Effect of processing history on corrosion behaviours of high purity Mg
Source abstract
Abstract
Abstract In this study, the effects of processing history on corrosion behaviours of pure Mg with controlled impurity content, were analysed systematically. Results revealed that impurity Fe and Si were precipitated into the Fe-Si phase by heat treatment prior to extrusion, leading to severe micro-galvanic corrosion of as-extruded pure Mg despite the same impurity contents with as-cast pure Mg. This result suggests that control of the actual tolerance limit, considering not only the impurity content but also the processing history, is required in designing alloys.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (45)
Show source-provided references
1. Review of recent developments in the field of magnesium corrosion10.1002/adem.201400434 ↗
2. Understanding magnesium corrosion—a framework for improved alloy performance10.1002/adem.200310405 ↗
3. Calculated phase diagrams and the corrosion of die-cast Mg–Al alloys10.1016/j.corsci.2008.12.015 ↗
4. Corrosion behaviour of a nominally high purity Mg ingot produced by permanent mould direct chill casting10.1016/j.corsci.2012.04.030 ↗
5. Influence of microstructure on corrosion of As-cast ZE4110.1002/adem.200700246 ↗
6. An innovative specimen configuration for the study of Mg corrosion10.1016/j.corsci.2010.09.016 ↗
7. Corrosion of ultra-high-purity Mg in 3.5% NaCl solution saturated with Mg(OH)210.1016/j.corsci.2013.05.018 ↗
8. Corrosion studies of magnesium and its alloys
9. The anodic dissolution of magnesium in chloride and sulphate solutions10.1016/S0010-938X(97)00090-5 ↗
10. The electrochemical corrosion of pure magnesium in 1 N NaCl10.1016/S0010-938X(96)00172-2 ↗
11. Corrosion behaviour of AZ21, AZ501 and AZ91 in sodium chloride10.1016/S0010-938X(98)00078-X ↗
12. Corrosion behaviour of magnesium/aluminium alloys in 3.5wt.% NaCl10.1016/j.corsci.2007.11.005 ↗
13. An exploratory study of the corrosion of Mg alloys during interrupted salt spray testing10.1016/j.corsci.2009.03.014 ↗
14. Corrosion behavior of equal-channel-angular-pressed pure magnesium in NaCl aqueous solution10.1016/j.corsci.2009.10.004 ↗
15. Electrochemical behaviour and corrosion of Mg–Y alloys10.1016/j.corsci.2011.03.010 ↗
16. Corrosion of high purity Mg, Mg2Zn0.2Mn, ZE41 and AZ91 in Hank’s solution at 37°C10.1016/j.corsci.2011.06.030 ↗
17. Structure, mechanical properties, corrosion behavior and cytotoxicity of biodegradable Mg-X (X=Sn, Ga, In) alloys10.1016/j.msec.2013.02.005 ↗
18. Corrosion behaviour in salt spray and in 3.5% NaCl solution saturated with Mg(OH)2 of as-cast and solution heat-treated binary Mg–x alloys: x=Mn, Sn, Ca, Zn, Al, Zr, Si, Sr10.1016/j.corsci.2013.06.030 ↗
19. Poisoning the corrosion of magnesium10.1016/j.elecom.2013.07.021 ↗
20. Effect of traces of silicon on the formation of Fe-rich particles in pure magnesium and the corrosion susceptibility of magnesium10.1016/j.jallcom.2014.09.040 ↗
21. Characteristics of surface films formed on Mg–Sn alloys in NaCl solution10.1149/2.0161608jes ↗
22. Effect of iron content on the corrosion of pure magnesium: critical factor for iron tolerance limit10.1016/j.corsci.2018.04.024 ↗
23. Effect of Y addition on removal of Fe impurity from magnesium alloys10.1016/j.scriptamat.2018.11.046 ↗
24. The effect of texture on the corrosion behavior of AZ31 Mg alloy10.1007/s11837-012-0341-1 ↗
25. In vitro corrosion and biocompatibility of binary magnesium alloys10.1016/j.biomaterials.2008.10.021 ↗
26. The effect of pre-processing and grain structure on the bio-corrosion and fatigue resistance of magnesium alloy AZ3110.1002/adem.200700200 ↗
27. Influence of hot rolling on the corrosion behavior of several Mg–X alloys10.1016/j.corsci.2014.10.012 ↗
28. Corrosion of hot extrusion AZ91 magnesium alloy: I-relation between the microstructure and corrosion behavior10.1016/j.corsci.2011.02.015 ↗
29. The surface, microstructure and corrosion of magnesium alloy AZ31 sheet10.1016/j.electacta.2010.02.068 ↗
30. Bio-corrosion of a magnesium alloy with different processing histories10.1016/j.matlet.2007.12.052 ↗
31. Corrosion behavior of a friction stir processed rare-earth added magnesium alloy10.1016/j.corsci.2012.01.007 ↗
32. Film breakdown and nano-porous Mg(OH)2Formation from corrosion of magnesium alloys in salt solutions10.1149/2.0171504jes ↗
33. Influence of the β-phase morphology on the corrosion of the Mg alloy AZ9110.1016/j.corsci.2008.04.010 ↗
34. Effect of heat treatment on corrosion and electrochemical behaviour of AZ91D magnesium alloy10.1023/A:1022698916817 ↗
35. Influence of heat treatment on degradation behavior of bio-degradable die-cast AZ63 magnesium alloy in simulated body fluid10.1016/j.msea.2006.12.020 ↗
36. Influence of homogenization annealing of AZ91 on mechanical properties and corrosion behavior10.1002/adem.200700234 ↗
37. Effect of heat treatment on corrosion behaviour of magnesium alloy AZ91D in simulated body fluid10.1016/j.corsci.2009.11.030 ↗
38. Corrosion resistance of aged die cast magnesium alloy AZ91D10.1016/j.msea.2003.08.060 ↗
39. Corrosion of heat treated magnesium alloy ZE4110.1016/j.corsci.2011.06.005 ↗
40. ASTM G1–03 · 2011
41. Kelvin Microprobe Analytics on iron-enriched corroded magnesium surface10.5006/2260 ↗
42. Volta potentials measured by scanning kelvin probe force microscopy as relevant to corrosion of magnesium alloys10.5006/1432 ↗
43. The effect of iron re-deposition on the corrosion of impurity-containing magnesium10.1039/C5CP05577F ↗
44. Experimental and thermodynamic studies of the Fe–Si binary system10.2355/isijinternational.52.540 ↗
45. Critical reassessment of the Fe-Si system10.1016/j.calphad.2016.11.003 ↗