journal article·2023-08

Native oxide film powered corrosion protection of underlying Pb-free Sn solder substrate

Chuang Qiao, Qiong Wu, Long Hao, Youzhi Wang, Xu Sun, Qingchuan Zou, Xizhong An

Corrosion Science· Volume 221
Publisher page

Abstract

The development of new Pb-free Sn-based solder alloys in the packaging industry increasingly focuses on corrosion resistance enhancing. In this work, the positive effect by surface native oxide film in postponing the solder substrate degradation has been identified, and besides the corrosion resistance of native oxide film varies greatly on different compositional phases in the substrate. It is suggested that obtaining a corrosion-resistant native oxide film is one promising method in improving the corrosion resistance of solder alloys, and thus small additions of elements, prone to form a passivated native oxide film, are preferentially of interest.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Electronic Packaging and Soldering Technologies · Advanced Welding Techniques Analysis · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (48)

Show source-provided references
1. Electronics without lead10.1126/science.1110168 ↗
2. Development of lead-free interconnection materials in electronic industry during the past decades: structure and properties10.1016/j.matdes.2022.110439 ↗
3. Materials modification of the lead-free solders incorporated with micro/nano-sized particles: A review10.1016/j.matdes.2020.109224 ↗
4. Thermal aging effects on microstructure, elastic property and damping characteristic of a eutectic Sn-3.5Ag solder
5. A critical review on performance, microstructure and corrosion resistance of Pb-free solders10.1016/j.measurement.2018.12.051 ↗
6. Effects of Ni nanoparticles addition on the microstructure, electrical and mechanical properties of Sn-Ag-Cu alloy10.1016/j.mtla.2019.100234 ↗
7. Effects of Cu, Bi, and In on microstructure and tensile properties of Sn-Ag-X (Cu, Bi, In) solders10.1007/s11661-005-0236-7 ↗
8. Effect of nano-particles TiO2 on the microstructures and properties of SnAgCu solders
9. Corrosion behavior of Sn-3.0Ag-0.5Cu alloy under chlorine-containing thin electrolyte layers10.1016/j.corsci.2018.08.041 ↗
10. In-situ EIS study on the initial corrosion evolution behavior of SAC305 solder alloy covered with NaCl
11. Microstructure induced galvanic corrosion evolution of SAC305 solder alloys in simulated marine atmosphere10.1016/j.jmst.2020.03.024 ↗
12. A perspective on effect by Ag addition to corrosion evolution of Pb-free Sn solder10.1016/j.matlet.2021.129935 ↗
13. Progress in corrosion science at atomic and nanometric scales10.1016/j.pmatsci.2018.03.001 ↗
14. Role of cerium in microstructure and corrosion properties of Sn-1.0Ag solder alloys10.1016/j.matlet.2018.06.015 ↗
15. Influence of oxidation on the performance of Zr55Cu30Al10Ni5 BMG10.1016/j.intermet.2016.08.007 ↗
16. Electrochemical corrosion and electrochemical migration characteristics of SAC-1Bi-xMn solder alloys in NaCl solution10.1016/j.corsci.2023.110965 ↗
17. Electrochemical corrosion of SAC alloys: a review10.3390/met10101276 ↗
18. Corrosion behavior of Sn-based lead-free solder alloys: a review
19. High-temperature aging time-induced composition and thickness evolution in the native oxides film on Sn solder substrate
20. Influence of native oxide film age on the passivation of carbon steel in neutral aqueous solutions with a dicarboxylic acid10.1016/j.corsci.2019.03.033 ↗
21. Influence of composition on the morphology of primary Cu6Sn5 in Sn-4Cu alloys10.1007/s11664-012-2222-3 ↗
22. Revealing significant effect of nitrogen on prolonging pitting corrosion lifetime of martensitic stainless steel by modelling approach10.1016/j.corsci.2022.110369 ↗
23. Correlation between corrosion potential and pitting potential for AISI 304L austenitic stainless steel in 3.5% NaCl aqueous solution10.1590/S1516-14392002000100013 ↗
24. The applicability of SnO2 coatings for corrosion protection of metals10.1149/1.1737713 ↗
25. UV-irradiation assisted corrosion protective oxides film on pure Sn solder substrate exposed to atmospheric environment
26. Constant-Phase-Element behavior caused by resistivity distributions in films I10.1149/1.3499564 ↗
27. Constant-phase-element behavior caused by resistivity distributions in films II10.1149/1.3499565 ↗
28. Corrosion behaviour assessment of lead-free Sn–Ag–M (M=In, Bi, Cu) solder alloys10.1016/j.matchemphys.2007.12.006 ↗
29. Orazem · 2008
30. Controlling the corrosion resistance of multi-principal element alloys10.1016/j.scriptamat.2020.06.065 ↗
31. X. Luo, W. Du, X. Lu, T. Yamaguchi, J. Gavin, L.L. Ye, J. Liu, Investigation of accelerated surface oxidation of Sn-3.5Ag-0.5Cu solder particles by TEM and STEM, Int. Symp. Adv. Packaging Mate. 2011, 73–79.10.1109/ISAPM.2011.6105674 ↗
32. Effect of surface oxide on the melting behavior of lead-free solder nanowires and nanorods10.1016/j.apsusc.2012.04.074 ↗
33. Oxidation of Ag-Sn-La alloy powders10.1007/s11085-008-9106-1 ↗
34. Evidence for Ag participating the electrochemical migration of 96.5Sn-3Ag-0.5Cu alloy10.1016/j.corsci.2019.05.004 ↗
35. Effect of Ag3Sn intermetallic compounds on corrosion of Sn-3.0Ag-0.5Cu solder under high-temperature and high-humidity condition10.1016/j.corsci.2012.05.006 ↗
36. Improved accuracy of quantitative XPS analysis using predetermined spectrometer transmission functions with UNIFIT 200410.1002/sia.2056 ↗
37. Resolving surface chemical states in XPS analysis of first row transition metals, oxides and hydroxides: Sc, Ti, V, Cu and Zn10.1016/j.apsusc.2010.07.086 ↗
38. Oxidation behavior and mechanism of Ag-9.8Sn-1.3Bi-0.4Cu alloy powders in different oxidant10.1016/j.corsci.2022.110667 ↗
39. Oxidation kinetics characteristics of Ag-5.08Sn-3.14Sb alloy powders in different oxidizing atmosphere10.1016/j.corsci.2022.110167 ↗
40. Initial corrosion observed on the atomic scale10.1038/nature04465 ↗
41. Influence of oxidation on structure, performance, and application of metallic glasses10.1002/adma.202110365 ↗
42. Hauffe · 1965
43. Influence of the corrosion products of copper on its atmospheric corrosion kinetics in tropical climate10.1016/j.corsci.2003.09.014 ↗
44. Aging induced structural and electrochemical corrosion behaviour of Sn-1.0Ag-0.5Cu and Sn-3.8Ag-0.7Cu solder alloys10.1016/j.jallcom.2018.01.292 ↗
45. Corrosion behavior, whisker growth, and electrochemical migration of Sn-3.0Ag-0.5Cu solder doping with In and Zn in NaCl solution, Microelectron
46. Evolution of the microstructure of Sn-Ag-Cu solder joints exposed to ultrasonic waves during solidification10.1016/j.actamat.2010.11.011 ↗
47. Corrosion behavior of Pb-Free Sn-1Ag-0.5Cu-XNi solder alloys in 3.5% NaCl solution10.1007/s11664-012-2452-4 ↗
48. Electrochemical corrosion behavior of Sn-0.7Cu