Deposition of corrosion products under pressurised water nuclear reactor conditions: The effect of flow velocity and dissolved hydrogen
Source abstract
Abstract
The effect of water flow velocity and dissolved hydrogen on the deposition rate of Corrosion-Related Unidentified Deposit (CRUD) was investigated under conditions relevant to pressurised water nuclear reactors using type 304 l stainless steel micro-orifices. The results indicate that the CRUD build-up rate increases with hydrogen concentration because the amount of iron in solution also increases. At the same time, the fluid shear forces induce a mechanical removal of the oxide for flow velocities above 15 m/s. This suggests that the CRUD deposition process occurs under mass transport control, but the overall build-up rate is also affected by flow-induced mechanical removal.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Heat Transfer and Boiling Studies · Nuclear Materials and Properties · Nuclear Engineering Thermal-Hydraulics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (40)
Show source-provided references
1. The concept of fouling
2. Yang · 2017
3. The thermal hydraulics of tube support fouling in nuclear steam generators10.13182/NT04-A3566 ↗
4. Fouling of enhanced tubes for condensers used in cooling tower systems: a literature review10.1016/j.applthermaleng.2015.01.014 ↗
5. Fundamentals of corrosion fouling10.1179/000705999101500752 ↗
6. Fouling of heat exchangers in the dairy industry10.1016/S0894-1777(96)00142-2 ↗
7. Fouling of heat exchangers10.1016/S0894-1777(96)00133-1 ↗
8. Elements of particle deposition onto nonporous solid surfaces parallel to suspension flows10.1016/S0894-1777(96)00135-5 ↗
9. Aspects of crystallization fouling10.1016/S0894-1777(96)00137-9 ↗
10. CRUD removal via hydrodynamic cavitation in micro-orifices10.1016/j.nucengdes.2019.01.012 ↗
11. Deposition behaviour of corrosion products on the Zircaloy heat transfer surface10.1016/j.jnucmat.2006.03.017 ↗
12. The effect of high-temperature water chemistry and dissolved zinc on the cobalt incorporation on type 316 stainless steel oxide10.1016/j.corsci.2018.05.041 ↗
13. Investigation of the role of electrokinetic effects in corrosion deposit formation10.1016/j.corsci.2014.06.001 ↗
14. Preliminary laboratory tests of investigation on the blockage phenomena observed on TSP of french SGs
15. Turner · 1994 · 800
16. Burrill · 1977
17. Particle dispersion in a turbulent natural convection channel flow10.1016/j.jaerosci.2011.09.002 ↗
18. Secondary side TSP deposit buildup: lab test investigation focused on electrokinetic considerations
19. Formation of deposits in HT water under high velocity conditions: a parametric study
20. Experimental and numerical study of deposit formation in secondary side SG and TSP by electrokinetic approach
21. Investigation on the Relation between pressure drops and fluid chemical treatment, Chem. 2002
22. Development of a microfluidic setup to study the corrosion product deposition in accelerated flow regions10.1038/s41529-017-0022-1 ↗
23. Investigation into the effect of water chemistry on corrosion product formation in areas of accelerated flow10.1016/j.jnucmat.2017.06.030 ↗
24. Micro-orifice single-phase flow at very high Reynolds number10.1016/j.expthermflusci.2017.10.006 ↗
25. Choked cavitation in micro-orifices: an experimental study10.1016/j.expthermflusci.2015.12.004 ↗
26. Stress corrosion cracking (SCC) of austenitic stainless steels in high temperature light water reactor (LWR) environments
27. Intergranular stress corrosion cracking of unsensitized stainless steels in BWR environments
28. Characterization of the oxide film formed on type 316 stainless steel in 288°C water in cyclic normal and hydrogen water chemistries10.5006/1.3293562 ↗
29. Effect of thickness to diameter ratio on micro-orifice single-phase liquid flow at low Reynolds number10.1016/j.expthermflusci.2018.04.016 ↗
30. The solubility of magnetite and the hydrolysis and oxidation of Fe2+ in water to 300 C10.1007/BF00645517 ↗
31. Solubility of magnetite in high temperature water and an approach to generalized solubility computations
32. Reaction kinetics of primary coolant deposit materials
33. Bohnsack · 1987
34. S. Delaunay, C. Mansour, E.-M. Pavageau, G. Cote, G. Lefèvre, M. Fédoroff, Formation and Deposition of Iron Oxides on Stainless Steel and Carbon Steel in Conditions of Secondary Circuits of Pressurized Water Reactors, (n.d.).
35. Kinetics of reduction of iron oxides by H2: part I: low temperature reduction of hematite10.1016/j.tca.2005.10.004 ↗
36. Solubility study of nickel ferrite in boric acid using a flow-through autoclave system under high temperature and high pressure10.1016/j.net.2016.01.001 ↗
37. Heat transfer and heat transfer fouling in Kraft black liquor evaporators10.1016/S0894-1777(96)00143-4 ↗
38. Egon · 1974
39. J.R. Taylor, An Introduction to Error Analysis, n.d.
40. Micro-orifice single-phase liquid flow: pressure drop measurements and prediction10.1016/j.expthermflusci.2015.03.005 ↗