfaces10.5006/0010-9312-19.5.165 ↗
55. Influence of Fe-Rich intermetallic inclusions on Pit initiation on aluminum alloys in aerated NaCl10.1149/1.1391637 ↗
56. Review of literature on pitting corrosion published since 196010.5006/0010-9312-27.6.223 ↗
57. Effect of iron-containing intermetallic particles on the corrosion behaviour of aluminium10.1016/j.corsci.2006.01.005 ↗