Corrosion behavior of a dual-phase FeNiCrCuAl high entropy alloy in supercritical water
Source abstract
Abstract
High-entropy alloys (HEAs) possess excellent irradiation resistance, however, their corrosion behavior in high temperature water requires further study. The corrosion behavior of a dual-phase FeNiCrCuAl HEA in supercritical water was investigated in this study. The oxidation kinetics follows a parabolic law. An outer FeAl 2O 4 layer and inner FeCr 2O 4 layer formed on the FeCr-rich BCC regions after 100 h of exposure. With an increase in the exposure period, the outer and inner layers gradually transformed into γ-Al 2O 3 and CrAl 2O 4, respectively. An outer γ-Al 2O 3 layer and inner NiAl 2O 4 layer formed on the NiAl-rich BCC regions regardless of the exposure period. Irregular Cu 2O particles were deposited on the samples owing to the localized corrosion of the Cu-rich FCC regions.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · High Entropy Alloys Studies · Subcritical and Supercritical Water Processes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (59)
Show source-provided references
1. Corrosion and stress corrosion cracking in supercritical water10.1016/j.jnucmat.2007.05.017 ↗
2. Oxidation behavior of 9Cr-4.5Al ODS steel in 600 °C supercritical water and the effect of pre-oxidation10.1016/j.corsci.2019.108380 ↗
3. Corrosion behavior of an Al added high-Cr ODS steel in supercritical water at 600 °C10.1016/j.apsusc.2019.03.019 ↗
4. Corrosion of alumina-forming austenitic steel Fe–20Ni–14Cr–3Al–0.6Nb–0.1Ti in supercritical water10.1016/j.jnucmat.2010.01.025 ↗
5. Oxidation of 9Cr oxide dispersion strengthened steel exposed in supercritical water10.1016/j.jnucmat.2007.05.018 ↗
6. High-temperature corrosion of Fe-Ni-based alloy HR6W, Ni-based alloys Haynes 282 and Inconel 740 in supercritical water at 450 °C and 25 MPa10.1016/j.jallcom.2021.160350 ↗
7. Corrosion characteristics and mechanisms of typical Ni-based corrosion-resistant alloys in sub- and supercritical water10.1016/j.supflu.2020.105138 ↗
8. Oxidation of ferritic and ferritic–martensitic steels in flowing and static supercritical water10.1016/j.corsci.2015.10.017 ↗
9. Effects of exposure temperature and time on corrosion behavior of a ferritic–martensitic steel P92 in aerated supercritical water10.1016/j.corsci.2014.10.022 ↗
10. Corrosion of austenitic alloys in supercritical water10.5006/1.3278237 ↗
11. Effect of exposure temperature on the corrosion behaviors of TP347H austenitic stainless steel in supercritical water10.1016/j.corsci.2019.108188 ↗
12. Nanostructured high-entropy alloys with multiple principal elements: novel alloy design concepts and outcomes10.1002/adem.200300567 ↗
13. Corrosion resistance of weight reduced AlxCrFeMoV high entropy alloys10.1016/j.apsusc.2019.03.173 ↗
14. Passivation of a corrosion resistant high entropy alloy in non-oxidizing sulfate solutions10.1016/j.actamat.2018.10.026 ↗
15. High-pressure torsion driven mechanical alloying of CoCrFeMnNi high entropy alloy10.1016/j.scriptamat.2018.08.031 ↗
16. Microstructural origins of high strength and high ductility in an AlCoCrFeNi2.1 eutectic high-entropy alloy10.1016/j.actamat.2017.07.041 ↗
17. On the enhanced wear resistance of CoCrFeMnNi high entropy alloy at intermediate temperature10.1016/j.scriptamat.2020.05.053 ↗
18. Effects of compositional complexity on the ion-irradiation induced swelling and hardening in Ni-containing equiatomic alloys10.1016/j.scriptamat.2016.03.030 ↗
19. Microstructural stability and mechanical behavior of FeNiMnCr high entropy alloy under ion irradiation10.1016/j.actamat.2016.05.007 ↗
20. Oxidation behavior of high-entropy alloys AlxCoCrFeNi (x=0.15, 0.4) in supercritical water and comparison with HR3C steel10.1016/S1003-6326(15)63733-5 ↗
21. Oxidation behavior of Al0.2CoCrFeNi high-entropy alloy film in supercritical water environment
22. A novel low-activation VCrFeTaxWx (x = 0.1, 0.2, 0.3, 0.4, and 1) high-entropy alloys with excellent heat-softening resistance10.3390/e20120951 ↗
23. Probing the phase transformation and dislocation evolution in dual-phase high-entropy alloys10.1016/j.ijplas.2018.10.014 ↗
24. Microstructure investigations of Fe50Mn30Co10Cr10 dual–phase high–entropy alloy under Fe ions irradiation10.1016/j.jnucmat.2021.153006 ↗
25. Probing the phase transformation and dislocation evolution in dual-phase high-entropy alloys10.1016/j.ijplas.2018.10.014 ↗
26. In situ lift-out using a FIB-SEM system10.1016/j.micron.2004.03.002 ↗
27. Microstructures and corrosion resistance properties of as-cast and homogenized AlFeNiCuCr high entropy alloy10.1016/j.matchemphys.2020.123440 ↗
28. Aluminum alloying effects on lattice types, microstructures, and mechanical behavior of high-entropy alloys systems10.1007/s11837-013-0776-z ↗
29. Corrosion behavior of Ni-base alloys in supercritical water10.5516/NET.2009.41.1.107 ↗
30. Corrosion behavior of austenitic and ferritic steels in supercritical water10.5516/NET.2008.40.2.147 ↗
31. Analyses of oxide films grown on Alloy 625 in oxidizing supercritical water10.1016/j.supflu.2008.07.010 ↗
32. Analyses of oxide films grown on AISI 304L stainless steel and Incoloy 800HT exposed to supercritical water environment10.1016/j.jnucmat.2011.05.007 ↗
33. Effects of Si, Mn on the corrosion behavior of ferritic–martensitic steels in supercritical water (SCW) environments10.1016/j.corsci.2020.108432 ↗
34. In situ oxidation of Cu2O crystal for electrochemical detection of glucose10.3390/s19132926 ↗
35. Raman spectroscopic study of cation disorder in poly- and single crystals of the nickel aluminate spinel10.1088/0953-8984/19/18/186217 ↗
36. Study of Raman spectra for γ-Al2O3 models by using first-principles method10.1016/j.ssc.2013.09.030 ↗
37. Raman fingerprint of chromate, aluminate and ferrite spinels10.1002/jrs.4764 ↗
38. Characterization of oxide films grown on 316L stainless steel exposed to H2O2-containing supercritical water10.1016/j.supflu.2006.12.020 ↗
39. Corrosion behavior of FeCoNiCrCux high-entropy alloys in 3.5% sodium chloride solution10.1016/j.matchemphys.2005.01.001 ↗
40. Effect of Al and Ti addition on performance of stainless steel 310 in supercritical water10.1179/1743278214Y.0000000225 ↗
41. The oxidation of iron-aluminum alloys10.1007/BF00665045 ↗
42. Solidus, subsolidus, and subdissociation phase equilibria in the system Fe-Al-O10.1111/j.1151-2916.1958.tb13532.x ↗
43. Corrosion mechanisms of candidate structural materials for supercritical water-cooled reactor10.1007/s11708-009-0024-y ↗
44. Corrosion behavior of ferritic–martensitic steel T91 in supercritical water10.1016/j.corsci.2005.08.021 ↗
45. Influence of the dissolved oxygen content on corrosion of the ferritic-martensitic steel P92 in supercritical water10.1016/j.corsci.2011.11.013 ↗
46. Transport processes during the growth of oxide films at elevated temperature10.1103/RevModPhys.57.437 ↗
47. Pourbaix diagrams for chromium, aluminum and titanium extended to high-subcritical and low-supercritical conditions10.1016/j.corsci.2012.02.002 ↗
48. Deposition, characterization and performance evaluation of ceramic coatings on metallic substrates for supercritical water-cooled reactors10.1016/j.surfcoat.2010.12.017 ↗
49. TEM investigation of pre-oxidised Fe–Al with improved aqueous corrosion resistance10.1016/j.corsci.2020.109170 ↗
50. Oxidation processes and involved chemical reactions of corrosion-resistant alloys in supercritical water10.1021/acs.iecr.0c01394 ↗
51. Cyclic oxidation behavior of Ni3Al-0.1B base alloys containing a Ti, Zr, or Hf addition10.1007/BF00655897 ↗
52. TEM studies of oxidized NiAl and Ni3Al cross sections10.1007/BF00666466 ↗
53. Corrosion behavior of alumina-forming and oxide dispersion strengthened austenitic 316 stainless steel in supercritical water10.1016/j.corsci.2018.04.026 ↗
54. Formation mechanism of porous anodic aluminium and titanium oxides10.1002/adma.200800845 ↗
55. Corrosion behavior of CuCrFeNiMn high entropy alloy system in 1 M sulfuric acid solution10.1002/maco.201106072 ↗
56. Effect of alloying ratios and Cu-addition on corrosion behaviour of CoCrFeNiMo high-entropy alloys in superheated steam containing CO2, H2S and HCl10.1016/j.corsci.2020.109083 ↗
57. Pitting characterization of 90/10 cupro-nickel chiller tubes10.1179/cmq.2007.46.4.473 ↗
58. Revised Pourbaix Diagrams for Copper at 25 to 300 °C10.1149/1.1838036 ↗
59. Deposition of nickel on electrodeposited Cu2O films at potentials more positive than the nernst potential of Ni2+/Ni010.1149/2.0751709jes ↗