journal article·2023-06

Improved wet-oxidation resistance of SiCf/SiC composites modified with Y2O3

Junmin Zhang, Xiaowu Chen, Feiyu Guo, Jinshan Yang, Xiangyu Zhang, Yanmei Kan, Jianbao Hu, Yudong Xue, Shaoming Dong

Corrosion Science· Volume 217
Publisher page

Abstract

Y 2O 3 was introduced into the SiC matrix to improving the wet-oxidation resistance of SiC f/SiC composites. The effects of Y 2O 3 on the mechanical properties and the wet-oxidation resistance of the composites were investigated. The results indicate that Y 2O 3 presents little negative effect on the mechanical properties. Besides, the introduction of Y 2O 3 effectively improves the wet-oxidation resistance of SiC f/SiC composites by forming a continuous Y 2Si 2O 7 layer on the surface during the oxidation process. Compared with original SiC f /SiC composites, the strength retention rates of SiC f/SiC-Y 2O 3 composites oxidized for 20 h, 60 h and 100 h at 1400 ℃ respectively increase 5.62%, 17.58% and 23.08%.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. Enhanced mechanical property and tunable dielectric property of SiCf/SiC-SiBCN composites by CVI combined with PIP10.1007/s40145-021-0470-5 ↗
2. Study on microstructures of 2D and 3D chemical vapor infiltration SiC/SiC composites10.1002/adem.201900880 ↗
3. Thermal stability of CVI and MI SiC/SiC composites with Hi-Nicalon (TM)-S fibers10.1016/j.jeurceramsoc.2022.03.009 ↗
4. Effect of heat treatment on the microstructure and mechanical behavior of SiC/SiC mini-composites10.1016/j.msea.2018.12.118 ↗
5. Advances in thermal spray coatings for gas turbines and energy generation: a review10.1007/s11666-013-9904-0 ↗
6. Microstructural evolution mechanism of plain-woven SiC/SiC during thermal ablation10.1016/j.corsci.2022.110679 ↗
7. Single-source-precursor derived SiHfBCN enhancing oxidation resistance of SiC/SiC composites in wet oxygen10.1016/j.corsci.2022.110602 ↗
8. Advanced structural ceramics in aerospace propulsion10.1038/nmat4687 ↗
9. Environmental degradation of high-temperature protective coatings for ceramic-matrix composites in gas-turbine engines10.1038/s41529-019-0075-4 ↗
10. Ceramic matrix composites taking flight at GE aviation
11. SiC recession caused by SiO2 scale volatility under combustion conditions: I, experimental results and empirical model10.1111/j.1151-2916.1999.tb02004.x ↗
12. SiC recession caused by SiO2 scale volatility under combustion conditions: II, thermodynamics and gaseous‐diffusion model10.1111/j.1151-2916.1999.tb02005.x ↗
13. High temperature oxidation behaviors of bulk SiC with low partial pressures of air and water vapor in argon10.1016/j.corsci.2020.108795 ↗
14. Damage development and lifetime prediction of fiber-reinforced ceramic-matrix composites subjected to cyclic loading at 1300 ℃ in vacuum, inert and oxidative atmospheres10.1016/j.ast.2019.01.060 ↗
15. Effect of frequency and environment on fatigue behavior of a CVI SiC/SiC ceramic matrix composite at 1200 degrees C10.1016/j.compscitech.2010.11.008 ↗
16. Accelerated oxidation of SiC CMC's by water vapor and protection via environmental barrier coating approach10.1016/S0955-2219(02)00141-3 ↗
17. Current status of environmental barrier coatings for Si-Based ceramics10.1016/S0257-8972(00)00889-6 ↗
18. Rare earth silicate environmental barrier coatings: present status and prospective10.1016/j.ceramint.2017.01.153 ↗
19. Application of rare earths in advanced ceramic materials10.1016/S1002-0721(07)60489-X ↗
20. High temperature water vapour corrosion of rare earth disilicates (Y, Yb, Lu)2Si2O7 in the presence of Al(OH)3 impurities10.1016/j.jeurceramsoc.2006.09.013 ↗
21. Z. Sun, M. Li, Y.J.Imr Zhou, Recent progress on synthesis, multi-scale structure, and properties of Y–Si–O oxides, 59 (2014) 357–383.10.1179/1743280414Y.0000000033 ↗
22. Effect of heat treatment on the microstructure and strength of yttrium silicate matrix-modified SiCf/SiC composites10.1016/j.jeurceramsoc.2021.09.031 ↗
23. Oxidation behaviour of pressureless liquid-phase-sintered α-SiC with additions of 5Al2O3+ 3RE2O3 (RE= La, Nd, Y, Er, Tm, or Yb)10.1016/j.jeurceramsoc.2010.07.013 ↗
24. Oxidation behavior of liquid‐phase sintered silicon carbide with aluminum nitride and rare‐earth oxides (Re2O3, where Re= Y, Er, Yb)10.1111/j.1151-2916.2002.tb00448.x ↗
25. High-temperature properties of liquid-phase-sintered α-SiC10.1016/S0921-5093(99)00769-8 ↗
26. Influence of rare-earth oxide additives on the oxidation resistance of Si3N4-SiC nanocomposites10.1016/j.jeurceramsoc.2013.01.008 ↗
27. Optimizing microstructure and properties of SiCf/SiC composites prepared by reactive melt infiltration10.15541/jim20210091 ↗
28. Oxidation/corrosion of polymer-derived SiAlCN ceramics in water vapor10.1111/j.1551-2916.2005.00791.x ↗
29. Paralinear oxidation of CVD SiC in water vapor10.1111/j.1151-2916.1997.tb02810.x ↗
30. The effect of oxide volatilization on the oxidation kinetics of Cr and Fe‐Cr alloys10.1149/1.2424115 ↗
31. Thermodynamic calculations and phase stabilities in the Y-Si-C-O system10.1007/s11669-006-9014-5 ↗
32. Thermal properties of single-phase Y2SiO510.1016/j.jeurceramsoc.2008.07.026 ↗
33. Fabrication of Y2Si2O7 coating and its oxidation protection for C/SiC composites10.1016/S1003-6326(17)60044-X ↗
34. Thermal properties and thermal shock resistance of gamma-Y2Si2O710.1111/j.1551-2916.2008.02470.x ↗
35. Effect of sintering temperature on BaO-Al2O3-SiO2 glass ceramic coating for carbon fibre reinforced silicon carbide matrix composites10.1179/174328408X323122 ↗
36. Yttrium silicate coatings for oxidation protection of carbon–silicon carbide composites10.1111/j.1151-2916.2000.tb01392.x ↗
37. Silicon nitride for high-temperature applications10.1111/j.1551-2916.2010.03839.x ↗
38. M. Fritsch, H. Klemm, M. Herrmann, A. Michaelis, B. Schenk, The water vapour hot gas corrosion of ceramic materials, in: CFI. Ceramic forum international, Göller, 2010.
39. Oxidation behavior of pressureless liquid phase sintered SiC
40. Strength improvement of LPS-SiC ceramics by oxidation treatment10.1016/j.ijrmhm.2009.08.004 ↗
41. Oxidation of SI3N4 in range 1300℃ to 1500℃10.1111/j.1151-2916.1976.tb09505.x ↗