A new Fe-Cr-Mo-B-Al steel with outstanding tribo-corrosion resistance in liquid aluminium

Zicheng Ling, Zhiqiang Fu, Xin Yang, Tiwen Lu, Weiping Chen

Corrosion Science· Volume 206
Publisher page

Abstract

The tribo-corrosion of a metal by liquid aluminium is problematic; thus, a new Fe-Cr-Mo-B-Al steel was constructed, and its tribo-corrosion behaviours in liquid aluminium were investigated. Our results show that this steel displays outstandingtribo-corrosion resistance in liquid aluminium, mainly arising from the coordinated effect of rod-like Cr-rich M 2B (M=Fe, Cr, Mo) borides and irregular blocky Mo-rich M 2 B borides. The interaction between corrosion and wear primarily contributed to the mass loss of this steel via the degradation of the borides coupled with the fracture and spallation of the corrosion products.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloys Composites Properties · Advanced ceramic materials synthesis · Boron and Carbon Nanomaterials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (45)

Show source-provided references
1. Characterisation of oxide films formed on Co–29Cr–6Mo alloy used in die-casting moulds for aluminium10.1016/j.corsci.2013.03.026 ↗
2. Corrosion mechanisms of steel and cast iron by molten aluminum10.1007/s11661-010-0306-3 ↗
3. Die soldering: Mechanism of the interface reaction between molten aluminum alloy and tool steel10.1007/s11663-002-0057-7 ↗
4. Evaluation of soldering, washout and thermal fatigue resistance of advanced metal materials for aluminum die-casting dies10.1016/j.msea.2004.03.020 ↗
5. Investigation of erosive-corrosive wear in the low pressure die casting of aluminum A35610.1016/j.msea.2006.07.052 ↗
6. Wear of metal stirring rods in molten aluminium and suspensions of alumina particles in molten aluminium10.1016/0301-679X(95)00033-Z ↗
7. Interfacial morphology and tribo-corrosion behaviour of Fe-15.3 wt% Cr-3.1 wt% B-6.2 wt% Mo alloy in molten aluminium10.1016/j.wear.2019.04.002 ↗
8. Intermetallic formation and its relation to interface mass loss and tribology in die casting dies10.1016/j.wear.2003.08.001 ↗
9. Corrosion behaviour of a surface-treated AISI H11 hot work tool steel in molten aluminium alloy10.1016/S0257-8972(00)00530-2 ↗
10. Corrosion of CrN and CrN/TiN coated heat-resistant steels in molten A356 aluminum alloy10.1016/S0257-8972(01)01484-0 ↗
11. Degradation behaviour of boronized carbon and high alloy steels in molten aluminium and zinc10.1016/S0167-577X(98)00077-9 ↗
12. Effect of nitriding treatment on corrosion behaviour of Co–Cr–Mo alloy in liquid Al10.1016/j.corsci.2013.10.004 ↗
13. Interaction of iron-nickel alloys with liquid aluminium Part II
14. Interaction of molten aluminum with porous TiB2-based ceramics containing Ti–Fe10.1016/j.jeurceramsoc.2011.10.053 ↗
15. The influence of A Mo addition on the interfacial morphologies and corrosion resistances of novel Fe-Cr-B alloys immersed in molten aluminum
16. Effect of micro alloying elements on the interfacial reactions between molten aluminum alloy and tool steel10.1016/j.jallcom.2008.11.127 ↗
17. Effect of Si on growth kinetics of intermetallic compounds during reaction between solid iron and molten aluminum10.1016/S1003-6326(13)62499-1 ↗
18. Effect of Si on the interaction between die casting die and aluminum alloy10.1016/j.matlet.2004.06.021 ↗
19. Effect of titanium and nitrogen additions on the microstructures and three-body abrasive wear behaviors of Fe–B cast alloys10.1007/s11249-014-0314-3 ↗
20. Corrosion resistance and interfacial morphologies of novel Fe-Cr-Mo-B cast steels in molten aluminum10.1016/j.corsci.2017.05.024 ↗
21. Effect of Fe 2 B orientation on erosion–corrosion behavior of Fe–3.5 wt% B steel in flowing zinc10.1016/j.corsci.2015.05.039 ↗
22. Effect of orientation and lamellar spacing of Fe2B on interfaces and corrosion behavior of Fe-B alloy in hot-dip galvanization10.1016/j.actamat.2016.06.016 ↗
23. Effect of molybdenum on the microstructures of As-cast Fe-B alloys and their corrosion resistance in molten zinc10.5006/2280 ↗
24. Interfacial morphology and corrosion-wear behavior of cast Fe-3.5 wt% B steel in liquid zinc10.1016/j.corsci.2017.12.003 ↗
25. Effect of 0.3 wt.% Al addition in flowing liquid zinc on the erosion-corrosion behavior of Fe-3.5 wt.% B alloy10.1007/s11665-015-1506-1 ↗
26. Interfacial morphologies and erosion–corrosion behavior of directional Fe-3.5 wt.% B steel in flowing liquid Zn containing 0.30 wt.% Al10.1016/j.corsci.2016.07.007 ↗
27. Microstructure and corrosion behavior of cast Fe–B alloys dipped into liquid zinc bath10.1016/j.matchar.2010.05.009 ↗
28. Effect of chromium on microstructure and properties of high boron white cast iron10.1007/s11661-007-9385-1 ↗
29. Effect of improving Fe2B toughness by chromium addition on the two-body abrasive wear behavior of Fe–3.0 wt% B cast alloy10.1016/j.triboint.2016.05.009 ↗
30. Effect of molybdenum and chromium on hardenability of low-carbon boron-added steels10.3365/met.mat.2008.12.667 ↗
31. Influence of Mo and Cr contents on hardenability of low-carbon boron steels10.3740/MRSK.2013.23.10.555 ↗
32. Effect of tungsten addition on the toughness and hardness of Fe2B in wear-resistant Fe–B–C cast alloy10.1016/j.matchar.2012.09.007 ↗
33. Corrosion mechanisms of steel and cast iron by molten aluminum10.1007/s11661-010-0306-3 ↗
34. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
35. Microstructure and crystallography of borides and secondary precipitation in 18 wt.% Cr–4 wt.% Ni–1 wt.% Mo–3.5 wt.% B–0.27 wt.% C steel10.1016/j.actamat.2011.11.004 ↗
36. Mechanisms of phase transformations within the miscibility gap of Fe-rich Fe-Al alloys10.1016/0001-6160(76)90063-8 ↗
37. A step towards designing Fe–Cr–B–C cast alloys10.1016/S0921-5093(00)01808-6 ↗
38. Boron-alloyed Fe–Cr–C–B tool steels—thermodynamic calculations and experimental validation10.1016/j.matdes.2015.08.157 ↗
39. Microstructure and crystallography of borides and mechanical properties of Fe–B–C–Cr–Al alloys10.1016/j.jallcom.2015.11.171 ↗
40. Interfacial morphologies and corrosion behaviours of novel Fe-Cr-B alloys immersed in molten aluminium10.1088/2053-1591/aafeb1 ↗
41. Kinetic interactions between solid iron and molten aluminium10.1016/S0921-5093(03)00469-6 ↗
42. Intermetallic compound layer growth between solid iron and molten aluminium10.1016/S0921-5093(98)00573-5 ↗
43. Crystallography of Fe 2 Al 5 phase at the interface between solid Fe and liquid Al10.1016/j.intermet.2015.07.011 ↗
44. AlFe2xCoxB2(x = 0–0.30):TC tuning through Co substitution for a promising magnetocaloric material realized by spark plasma sintering10.1021/acs.inorgchem.6b01467 ↗
45. Phase stability and weak metallic bonding within ternary‐layered borides CrAlB, Cr2AlB2, Cr3AlB4, and Cr4AlB610.1111/jace.16206 ↗