Study on the roles of bisulfite in the stress corrosion cracking of 7050-T7451 aluminum alloy in the thin electrolyte layer environment

Mingtao Wang, Liwei Wang, Wendi Yang, Yuxi Liu, Herman Terryn, Zhongyu Cui

Corrosion Science· Volume 215

Abstract

Effect of bisulfite (HSO 3 - ) on the stress corrosion cracking (SCC) behavior of 7050-T7451 aluminum alloy in the thin electrolyte layer environment in the presence of Cl - is investigated. Addition of HSO 3 - inhibits the corrosion initiation but promotes the corrosion propagation and hydrogen uptake. With a quantitative calculation, the HSO 3 - is demonstrated to significantly facilitate the synergistic effect between stress, corrosion, and hydrogen during the in-situ tensile test , resulting in the change of the SCC controlling step from corrosion-induced hydrogen to mechanical-electrochemical-hydrogen interactions. The buffer effect of HSO 3 - plays a dominant role in the HSO 3 - -induced acceleration of the SCC degradation.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (54)

Show source-provided references
1. How aluminum changed the world: a metallurgical revolution through technological and cultural perspectives10.1016/j.techfore.2019.03.011 ↗
2. Enhancing the stress corrosion cracking resistance of a low-Cu containing Al-Zn-Mg-Cu aluminum alloy by step-quench and aging heat treatment10.1016/j.corsci.2019.108184 ↗
3. Hydrogen - dislocation interactions in a low-copper 7xxx aluminium alloy: About the analysis of interrupted stress corrosion cracking tests10.1016/j.msea.2020.139654 ↗
4. Stress corrosion cracking in Al-Zn-Mg-Cu aluminum alloys in saline environments10.1007/s11661-012-1528-3 ↗
5. Review on modelling of corrosion under droplet electrolyte for predicting atmospheric corrosion rate10.1016/j.jmst.2020.04.061 ↗
6. Influence of environmental factors on atmospheric corrosion in dynamic environment10.1016/j.corsci.2018.03.042 ↗
7. Study on influence of native oxide and corrosion products on atmospheric corrosion of pure Al10.1016/j.corsci.2013.11.027 ↗
8. Five-year atmospheric corrosion of Cu, Cr and Ni weathering steels in a wide range of environments10.1016/j.corsci.2018.06.039 ↗
9. Experimental and theoretical studies of corrosion-induced mechanical properties degradation of aircraft 2024 aluminum alloy10.1016/j.msea.2008.08.024 ↗
10. The initiation and propagation of chloride-induced transgranular stress-corrosion cracking (TGSCC) of 304L austenitic stainless steel under atmospheric conditions10.1016/j.corsci.2014.07.017 ↗
11. Atmospheric corrosion of aluminium alloy 2024-T3 exposed to salt lake environment in Western China10.1016/j.corsci.2012.02.015 ↗
12. On the atmospheric corrosion of metals which are covered with thin electrolyte layers—I. Verification of the experimental technique10.1016/0010-938X(90)90032-Z ↗
13. A study of the corrosion of aluminum alloy 2024-T3 under thin electrolyte layers10.1016/j.corsci.2003.10.005 ↗
14. Dependence of the corrosion behavior of aluminum alloy 7075 on the thin electrolyte layers10.1016/j.mseb.2009.01.003 ↗
15. Mechanistic Studies of Intergranular Stress Corrosion Cracking in Al-Mg Alloys under Atmospheric Exposure Conditions10.5006/2853 ↗
16. Fundamental investigation of stress corrosion cracking of E690 steel in simulated marine thin electrolyte layer10.1016/j.corsci.2018.12.029 ↗
17. Quantitative study of the corrosion evolution and stress corrosion cracking of high strength aluminum alloys in solution and thin electrolyte layer containing Cl-10.1016/j.corsci.2020.109076 ↗
18. Comparative study of the stress corrosion behavior of a multiuse bainite steel in the simulated tropical marine atmosphere and seawater environments10.1016/j.conbuildmat.2019.117903 ↗
19. Stress corrosion cracking behavior and mechanism of Fe-Mn-Al-C-Ni high specific strength steel in the marine atmospheric environment10.1016/j.corsci.2021.109760 ↗
20. Influence of ppb levels of SO2 on the atmospheric corrosion of aluminum in the presence of NaCl10.1149/1.2008977 ↗
21. Stress corrosion cracking behavior of rusted X100 steel under the combined action of Cl− and HSO3− in a wet–dry cycle environment10.1016/j.corsci.2019.108382 ↗
22. Long-term corrosion behavior of the 7A85 aluminum alloy in an industrial-marine atmospheric environment10.1016/j.jmrt.2021.03.085 ↗
23. Galvanic corrosion of the anodized 7050 aluminum alloy coupled with the low hydrogen embrittlement CdTi plated 300M steel in an industrial-marine atmospheric environment10.1016/j.surfcoat.2019.125171 ↗
24. Effect of coastal atmospheric corrosion on fatigue properties of 2024-T4 aluminum alloy structures10.1016/j.jallcom.2019.06.235 ↗
25. Studies of long-term weathering of aluminium in the atmosphere10.1016/j.corsci.2007.01.006 ↗
26. Stochastic theory of pitting corrosion10.5006/0010-9312-33.7.243 ↗
27. Corrosion behavior of AZ31 magnesium alloy in the chloride solution containing ammonium nitrate10.1016/j.electacta.2018.05.059 ↗
28. Damage and fracture prediction of 7075 high-strength aluminum alloy during cryogenic stamping process10.1016/j.mechmat.2021.104080 ↗
29. Fractographic features of technically pure magnesium, AZ31 and ZK60 alloys subjected to stress corrosion cracking10.1016/j.msea.2019.138744 ↗
30. M.J.N. Pourbaix, Atlas of Electrochemical Equilibria in Aqueous Solutions, 1974.10.1007/978-1-4684-1806-4_4 ↗
31. The electrochemical oxidation of aqueous sulfur dioxide: A critical review of work with respect to the hybrid sulfur cycle10.1016/j.electacta.2009.09.067 ↗
32. On the role of pre-exposure time and corrosion products in stress-corrosion cracking of ZK60 and AZ31 magnesium alloys10.1016/j.msea.2021.140876 ↗
33. Synergy of corrosion-induced micro-cracking and hydrogen embrittlement on the structural integrity of aluminium alloy (Al-Cu-Mg) 202410.1016/j.corsci.2017.03.001 ↗
34. Corrosion-induced hydrogen embrittlement in aluminum alloy 202410.1016/j.corsci.2005.05.015 ↗
35. Electrochemical conditions for environment-assisted cracking of 6061 Al alloy10.1016/j.corsci.2004.10.011 ↗
36. Slow strain rate tests coupled with hydrogen permeation: New possibilities to assess the role of hydrogen in stress corrosion cracking tests part I: Methodology and commissioning results10.1016/j.corsci.2019.02.028 ↗
37. Effect of tensile stress on the hydrogen adsorption of X70 pipeline steel10.1016/j.ijhydene.2022.04.266 ↗
38. The effect of a constant tensile load on the hydrogen diffusivity in dual phase steel by electrochemical permeation experiments10.1016/j.msea.2019.138872 ↗
39. Influence of the plastic strain on the hydrogen evolution reaction on polycrystalline nickel electrodes in H2S0410.1016/j.electacta.2006.01.012 ↗
40. Effect of plastic deformation on the electrochemical and stress corrosion cracking behavior of X70 steel in near-neutral pH environment10.1016/j.msea.2016.09.033 ↗
41. Influence of tensile straining on the permeation of hydrogen in low alloy Cr–Mo steels10.1016/j.corsci.2005.01.007 ↗
42. Effect of pre-deformation on the pre-corrosion multiaxial fatigue behaviors of 2024-T4 aluminum alloy10.1016/j.ijfatigue.2017.11.008 ↗
43. Hydrogen embrittlement of API 5L X65 pipeline steel in CO2 containing low H2S concentration environment10.1016/j.engfailanal.2020.105081 ↗
44. Correlation between stress corrosion cracking resistance and grain-boundary precipitates of a new generation high Zn-containing 7056 aluminum alloy by non-isothermal aging and re-aging heat treatment10.1016/j.jallcom.2020.156717 ↗
45. The effect of pitting on fatigue lives of peak-aged and overaged 7075 aluminum alloys10.1007/s11661-010-0395-z ↗
46. Grain boundary segregation and hydrogen-induced fracture in 7050 aluminium alloy10.1016/1359-6454(95)00406-8 ↗
47. About the role of the hydrogen during stress corrosion cracking of a low-copper Al-Zn-Mg alloy10.1016/j.jallcom.2021.163391 ↗
48. Cleavage cracking of ductile-metal substrates induced by brittle coating fracture10.1016/j.actamat.2018.04.017 ↗
49. The contribution of hydrogen to the corrosion of 2024 aluminium alloy exposed to thermal and environmental cycling in chloride media10.1016/j.corsci.2012.12.005 ↗
50. Intergranular corrosion of 2024 alloy in chloride solutions10.1149/1.2778224 ↗
51. Hydrogen evolution in aqueous solutions containing dissolved CO2: Quantitative contribution of the buffering effect10.1016/j.corsci.2007.12.007 ↗
52. Influence of ammonium sulfate on the corrosion behavior of AZ31 magnesium alloy in chloride environment10.1016/j.jma.2021.02.004 ↗
53. Hydrogen embrittlement of high strength pipeline steels10.1016/j.corsci.2006.02.011 ↗
54. Corrosion evolution and stress corrosion cracking behavior of a low carbon bainite steel in the marine environments: Effect of the marine zones10.1016/j.corsci.2022.110490 ↗