Revealing fretting corrosion synergistic mechanism of 316 stainless steel in liquid lead-bismuth eutectic (LBE)
Source abstract
Abstract
The synergistic effect of lead-bismuth eutectic (LBE) corrosion and fretting on the damage of a 316 stainless steel was thoroughly investigated. The interaction between the LBE corrosion and fretting plays a key role in materials damage. The dissolution of Ni element leads to a large number of vacancies, lattice defects and built-in internal strain, making the material itself more prone to damage during the wear. Additionally, the shear strain induced by fretting can break the oxide layer formed during friction, leading to the exposure of new materials. This study can provide essential information on damage of heat transfer tubes.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Nuclear Materials and Properties · Fusion materials and technologies · High Temperature Alloys and Creep
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (41)
Show source-provided references
1. Opportunities, barriers and issues with renewable energy development – a discussion10.1016/j.rser.2016.09.137 ↗
2. The role of renewable energy, alternative and nuclear energy in mitigating carbon emissions in the CPTPP countries10.1016/j.renene.2020.07.093 ↗
3. The effect of coupled wear and creep during grid-to-rod fretting10.1016/j.nucengdes.2017.04.018 ↗
4. Developments of analyses on grid-to-rod fretting problems in pressurized water reactors10.1016/j.pnucene.2018.03.015 ↗
5. Effect of the frequency on fretting corrosion behavior between Alloy 690TT tube and 405 stainless steel plate in high temperature pressurized water10.1016/j.triboint.2021.107229 ↗
6. A research on the corrosion and stress corrosion cracking susceptibility of 316L stainless steel exposed to supercritical water10.1016/j.corsci.2017.08.027 ↗
7. The synergistic effect of wear-corrosion in stainless steels: a review
8. Micro abrasion-corrosion of ferritic stainless steels10.1016/j.wear.2017.01.083 ↗
9. Effect of Y2O3 addition on the microstructure and liquid LBE cavitation erosion behaviors of Fe-Cr-Al-Ti-C-xY2O3 laser clade coatings10.1016/j.jnucmat.2022.154030 ↗
10. Corrosion behavior of refractory TiNbZrMoV high-entropy alloy coating in static lead‑bismuth eutectic alloy: A novel design strategy of LBE corrosion-resistant coating10.1016/j.surfcoat.2022.128884 ↗
11. Corrosion behavior of ion-irradiated 12Cr2W2Mn F/M steel in liquid LBE
12. Investigation on fretting wear mechanism of 316 stainless steel induced by Ni dissolution during pre-immersion corrosion in the liquid lead-bismuth eutectic (LBE)10.1016/j.triboint.2022.107772 ↗
13. Understanding the surface oxide evolution of T91 ferritic-martensitic steel in supercritical water through advanced characterization10.1016/j.actamat.2020.05.016 ↗
14. Materials challenges in nuclear energy10.1016/j.actamat.2012.11.004 ↗
15. Structure of surface oxides on martensitic steel under simultaneous ion irradiation and molten LBE corrosion10.1016/j.corsci.2021.109953 ↗
16. Cracking and exfoliation behavior of oxide scale on T91 steel under different tensile stresses in oxygen-controlled lead-bismuth eutectic at 550 °C10.1016/j.corsci.2021.109324 ↗
17. Overview of lead-cooled fast reactor activities10.1016/j.pnucene.2013.11.011 ↗
18. Investigation on fretting wear behavior of 690 alloy in water under various temperatures10.1016/j.triboint.2016.05.012 ↗
19. Effect of environmental condition on the chemical behavior of 690 alloy during fretting wear10.1016/j.triboint.2020.106202 ↗
20. The subsurface damage mechanism of Inconel 690 during fretting wear in pure water10.1016/j.triboint.2017.08.024 ↗
21. Investigation of the fretting corrosion mechanism of QPQ-treated TP316H steel in liquid sodium at 450 °C10.1016/j.corsci.2022.110282 ↗
22. Liquid metal embrittlement of 12Cr ferritic/martensitic steel thin-walled tubes exposed to liquid lead-bismuth eutectic10.1016/j.corsci.2021.110024 ↗
23. Effects of pre-exposure and simulated corrosion “pits” on liquid metal embrittlement of T91 steel exposed to liquid lead-bismuth eutectic at 350 °C10.1016/j.jnucmat.2022.153641 ↗
24. Microstructure response of ferritic/martensitic steel HT9 after neutron irradiation: Effect of temperature10.1016/j.jnucmat.2019.151845 ↗
25. Corrosion behavior of CLAM steel weld bead in flowing Pb-Bi at 550 °C10.1016/j.jnucmat.2018.12.038 ↗
26. Corrosion resistance of 316 stainless steel in a simulated pressurized water reactor improved by laser cladding with chromium10.1016/j.surfcoat.2022.128534 ↗
27. Review of the studies on fundamental issues in LBE corrosion10.1016/j.jnucmat.2007.06.019 ↗
28. A review of steel corrosion by liquid lead and lead–bismuth10.1016/j.corsci.2009.03.013 ↗
29. Corrosion behavior of T91 steel in liquid lead-bismuth eutectic at 550 °C: Effects of exposure time and dissolved oxygen concentration10.1016/j.corsci.2022.110405 ↗
30. Liquid metal embrittlement susceptibility of an oxide-dispersion strengthened FeCrAl alloy in contact with liquid lead-bismuth eutectic at 350 °C10.1016/j.corsci.2022.110603 ↗
31. Twin boundary-accelerated ferritization of austenitic stainless steels in liquid lead–bismuth eutectic10.1016/j.scriptamat.2016.02.029 ↗
32. Environmental degradation of structural materials in liquid lead- and lead-bismuth eutectic-cooled reactors10.1016/j.pmatsci.2022.100920 ↗
33. A review of fretting study on nuclear power equipment10.1016/j.triboint.2019.106095 ↗
34. Interactions between dislocations and three-dimensional annealing twins in face centered cubic metals10.1016/j.commatsci.2019.02.024 ↗
35. An experimental investigation on fretting wear behavior of copper–magnesium alloy
36. Effect of the third body layer formed at different temperature on fretting wear behavior of 316 stainless steel in the composite fretting motion of slip and impact
37. The impact of fretting wear on structural dynamics: Experiment and Simulation10.1016/j.triboint.2019.05.023 ↗
38. Dependence of fretting wear on the microstructure characteristics and impact on the subsurface stability of a metastable β titanium alloy10.1016/j.triboint.2021.107351 ↗
39. Fretting fatigue crack nucleation: A review10.1016/j.triboint.2018.01.029 ↗
40. Contact mechanics in tribological and contact damage-related problems: A review10.1016/j.triboint.2022.107534 ↗
41. Effect of various phase fractions of bainite, retained austenite, intercritical ferrite and pearlite on the wear behaviour of multiphase steels