In this study, the corrosion behaviors of Yb 2Si 2O 7 ceramic exposed to CFAS melt at 1400 ℃ in a 50%H 2O-50%O 2 environment were investigated and the synergistic effects of water vapour on the thermal corrosion of CFAS melt on Yb 2Si 2O 7 environmental barrier coating material were obtained. Water vapor not only promotes the penetration and corrosion of CFAS by formation of pores and short cracks derived from water vapour corrosion but also significantly changes the corrosion and crystallization reactions of CFAS and the structural evolution of Yb 2Si 2O 7 ceramic, which may be more lethal for Yb 2Si 2O 7 as an environmental barrier coating.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · High-Temperature Coating Behaviors · Nuclear materials and radiation effects
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (30)
Show source-provided references
1. Performance analysis of an aero engine with inter-stage turbine burner10.1017/aer.2017.93 ↗
2. Effect of thermal exposure on the microstructure and creep properties of a fourth-generation Ni-based single crystal superalloy10.1016/j.jmst.2020.07.008 ↗
3. In situ SANS investigation of the kinetics of rafting of γ′ precipitates in a fourth-generation single-crystal nickel-based superalloy10.1016/j.scriptamat.2008.07.031 ↗
4. Advanced structural ceramics in aerospace propulsion10.1038/nmat4687 ↗
5. J. DiCarlo. Advances in SiC/SiC Composites for Aero-Propulsion, NASA Glenn Research Center, Cleveland, 2015.10.1002/9781118832998.ch7 ↗
6. Degradation mechanism of SiCf/SiC composites after long-time water vapor and oxygen corrosion at 1300℃10.1016/j.corsci.2022.110099 ↗
7. A review on environmental barrier coatings: History, current state of the art and future developments10.1016/j.jeurceramsoc.2020.10.057 ↗
8. Fracture mechanisms of ytterbium monosilicate environmental barrier coatings during cyclic thermal exposure10.1016/j.actamat.2015.10.019 ↗
9. Functionally graded chemical vapor deposited mullite environmental barrier coatings for Si-based ceramics10.1016/j.jeurceramsoc.2007.03.007 ↗
10. Upper temperature limit of environmental barrier coatings based on mullite and bass10.1111/j.1151-2916.2003.tb03466.x ↗
11. Oxidation and thermal cycling behavior of c-AlPO4 and SiC whisker co-modified mullite deposited on SiC-C/SiC composites
12. Thermal cycling behavior of La2Zr2O7/Yb2Si2O7/SiC coated PIP Cf/SiC composites under burner rig tests10.1016/j.jeurceramsoc.2021.02.005 ↗
13. Oxidation properties of tri-layer ytterbium-disilicate/mullite/silicon-carbide environment barrier coatings for Cf/SiC composites10.1016/j.surfcoat.2020.126329 ↗
14. Environmental-bar-rier coating ceramics for resistance against attack by molten calcia-magnesia-alu-minosilicate (CMAS) glass: Part I, YAlO3 and γ-Y2Si2O710.1016/j.jeurceramsoc.2018.03.021 ↗
15. Theoretical and experimental determination of the major thermo-mechanical properties of RE2SiO5 (RE = Tb, Dy, Ho, Er, Tm, Yb, Lu, and Y) for environmental and thermal barrier coating applications10.1016/j.jeurceramsoc.2015.09.013 ↗
16. On the Crystal Chemistry of RE2Si2O7: Revisited Structures, Group–Subgroup Relationship, and Insights of Ce3+-Activated Radioluminescence10.1021/acs.chemmater.3c00245 ↗
17. Rare earth silicate environmental barrier coatings for SiC/SiC composites and Si3N4 ceramics10.1016/j.jeurceramsoc.2004.12.013 ↗
18. Role of environment deposits and operating surface temperature in spallation of air plasma sprayed thermal barrier coatings10.1016/S0257-8972(96)02994-5 ↗
19. Composition effects of thermal barrier coating ceramics on their interaction with molten Ca–Mg–Al–silicate (CMAS) glass10.1016/j.actamat.2012.06.053 ↗
20. Mechanisms of cracking and delamination within thick thermal barrier systems in aero-engines subject to calcium-magnesium-alumino-silicate (CMAS) penetration10.1016/j.msea.2008.01.006 ↗
21. Thermal-gradient testing of thermal barrier coatings under simultaneous attack by molten glassy deposits and its mitigation10.1016/j.surfcoat.2010.02.026 ↗
22. Gas/aerosol–ash interaction in volcanic plumes: new insights from surface analyses of fine ash particles10.1016/j.epsl.2007.04.052 ↗
23. The accumulation of molten volcanic ash in jet engines; simulating the role of magma composition, ash particle size and thermal barrier coatings10.1016/j.jvolgeores.2019.106707 ↗
24. High temperature viscosity of calcium-magnesium-aluminosilicate glass from synthetic sand10.1016/j.scriptamat.2016.07.020 ↗
25. Recession of an EB-PVD YSZ coated turbine blade by CaSiO4 and Fe, Ti -Rich CMAS-Type deposits10.1111/j.1551-2916.2011.04747.x ↗
26. Corrosion behavior of Yb4Hf3O12 ceramics exposed to Calcium-Ferrum-Alumina-Silicate (CFAS) coupled with water vapor at 1400 °C10.1016/j.corsci.2022.110954 ↗
27. Thermal corrosion behavior of Yb4Hf3O12 ceramics exposed to calcium-ferrum-alumina-silicate (CFAS) at 140010.1016/j.jeurceramsoc.2023.02.041 ↗
28. Interaction of Yb2Si2O7 environmental barrier coating material with Calcium-Ferrum-Alumina-Silicate (CFAS) at high temperature10.1016/j.ceramint.2021.08.043 ↗
29. Corrosion behavior and mechanism of ytterbium silicates environmental barrier coatings to thermal cycling in water vapor
30. Thermochemical stability and microstructural evolution of Yb2Si2O7 in high-velocity high-temperature water vapor10.1016/j.jeurceramsoc.2020.05.071 ↗